Bonding Mechanism and Strength of Metals to Ceramics (금속과 세라믹의 접합기구와 접합강도)

  • Kee, Se-Ho;Jung, Jae-Pil;Kim, Won-Joong
    • Journal of Welding and Joining
    • /
    • v.32 no.1
    • /
    • pp.40-46
    • /
    • 2014
  • Bonding technology and bonding mechanism of metal to ceramic including brazing, diffusion bonding, friction welding and etc were reviewed in this study. Various factors should be considered from a bonding design step to acquire a good bonding joint because of a large difference between metal and ceramic in crystal lattice, coefficient of thermal expansion and various properties. In addition, metal and ceramic bonding technologies are constantly being developed according to precise components, multi-function and application to harsh environment. However, improvement of bonding properties and bonding reliability also should be accompanied. Bonding of ceramics, such as $ZrO_2$, $Ti_3AlC_2$ and SiC, to metals like Ti-alloy, TiAl and steel were described in this paper.

Microstructure and Bonding Strength of Tungsten Coating Deposited on Copper by Plasma Spraying

  • Song, Shu-Xiang;Zhou, Zhang-Jian;Du, Juan;Zhong, Zhi-Hong;Ge, Chang-Chun
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.511-512
    • /
    • 2006
  • Tungsten coatings with different interlayers onto the oxygen-free copper substrates were fabricated by atmosphere plasma spraying. The effects of different interlayers of NiCrAl, NiAl and W/Cu on bonding strength were studied. SEM, EDS and XRD were used to investigate the photographs and compositions of these coatings. The tungsten coatings with different initial particle sizes resulted in different microstructures. Oxidation was not detected in the tungsten coating, but in the interlayer, it was found by both XRD and EDS. The tungsten coating deposited directly onto the copper substrate presented higher bonding strength than those with different interlayers.

  • PDF

BONDING BETWEEN RESIN AND CERAMICS (레진과 치과용 도재의 접착)

  • Kim, Sun-Jai;Lee, Keun-Woo;Han, Chong-Hyun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.2
    • /
    • pp.159-168
    • /
    • 2007
  • Statement of problem: Literature showed different results on the durability of bonded ceramic restoration. Purpose: The purpose of this article is to review the effect of surface treatment of ceramics in resin-ceramic bond to get predictable results. Material and method: PubMed data base was utilized to search the articles which were written in English and published in 1986 and 2006. Some electronic published articles which are forthcoming to publish in paper were also included for this review. This review article focused on the effect of acid etching and silane application on the silica based ceramics. The durability of resin-ceramic bonding, the methodology for bond strength test and resin bonding to alumina or zirconia based ceramics were compared in brief at the end of the review. Results and Conclusion: the effect of silane application can be influenced by the contaminations of saliva or solutions. Micromechanical retention by acid etching as well as silane application plays an important role in initial and durable bond strength between resin and ceramic. The use of phosphate modified resin cement following tribochemical silica coating and silane application produced best bond strength for alumina or zirconia based ceramics.

A study on the diffusion bonding of the $Al_2$O$_3$ ceramics to metal (A$_2$O$_3$세라믹과 Ni-Cr-Mo鋼과의 인서트 合金을 이용한 擴散接合에 關한 硏究)

  • 김영식;박훈종;김정일
    • Journal of Welding and Joining
    • /
    • v.10 no.3
    • /
    • pp.63-72
    • /
    • 1992
  • The joining methods of ceramics to metals which can be expected to obtain high temperature strength are mainly classified into the solid-state diffusion bonding method and the active brazing method. Between these two, the solid-state diffusion bonding method is given attentions as substituting method for active brazing method due to being capable of obtaining higher bonding strength at high temperature and accurate bonding. In this paper, the solid-state diffusion bonding of $Al_{2}$O$_{3}$ ceramics to Ni-Cr-Mo alloy steel (SNCM21) using insert metal was carried out. The insert metal employed in this study was experimentally home-made, Ag-Cu-Ti alloy. Influence of several bonding parameters of $Al_{2}$O$_{3}$SNCM21 joint was quantitatively evaluated by bonding strength test, and microstructural analyses at the interlayer were performed by SEM/EDX. From above experiments, the optimum bonding condition of the solid-state diffusion bonding of $Al_{2}$O$_{3}$/SNCM21 using Ag-Cu-Ti insert metal was determined. Futhermore, high temperature strength and thermal-shock properties of $Al_{2}$O$_{3}$/SNCM21 joint were also examined. The results obtained are as follows. 1. The maximum bonding strength was obtained at the temperature of 95% melting point of insert metal. 2. The high temperature strength of $Al_{2}$O$_{3}$/SNCM21 joint appeared to bemaximum value at test temperature 500.deg.C and the bonding strength with increasingtemperature showed parabolic curve. 3. The strength of thermal-shocked specimens was far deteriorated than those of as-bonded specimens. Especially, water-quenched specimen after heated up to 600.deg. C was directly fractured in quenching.

