Comparison of Shear Bond Strength of Veneer Ceramics to Co-Cr Alloys Produced by Selective Laser Melting and Casting Technique (선택적 레이저 용융 그리고 전통적인 주조 기술에 의해 제조된 Co-Cr 합금에 대한 전장용 세라믹의 전단 결합 강도 비교)

  • Hong, Min-Ho
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.21 no.12
    • /
    • pp.434-439
    • /
    • 2020
  • Selective laser melting (SLM) manufactures an alloy using laser as a heat source, and has recently been introduced in the dental industry. However, there is a lack of analytical research on metal-ceramic restorations achieved by SLM. This study evaluates and compares the metal-ceramic bond strength of Co-Cr alloys produced by selective laser melting and casting methods. Co-Cr samples required for this study were produced through the sintering process of ceramics, by applying the SLM and CAST methods. The metal-ceramic bond strength was measured by applying the shear bond strength test. In order to determine the area fraction of adherent ceramic, Si content of the specimen was measured using scanning electron microscopy SEM/ EDS. Results of the metal-ceramic bond strength and AFAC were analyzed by t-test (α = 0.05). No significant difference was observed comparing the bond strength of SLM and CAST Co-Cr alloys (P> 0.05). However, the SLM group had much better ceramic adherence than the CAST group (P < 0.001). Moreover, oxidation characteristics were similar for both SLM and CAST Co-Cr alloys, but metal structures were different. These results imply that although the bond of ceramic and Co-Cr alloy is not related to the manufacturing method, SLM alloys impart better ceramic adherence. This indicates that alloys made with SLM can be used to fabricate upper implant prostheses in the future. In particular, it is expected to overcome the shortcomings of the CAST method, and save time and cost.

The Influence of Bonding Strength and Interface Characteristics to Bonding Agent and Veneer Ceramics on Metal-Ceramic Prosthetics (결합재와 베니어세라믹이 금속-세라믹 보철물의 전단결합강도와 계면특성에 미치는 영향)

  • Kim, Min-Jung;Choi, Sung-Min;Chung, In-Sung
    • Journal of Technologic Dentistry
    • /
    • v.33 no.4
    • /
    • pp.349-357
    • /
    • 2011
  • Purpose: In this study, for the reasons of observing the changes when using bonding agent with Ni-Cr alloy and Co-Cr alloy and using VM13 and Vintage MP ceramic which have the disparity in coefficient of thermal expansion, it is carried out to evaluate the characteristics of the bonding agent through the analysis of the interface between metal and ceramic and the analysis of bond strength by variable. Methods: The surface treatment was performed on the two kinds of alloy(Ni-Cr alloy and Co-Cr alloy) specimens, which were sandblasted and were treated with bonder application. The metal-ceramic interfaces were analyzed with EPMA in order to ionic diffusion, and the shear test was performed. Results: As a result of observation of metal-ceramic interfacial properties, it was observed that Cr atoms were spread from the alloy body to the ceramic floor in the specimen of Group B. It was also seen that Cr, W atoms were spread from the alloy body to the ceramic floor in the specimen of Group S. In consequence of observing Shear bond strength, it was calculated that the specimen of BSV was 27.75(${\pm}11.21$)MPa, BSM was 27.02(${\pm}5.23$)MPa, BCV was 30.20(${\pm}5.99$)MPa, BCM was 27.94(${\pm}10.76$)MPa, SSV was 20.83(${\pm}2.58$)MPa, SSM was 23.98(${\pm}3.94$)MPa, SCV was 32.32(${\pm}4.68$)MPa, and SCM was 34.54(${\pm}10.63$)MPa. Conclusion: In the metal-ceramic interface of Bellabond plus sample group, diffusion of Cr atoms was incurred and diffusion of C Cr atoms and W atoms in the sample group of $Starloy{(R)}\;C$ was observed. Using bonding agent showed the higher bond strength than using the sand blasting treatment. In the Bellabond plus alloys, the specimen group with the use of binding materials showed higher shear bond strength, but didn't show statistically significant differences (p>0.05). In the $Starloy{(R)}\;C$ alloys, the specimen group with the use of binding materials showed higher shear bond strength and statistically significant differences(p<0.05). In terms of VM13 ceramic, it was in the Bellabond plus alloys that the high shear bond strength was showed, but there's no statistically significant differences(p>0.05). In terms of Vintage MP ceramic, it was in the $Starloy{(R)}\;C$ alloys that the high shear bond strength was showed and statistically significant differences(p<0.05). Metal-ceramic to fracture of the shear strength measurements and an analysis of all aspects of military usage fracture of the composite, respectively.

