• 제목/요약/키워드: Cast Stainless Steels

검색결과 37건 처리시간 0.024초

배기다기관용 주강소재의 고온특성 평가 (Characterization of High Temperature Mechanical Properties of Cast Stainless Steels for Exhaust Manifold)

  • 이규동;하태권;정재영
    • 소성∙가공
    • /
    • 제18권3호
    • /
    • pp.217-222
    • /
    • 2009
  • Automobile industries have been focusing their efforts on the development of exhaust manifolds using high temperature stainless steels. Exhaust manifolds fabricated with stainless steels can be categorized into tubular and cast ones. The former is usually manufactured by forming and welding process and the latter by vacuum casting process. In the present study, high temperature mechanical properties of 5 austenitic and 4 ferritic stainless steels were investigated by performing a series of high temperature tensile and low cycle fatigue tests. One of the austenitic stainless steels was vacuum cast and the others sand cast. Fatigue life of ferritic stainless steels was higher than that of austenitic ones.

고내열 페라이트계 스테인레스 주강의 고온인장특성 평가 (High Temperature Tensile Properties of Heat-resistant Cast Ferritic Stainless Steels)

  • 정현경;이동근
    • 열처리공학회지
    • /
    • 제34권1호
    • /
    • pp.10-16
    • /
    • 2021
  • Exhaust manifold is a very important component that is directly connected to air environment pollution and that requires strict mechanical properties such as high temperature fatigue and oxidation. Among stainless steels, the ferritic stainless steel with body-centered cubic structure shows excellent resistance of stress-corrosion cracking, ferromagnetic at room temperature, very excellent cold workability and may not be enhanced by heat treatment. The microstructural characteristics of four cast ferritic stainless steels which are high heat-resistant materials, were analyzed. By comparing and evaluating the mechanical properties at room temperature and high temperature in a range of 400℃~800℃, a database was established to control and predict the required properties and the mechanical properties of the final product. The precipitates of cast ferritic stainless steels were analyzed and the high-temperature deformation characteristics were evaluated by comparative analysis of hardness and tensile characteristics of four steels at room temperature and from 400℃ to 800℃.

Exhaust Manifold 용 오스테나이트계 스테인리스 강의 고온 변형특성 (HIGH TEMPERATURE DEFORMATION BEHAVIOR OF AUSTENITIC STAINLESS STEELS FOR EXHAUST MANIFOLD)

  • 이규동;하태권;정효태
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 추계학술대회 논문집
    • /
    • pp.314-317
    • /
    • 2007
  • Domestic automobile industries have been focusing their effort on development of exhaust manifolds using high temperature stainless steel. Exhaust manifolds fabricated with stainless steels can be categorized into tubular and cast ones. The former is usually manufactured by forming and welding process and the latter by vacuum casting process. In the present study, high temperature mechanical properties of 5 austenitic stainless steels, one was sand cast and the others vacuum cast, were investigated by performing a series of high temperature tensile tests and high temperature low cycle fatigue tests.

  • PDF

CF8M 주조 스테인리스강의 2축 피로수명 예측을 위한 파라미터의 제안 (A Proposal of Parameter to Predict Biaxial Fatigue Life for CF8M Cast Stainless Steels)

  • 박중철;권재도
    • 대한기계학회논문집A
    • /
    • 제29권6호
    • /
    • pp.815-821
    • /
    • 2005
  • Biaxial low cycle fatigue test was carried out to predict fatigue life under combined axial-torsional-loading condition which is that of in-phase and out-of-phase for CF8M cast stainless steels. Fatemi-Socie(FS) parameter which is based on critical plane approach is not only one of methods but also the best method that can predict fatigue life under biaxial loading condition. But the result showed that, biaxial fatigue life prediction by using FS parameter with several different parameters for the CF8M cast stainless steels is not conservative but best results. So in this present research, we proposed new fatigue life prediction parameter considering effective shear stress instead of FS parameter which considers the maximum normal stress acting on maximum shear strain and its effectiveness was verified.