  • PDF

Bonding Strength of Conductive Inner-Electrode Layers in Piezoelectric Multilayer Ceramics

  • Wang, Yiping;Yang, Ying;Zheng, Bingjin;Chen, Jing;Yao, Jinyi;Sheng, Yun
    • Transactions on Electrical and Electronic Materials
    • /
    • v.18 no.4
    • /
    • pp.181-184
    • /
    • 2017
  • Multilayer ceramics in which piezoelectric layers of $0.90Pb(Zr_{0.48}Ti_{0.52})O_3-0.05Pb(Mn_{1/3}Sb_{2/3})O_3-0.05Pb(Zn_{1/3}Nb_{2/3})O_3$ (0.90PZT-0.05PMS-0.05PZN) stack alternately with silver electrode layers were prepared by an advanced low-temperature co-fired ceramic (LTCC) method. The electrical properties and bonding strength of the multilayers were associated with the interface morphologies between the piezoelectric and silver-electrode layers. Usually, the inner silver electrodes are fabricated by sintering silver paste in multi-layer stacks. To improve the interface bonding strength, piezoelectric powders of 0.90PZT-0.05PMS-0.05PZN with an average particle size of $23{\mu}m$ were added to silver paste to form a gradient interface. SEM observation indicated clear interfaces in multilayer ceramics without powder addition. With the increase of piezoelectric powder addition in the silver paste, gradient interfaces were successfully obtained. The multilayer ceramics with gradient interfaces present greater bonding strength as well as excellent piezoelectric properties for 30~40 wt% of added powder. On the other hand, over addition greatly increased the resistance of the inner silver electrodes, leading to a piezoelectric behavior like that of bulk ceramics in multilayers.

Densification and Thermo-Mechanical Properties of Al2O3-ZrO2(Y2O3) Composites

  • Kim, Hee-Seung;Seo, Mi-Young;Kim, Ik-Jin
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.9 s.292
    • /
    • pp.515-518
    • /
    • 2006
  • The microstructure of $ZrO_2$ toughened $Al_2O_3$ ceramics was carefully controlled so as to obtain dense and fine-grained ceramics, thereby improving the properties and reliability of the ceramics for capillary applications in semiconductor bonding technology. $Al_2O_3-ZrO_2(Y_2O_3)$ composite was produced via Ceramic Injection Molding (CIM) technology, followed by Sinter-HIP process. Room temperature strength, hardness, Young's modulus, thermal expansion coefficient and toughness were determined, as well as surface strengthening induced by the fine grained homogenous microstructure and the thermal treatment. The changes in alumina/zirconia grain size, sintering condition and HIP treatment were found to be correlated.

Fabrication of β-SiAlONs by a Reaction-Bonding Process Followed by Post-Sintering

  • Park, Young-Jo;Noh, Eun-Ah;Ko, Jae-Woong;Kim, Hai-Doo
    • Journal of the Korean Ceramic Society
    • /
    • v.46 no.5
    • /
    • pp.452-455
    • /
    • 2009
  • A cost-effective route to synthesize $\beta$-SiAlONs from Si mixtures by reaction bonding followed by post-sintering was investigated. Three different z values, 0.45, 0.92 and 1.87, in $Si_{6-z}Al_zO_zN_{8-z}$ without excess liquid phase were selected to elucidate the mechanism of SiAlON formation and densification. For RBSN (reaction-bonded silicon nitride) specimens prior to post-sintering, nitridation rates of more than 90% were achieved by multistep heating to $1400^{\circ}C$ in flowing 5%$H_2$/95%$N_2$; residual Si was not detected by XRD analysis. An increase in density was acquired with increasing z values in post-sintered specimens, and this tendency was explained by the presence of higher amounts of transient liquid phase at larger z values. Measured z values from the synthesized $\beta$-SiAlONs were similar to the values calculated for the starting compositions. Slight deviations in z values between measurements and calculations were rationalized by a reasonable application of the characteristics of the nitriding and post-sintering processes.

