• 제목/요약/키워드: Butt-fusion welding

검색결과 38건 처리시간 0.022초

Narrow Gap 맞대기 TIG 용접에서 생산성 향상을 위한 연구 (A Study on Productivity Improvement in Narrow Gap TIG Welding)

  • 전재호;김성률;조상명
    • Journal of Welding and Joining
    • /
    • 제34권1호
    • /
    • pp.68-74
    • /
    • 2016
  • Adoption of narrow gap welding shall be increased for the butt joint of thick plate, because the deformation and welding cost is reduced by decrease of cross-sectional area. However, sometimes narrow gap causes defects such as lack of fusion since it has small groove angle and narrow groove width. Therefore, GMAW, GTAW and SAW process shall be adopted to narrow gap welding with small bead hight and low deposition rate. In this study, Super-TIG welding using C-type strip was applied to semi-narrow gap butt joint in order to increase the welding productivity. High deposition rate 10kg/hr was obtained by high current 600A without undercut, humping bead and other welding defects. Measuring the mean and standard deviation of the melting depth to evaluate the developed processes, the fusion line type was determined by measuring the difference between maximum and minium melting depth. Furthermore, a model on arch fusion line and linear fusion line was suggested in order to prevent LF on groove wall in narrow gap butt welding.

굴곡 융착면을 이용한 고밀도폴리에틸렌 관의 버트 융착 공정에서의 열유체 거동 수치모사 (Numerical Simulation of Heat and Flow Behaviors in Butt-fusion Welding Process of HDPE Pipes with Curved Fusion Surface)

  • 유재현;최선웅;안경현;오주석
    • Korean Chemical Engineering Research
    • /
    • 제55권4호
    • /
    • pp.561-566
    • /
    • 2017
  • 폴리머 재질의 관을 융착 시키기 위해서는 버트 융착 공정을 거치는데, 최근 융착면에 굴곡을 주어 융착 강도를 높이고자 하는 시도가 있었다. 본 연구에서는 융착면의 굴곡이 폴리머의 열유체 거동 및 융착 강도에 어떠한 영향을 미칠 것인지 2차원 축대칭 평면에서 유한요소법을 사용하여 살펴보았으며, 고밀도폴리에틸렌 관을 대상으로 하였다. 열유화 단계에서 융착면의 형상을 따라 굴곡진 상경계면이 나타남을 확인할 수 있었다. 접합 단계에서는 굴곡진 상경계면과 융착면 사이에서의 멜트의 압착 흐름이 나타남을 확인할 수 있었으며, 굴곡융착부의 낮은 전단율은 관의 축과 수직 방향 배향을 완화시켜 융착부 강도 향상에 도움을 줄 수 있을 것으로 예상된다.

LASER WELDING OF SINGLE CRYSTAL NICKEL BASE SUPERALLOY CMSX-4

  • Yanagawa, Hiroto;Nakamura, Daisuke;Hirose, Akio;Kobayashi, Kojiro F.
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.193-198
    • /
    • 2002
  • In 1his paper, applicability of laser welding to joining process of single crystal nickel base superalloy turbine blades was investigated. Because heat input of laser welding is more precisely controlled 1han TIG welding, it is possible to optimize solidification microstructure of the welds. Since in single crystal nickel base superalloy the crystal orientation have a significant effect on the strength, it is important to control the solidification microstructure in the fusion zone. A single crystal nickel base supera1loy, CMSX-4, plates were bead-on welded and butt welded using a $CO_2$ laser. The effects of microstructure and crystal orientation on properties of the weld joints were investigated. In bead-on weldling, welding directions were deviated from the base metal [100] direction by 0, 5, 15 and 30 degrees. The welds with deviation angles of 15 and 30 degrees showed fusion zone transverse cracks. As the deviation angles became larger, the fusion zone had more cracking. In the cross section microstructure, the fusion zone grains in 0 and 5 degrees welds grew epitaxially from the base metal spins except for the bead neck regions. The grains in the bead neck regions contained stray crystals. As deviation angles increased, number of the stray crystals increased. In butt welding, the declinations of the crystal orientation of the two base metals varied 0, 5 and 10 degrees. All beads had no cracks. In the 5 degrees bead, the cross section and surface microstructures showed that the fusion zone grains grew epitaxially from the base metal grains. However, the 10 degrees bead, the bead cross section and surface contained the stray crystals in the center of the welds. Orientations of the stray crystals accorded with the heat flow directions in the weld pool. When the welding direction was deviated from the base metal [100] direction, cracks appeared in the area including the stray crystals. The cracks developed along the grain boundaries of the stray crystals with high angles in the final solidification regions at the center of the welds. The fracture surfaces were covered with liquid film. The cracks, therefore, found to be solidification cracks due to the presence of low melting eutectic. As the results, in both bead-on welding and butt welding the deviation angles should be control within 5 degrees for preventing the fusion zone cracks. To investigate the mechanical properties of the weld joints, high temperature tensile tests for bead-on welds with deviation angles of 0 and 5 degrees and the butt welds with dec1ination angles of 0, 5 and 10 degrees were conducted at 1123K. The the tensile strength of all weld joints were more 1han 800MPa that is almost 80% of the tensile strength of the base metal. The strength of the laser weld joints were more than twice that of tue TIG weld joints with a filler metal of Inconel 625. The results reveals 1hat laser welding is more effective joining process for single crystal nickelbase superalloy turbine blades 1han TIG welding.

