Optical and Structural Properties of Emerging Dilute III-V Bismides

  • Santos, B.H. Bononi Dos;Gobatoa, Y. Galvao;Heninib, M.
    • Applied Science and Convergence Technology
    • /
    • v.23 no.5
    • /
    • pp.211-220
    • /
    • 2014
  • In this paper, we present a review of optical and structural studies of $GaBi_xAs_{1-x}$ epilayers grown by Molecular Beam Epitaxy (MBE) on (311)B and (001) GaAs substrates with different As fluxes. The results indicate that under near-stoichiometric conditions the bismuth incorporation is higher for samples grown on (311)B GaAs substrates than for those grown on (001) GaAs. In addition, carrier localization effects in GaBiAs layers are clearly revealed for both samples by optical measurements. The (311)B samples showed evidence of higher density of defects. It has also been found that the nonradiative centers play a significant role in the recombination process in this material system. The influence of post-growth annealing on the microstructural, optical, and magneto-optical properties was also investigated. An important improvement of optical and spin properties after thermal annealing due to the reduction of defects in the GaBiAs layers was observed.

Experimental fabrication and analysis of thermoelectric devices (복합재료에 의한 열전변환 냉각소자의 개발에 관한 연구)

  • 성만영;송대식;배원일
    • Electrical & Electronic Materials
    • /
    • v.9 no.1
    • /
    • pp.67-75
    • /
    • 1996
  • This paper has presented the characteristics of thermoelectric devices and the plots of thermoelectric cooling and heating as a function of currents for different temperatures. The maximum cooling and heating(.DELTA.T) for (BiSb)$\_$2/Te$\_$3/ and Bi$\_$2/(TeSe)$\_$3/ as a function of currents is about 75.deg. C, A solderable ceramic insulated thermoelectric module. Each module contains 31 thermoelectric devices. Thermoelectric material is a quaternary alloy of bismuth, tellurium, selenium, and antimony with small amounts of suitable dopants, carefully processed to produce an oriented polycrystalline ingot with superior anisotropic thermoelectric properties. Metallized ceramic plates afford maximum electrical insulation and thermal conduction. Operating temperature range is from -156.deg. C to +104.deg. C. The amount of Peltier cooling is directly proportional to the current through the sample, and the temperature gradient at the thermoelectric materials junctions will depend on the system geometry.

  • PDF

Enhanced sticking coefficient in the BSCCO single crystal grown by the sputtering method (스퍼터링 법에 의한 BSCCO 단결정 성장의 부착 계수 향상)

  • Cheon, Min-Woo;Yang, Sung-Ho;Park, Yong-Pil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.585-586
    • /
    • 2005
  • BSCCO thin films were fabricated by an ion beam sputtering method with an ultra-low growth rate, and sticking coefficients of the respective elements are evaluated. The sticking coefficient of Bi element in BSCCO film formation was observed to show a unique temperature dependence; it was almost a constant value of 0.49 below about $730^{\circ}C$ and decreased linearly over about $730^{\circ}C$. In contrast, Sr and Ca, displayed no such remarkable temperature dependence. This behavior of the sticking coefficient was explained consistently on the basis of the evaporation and sublimation processes of Bi2O3. It is considered that the liquid phase of the bismuth oxide plays an important role in the Bi 2212 phase formation in the co-deposition process.

  • PDF

Fabrication of Real 3D Shape Components Using Bi-Sn Alloys (Bi-Sn 합금을 이용한 3차원 미세 구조물의 제작기술 개발)

  • Chung, Sung-Il;Park, Sun-Joon;Im, Yong-Gwan;Choi, Jae-Young;Jeong, Hae-Do
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.28 no.5
    • /
    • pp.624-631
    • /
    • 2004
  • In this paper, new replication techniques fur a metal microcomponent having a real 3D shape were introduced. Helical gear was selected as one of a real 3D microcomponents for this study. The helical gear, which was made of photo-curable resin, was fabricated as a master pattern by microstereolithography technology. Then, a silicone rubber mold was fabricated from the master pattern. Lastly, a final bismuth alloy pattern was transferred from the silicone rubber mold by the microcasting process. In this paper, the replication technique is described in detail from the master pattern to the final pattern with some investigation on factors related to the technique.

Fabrication of barium titanate-bismuth ferrite fibers using electrospinning

  • Baji, Avinash;Abtahi, Mojtaba
    • Advances in nano research
    • /
    • v.1 no.4
    • /
    • pp.183-192
    • /
    • 2013
  • One-dimensional multiferroic nanostructured composites have drawn increasing interest as they show tremendous potential for multifunctional devices and applications. Herein, we report the synthesis, structural and dielectric characterization of barium titanate ($BaTiO_3$)-bismuth ferrite ($BiFeO_3$) composite fibers that were obtained using a novel sol-gel based electrospinning technique. The microstructure of the fibers was investigated using scanning electron microscopy and transmission electron microscopy. The fibers had an average diameter of 120 nm and were composed of nanoparticles. X-ray diffraction (XRD) study of the composite fibers demonstrated that the fibers are composed of perovskite cubic $BaTiO_3$-$BiFeO_3$ crystallites. The magnetic hysteresis loops of the resultant fibers demonstrated that the fibers were ferromagnetic with magnetic coercivity of 1500 Oe and saturation magnetization of 1.55 emu/g at room temperature (300 K). Additionally, the dielectric response of the composite fibers was characterized as a function of frequency. Their dielectric permittivity was found to be 140 and their dielectric loss was low in the frequency range from 1000 Hz to $10^7$ Hz.