A comparative study of the shear bond strength and failure mode between zirconia copings and veneering ceramics (지르코니아 코핑과 전장도재 간의 전단결합강도와 파절양상 비교)

  • Kim, Won-Young;Jeon, Byung-Wook;Chung, In-Sung
    • Journal of Technologic Dentistry
    • /
    • v.37 no.4
    • /
    • pp.243-250
    • /
    • 2015
  • Purpose: The aim of this study was to investigate the shear bond strength between various commercial zirconia coping and veneering ceramic, and to observe the failure mode. Methods: For each zirconia block (iJAM Emerald, LUXEN Smile block, ICE Zirkon transluzent), 10 rectangular specimens were layered with Cercon ceram kiss, IPS e.max ceram, ICE Zirkon ceramic according to recommended by the manufacturer. The shear bond strength tests of the veneering porcelain to zirconia were carried out until fracture by a universal testing machine. After the shear bond tests, failure modes were characterized visually, under a stereomicroscope, such as adhesive, cohesive, or mixed. Data were analyzed with One-way ANOVA followed by Scheffe's tests. Results: The shear bond strength ($mean{\pm}SD$) of zirconia-veneer ceramic were JC group $13.9{\pm}3.6MPa$; JE group $17.7{\pm}2.4MPa$; JI group $15.1{\pm}2.5MPa$; LC group $9.5{\pm}1.5MPa$; LE group $16.2{\pm}2.3MPa$; LI group $12.6{\pm}0.8MPa$; ZC group $16.0{\pm}2.3MPa$; ZE group $18.5{\pm}3.4MPa$; and ZI group $15.3{\pm}3.2MPa$. The One-way ANOVA showed a significant difference between groups (p<0.05). The failure mode in most experimental groups was mixed failure, except for the LC group, which showed adhesive failure, and JE group, LE group and ZE group showed cohesive failure. Conclusion: For IPS e.max ceram, the shear bond strength value was highest for all kinds of zirconia blocks. For ICE Zirkon transluzent, the shear bond strength value was highest for all kinds of veneering ceramics. Most of experimental group interfaces revealed mixed failure mode.

Color changes of ceramic veneers following glazing with respect to their composition

  • Kim, Sung-Joon;Woo, Jae-Man;Jo, Chan Woo;Park, Ju-Hee;Kim, Soo Kyung;Kahm, Se Hoon
    • The Journal of Advanced Prosthodontics
    • /
    • v.11 no.1
    • /
    • pp.16-22
    • /
    • 2019
  • PURPOSE. The purpose of this study was to compare the translucency and color changes of ceramic laminate veneers of different composition following glazing process. MATERIALS AND METHODS. $10mm{\times}10mm$ square specimens of 0.6 mm and 1.0 mm thicknesses were fabricated with IPS e.max Press (EM) and IPS e.max ZirPress (ZP) (n=10 per group). The color coordinates (CIE $L^*$ $a^*$ $b^*$) of the specimens were recorded with a colorimeter before and after glazing. The color changes and translucency parameter (TP) were calculated. For the comparisons with the composition and thicknesses between the 'not glazed' and 'glazed' groups, statistical analyses were done through paired T-test, independent two-sample T-test, and multiple regression analysis using SPSS 18.0 (P<.05). RESULTS. The TP of 0.6 mm EM was higher than that of 0.6 mm ZP. Total color difference (${\Delta}E^*$) between bare and glazed specimens of 1.0 mm EM was greater than that of 1.0 mm ZP with statistical significance. Following glazing, specimens from all groups showed statistically significant amount of decrease in $L^*$ and $a^*$, and statistically significant increase in $b^*$. The result of multiple regression analysis of EM and ZP showed that ${\Delta}L^*$ improved ${\Delta}E^*$. CONCLUSION. Within the limitations of present study, we conclude that translucency and color of ceramic laminate veneers change significantly after glazing process, and the nature and amount of changes vary with different compositions.

