Properties of Non Sintered Cement Mortar using Ferro Nickel Slag (페로니켈 슬래그를 사용한 비소성 시멘트 모르타르의 특성)

  • Youn, Min-Sik;Na, Hyeong-Won;Hyung, Won-Gil
    • Journal of the Korea Institute of Building Construction
    • /
    • v.22 no.6
    • /
    • pp.641-649
    • /
    • 2022
  • This study aims to completely develop a non sintered cement mortar using industrial by-products. To replace Portland cement, blast furnace slag, circulating fluidized bed fly ash, and pulverized coal fly ash were used, and natural aggregates were substituted with ferronickel slag. To understand the characteristics of the non sintered cement mortar to which ferronickel slag is applied, an experiment was conducted by classifying the particle size. Fluidity and workability were confirmed through the flow test, and bending and compressive strength tests were conducted at 3, 7, and 28 days of age. In addition, durability was identified through a chloride ion penetration test. Through the study, it is judged that the binder, which completely replaced cement and aggregate, has high potential of being used as a construction material. Notably, it was confirmed to be advantageous for strength and durability.

Fludity and Strength Properties of Concrete by Mixing Ratio of Mixed Slag Aggregates (혼합슬래그 골재 혼합비율에 따른 콘크리트의 유동성 및 강도특성)

  • Lee, Jae-In;Roh, Young-Hwan;Park, Sa-Min;Bae, Sung-Ho;Kim, Ji-Hwan;Choi, Se-Jin
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2021.11a
    • /
    • pp.78-79
    • /
    • 2021
  • In this study, the fluidity and compressive strength properties of concrete according to the mixing ratio of mixed slag aggregates were compared as part of research to alleviate the aggregate supply problem and improve environmental pollution by utilizing industrial by-products.

  • PDF

A Study on the Factors Affecting the High Fluid Mortar Containing Ground Granulated Blast-furnace Slag (고로슬래그 미분말을 함유한 고유동 모르터의 유동성상에 미치는 영향 요인에 관한 연구)

  • 김재훈;윤상천;지남용
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2002.11a
    • /
    • pp.29-36
    • /
    • 2002
  • High fluid concrete unlike OPC concrete is made with various material, and the phase of fresh concrete is considerably different. In order to understand fluidity phase and mix properties of high fluid concrete, concrete is required to access as suspension structure which consists of aggregate and paste. The focus of this paper is to analyze the test results and quantify the effect of mix proportions of molar and fineness modulus of ,and on the properties of fresh mortar. The effect of water-binder ratio, sand-binder ration, content; of ggbs (by mass of total cementitious materials), and various contents of water reducing agent on the yield stress and plastic viscosity of the mix is studied. Based on the experimental results, the following conclusion; can be drawn: (1) The mixing time needed (or high fluid mortar was approximately two times more than that of ordinary portland mortar. (2) The fluidity phase of mortar could be explained by yield stress of mix and the fluidity of mortar. (3) As the content of ggbs increased, yield stress of mortar was decreased and plastic viscosity of it was increased. (4) For the high fluid mortar, it was appeared that sand-binder ratio should be below 1.5.

  • PDF

Flowing and Strength Properties of Low Carbon Inorganic Composite Depending to Fine Aggregate Types and Replacement Ratio (잔골재 종류 및 치환율에 따른 저탄소 무기결합재의 유동 및 강도특성)

  • Park, Jong-Pil;Bae, Sang-Woo;Lee, Yun-Seong;Lee, Kang-Pil;Lee, Sang-Soo;Song, Ha-Young
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2011.11a
    • /
    • pp.235-236
    • /
    • 2011
  • This study analyzed flowing and strength properties of mortar depending to fine aggregate types and replacement ratio by using blast furnace slag, red mud, and silica fume that are industrial by products. The findings showed that higher replacement level of fine aggregate increased air content while decreased table flow. In addition, compressive strength showed that the higher replacement level was regardless of fine aggregate types, the lower strength became. Mortar substituted by the dredged sand showed high strength.

  • PDF

Effect of Fine Particle Cement and Recycled Aggregates as Alkali Activator on the Engineering Properties and Micro-Structure of High Volume Blast Furnace Slag Concrete (알칼리 자극제로서 미분시멘트와 순환골재가 고로슬래그 다량치환 콘크리트의 공학적 특성 및 미세구조에 미치는 영향)

  • Han, Min-Cheol;Lee, Hyang-Jae;Han, Cheon-Goo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.13 no.6
    • /
    • pp.602-608
    • /
    • 2013
  • The aim of this study is to investigate experimentally the effect of the combination of fine particle cement with high Blaine fineness (FC) and recycled aggregates on the engineering properties and micro structure of high volume blast furnace slag (BS) concrete with 75% BS and 21 MPa. FC manufactured by particle classification at the plant with Blaine fineness of more than $7000cm^2/g$ was used as additional alkali activator for high volume blast furnace slag concrete made with recycled fine and coarse aggregates. FC was replaced by 15, 20 and 25% OPC. Test results showed that the incorporation of FC resulted in an increase in the compressive strength compared to BS concrete without FC by as much as 30% due to accelerated hydration and associated latent hydraulic reaction. It was found that the use of FC and recycled aggregates played an important role in activating BS for high volume BS concrete by offering sufficient alkali.