Current Status of Joining Ceramics and Metals (세라믹스의 접합기술)

  • Suganuma, Katsuaki
    • Ceramist
    • /
    • v.9 no.6
    • /
    • pp.30-36
    • /
    • 2006
  • Joining ceramics to metals has a variety of applications both in the structural and the electronics fields. One of the great benefits of the adoption of joining into the structural applications is to provide reliability to the ceramic components by backing up with metal components. In joining ceramics and metals, two key factors, i.e., establishing chemical bonding at interfaces and dissipation of thermal stress across interfaces, should be paid for attention. Many joining methods have been already established such as adhesive and mechanical joining, brazing and soldering, and solid state bonding. Each has its own benefits with some drawbacks. One can select a suitable process and materials following the requirements of the application. This report focuses on the current status of joining technology for ceramics/metal system.

  • PDF

Performance Improvement of Thin Pavement Layer using Epoxy and Ceramics Composite Materials (에폭시와 세라믹스를 결합한 혼합물 이용 박층 포장공법의 성능개선)

  • Kim, Wan-Sang;Kim, Nak-Seok
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.8 no.5
    • /
    • pp.65-70
    • /
    • 2008
  • Asphalt concrete pavements are susceptible to deformation and failure compared to cement concrete pavements. Epoxy is commonly used to enhance the bonding and durability of structures. Based on this concept, an epoxy and ceramics combined mixture was developed and applied to the field to estimate the pavement performance, Laboratory and field performance tests were conducted to observe the applicability of epoxy and ceramics composite materials compared to the conventional one. In this research, the epoxy and ceramics composite mixturewas used in two ways. 7 mm and 15 mm of thin surface layers using the mixture were constructed on cement and asphalt concrete pavements, respectively, after surface treatment. 12 months of field performance surveys were conducted to observe the resistances to the crack and deformation. According to the field performance tests, epoxy and ceramics combined mixture showed better bonding and field performances than the conventional one.

Effect of Surface Condition on the Bonding Characteristics of 3Y-$ZrO_2$-Metal Bracket System (3Y-$ZrO_2$ 세라믹과 교정용 브라켓계에서 세라믹의 표면 조건에 따른 접착 거동의 변화)

  • O, Seon-Mi;Kim, Jin-Seong;Lee, Chae-Hyun
    • Journal of Technologic Dentistry
    • /
    • v.33 no.1
    • /
    • pp.47-54
    • /
    • 2011
  • Purpose: To investigate shear bonding strength between dental zirconia ceramics with different surface treatment and metal bracket. Methods: Zirconia ceramics(LAVA, 3M ESPE, USA) were divided to 4 groups according to their surface treatment; no surface treatment(G1), sand blasting(G2), silane coating(G3), and sand blasting+silane coating(G4). Specimens were bonded to metal bracket using resin bond($Transbond^{TM}XT$, 3M Unitek, USA). Shear bond strength was measured using universal test machine(3366 INSTRON. U.S.A) with cross head speed of 1 mm/min. Microstructural investigation for fracture surface was performed after shear test. Results: Shear bonding strengths of single surface treatment groups (G2 and G3) were higher than no treatment group(G1). Combined Treatment Group (G4) showed the highest shear bond strength of 9.15MPa. Microstructural observation shows that higher shear bonding strength was obtained when debonding was occurred at metal bracket/resin interface rather than zirconia ceramic/resin interface. Conclusion: Surface treatment of zirconia is necessary to obtain higher bonding strength. Combined treatment can be more effective when surface the surfaces are kept clean and homogeneous.