  • Some pretreatment methods have been proposed to enhance the biodegradability and to shorten the hydrolysis reaction time. By means of efficient pretreatment the suspended solids (SS) can be made of better accessible for the anaerobic bacteria. There are several ways how this can be accomplished, which include biological, mechanical, thermal, and chemical methods. For the sludge solubilization using the cavitation phenomenon, we have tried to develop a pretreatment process consisted of a reactor and pumps. The objectives of this study were to develop a advanced wastewater treatment consisted of IABR and the cavitation with PGA. The most effective removal for organic matter and nutrients were occured when both cavitation pretreatment and ${\gamma}$-PGA were applied at the IABR process. Only small portion of ${\gamma}$-PGA at a rate of 1.38mg/L, was enough to improve sedimentation ability, SS removal efficiencies, and sludge volume reduction. After the sludge solubilization by the cavitation, SCOD increased to 193% and SS decreased to 36%. The removal ratio of BOD was 94.5%, T-N removal ratio was 85.5% and T-P removal ratio was 84.9%. The combination process of the IABR with the cavitation and PGA addition seems to be very effective alternative wastewater treatment process.

양극산화 후 실링처리된 알루미늄 합금의 해수 내 내식성과 캐비테이션 침식 저항성 평가 (Evaluation of Corrosion and Cavitation Erosion Resistance of Sealed Aluminum Alloy after Anodizing Treatment in Seawater)

  • 박일초;이정형;한민수;김성종
    • 한국표면공학회지
    • /
    • 제51권2호
    • /
    • pp.87-94
    • /
    • 2018
  • Various sealing techniques were applied to the anodized 5083 aluminum alloy for marine environment to reduce corrosion and cavitation erosion damage. Electrochemical experiments and cavitation erosion tests were conducted to evaluate the corrosion resistance and cavitation resistance of the anodic oxide film treated with sealing in natural seawater solution. Then, damaged surface morphology was analyzed by scanning electron microscope(SEM) and 3D microscope. As the results of the electrochemical experiments, it was observed that the surface damage of all the experimental conditions in the anodic polarization experiment was locally grown by the combination of crack and corrosion damage. In the Tafel analysis, the corrosion resistance of all sealing treatment conditions was improved compared to the anodizing. On the other hand, cavitation erosion tests showed that the anodizing and all the sealing treatment conditions generated local pit damage by cavitation erosion attack and grew to crater damage in the observation of damaged surface by SEM. Also, the weight loss and the surface damage depth measured with the experiment time presented that most of the sealing treatment conditions showed better cavitation erosion resistance than the anodizing, and they had an incubation period at the beginning of the experiment.

선박 프로펠러의 케비테이션 침식 저항 향상을 위한 Ni-P 무전해 도금층 형성 및 열처리를 통한 미세조직 제어 (Electroless Ni-P Plating and Heat Treatments of the Coating Layer for Enhancement of the Cavitation Erosion Resistance of Vessel Propellers)

  • 김영재;손인준;이승훈
    • 한국재료학회지
    • /
    • 제27권8호
    • /
    • pp.409-415
    • /
    • 2017
  • For enhanced cavitation erosion resistance of vessel propellers, an electroless Ni-P plating method was introduced to form a coating layer with high hardness on the surface of Cu alloy (CAC703C) used as vessel propeller material. An electroless Ni-P plating reaction generated by Fe atoms in the Cu alloy occurred, forming a uniform amorphous layer with P content of ~10 wt%. The amorphous layer transformed to (Ni3P+Ni) two phase structure after heat treatment. Cavitation erosion tests following the ASTM G-32 standard were carried out to relate the microstructural changes by heat treatment and the cavitation erosion resistance in distilled water and 3.5 wt% NaCl solutions. It was possible to obtain excellent cavitation erosion resistance through careful microstructural control of the coating layer, demonstrating that this electroless Ni-P plating process is a viable coating process for the enhancement of the cavitation erosion resistance of vessel propellers.

열처리에 따른 무전해 니켈 도금 층의 상변태 거동이 부식과 캐비테이션 침식에 미치는 영향 (Effect of Phase Transformation Behavior of Electroless Nickel Plating Layer on Corrosion and Cavitation-Erosion with Heat Treatment)

  • 박일초;김성종
    • Corrosion Science and Technology
    • /
    • 제23권1호
    • /
    • pp.64-71
    • /
    • 2024
  • The objective of this study was to investigate corrosion and cavitation-erosion characteristics of the electroless nickel plating layer with heat treatment. The crystallization temperature of the electroless nickel plating layer was about 410 ℃. The phase transformation energy was confirmed to be 12.66 J/g. With increasing heat treatment temperature, the amorphous electroless nickel plating layer gradually changed to crystalline Ni and Ni3P. At the same time, the crystal grain size was also increased. Additionally, when heat treatment was performed at a temperature above 400 ℃, NiO phase was observed due to oxidation phenomenon. As a result of the electrochemical polarization experiment, the corrosion resistance of the heat-treated electroless nickel plating layers was superior to that of the as-deposited plating layer. This was because crystal grains became larger and grain boundaries decreased during heat treatment. The cavitation-erosion resistance of heat-treated plating layers tended to be superior to that of as-deposited plating layers due to increased microhardness.