Experimental Study of Manufacturing Artificial Lightweight Aggregates using Industrial Wastes (산업폐기물을 이용한 인공 경량골재 제조에 관한 실험적 연구)

  • Yoon, Seob;Kim, Jung-Bin;Jeong, Yong
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2010.05a
    • /
    • pp.247-248
    • /
    • 2010
  • This study is of manufacturing artificial lightweight aggregates using industrial wastes. The ingredients for manufacturing lightweight aggregate were stone sludge and bottom ash for main materials, and steel slag(SS), glass abrasive sludge(GS) and blast furnace slag(BS) respectively for accessory material. Their precursors were sintered in the range of $1,050{\sim}1,150^{\circ}C$ for 5 min. The sintered results show that the lightweight aggregate with SS had low water absorption ratio and density at $1,150^{\circ}C$. There's a possibility that if GS is used more than the range of this study, GS can be manufactured lightweight aggregate. But it is judged that BS are incongruent to be used for a raw material of lightweight aggregate.

  • PDF

Flexural studies on reinforced geopolymer concrete beams under pure bending

  • Sreenivasulu, C.;Jawahar, J. Guru;Sashidhar, C.
    • Advances in concrete construction
    • /
    • v.8 no.1
    • /
    • pp.33-37
    • /
    • 2019
  • The present investigation is mainly focused on studying the flexural behavior of reinforced geopolymer concrete (RGPC) beams under pure bending. In this study, copper slag (CS) was used as a partial replacement of fine aggregate. Sand and CS were blended in different proportions (100:0, 80:20, 60:40 and 40:60) (sand:CS) by weight. Fly ash and ground granulated blast furnace slag (GGBS) were used as binders and combination of sodium hydroxide (8M) and sodium silicate solution were used for activating the binders. The reinforcement of RGPC beam was designed as per guidelines given in the IS 456-2000 and tested under pure bending (two-point loading) after 28 days of ambient curing. After conducting two point load test the flexural parameters viz., moment carrying capacity, ultimate load, service load, cracking moment, cracking load, crack pattern and ultimate deflection were studied. From the results, it is concluded that RGPC beams have shown better performance up to 60% of CS replacement.

Compressive strength prediction of concrete using ground granulated blast furnace slag by accelerated testing (촉진양생법에 의한 고로슬래그 미분말 혼합 콘크리트의 압축강도 예측)

  • Kim, Yong Jic;Kim, Young Jin;Choi, Yun Wang
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.4
    • /
    • pp.91-98
    • /
    • 2009
  • Recently, production cost of ready mixed concrete has been increased due to the rising cost of raw materials such as cement and aggregate etc. cause by the upturn of oil price and increase of shipping charge. The delivery cost of ready mixed concrete companies, however, has been decreased owing to their excessive competition in sale. Consequently, ready mixed concrete companies began to manufacture the concrete by mixing ground granulated blast furnace slag(GGBF) and fly-ash in order to lower the production cost. Therefore, the objective of this study was to predict 28 days strength of GGBF slag concrete by early strength(warm and hot water curing method) for the sake of managing with ease the quality of ready mixed concrete. In experimental results, the prediction equation for 28 days compressive strength of GGBF slag concrete could be produced through the linear regression analysis of early strength and 28 days strength. In order to acquire the reliability, all mixture were repeated as 3 times and each mixture order was carried out by random sampling. The prediction equation for 28 days strength of GGBF slag concrete by 1 day compressive strength(accelerated testing) according to warm and hot water curing method won the good reliability.

  • PDF

Properties of Environmental Friendly Recycled Polymer Concrete (환경친화형 재생 폴리머 콘크리트의 특성)

  • Sung, Chan-Yong;Kim, Young-Ik;Youn, Joo-No
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2004.05a
    • /
    • pp.328-331
    • /
    • 2004
  • Recently, the study for practical construction application of recycled aggregate concrete is actively being proceeded, on the purpose of technical development for recycling on the construction waste concrete occurred at the time of destruction of building construction by the rapid increase of building wastes and exhaustion of natural aggregates. This study is performed to develop the permeable polymer concrete using recycled coarse aggregate and blast furnace slag for application of structures needed permeability. At 7 days of curing, compressive strength, flexural strength, water permeability and flexural load are in the ragge of $18\~20MPa,\;6\~7MPa,\;4.6\times10^{-2}\~6.9\times10^{-2}cm/s$ and $20\~25kN$, respectively. It is concluded that the recycled aggregate can be used in the permeable polymer concretes.

  • PDF

The Strength and Flowing Properties of PVA Fiber Mortar using the Low-carbon Inorganic Composite according the Replacement Ratio of Fine Aggregate (잔골재 치환율별 저탄소 무기결합재를 사용한 PVA섬유 모르타르의 유동 및 강도특성)

  • Park, Jong-Pil;Moon, Ji-Hwon;Kim, Gyu-Yong;Lee, Sang-Soo;Song, Ha-Young
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2012.05a
    • /
    • pp.89-90
    • /
    • 2012
  • This study analyzed and compared the flowing and strength properties of mortar depending on the different fine aggregate replacement ratios and whether or not the mixing of PVA fiber was applied. blast furnace slag, red mud, and silica fume that are industrial by-products were used for the analysis. The findings showed that higher replacement level of fine aggregate increased air content while decreasing the table flow. In addition, in case of the compressive strength, Plain mortar and PVA fiber with the replacement ratios of 15% and 30%, respectively showed the greatest strength development.

  • PDF