PRODUCTION AND MACHINABILITY OF SiCp-REINFORCED AL-2014 ALLOY MATRIX COMPOSITES

  • Ciftci, I.;Sahin, Y.
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2002년도 proceedings of the second asia international conference on tribology
    • /
    • pp.313-314
    • /
    • 2002
  • SiCp-reinforced metal matrix composites (MMCs) containing 8 wt % and 16 wt % of $SiC_p-reinforced$ with 30 and $45\;{\mu}m$ in sizes were prepared by a melt stirring-squeeze casting technique. Microstructural observation showed that particle distributions were reasonably well. Turning experiments were carried out on the composites using uncoated and triple-layer coated carbide tools at various cutting speeds under a constant feed rate and depth of cut. Coated tools indicated better performance than uncoated tools for all the materials while the poor surface finish was obtained for coated tools.

  • PDF

Aluminium Based Brazing Fillers for High Temperature Electronic Packaging Applications

  • Sharma, Ashutosh;Jung, Jae-Pil
    • 마이크로전자및패키징학회지
    • /
    • 제22권4호
    • /
    • pp.1-5
    • /
    • 2015
  • In high temperature aircraft electronics, aluminium based brazing filler is the prime choice today. Aluminium and its alloys have compatible properties like weight minimization, thermal conductivity, heat dissipation, high temperature precipitation hardening etc. suitable for the aerospace industry. However, the selection of brazing filler for high temperature electronics requires high temperature joint strength properties which is crucial for the aerospace. Thus the selection of proper brazing alloy material, the composition and brazing method play an important role in deciding the final reliability of aircraft electronic components. The composition of these aluminium alloys dependent on the addition of the various elements in the aluminium matrix. The complex shapes of aluminium structures like enclosures, heat dissipaters, chassis for electronic circuitry, in avionics are designed from numerous individual components and joined thereafter. In various aircraft applications, the poor strength caused by the casting and shrinkage defects is undesirable. In this report the effect of various additional elements on Al based alloys and brazing fillers have been discussed.

비대칭 노즐을 이용한 쌍롤 박판주조법으로 제조한 Al-Mg 합금의 Mg 조성에 따른 기계적 특성 평가

  • 김홍규;천부현;김형욱;이재철
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2011년도 춘계학술발표대회
    • /
    • pp.55.2-55.2
    • /
    • 2011
  • 최근 자동차용 강판을 대체하기 위한 재료로서 알루미늄 합금에 대한 관심이 높아지고 있다. 알루미늄 합금은 철강 재료에 비해 비강도가 높으며 재활용이 용이하고 내식성이 뛰어난 활용 가치가 높은 소재이다. 하지만 기존의 강판을 알루미늄 합금으로 대체하기 위해서는 높은 경제성, 강도 및 성형성이 요구되고 있는 현실이다. 따라서 고강도 알루미늄 합금 판재를 경제적으로 제조하기 위한 제조 공정기술 및 후가공 기술의 개발이 필요하다. 본 연구에서는 기존의 쌍롤 박판주조법에 비대칭 노즐을 이용하여 높은 주조 속도를 유지하면서도 중심 편석 및 열간 균열을 완화시켜 첨가되는 용질 원소의 양을 증가시켰다. 제조한 다양한 조성을 가진 알루미늄 합금 판재의 후속 압연성, 기계적 특성 및 성형성을 평가하기 위하여 미세조직 및 집합조직을 분석하였으며 이에 따른 실용화 가능성을 평가하였다.

  • PDF

금속복합재료의 열간압출공정에 있어서 압출비가 섬유의 파단 및 배향에 미치는 영향 (Effect of the Extrusion Ratios on Fiber Breakage and Orientation in Hot Extrusion Process in Metal Matrix Composites)

  • 강충길;강성수;김봉향
    • 대한기계학회논문집
    • /
    • 제17권7호
    • /
    • pp.1740-1750
    • /
    • 1993
  • The aluminar short fiber reinforced composite materials for hot extrusion were fabricated by semi-solid stirring method, and extruded at extrusion temperature $400^{\circ}C$ with various extrusion ratio. The hot extrusion load of volume fraction 15% metal matrix composites and base alloy Al7075 has been compared. The fiber length distribution, fiber breakage and fiber orientation are investiged to know the fiber behaviour in before and after hot extrusion. The tensile strength of the hot extruded billet are experimentally determined for different of extrusion ratios, and compared with theorically calculated strength.

