• 제목/요약/키워드: CaWO$_4$

검색결과 48건 처리시간 0.025초

CaWO4:Eu3+ 형광체의 합성과 발광 특성 (Synthesis and Photoluminescence Properties of CaWO4:Eu3+ Phosphors)

  • 조신호;조선욱
    • 한국재료학회지
    • /
    • 제22권5호
    • /
    • pp.215-219
    • /
    • 2012
  • Red phosphors $Ca_{1-1.5x}WO_4:{Eu_x}^{3+}$ were synthesized with different concentrations of $Eu^{3+}$ ions by using a solid-state reaction method. The crystal structure of the red phosphors was found to be a tetragonal system. X-ray diffraction (XRD) results showed the (112) main diffraction peak centered at $2{\theta}=28.71^{\circ}$, and the size of crystalline particles exhibited an overall decreasing tendency according to the concentration of $Eu^{3+}$ ions. The excitation spectra of all the phosphors were composed of a broad band centered at 275 nm in the range of 230-310 nm due to $O^{2-}{\rightarrow}W^{6+}$ and a narrow band having a peak at 307 nm caused by $O^{2-}{\rightarrow}Eu^{3+}$. Also, the excitation spectrum presents several strong lines in the range of 305-420 nm, which are assigned to the 4f-4f transitions of the $Eu^{3+}$ ion. In the case of the emission spectrum, all the phosphor powders, irrespective of $Eu^{3+}$ ion concentration, indicated an orange emission peak at 594 nm and a strong red emission spectrum centered at 615 nm, with two weak lines at 648 and 700 nm. The highest red emission intensity occurred at x = 0.10 mol of Eu3+ ion concentration with an asymmetry ratio of 12.5. Especially, the presence of $Eu^{3+}$ in the $Ca_{1-1.5x}WO_4:{Eu_x}^{3+}$ shows very effective use of excitation energy in the range of 305-420 nm, and finally yields a strong emission of red light.

DBPAS를 이용한 CaWO4 결정의 결함특성 (The Defect Characterization of CaWO4 Crystals by Doppler Broadening Positron Annihilation Spectroscopy)

  • 김창규;안창모;송기영;이종용
    • 한국재료학회지
    • /
    • 제12권5호
    • /
    • pp.359-362
    • /
    • 2002
  • DBPAS has been used to characterize atomic level defect structures in materials. In this investigation the numerical analysis of the Doppler spectra was restricted to the determination of the shape parameter, S, defined as the ratio between the total amount of counts in a central portion of the spectrum and the total amount of counts. As samples were exposed by X-ray increasing from 3, 6, and 9 Gy with 6 MV, and 10 MV each and also by E-beam increasing the energies with 6 MeV, 9 MeV, 12 MeV, and 20 MeV. The S-parameter values were increased as increasing the exposed time and the energies. The S-parameters of the large and small size grains in $CaWO_4$ were measured. The S-parameter of the small size grains in $CaWO_4$ was resulted in larger values.

$CaWO_4$$Gd_2O_2S$ : Tb 증감지의 형광체 형태와 사진감도 특성에 관한 연구 (A Study on the Photographic Characteristics Related to the Morphology of Phosphor Layers in the $CaWO_4$ and $Gd_2O_2S$ : Tb Screen)

  • 이인자;허준
    • 대한방사선기술학회지:방사선기술과학
    • /
    • 제16권1호
    • /
    • pp.41-55
    • /
    • 1993
  • Recently, various screen film system have been introduced in diagnostic radiology. There are two kinds of screen film system : blue emitting $CaWO_4$ screen has been largely used in these days. However, it tends to be changed to use green emitting $Gd_2O_2S$ : Tb screen. In this study, photographic characteristics of $CaWO_4$ and $Gd_2O_2S$ : Tb screen were investigated with luminescence, spectroscopy. The morphology of $CaWO_4$ and $Gd_2O_2S$ : Tb were also observed by using scanning electron microscope. The result obtained were as follows : 1. There was small difference in the thickness of phosphor layers for the front and back screen of blue emitting system, but little difference in those of green emitting system. 2. There was no difference in the size of phosphor particles between the front and back screen for each screen. However, the particle size was different for the various kinds of screens. 3. The shape of phosphor particle was round with many faces for all the screens. 4. In the exposure of X-ray with the same intensity, luminescent intensity of a green emitting system was $6{\sim}7$ times larger than that of a blue emitting system. 5. The thickness of phosphor layers does not affect on the sensitivity of the screens exposed by X-ray.

