• 제목/요약/키워드: Cast Alloy 718

검색결과 5건 처리시간 0.028초

Cast alloy 718의 고온압축시 동적/정적재결정에 대한 연구 (Study about dynamic/static recrystallization during hot compression of Cast alloy 718)

  • 김남용;김정한;염종택;박노광;윤종원
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.207-210
    • /
    • 2006
  • Behavior of dynamic/static recrystallization during hot deformation of Cast alloy 718 was investigated. For this purpose, hot compression test and FE-simulation were conducted via Thermecmaster-Z and DEFORM-3D, respectively. The microstructural evolution during hot compression and post heat-treatment was investigated and deformation mechanism were analyzed by stress-strain curve, FE-simulation and microstructure. FE-simulation results show that the temperature difference between top-die and billet has considerable influence on the final shape of compressed specimen. The relation between applied load and processing time was predicted by the FE-simulation.

  • PDF

주조 합금 Alloy 718에서 미세조직과 인장특성에 미치는 열처리의 영향 (Effect of Heat-treatment on Microstructure and Tensile Properties in Cast Alloy 718)

  • 도정현;김인수;최백규;정중은;정인용;조창용
    • 한국주조공학회지
    • /
    • 제36권5호
    • /
    • pp.167-173
    • /
    • 2016
  • The effect of various types of heat-treatment on the mechanical properties of cast Alloy 718 has been investigated. Cast Alloy 718 bars were subjected to 'standard heat-treatment'_(SHT), 'HIP (Hot Isostatic Pressing) heat-treatment'_(HHT), and 'HIP-simulated heat-treatment'_(HS). In the absence of long time high temperature heat-treatment, a small amount of Laves phase remained in the 'SHT' specimen, and needle shaped ${\delta}$ precipitated in the vicinity of the Laves phase. Due to the formation of the Laves and ${\delta}$ phases in the 'SHT' specimen, it exhibited lower tensile properties than those of the others_specimens. On the other hand, the Laves phase was completely dissolved into the matrix after 'HHT' and 'HS' treatments. It is known that isostatic pressure reduces the self-diffusion coefficient, because of the lower self-diffusivity under HIP conditions in the interdendritic region, Nb segregation and the high amount of ${\gamma}^{{\prime}{\prime}}$ precipitation that occurs. Due to the higher fraction of coarse ${\gamma}^{{\prime}{\prime}}$ phases, the 'HHT' treated Alloy 718 showed excellent tensile strength.

A Study on Silicon Nitride Based Ceramic Cutting Tool Materials

  • Park, Dong-Soo
    • Tribology and Lubricants
    • /
    • 제11권5호
    • /
    • pp.78-86
    • /
    • 1995
  • The silicon nitride based ceramic cutting tool materials have been fabricated by gas pressure sintering (GPS) or hot pressing (HP). Their mechanical properties were measured and the effect of the fabrication variables on the properties were examined. Also, effect of adding TiN or TiC particulates on the mechanical properties of the silicon nitride ceramics were investigated. Ceramic cutting tools (ISO 120408) were made of the sintered bodies. Cutting performance test were performed on either conventional or NC lathe. The workpieces were grey cast iron, hardened alloy steel (AISI 4140, HRc>60) and Ni-based superalloy (Inconel 718). The results showed that fabrication variables, namely, sintering temperature and time, exerted a strong influence on the microstincture and mechanical properties of the sintered body, which, however, did not make much difference in wear resistance of the tools. High hardness of the tool containing TiC particulates exhibited good cutting performance. Extensive crater wear was observed on both monolithic and TiN-containing silicon nitride tools after cutting the hardened alloy steel. Inconel 718 was extremely difficult to cut by the current cutting tools.

주조용 718합금의 고온 인장 성질에 미치는 석출물의 영향 (Effect of Precipitates on the High Temperature Tensile Properties of Cast Alloy 718)

  • 주동원;조창용;김두현;류영수;김인수;조해용;최승주
    • 한국재료학회지
    • /
    • 제10권7호
    • /
    • pp.515-521
    • /
    • 2000
  • 주소용 718합금의 고온 인장 성질에 미치는 석축물의 영향을 상추출법과 미세조직관찰을 통해 고찰되었다. 고온 인장시험에서 $760^{\circ}C$까지는 인장강도와 연신율이 동시에 감소하였고, 그보다 높은 온도에서는 인장강도는 급격히 감소하고 연신율은 증가하였다. 고온 인장시험에의한 응력의 영향으로 인하여 ${\gamma}',{\gamma}"$석출물의 양은 $760^{\circ}C$에서 최대의 값을 나타내었다. 미세한 ${\gamma}',{\gamma}"$상의 석출이 최대로 일어나는 온도에서 석출물에의한 유동응력의 증가로 인해 항복강도의 저하폭이 작았으며, 연신율은 가장 낮은값을 나타내었다. $760^{\circ}C$보다 높은 온도에서는 전체적인 석출물의 양도 감소하였고, 특히 강화석출상의 양이 적어 연화현상이 급격히 나타났다. 급격히 나타났다.

  • PDF