열처리온도 및 시간에 따른 알루미늄 주조재의 고상확산 접합 특성 (Solid State Diffusion Brazing of the Aluminum Alloy Castings According to the Heat Treatment Conditions)

  • 선주현;신승용;홍주화
    • 열처리공학회지
    • /
    • 제21권6호
    • /
    • pp.300-306
    • /
    • 2008
  • Solid state diffusion brazing of aluminum castings (AC4C) and wrought alloys (Al6061) was conducted in order to improve thermal conductivity and temperature uniformity of the aluminum heater which was generally fabricated by casting method. Tensile strength and thermal conductivity are raised with increasing brazing temperature, obtaining 122.5 MPa and $206W/m{\cdot}K$ at $540^{\circ}C$ 5hrs brazing conditions, respectively. The diffusion brazed heater, shows maximum temperature difference of $4^{\circ}C$, exhibits a enhanced temperature uniformity compared with the cast heater having the maximum temperature difference of $11^{\circ}C$.

알루미늄 주조용 SKD61 금형강의 표면처리 방법에 따른 특성 평가 (Characteristic Evaluation According to the Surface Treatment Method of SKD61 Mold Steel for Aluminum Casting)

  • 최세원;김철우;김용호;유효상
    • 열처리공학회지
    • /
    • 제34권6호
    • /
    • pp.281-286
    • /
    • 2021
  • Arc ion plating (AIP), laser cladding, and nitriding are methods that can prevent mold damage or repair and create cracks and breakages on the die surface. The dissolution and soldering behavior of coated SKD61 by using arc ion plating, laser cladding, and nitriding was investigated. The structure of the coating was investigated as a function of deposition conditions by X-ray diffraction and the crystallographic orientation was determined using the texture factor. The TiAlN film deposited with AIP showed excellent corrosion resistance in the molten aluminum alloy at 680℃. In this paper, we have detailed the corrosion and mass loss phenomena associated with these steel-cast metal interactions.

도재용착주조관용 Ni-Cr 합금의 반복주조가 부식거동에 미치는 영향 (The Effect of Recasting on the Corrosion behavior of Ni-Cr alloy for Porcelain Fused to Metal Crown)

  • 배수현;김부섭;정인성
    • 대한치과기공학회지
    • /
    • 제28권2호
    • /
    • pp.355-366
    • /
    • 2006
  • The purpose of this study was to determine if repeated casting has a detrimental effect on the corrosion behavior of nickel-chrome casting alloys. The X-ray diffraction analysis, vickers hardness test, SEM, EDX and corrosion test were performed to determine the effects of recasting on chemical composition, microstructure, physical property, castability and corrosion behavior of nickel-chrome casting alloys. The X-ray diffraction analysis results for the cast and recast specimens of the VeraBond and the Rexillium V showed that major crystal phase contained nickel-chrome compounds, Nickel carbide and Chrome carbide. Microstructure analysis results for the cast and recast specimens of the VeraBond and the Rexillium V showed recasting has no effect on microstructure. EDX analysis results indicated the percentage of the main component nickel(Ni) in the specimens of the VeraBond showed a tendency to increase with recasting, but those of other components Carbon(C) showed a tendency to decrease with recasting, Chrome(Cr), Silicon(Si), Aluminium(Al) and molybdenum(Mo) showed no changes in the percentage. The percentage of the main component nickel(Ni) in the specimens of the Rexillium V showed a tendency to increase with recasting, but those of other components silicon(Si), carbon(C) and molybdenum(Mo) showed a tendency to decrease with recasting, chrome(Cr) and aluminium(Al) showed no changes in the percentage. The vickers hardness results for the cast and recast specimens of the VeraBond and the Rexillium V showed a tendency to decrease with recasting, but the differences for the first to fifth cast were not statistically significant. The castability results for the cast and recast specimens of the VeraBond and the Rexillium V showed a tendency to decrease with recasting, but the differences for the first to fifth cast were not statistically significant. The cast and recast specimens of the VeraBond and the Rexillium V showed no differences in the corrosion resistance. The results indicate that the VeraBond and the Rexillium V can be safely recast.