  • PDF

X-ray Sensitivity of Hybrid-type Sensor based on CaWO4-Selenium for Digital X-ray Imager

  • Park, Ji-Koon;Park, Jang-Yong;Kang, Sang-Sik;Lee, Dong-Gil;Kim, Jae-Hyung;Nam, Sang-Hee
    • Transactions on Electrical and Electronic Materials
    • /
    • 제5권4호
    • /
    • pp.133-137
    • /
    • 2004
  • The development of digital x-ray detector has been extensively progressed for the application of various medical modalities. In this study, we introduce a new hybrid-type x-ray detector to improve problems of a conventional direct or indirect digital x-ray image technology, which composed of multi-layer structure using a CaWO$_4$ phosphor and amorphous selenium (a-Se) photoconductor. The leakage current of our detector was found to be ∼180 pA/cm$^2$ at 10 V/m, which was significantly reduced than that of a single a-Se detector. The x-ray sensitivity was measured as the value of 4230 pC/cm$^2$/mR at 10 V/m. We found that the parylene thin film between a CaWO$_4$ phosphor and an a-Se layer acts as an insulator to prevent charge injection from indium thin oxide (ITO) electrode into an a-Se layer under applied bias.

$CaWO_4/a-Se$ 구조의 X선 변환센서에서 a-Se의 Arsenic 첨가량에 따른 반응 특성 (The Response Characteristics of as Addition Ratio of Arsenic in $CaWO_4/a-Se$ based X-ray Conversion Sensor)

  • 강상식;석대우;조성호;김재형;남상희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 추계학술대회 논문집 Vol.15
    • /
    • pp.416-419
    • /
    • 2002
  • There are being two prominent studying for Digital Radiography. Direct and Indirect method of Digital Radiography are announced for producing high quality digital image. The one is using amorphous selenium as photoconductor and the other is using phosphor layer as a light conversion. But each two systems have strength and weakness such as high voltage and blurring effect. In this study, we investigated the electrical characteristic of $multi-layer\left(CaWO_{4}+a-Se \right)$ as a photoconductor according to the changing arsenic composition ratio. This is a basic research for developing of Hybrid digital radiography which is a new type X-ray detector. The arsenic composition ratio of a-Se compound is classified into 7 different kinds which have 0.1%, 0.3%, 0.5%, 1%, 1.5%, 5%, 10% and were made test sample throught thermo-evaporation. The phosphor layer of $CaWO_4$ was overlapped on a-Se using EFIRON optical adhesives. We measured the dark and photo current about the test sample and compared the electrical characteristic of the net charge and signal-to-noise ratio. Among other things, test sample of compound material of 0.3% arsenic showed good characteristic of $2.45nA/cm^2$ dark current and $357.19pC/cm^2/mR$ net charge at $3V/{\mu}m$.

  • PDF

다층구조($CaWO_4/a-Se$) 기반의 X선 검출센서에서 a-Se에 첨가된 As의 특성비 연구 (The Study on Characteristic Composition of As in a-Se with X-ray Detection Sensor using $CaWO_4/a-Se$)

  • 최장용;이동길;신정욱;김재형;남상희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 추계학술대회 논문집 Vol.15
    • /
    • pp.432-435
    • /
    • 2002
  • The ultimate study of this research is to improve the properties of digital X-ray receptor based on amorphous selenium. There are being two prominent studying for Digital Radiography. Direct and Indirect method of Digital Radiography are announced for producing high quality digital image. But each two systems have strength and weakness. This is a basic research for developing of Hybrid digital radiography which is a new type X-ray detector. ln this study, we investigated the electrical characteristic of multi-layer$(CaWO_4+a-Se)$ as a photoconductor according to the changing iodine composition ratio. The iodine composition ratio of a-Se compound is classified into 5 different kinds which have 30ppm, 100ppm, 300ppm, 500ppm, 700ppm and were made test sample throught thermo-evaporation. The phosphor layer of $CaWO_4$ was overlapped on a-Se using EFIRON optical adhesives. We measured the dark and photo current about the test sample and compared the electrical characteristic of the net charge and signal-to-noise ratio. Among other things, test sample of compound material of 700ppm iodine showed good characteristic of $2.53nA/cm^2$ dark current and $479nC/cm^2{\cdot}mR$ net charge at $3V/{\mu}m$.

  • PDF

희토류계(稀土類系) 증감지(增感紙)에 관(關)한 연구(硏究) (Study on the Rare-earth Phosphors Intensifying Screen)

  • 허준;김창균
    • 대한방사선기술학회지:방사선기술과학
    • /
    • 제1권1호
    • /
    • pp.15-24
    • /
    • 1978
  • The characteristics of the rare earth phosphors intensifying screen (LM-6, Grenex-8) as compared with $CaWO_4$ intensifying screen had been studied utilizing several common x-ray films, and found the following results. 1. Compared with the conventional CaWO4 intensifying screen, the rare earth phosphors intensifying screen was found to be more sensitive over to 1.26-3.47 times. So the radiation exposure could be reduced to 1/1.26 -1/3.47. 2. Sharpness as well as the film speed were both increased. So the motion blurring and geometrical unsharpness could be decreased. 3. In spite of that the film speed was increased, photographic contrast was kept up. Therefore, the more ideal film of greater latitude could be obtained. 4. The effects of the rare earth phosphors intensifying screen would be much increased as using with orthochromatic x-ray films.

  • PDF