볼 압입시험을 이용한 2상 주조 스테인리스강의 열화 평가 (Aging Evaluation of Duplex Cast Stainless Steel Using Ball Indentation Test)

  • 김진원
    • 대한기계학회논문집A
    • /
    • 제29권9호
    • /
    • pp.1253-1261
    • /
    • 2005
  • Cast stainless steel (CSS) is thermally aged by a long term exposure in the range of nuclear power plant operating temperature. The thermal aging is a cause of concern for the continued safe and reliable operation of CSS nuclear components. Therefore, an assessment of degradation in material properties of these components has been importantly considered. In this study the ball indentation tests were performed on four cast stainless steels aged at $400^{\circ}C$ for 3600 hours, to investigate the applicability of ball indentation test to the assessment of aging degradation of cast stainless steels. Thus, the reliability of ball indentation test for aged CSS was analyzed by evaluating the scattering of data tested from each material and by comparing tensile properties obtained from ball indentation test and standard tensile test. Also, the tensile properties of aged CSS obtained from ball indentation test were compared with those predicted by the evaluation procedure developed on the basis of material database for aged CSS.

Thermal aging effect on fracture toughness of GTAW/SMAW of 316L stainless steel: experiments and applicability of existing CASS models

  • Youn, Gyo-Geun;Kim, Yun-Jae;Miura, Yasufumi
    • Nuclear Engineering and Technology
    • /
    • 제53권4호
    • /
    • pp.1357-1368
    • /
    • 2021
  • This paper presents thermal aging effect on fracture toughness properties of GTAW (gas tungsten arc welding) and SMAW (shielded metal arc welding) of 316L stainless steels, and investigates the applicability of the existing three thermal aging models for CASS (cast stainless steels). Thermal aging was carried out at 350 ℃ for up to 15,000h and at 400 ℃ up to 8,000h. After aging, tensile and fracture toughness tests using 0.5T C(T) specimens were carried out at room temperature and at 288 ℃. Comparing with the predictions using three (ANL, French and H3T) thermal aging models for CASS show that the predictions can be very non-conservative at operating temperature, and thus that the existing thermal aging models for CASS cannot be applied to the welded stainless steels.

UNDERLIGNING THERMOCAPILLARY EFFECTS BY ELECTRON BEAM MELTING OF THIN SPECIMENS

  • Domergue, L.;Camel, D.;Marya, S.
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.199-204
    • /
    • 2002
  • Extensive investigations on cast to cast variations observed in steels have underlined the role of thermocapillary or surface tension driven fluid flow in welding operations. The behavior of weld pool under the electric arc is however affected by possible arc modifications linked to microchemistry variations in materials & this limits to some extent the real contribution from surface tension effects. Thus, electron beam welding with high vacuum was used to investigate thermo-capillary effects on thin austenitic stainless steels & nickel based alloys. The weld pool was monitored by video observations to estimate the importance of fluid flow during the melting & solidification phase. The results underline the importance of fluid flow on [mal solidification.

  • PDF

중성자 흡수소재용 냉간 압연된 Gd-저합금 이상 스테인레스 강의 부식 및 마모성 (Corrosion and Wear Properties of Cold Rolled 0.087% Gd-Lean Duplex Strainless Steels for Neutron Absorbing Material)

  • 백열;최용
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2015년도 춘계학술대회 논문집
    • /
    • pp.123-123
    • /
    • 2015
  • 0.087 wt.% Gd-lean duplex stainless steels were inert arc-melted and cast in a mold. The micro-hardnesses of the rolling, transverse, short transverse directions were 258.5, 292.3, 314.7 HV, respectively. The 33% cold rolled specimen had the crystallographic texture that mainly (100) pole was concentrated to normal direction and (110) pole was concentrated in the center of normal and rolling directions. The corrosion potential and corrosion rate in artificial sea water were in the range of $105.6-221.6mV_{SHE}$, $0.59-1.06mA/cm^2$, respectively. The friction coefficient and wear loss of the 0.087 wt.% Gd-lean duplex stainless steels in artificial sea water were about 67% and 65% lower than in air, whereas, the wear efficiency was 22% higher. The corrosion and wear behaviors of the 0.087 wt.% Gd-lean duplex stainless steels significantly depended on the gadolinium phases.

  • PDF