  • PDF

Al5083-O GMA 용접시 불활성가스 혼합비가 용접부의 인성에 미치는 영향에 관한 연구 (The Influence of Shield Gas Ratio on the Toughness of Al5083-O GMA Welding Zone)

  • 이동길;조상곤;김건호
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제26권6호
    • /
    • pp.653-660
    • /
    • 2002
  • In this study, the toughness was evaluated by using the instrumented Charpy impact testing procedures for A15083-O aluminum alloy used in the LNG carrying and storing tank. The specimens were GMAW welded with four different mixing shield gas ratios (Ar100%+He0%, Ar67%+He33%, Ar50%+He50%, and Ar33%+He67%), and tested at four different temperatures(+25, -30, -85, and $-196^{\circ}C$) in order to investigate the influence of the mixing shield gas ratio and the low temperature. The specimens were divided into base metal, weld metal, fusion line, and HAZ specimen according to the worked notch position. From experiment, the maximum load increased a little up to -$85^{\circ}C$ , and the maximum load and maximum displacement were shown the highest and the lowest at -$196^{\circ}C$ than the other test temperatures. The absorption energy of weld metal notched specimens was not nearly depends on test temperature and mixing shield gas ratio because the casting structure was formed in weld metal zone. In the other hand, the other specimens were shown that the lower temperature, the higher absorption energy slightly up to $-85^{\circ}C$ but the energy was decreased so mush at $-196^{\circ}C$.

용탕단조법에 의해 제조된 Mg-9Al-2Zn합금의 시효거동 및 기계적 성질 (The Aging Behaviors and Mechanical Properties of Mg-9Al-2Zn Alloy Fabricated by Squeeze Casting)

  • 강민철;김인배
    • 한국재료학회지
    • /
    • 제7권6호
    • /
    • pp.453-459
    • /
    • 1997
  • 용탕단조법에 의해 제조된 Mg-9AI-2Zn 합금을 미세조직관찰, 미소경도측정, 인장시험 등을 행하여 시효거동과 기계적 성질을 조사하였다. 용탕에 가압을 한 결과 주조결함이 제거된 미세한 주조조직을 얻었으며 미세조직은 초정 $\alpha$(Mg 고용체), 과포화고용체 $\alpha$상 및 $\beta$(Mg$_{17}$AI$_{12}$)화합물의 3가지 상으로 구성되어 있었다. 16$0^{\circ}C$및 20$0^{\circ}C$에서 시효열처리한 결과 $\beta$석출물에 의한 피크 경도값이 나타났으며 피크경도에서의 석출물의 형태는 lamella 형태의 불연속 석출물이 대부분이었고 과시효에 따라 불연속석출물의 조대화와 함께 연속석출물의 분율이 증가하였다. 용탕단조방법에 의해 제조된 Mg-9AI-2Zn 합금의 인장특성은 인장강도 261.4MPa, 연산율 7.6%로서 상용 AZ 92 합금보다 인장강도 및 연신율에서 우수한 기계적 성질을 가졌는데 이는 Zn의 고용강화 및 용탕의 가압에 의한 효과였다.다.

  • PDF

교반관법으로 제조한 Mg-Al-Zn-X합금의 기계적 특성 (Microstructure and Mechanical Properties of Mg-Al-Zn-X Alloys Fabricated by Rotation-Cylinder Method)

  • 이정일;이주호;김영호;홍태환;이후인;박진태;김준수;박형규
    • 열처리공학회지
    • /
    • 제19권2호
    • /
    • pp.96-102
    • /
    • 2006
  • Development of Rotation-Cylinder Method(RCM) is given for Mg-Al-Zn-X(X=Sr) alloys, identifying some of the key factors that need to be controlled and indicating subsequent casting processes. Effects of Sr addition on the microstructure and mechanical properties of as-cast and T6 heat-treated Mg-Al-Zn-X alloys fabricated by the RCM were investigated. The microstructural and mechanical characterizations were performed by utilizing optical microscope, scanning electron microscope, transmission electron microscope, hardness test and ultimate tensile test. The solution and aging treatment time was varied to optimize the T6 heat treatment conditions, and experimental results were discussed. The grain size of Sr containing alloys was refined by increasing Sr content, but the tensile and yield strengths were increased by addition up to 1wt% Sr.