수리동력학적 캐비테이션을 이용한 하수 슬러지의 전처리-I: 전처리 시스템의 최적화 (Sludge Pre-Treatment by Hydrodynamic Cavitation-I: Optimization of Pre-Treatment System)

  • 맹장우;이은영;배재호
    • 대한환경공학회지
    • /
    • 제32권12호
    • /
    • pp.1119-1125
    • /
    • 2010
  • 하수 슬러지의 혐기성 소화성을 향상시키기 위한 다양한 전처리 방법이 제시되어 있지만, 대부분 낮은 경제성 등의 문제로 현장 적용에 제한을 받고 있다. 본 연구는 장치의 구성 및 유지관리가 용이한 수리동력학적 캐비테이션 방법을 이용한 venturi cavitation system (VCS)의 전처리 효율을 향상시키기 위한 최적 설계 및 운전조건을 도출하기 위하여 수행하였다. VCS에서 벤츄리의 직렬 연결 개수는 3개일 때 가장 높은 전처리 효율을 나타내었고, 펌프는 흡입방식이 압송방식에 비하여 단위 에너지 투입량 당 1.6배 높은 전처리 효율을 나타내었다. 캐비테이션이 발생하는 조건에서 벤츄리의 목 직경 조합은 전처리 효율에 영향을 주지 않았다. 또한 3개의 벤츄리가 직렬로 연결된 벤츄리를 병렬로 설치할 경우 에너지 투입량 당 전처리 효율이 30% 향상되었다. 병렬 연결 운전조건으로 슬러지를 처리하였을 때, 에너지 소모량 당 가용화 효율은 5.6 mg ${\Delta}SCOD/g$ TS/kWh로 기존의 수리동력학적 전처리장치보다 우수하였다.

해양환경 하에서 Ni-Cr계 자용성 합금 코팅된 ALBC3 합금의 캐비테이션 특성 평가 (Evaluation of Cavitation Characteristics for ALBC3 Alloy Coated with Ni-Cr Series Self Fluxing Alloy in Marine Environment)

  • 이승준;김성종
    • 해양환경안전학회지
    • /
    • 제19권5호
    • /
    • pp.538-544
    • /
    • 2013
  • 본 연구에서는 ALBC3 합금에 Ni기 자용성 합금으로 내마모성 및 내캐비테이션 특성을 향상시키기 위하여 용사코팅 후 열처리를 실시하여 캐비테이션 특성을 평가하였다. 본 연구 결과, 자용성 합금 코팅층이 높은 경도를 나타내어 내마모성이 우수할 것으로 판단되나, 다공질의 조직으로 인해 열악한 내캐비테이션 특성을 나타냈다. 따라서 열처리 조건의 최적화가 중요하며, 본 조건에서는 열처리 온도를 높여 자용성 합금 내 B와 Si의 유동성을 증가시킴으로써 기공이나 결함을 제거하여 특성개선 효과를 기대할 수 있을 것으로 판단된다.

화염급냉 표면처리된 Cu-9Al-4.5Ni-4.5Fe 합금의 $\beta$' 마르텐사이트 형성에 의한 케비테이션 침식 저항성 향상에 관한 연구 (Improvement of the Resistance to Cavitation Erosion by the Formation of $\beta$' Martensite in Flame-Quenched Cu-9Al-4.5Ni-4.5Fe Alloys)

  • 홍성모;이민구;김광호;김경호;김흥회;홍순익
    • 한국표면공학회지
    • /
    • 제37권4호
    • /
    • pp.234-241
    • /
    • 2004
  • Cavitation erosion properties of the Cu-9Al-4.5Ni-4.5Fe alloys (Al-bronze) surface-modified by flame quenching process have been investigated. After flame quenching at above $T_{\beta}$, the surfaces of Al-bronze with $\alpha$ + $\textsc{k}$ structure have been changed into the $\alpha$ + $\beta$' martensite phases by the eutectoid reaction of $\alpha$ + $\textsc{k}$\longrightarrow$\beta$ followed by the martensite transformation of $\beta$\longrightarrow$\beta$'. As a result of cavitation test, the measured incubation time and erosion rate of the $\alpha$ + $\beta$' alloy was 1.2 times higher and 1.5 times lower, respectively, compared to those of the conventional $\alpha$ + $\textsc{k}$ alloys, showing a remarkable increase of cavitation resistance with the formation of $\beta$' martensite. This is attributed to a preferential erosion of the $\textsc{k}$ precipitates that show the lowest resistance among the $\alpha$, $\textsc{k}$, $\beta$' phases under cavitation loading.ases under cavitation loading.

A Preconditioning Method for Two-Phase Flows with Cavitation

  • Shin B.R.;Yamamoto S.
    • 한국전산유체공학회:학술대회논문집
    • /
    • 한국전산유체공학회 2003년도 The Fifth Asian Computational Fluid Dynamics Conference
    • /
    • pp.181-182
    • /
    • 2003
  • A preconditioned numerical method for gas-liquid to-phase flow is applied to solve cavitating flow. The present method employs a density based finite-difference method of dual time-stepping integration procedure and Roe's flux difference splitting approximation with MUSCL-TVD scheme. A homogeneous equilibrium cavitation model is used. The method permits simple treatment of the whole gas-liquid two-phase flow field including wave propagation, large density changes and incompressible flow characteristics at low Mach number. By this method, two-dimensional internal flows through a venturi tuve and decelerating cascades are computed and discussed.

  • PDF