  • PDF

파이프 융착기의 구조해석 및 설계변경 (Structural Analysis and Design Change of Pipe Butt Welding Machine)

  • 이종선
    • 한국산학기술학회논문지
    • /
    • 제11권11호
    • /
    • pp.4075-4079
    • /
    • 2010
  • 본 논문의 목적은 현재 도기가스, 상하수도 및 화학배관 파이프 등의 플라스틱 배관 공사에서 사용되는 파이프 융착기를 3차원 설계하고 융착 시 발생하는 문제점을 해결하기 위하여 구조해석에 의한 검증작업을 거쳐 구조를 개선한다. 현장에서 파이프 융착 작업 시 융착기 크램프에 크랙이 발생하므로 이를 개선하기 위하여 융착기의 구조를 변경하는 설계치를 제시함으로서 작업의 효율성을 높이고 기술경쟁력을 향상시킨다.

Effects of Defect Size on Crush Test Load of Butt Fusion Welded MDPE Pipes

  • Tun, Nwe Ni;Lai, Huan Sheng;Jeon, Gyu Min;Yoon, Kee Bong;Kil, Seong Hee
    • 에너지공학
    • /
    • 제24권4호
    • /
    • pp.55-62
    • /
    • 2015
  • It is expected that the size of welding defect affects the mechanical performance of welded medium density polyethylene (MDPE) pipe joints. In this study, butt fusion welded MDPE pipe joints with a single spherical or planar defect of various sizes were studied using experimental crush testing and also by finite element method. The crush test showed that the mechanical performance of crush was not affected by the size and geometry of a single welding defect when the defect size was increased to 45% of the pipe's wall thickness. The simulation results indicated that the effect of the single welding defect on the Von Mises stress distribution near the defect explained the reason of the test results.

오스테나이트계 304 스테인리스강의 Nd:YAG 레이저 맞대기 용접특성 (Butt Welding Characteristics of Austenitic 304 Stainless Steel Using a Continuous Wave Nd:YAG Laser Beam)

  • 유영태;오용석;신호준;임기건
    • 대한기계학회논문집A
    • /
    • 제28권2호
    • /
    • pp.165-173
    • /
    • 2004
  • Laser beam welding is increasingly being used in welding of structural steels. The laser welding process is one of the most advanced manufacturing technologies owing to its high speed and deep penetration. The thermal cycles associated with laser welding are generally much faster than those involved in conventional arc welding processes, leading to a rather small weld zone. Experiments are performed for 304 stainless steel plates changing several process parameters such as laser power, welding speed, shielding gas flow rate, presence of surface pollution, with fixed or variable gap and misalignment between the similar and dissimilar plates, etc. The following conclusions can be drawn that laser power and welding speed have a pronounced effect on size and shape of the fusion zone. Increase in welding speed resulted in an increase in weld depth/ aspect ratio and hence a decrease in the fusion zone size. The penetration depth increased with the increase in laser power.

