• Title/Summary/Keyword: Boiler Tube

Search Result 198, Processing Time 0.026 seconds

A Study on the Characteristics of Pressure Distribution for Heat Exchanger Types of Domestic Gas Boiler (가정용 가스보일러 열교환기 유형에 따른 압력분포특성에 관한 연구)

  • 최경석;오율권;차경옥
    • Journal of the Korean Society of Safety
    • /
    • v.16 no.4
    • /
    • pp.22-28
    • /
    • 2001
  • Heat transfer and pressure distribution for heat exchanger type of domestic gas boiler are different from shape, pitch, thickness of fin and array of pipe respectively. In order to measure the pressure distribution across the heat exchanger, a suction type wind tunnel was constructed and velocity distribution was measured for pilot tube(4 point) of rack type. The experiments were performed for 5 different air flow mass, rpm=3,6,9,12,15 and transverse axis of heat exchanger(x-length) is 5cm respectively. Results showed that above 9.5m/s, pressure distribution dispersion for wet type of heat exchanger is on the increase and above 5.5m/s, pressure distribution dispersion for dry type of heat exchanger is on the increase. Also, pressure distribution dispersion by comparing two different types heat exchanger, dry type of heat exchanger showed a higher augmentation than wet type of heat exchanger.

  • PDF

A Study on the Tube Sinking Process of the Industrial Boiler Tube (산업용 보일러 Tube의 Sinking 공정에 관한 연구)

  • Kwon, I.K.;Kang, K.P.;Lee, W.J.
    • Proceedings of the KSME Conference
    • /
    • 2001.06c
    • /
    • pp.94-99
    • /
    • 2001
  • Theoretical analysis using finite element method are peformed in order to clarify the formation of the flare-shape defect for multi-step tube sinking process. The parameters of concern were the friction between the tube and the die, and geometrical parameters, such as the die inclination angle, the diameters of the die entrance and exit, and the curvature at the corner of the die exit. The effect of the curvature at the comer of the die exit is dominant for determining the flare-shape defect. In order to minimize the flare-shape defect the curvature at the corner of the die exit should be increased up to a certain level(120mm). Using three-step tube sinking die sets which have different curvatures at the comer of the die exit, several numbers of tests were performed and its results are compared with that of theoretical analysis.

  • PDF

A Case Study on the Reduction of Noise and Vibration at the Backpass Heat Surface in the Power Plant Boiler (발전용 보일러 후부 전열면 소음진동 저감에 관한 연구)

  • Lee, Gyong-Soon;Lee, Tae-Gu;Moon, Seung-Jae;Lee, Jae-Heon
    • Plant Journal
    • /
    • v.4 no.3
    • /
    • pp.54-59
    • /
    • 2008
  • The resonance of boiler is caused by exciting force in the gas path and it generates the vibration by the harmony of boiler's dimensional factor. According to trending toward the boiler of increasing capacity and a bigger size, it has a problem of the vibration at back-pass heating surfaces. We can predict such vibrations as comparison between vortex frequency and gas column's natural frequency. We can't rely on the method for the past decades because of changing parameters, such as an allowable error, gas temperature, gas velocity, Strouhal number. We can reduce the vibration to use the seasoning effect and change the operating condition in coal fired boiler but it's not essential solution. When the vibration occurred in the model boiler, we must measures the acoustic pressure and frequency of places for considering the means. So far, we confirmed the problem from field measures and theoretical analysis about the acoustic vibration of boiler. We installed anti-acoustic baffle in a existing boiler to change the acoustic natural frequency at the cavity, which results in reducing the acoustic vibration. The first, we prove that the acoustic resonance is caused by harmonizing vortex shedding frequency of tube heat surface with acoustic natural frequency of cavity in the range of 650~750 MW loads. The second, the acoustic resonance at the back-pass heating surface has the third order of acoustic natural frequency at the second economizer. We install five anti-acoustic baffles at the second economizer to reducing the resonance. We confirm considerably reducing the acoustic vibration of boiler during the commercial boiler.

