서스펜션 플라즈마 용사법을 이용한 La2Zr2O7/YSZ 2층세라믹 열차폐코팅의 제조와 특성평가 (Fabrication and Characterization of La2Zr2O7/YSZ Double-Ceramic-Layer Thermal Barrier Coatings Fabricated by Suspension Plasma Spray)

  • 권창섭;이수진;이성민;오윤석;김형태;장병국;김성원
    • 한국표면공학회지
    • /
    • 제48권6호
    • /
    • pp.315-321
    • /
    • 2015
  • Rare-earth zirconates, such as $La_2Zr_2O_7$ and $Gd_2Zr_2O_7$, have been investigated as one of the candidates for replacing conventional yttria-stabilized zirconia (YSZ) for thermal barrier coating (TBC) applications at higher turbine inlet temperatures. In this study, double-ceramic-layer (DCL) TBCs of YSZ 1st layer and $La_2Zr_2O_7$ top coat layer are fabricated by suspension plasma spray with serial liquid feeders. Microstructures, hardness profiles, and thermal durability of DCL-TBCs are also characterized. Fabricated DCL-TBCs of YSZ/$La_2Zr_2O_7$ exhibit excellent properties, such as adhesion strength (>25 MPa) and electrical thermal fatigue (~1429 cycles), which are comparable with TBCs fabricated by atmospheric plasma spray.

Variation in adhesion of Streptococcus mutans and Porphyromonas gingivalis in saliva-derived biofilms on raw materials of orthodontic brackets

  • Park, So-Hyun;Kim, Kyungsun;Cho, Soha;Chung, Dong-Hwa;Ahn, Sug-Joon
    • 대한치과교정학회지
    • /
    • 제52권4호
    • /
    • pp.278-286
    • /
    • 2022
  • Objective: To evaluate differences in the adhesion levels of the most common oral pathogens, Streptococcus mutans and Porphyromonas gingivalis, in human saliva-derived microcosm biofilms with respect to time and raw materials of orthodontic brackets. Methods: The samples were classified into three groups of bracket materials: 1) monocrystalline alumina ceramic (CR), 2) stainless steel metal (SS), and 3) polycarbonate plastic (PL), and a hydroxyapatite (HA) group was used to mimic the enamel surface. Saliva was collected from a healthy donor, and saliva-derived biofilms were grown on each sample. A real-time polymerase chain reaction was performed to quantitatively evaluate differences in the attachment levels of total bacteria, S. mutans and P. gingivalis at days 1 and 4. Results: Adhesion of S. mutans and P. gingivalis to CR and HA was higher than the other bracket materials (SS = PL < CR = HA). Total bacteria demonstrated higher adhesion to HA than to bracket materials, but no significant differences in adhesion were observed among the bracket materials (CR = SS = PL < HA). From days 1 to 4, the adhesion of P. gingivalis decreased, while that of S. mutans and total bacteria increased, regardless of material type. Conclusions: The higher adhesion of oral pathogens, such as S. mutans and P. gingivalis to CR suggests that the use of CR brackets possibly facilitates gingival inflammation and enamel decalcification during orthodontic treatment.

저순도 알루미나 예비소결체 선삭시의 세라믹, CBN 및 다이아몬드 공구의 마멸 특성 (Tool-Wear Characteristics of the Ceramic, CBN and Diamond Tools in Turning of the Presintered Low Purity Alumina)

  • 이재우
    • 한국정밀공학회지
    • /
    • 제23권1호
    • /
    • pp.80-88
    • /
    • 2006
  • In this study, unsintered and presintered low purity alumina ceramics were machined with various tools to clarify the machinability and the optimum cutting conditions. The main conclusions obtained were as fellows. Machined with ceramic tool, the ceramics presintered at the temperature range of $1000\~1100^{\circ}C$ showed the best machinability due to the adhesion formed in weared surface within a certain cutting speed range. In the above combination and conditions, the ceramic tool showed the highest productivity through all experiments. The life of CBN tool was longer in machining of the ceramics presintered at $1000^{\circ}C$ than in the case of that presintered at $600^{\circ}C$, but the diamond tool showed adverse tendency. In machining of the ceramics presintered at $1000^{\circ}C$, the ceramic tool exhibits the longest tool life in high speed, the tool lives became extremely worse in the order of CBN tool and diamond tool. However, in the case of the ceramics presintered at $600^{\circ}C$, the diamond tool shows the longest tool life, the tool lives was much worse in the order of CBN tool and ceramic tool.

습식 공정법에 의한 고경도 투명 전도막 제조 (Fabrication of Transparent Conducting Thin Film with High Hardness by Wet Process)

  • 박종국;전대우;이미재;임태영;황종희;김진호
    • 한국전기전자재료학회논문지
    • /
    • 제28권12호
    • /
    • pp.826-830
    • /
    • 2015
  • Transparent Ag nanowire conducting thin films with high surface hardness were fabricated by bar coating method. When coating speed was changed from 35 mm/sec to 50 mm/sec, the transmittance of coated glass increased from 65.3% to 80.8% in visible light range and the surface resistance was changed from $10.1{\Omega}/sq$ to $23.3{\Omega}/sq$. The surface hardness and adhesion of thin film were 5H and 5B.

Ion Beam을 이용한 사파이어($Al_2O_3$) 표면개질 및 금(Au) 박막증착: 접합성 향상 및 접학기구에 대한 연구 (Ion beam induced surface modifications of sapphire and gold film deposition: studies on the adhesion enhancement and mechanisms)

  • 박재원;이광원;이재형;최병호
    • 한국진공학회지
    • /
    • 제8권4B호
    • /
    • pp.514-518
    • /
    • 1999
  • Gold (Au) is not supposed to react with sapphire(single crystalline ) under thermodynamic equillibrium, therefore, a strong adhesion between these two dissimilar materials is not expected. However, pull test showed that the gold film sputter-deposited onto annealed and pre-sputtered sapphire exhibited very strong adhesion even without post-deposition annealing. Strongly and weakly adhered samples as a result of the pull testing were selected to investigate the adhesion mechanisms with Auger electron spectroscopy. The Au/ interfaces were analyzed using a new technique that probes the interface on the film using Auger electron escape depth. It revealed that one or two monolayers of Au-Al-O compound formed at the Au/Sapphire interface when AES in the UHV chamber. It showed that metallic aluminum was detected on the surface of sapphire substrates after irradiating for 3 min. with 7keV Ar+ -ions. These results agree with TRIM calculations that yield preferential ion-beam etching. It is concluded that the formation of Au-Al-O compound, which is responsible for the strong metal-ceramic bonding, is due to ion-induced cleaning and reduction of the sapphire surface, and the kinetic energy of depositing gold atoms, molecules, and micro-particles as a driving force for the inter-facial reaction.