강교량 맞대기용접 결함부의 피로수명 평가 (Fatigue Life Assessment of Steel Bridge Butt Joint Weld with Defects)

  • 백영남;장영권
    • Journal of Welding and Joining
    • /
    • 제18권2호
    • /
    • pp.204-204
    • /
    • 2000
  • There are many weld defects such as surface crack, lack of fusion, and incomplete penetration(IP) in the butt joint weld of the existing steel bridges. The crack-like defects may significantly reduce the life of the structure. This paper presents the procedure and the results of the fatigue life assessment of the butt joints with weld defects in the existing steel girder bridge. The butt joint welds with incomplete penetration were instrumented with strain gages to determine the stress histogram under normal traffic. Based on the measured stress histogram the crack propagation analysis were performed for the fatigue life assessment. By using the suggested procedure and methodology, one can decide the time of periodic inspection and the necessity of repair of the butt joint welds with serious weld defects in the existing steel bridge. (Received October 1, 1999)

강교량 맞대기용접 결함부의 피로수명 평가 (Fatigue Life Assessment of Steel Bridge Butt Joint Weld with Defects)

  • 백영남;장영권
    • Journal of Welding and Joining
    • /
    • 제18권2호
    • /
    • pp.77-85
    • /
    • 2000
  • There are many weld defects such as surface crack, lack of fusion, and incomplete penetration (IP) in the butt joint weld of existing steel bridges. The crack-like defects may significantly reduce the fatigue life of the structure. This paper presents the procedure and the results of the fatigue life assessment of the butt joints with weld defects in the existing steel girder bridge. The butt joint welds with incomplete penetration were instrumented with strain gages to determine the stress histogram under normal traffic. Based on the measured stress histogram the crack propagation analysis were performed for the fatigue life assessment. By using the suggested procedure and methodology, one can decide the time of periodic inspection and the necessity of repair of the butt joint welds with serious weld defects in the existing steel bridge.

  • PDF

PE 이중벽관의 맞대기 융착 용접 강도 향상에 관한 연구 (Studies on the Improvement of Butt Welding Characteristic of Polyethylene Pipes)

  • 안주선;이경원;김재성;이보영
    • Journal of Welding and Joining
    • /
    • 제29권1호
    • /
    • pp.85-89
    • /
    • 2011
  • Waste water is disposed to sewage disposal plant by underground PE double wall pipes. Various processes have been introduced to join PE pipes, but most of these methods have many disadvantages such as costs, lack of reliability and difficulties in joining, etc. Recently butt welding has been paid much attention to joint PE pipes as this process has many advantages such as cost, safety and reliability. In this study, newly developed heat plate, a patent-pending heat plate with a groove, was used to butt-weld PE double wall pipes with different misalignment gaps to simulate real underground conditions, and the butt welding temperature of PE pipe was determined by thermal analysis (Thermal Gravimetric Analysis, Differential Scanning Calorimetry and Dynamic Mechanical Analysis). The resulting joining characteristics of double wall pipes were compared with those from a conventional heat plate, in terms of stiffness, flattening and leakage tests. The results from the stiffness and flattening test showed that there were no big differences between the butt-welded joints made from these two plates. From the leakage test, although PE pipes welded with a conventional heat plate did leak below the required test conditions (10 min. at 0.75kgf/cm2), the pipes welded with a patent-pending grooved heat plate did not show any leakage even at a pressure 1.5 times higher than the required conditions. It was noted that by utilizing a grooved heat plate more complete fusion at the pipe joints could be obtained, which in turn induced a high quality joints.

PE배관의 융착 강도에 관한 연구 (A Study on Fusion Welding Strength of PE pipe)

  • 전흥원;김용수;태순호
    • 한국안전학회지
    • /
    • 제17권2호
    • /
    • pp.16-21
    • /
    • 2002
  • At present the Polyethylene piping, on supporting LNG is widely used because of it's disposition which are anti-corrosion flexible and so on. However, it has a few kinds of risk which are the possibility of piping leak, the character of easily corroded and so on. For giving solution, this study is intended to experiment the intension of the PE pipe after melted and when it is melting, the condition which are temperature and pressure is changed. the melting condition in temperature and pressure is adapted identically. After melting, it's joint is tested as intension. The result is that the effect of temperature in intension is more effective than pressure. In $210^{\circ}C$, $20kg/cm^{2}$ condition, the melting intension has the highest. Compare to the Butt melting joint and the Saddle melting joint, the former was $214kg/cm^{2}$ and the latter was $50kg/cm^{2}(bead\;2{\sim}3mm)$ and $73kg/cm^{2}(bead\;5{\sim}7mm)$. It means that the Butt melting method has more intensive than saddle. Consequently, the result shows that the liability and safety when pipe melting method is used will improve in pipe installation.