  • PDF

A Study on the Condensation Performance for the Horizontal Heat Transfer Tubes with Various Fin Attached (형상이 다른 수평 원형 전열관의 응축 성능에 관한 연구)

  • Han, Kyu-Il;Park, Jong-Un
    • Journal of Fisheries and Marine Sciences Education
    • /
    • v.4 no.1
    • /
    • pp.47-61
    • /
    • 1992
  • An experimental study was carried out to investigate the condensation performance for the horizontal cylindrical heat transfer tube with various fin attached using R-11 vapor. The heat transfer tube used in this study was supplied by SUNG HYUNG METAL CO., LTD. Four different types of heat transfer tubes (plain tube, SH-CYR tube, thermocor tube and thermoexcel tube) were used. Each tube was surrounded by circular acrylate tube, and R-11 gas heated by boiler flows into the acrylate tube. Cooling water counter-flows in heat transfer tubes. Heat transfer coefficient of the plain tube from measured data was compared with those of three other tubes. The results are summarized as follows: 1. As the cooling water temperature decreased, the liquid film of R-11 turned to droplet drop on the top surface of the horizontal tube. 2. Heat transfer coefficient calculated theoretically was higher than that obtained from the experimental data. 3. As far as the condensation concerns the thermocor tube is the highest, the SH-CYR tube is the second, and the thermoexcel tube is the third excluding the plain tube.

  • PDF

Comparative Reliability of Nondestructive Testing for Weld: Water Wall Tube in Thermal Power Plant Boiler Case Study (용접부 비파괴 검사의 신뢰성 비교: 화력 발전소의 보일러 수냉벽 배관 사례연구)

  • Choi, Chang Deok;Lim, Ik Sung
    • Journal of Applied Reliability
    • /
    • v.18 no.3
    • /
    • pp.240-249
    • /
    • 2018
  • Purpose: The purpose of this research is to find which technique, between the PAUT (Phased array ultrasonic test) that has been used widely in practice and RT (Radiographic test) that was used widely in the past, has the higher reliability as a non-destructive testing of welding points in water wall tubes. Methods: To evaluated the reliability of non-destructive testing, eleven test pieces that were fabricated intentionally, which have the most frequently occurred defect types in water wall tubes and then both the PAUT and RT were performed on those eleven test pieces to compare their reliability. Results: The differences of type of defect, length are occurred due to the characteristics of nondestructive testing. The RT could not detect the lack of fusion defect type in specimen #4 and #8 while PAUT could not detect the lateral crack and 1 mm size small porosity in specimen #11. Conclusion: It is concluded that applying both the RT and PAUT result the best reliability rather than applying only one test method, if it is possible, in nondestructive testing of weld water wall tube in thermal power plant boiler case.

Development of Portable Boiler Tube Health Evaluation System (휴대용 보일러튜브 건전성 평가시스템 개발)

  • Chang Min Lee;Han Sang Lee;Bum Shin Kim
    • Journal of Korean Society of Industrial and Systems Engineering
    • /
    • v.46 no.3
    • /
    • pp.101-108
    • /
    • 2023
  • Although the proportion of coal-fired power generation is decreasing, efficient operating technology is needed to continuously invest in facilities and reduce maintenance costs until it is abolished. Boilers, one of the main facilities of power plants, operate for a long time in harsh environments of high temperature and high pressure. In addition, damage due to deterioration is likely to occur depending on the fuel and tube material used. It is very important to judge soundness because damage caused by deterioration adversely affects facility operation. Previously, replication method was used to analyze the progress of deterioration. In the replication method, pre-treatment such as chemical treatment is performed on the boiler tube in the field, the area is reproduced by attaching a film, and the replicated film is determined by an expert in the laboratory with an expensive microscope. However, this method involves substantial costs and time requirements, as well as the possibility of human errors. To address these issues, we developed a mobile health assessment system in this research. Since it is detachable and takes images in real time, this system enables swift evaluations across a broad range and facilitates the assessment of preprocessing quality. In addition, it was intended to reduce existing human mistakes by developing a degradation classification algorithm using the merger cluster method.