Full-mouth rehabilitation with pressed ceramic technique using provisional restorations (Pressed ceramic technique을 이용하여 제작되는 완전 도재관 완전 구강 회복 증례)

  • Roh, Hyun-Sik;Woo, Yi-Hyung;Pae, Ahran
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.51 no.1
    • /
    • pp.47-51
    • /
    • 2013
  • With the introduction of dental implants, restoration of missing teeth with conventional fixed or removable partial dentures is being replaced with implants. Especially, with young patients, not only longevity but also esthetic factors need to be considered. Implant restorations provide long-term success functionally but, esthetic complications such as, marginal exposure due to gingival recession, loss of the papilla and dark color of metal abutments may occur. Recently, zirconia restorations with CAD/CAM technology provide functional, biocompatible and esthetic restorations possible. All-ceramic restorations using the pressed ceramic technique show better fracture toughness values than those of the conventional porcelain veneering technique. Pressed ceramic technique creates the veneer design in wax and the lost wax technique is used to create the restoration. The final contour of the restoration may be controlled during wax-up. A 22-year old female patient was restored with dental implants and zirconia restorations using the pressed ceramic technique presenting short-term but optimistic prognosis.

Considerations in Porcelain Fused Metal Restorations (Porcelain 제작시 고려 사항)

  • Kim, Jin-Wan
    • Journal of the Korean Academy of Esthetic Dentistry
    • /
    • v.8 no.1
    • /
    • pp.90-95
    • /
    • 1999
  • Although various kinds of porcelain restorations, including full porcelain jacked crowns and laminate crowns, are used for Esthetic Dentistry nowadays, the most widely used one so far is porcelain metal restoration. It goes without saying that shade matching in porcelain-metal restoration is much more difficult than in full ceramic veneer restoration because of the metal substructure limitation of the porcelain to metal restoration and then let it go even when shade matching is a little bit unsatisfactory. I think a more satisfactory shade matching can be achieved by developing more elaborate techniques, by selecting proper metal and porcelain and by enabling more detailed communication between the dentists and the dental technicians. Some considerations will be made in an attempt to achieve more successful outputs.

  • PDF

An esthetic appliance for the management of crown-root fracture: a case report

  • Jeon, Sang-Min;Lee, Kang-Hee;Jung, Bock-Young
    • Restorative Dentistry and Endodontics
    • /
    • v.39 no.3
    • /
    • pp.226-229
    • /
    • 2014
  • Orthodontic extrusion is usually performed by means of a fixed orthodontic appliance that utilizes arch wire attached to adjacent teeth and transfers the desired force by elastic from the wire to the root. However, clinicians often encounter cases where the bonding required for tooth traction is not possible because the adjacent teeth have been restored with ceramic or veneer. The purpose of this case report is to describe a modified orthodontic extrusion appliance that is useful when conventional orthodontic treatment is not possible. The modified appliance was fabricated using an artificial tooth, clear plastic sheeting, and a braided fiber-reinforced composite strip that covered adjacent teeth without bonding. It satisfied the esthetic and functional needs of the patient and established the optimal biologic width.

Combined periodontal regenerative and prosthetic treatment of pathologic migration of anterior teeth

  • Lee, Ju-Youn
    • Journal of Periodontal and Implant Science
    • /
    • v.38 no.sup2
    • /
    • pp.405-412
    • /
    • 2008
  • Purpose: Pathologic tooth migration (PTM) commonly occurs in the anterior region and is associated with periodontal disease. The treatment of PTM of anterior teeth can be complex and time consuming, and a multidisciplinary approach is often required. Materials and Methods: The patient was a 38-year-old woman with a chief complaint of saving and realigning her elongated maxillary left central incisor. This paper describes the successful combined periodontal regenerative (guided tissue regeneration) and prosthetic treatment and a 2-year follow-up of maxillary central incisor with pathologic tooth migration, deep intrabony defect, and poor prognosis. Results: The right maxillary central incisor was restored by laminate veneer and the left by all-ceramic crown. The patient had no pain and discomfort and was satisfied with the outcomes of her treatment for 2 years. She has maintained her recall program at the Department of Periodontology at 3 months interval. Conclusion: The key step in the successful treatment of PTM in anterior region is to obtain a high level of cooperation from the patient. Maintenance of the treatment result of PTM is dependent on the continuous preservation of periodontal health.