A Study on the Development of the Continuous 3D Tube Bending Machine (연속 3 차원 튜브 벤딩장치 개발에 관한 연구)

  • Mun, Hyeon-Jun;Kim, Chung-Sup;Kim, Jong-Doo
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.32 no.8
    • /
    • pp.701-706
    • /
    • 2008
  • A continuous 3D tube bending machine has been developed for industrial boiler panel production. The machine consists of a main bender, a sub bender, a side bender, tube feeding rollers and control system that includes data management system. Tube position is controlled by a numerical control system. The bending former can be easily replaced according to the shape of bending form. Reduction of working time and improvement of production capacity from the practice have been achieved by bending a long tube in the machine developed.

Development of Evaluation Technique of High Temperature Creep Characteristics by Small Punch-Creep Test Method (I) - Boiler Superheater Tube - (SP-Creep 시험에 의한 고온 크리프 특성 평가 기술 개발(I) - 보일러 과열기 튜브 -)

  • Baek, Seung-Se;Na, Seong-Hun;Na, Ui-Gyun;Yu, Hyo-Seon
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.25 no.12
    • /
    • pp.1995-2001
    • /
    • 2001
  • In this study, a small punch creep(SP-Creep) test using miniaturized specimen(10${\times}$10${\times}$0.5mm) is described to develop the new creep test method for high temperature structural materials. The SP-Creep test is applied to 2.25Cr-lMo(STBA24) steel which is widely used as boiler tube material. The test temperatures applied for the creep deformation of miniaturized specimens are between 550∼600$^{\circ}C$. The SP-Creep curves depend definitely on applied load and creep temperature, and show the three stages of creep behavior like in conventional uniaxial tensile creep curves. The load exponent of miniaturized specimen decreases with increasing test temperature, and its behavior is similar to stress exponent behavior of uniaxial creep test. The creep activation energy obtained from the relationship between SP-Creep rate and test temperature decreases as the applied load increases. A predicting equation or SP-Creep rate for 2.25Cr-lMo steel is suggested. and a good agreement between experimental and calculated data has been found.

Degradation Degree Evaluation of Heat Resisting Steel by Electrochemical Technique Part 2 : Effect of Testing Conditions on Evaluation Value of Degradation Degree and Changes of Mechaical Properties (전기화학적 방법에 의한 내열강의 열화도측정 제2보 : 열화도측정치에 미치는 측정조건들의 영향과 기계적성질 변화에 대해서)

  • 정희돈;권영각;장래웅
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.17 no.2
    • /
    • pp.300-312
    • /
    • 1993
  • The material deterioration of service-exposed boiler tube steels in fossil power plant was evaluated by using the electrochemical technique namely, modified electrochemical potentiokinetic reactivation(EPR). It was focused that the passivation of Mo$_{6}$C carbide which governs the mechanical properties of Mo alloyed steels did not occur even in the passivity region of steel in sodium molybdate solution and the reactivation peak current (Ip) observed as the result of non-passivation indicating the precipitation of Mo$_{6}$C carbides. To obtain the optimal test conditions for the field test by using the specially designed electrochemical cell, the effects of scan rate, the surface roughness and the pH of electrolyte on Ip value were also investigated. Furthermore, the change of mechanical properties occurred during the long time exposure at high temperature was evlauated quantitatively by small punch(SP) tests and micro hardness test taking account of the metallurgical changes. It is known that reactivation peak current (Ip) has a good relationship with Larson-Miller Parameter(LMP) which represents the information about material deterioration occurred at high temperature environment. In addition it was possible to estimate the ductile-brittle transition temperature (DBTT) by means of the SP test. The Sp test could be, therefore, suggested as a reliable test method for evaluating the material degradation of boiler tube steels. From the good correaltion between the SP DBTT and Ip values shown in this study, it was knows that the change of mechanical properties could be evaluated non-destructively by measurring only Ip values.ues.