Influences of luting cement shade on the color of various translucent monolithic zirconia and lithium disilicate ceramics for veneer restorations

  • Ghada Alrabeah;Nawaf Alamro;Atif Alghamdi;Ahmed Almslam;Meshari Azaaqi
    • The Journal of Advanced Prosthodontics
    • /
    • v.15 no.5
    • /
    • pp.238-247
    • /
    • 2023
  • PURPOSE. The purpose of this study was to assess the effect of resin cement shade on the color of different novel ultratranslucent monolithic zirconia and lithium disilicate veneer materials. MATERIALS AND METHODS. For a total of 40 specimens, flat cylindrical discs with a 9-mm diameter and 0.5-mm thickness were created using CAD/CAM technology. The specimens were divided into five groups according to their material (n = 8) (e.max, Prettau, Aidite, Shofu and Dima) using A1 shade. Resin discs with the same diameter and shade as the specimens served as tooth-colored substructures. Three shades (neutral, light and warm) of resin cement try-in pastes (Variolink Esthetic LC) were used as the luting cement material. The color of each material group was measured before and after cementation using the three cement shades, and the CIE L*a*b* coordinates were obtained with a spectrophotometer. Values for the translucency parameter (TP) and color change delta E (E) before (baseline) and after cementation of each specimen were determined. To compare differences among the material groups within each shade of cement and among various shades of cement within each material, the data were analyzed using one-way ANOVA and post hoc testing. RESULTS. Color coordinates L*, a* and b* significantly changed after the application of try-in pastes relative to baseline values, with a noticeable decrease in lightness (L*) (P < .05). A significant color change (ΔE) was observed in all tested materials after cementation, with ΔE values exceeding 3.3 (P < .05). Although TP changed after cementation for most materials tested, these changes were not statistically significant (P > .05). Shofu and Dima ceramics showed the lowest TP values, while Aidite and Prettau showed the highest TP values. For e.max, translucency decreased after cementation with neutral and warm shades, and it significantly increased after cementation with a light shade. CONCLUSION. The shade of cement significantly altered the final color of the ceramic veneer material to a level above the threshold at which the clinical perception of color change occurred (> 3.3). The TP was not influenced by the cement shade. The translucency levels of the novel ultratranslucent multilayer monolithic zirconia ceramics Aidite and Prettau were higher than that of the lithium disilicate e.max material.

Comparison of Shear Bonding Strength of Laminate Veneer by Lithium Disilicate Ceramics and Surface Treatment Methods (리튬디실리케이트 세라믹과 표면처리방법에 따른 라미네이트 베니어의 전단결합강도 비교)

  • Park, Sang-Joon;Chung, In-Sung
    • Journal of Technologic Dentistry
    • /
    • v.41 no.3
    • /
    • pp.177-185
    • /
    • 2019
  • Purpose: This study was to investigate the effect of three different surface treatments on the shear bond strength of lithium disilicate ceramics to enamel. Methods: Totally 60 lithium disilicate ceramic disc specimens were fabricated with IPS e.max press (Ivoclar Vivadent, Schaan, Liechtenstein) and Mazic Claro (Vericom, Korea). 30 specimens in each lithium disilicate ceramic were assigned to 3 groups of the each following surface treatment: 1) $50{\mu}m$ airborne particle abrasion+silane, 2) 9.5% hydroflouric acid etching (HF)+silane, 3) $50{\mu}m$ airborne particle abrasion+9.5% HF+silane. Lithium disilicate ceramic surfaces after surface treatments were AFM examined. The shear bond strength was measured in a universal testing machine at 0.5mm/min crosshead speed. All data were analyzed using a two-way ANOVA and Tukey's test(${\alpha}=0.05$). Results: The mean surface roughness of lithium disilicate ceramics ranged from $0.178{\mu}m$ to $0.441{\mu}m$. The mean shear bond strengths ranged from $23.81{\pm}2.78MPa$ to $33.99{\pm}4.85MPa$. Conclusion: 1. Mazic Claro showed higher shear bond strength than IPS e.max press at 3 different surface treatments, and no statistically significant was observed. 2. The shear bond strength of IPS e.max press was strongly enhanced as surface treated with $50{\mu}m$ airborne particle abrasion and 9.5% hydroflouric acid etching. And there was no statistical significance at the shear bond strength of Mazic Claro with surface treatments.