The Sublimation Pressure and Standard Enthalpy of Sublimation of Bismuth Triiodide ($BiI_3$에 대한 승화압과 승화 표준 엔탈피)

  • 김준학
    • Journal of the Korean Ceramic Society
    • /
    • v.27 no.7
    • /
    • pp.943-951
    • /
    • 1990
  • Steady-state sublimation vapour pressures of anhydrous bismuth triiodide have been measured by the continuous gravimetric Kundsen-effusion method from 430.0 to 558.9 K and equilibrium sublimation pressures were obtained from the steady-state data. Condensation coefficients and their temperature dependence have been derived from the effusiion measurement. Condensation coefficients ranged from 0.159 to 0.048(475 to 500K), the activation enthalpy and entropy for condensation have been obtained as -93.38kTmol-1 and -212.70JK-1mol-1. The standard sublimation enthalpy changes derived by both second(modified sigma function) and third(average enthalpy method) law methods were 138.261$\pm$0.023, 138.74$\pm$0.002kJmol-1 respectively. The standard sublimation entropy change derived by modified sigma function was 191.98$\pm$0.047 JK-1mol-1. The reliable standard sublimation enthalpy change based on a correlation of ΔgcrHom(298.15K) and ΔgcrSom(298.15K), a recommended p(T) equation has been obtained for BiI3(cr) ; 1g(p/Pa)=-C/(T/K)+5.0711g(T/K)-2.838$\times$10-3(T/K)-7.758$\times$103(K/T)2+1.4519 where p is in Pa, T in Kelvin, ΔgcrHom(298.15K) in kJmol-1 and C=(ΔgcrHom(298.15K)-8.7358)/1.9146$\times$10-2.

  • PDF

A Simple and Quick Chemical Synthesis of Nanostructured Bi2Te3, Sb2Te3, and BixSb2-xTe3

  • Kim, Hee-Jin;Lee, Ki-Jung;Kim, Sung-Jin;Han, Mi-Kyung
    • Bulletin of the Korean Chemical Society
    • /
    • v.31 no.5
    • /
    • pp.1123-1127
    • /
    • 2010
  • We report a simple and quick route for the preparation of high-quality, nearly monodisperse $Bi_2Te_3$, $Sb_2Te_3$, and $Bi_xSb_{2-x}-Te_3$ nanocrystallites. The reactions of bismuth acetate or antimony acetate with Te in oleic acid result in pure phase of $Bi_2Te_3$ or $Sb_2Te_3$ nanoparticles, respectively. Also, ternary $Bi_xSb_{2-x}Te_3$ nanoparticles were successfully synthesized using the same method. The size and morphology of the nanoparticles were controlled by varying the stabilizing agents. The as-prepared nanoparticles are characterized by X-ray diffraction, scanning electron microscope, and high-resolution transmission electron microscope using an energy dispersive spectroscopy.

A Study on Energy Band Change and Stability in Photoelectrolysis by Use of Titanium Oxide Films on Ti-Bi Alloy (Ti-Bi 합금 위에 형성된 산화티타늄 피막의 광 전기분해시 에너지밴드와 안정성에 관한 연구)

  • Park, Seong-Yong;Cho, Byung-Won;Yun, Kyung-Suk
    • Journal of Hydrogen and New Energy
    • /
    • v.5 no.1
    • /
    • pp.41-49
    • /
    • 1994
  • Ti-Bi alloy was prepared by arc melting of appropriate amounts of titanium and bismuth powder. The photocurrent($I_{ph}$) of Ti-Bi oxide electrode was increased with the increase of Bi content, up to 10wt%. The maximum $I_{ph}$ showed $7.6mA/cm^2$ at V=0.5V vs. SCE. The band gap energy of Ti-Bi oxide electrode was observed to 3.0~2.87eV. Surface barrier($V_s$) of Ti-10Bi oxide electrode showed maximum value(1.08V) but didn't exceed 1.23V, then it was impossible to run $H_2$ generation without any other energy sources other than the light. Ti-Bi oxide electrode was found to be quite stable under alkaline solution and showed no signs of photodecomposition.

  • PDF

Catalytic Activity of BiVO4-graphene Nanocomposites for the Reduction of Nitrophenols and the Photocatalytic Degradation of Organic Dyes

  • Li, Jiulong;Ko, Jeong Won;Ko, Weon Bae
    • Elastomers and Composites
    • /
    • v.51 no.3
    • /
    • pp.240-249
    • /
    • 2016
  • $BiVO_4$ nanomaterial was synthesized from bismuth (III) nitrate pentahydrate [$Bi(NO_3)_3{\cdot}5H_2O$] and ammonium vanadate (V) [$NH_4VO_3$]. The $BiVO_4$-graphene nanocomposite was fabricated by calcining the $BiVO_4$ nanomaterial and graphene under an oxygen-free atmosphere at $700^{\circ}C$. X-ray diffraction (XRD) and scanning electron microscopy (SEM) were employed to characterize structural and morphological properties of samples. The catalytic activity of the $BiVO_4$-graphene nanocomposite was studied for the reduction of 4-nitrophenol, 3-nitrophenol and 2-nitrophenol by sodium borohydride [$NaBH_4$]. The photocatalytic activity of the $BiVO_4$-graphene nanocomposite was demonstrated by the degradation of organic dyes like BG, MB, MO and RhB under irradiation at 365 nm. The catalytic and photocatalytic activity were studied by UV-vis spectrophotometry.

Fabrication Process and Power Generation Characteristics of the Micro Thermoelectric Devices Composed of n-type Bi-Te and p-type Sb-Te Nanowires (n형 Bi-Te 나노와이어와 p형 Sb-Te 나노와이어로 구성된 미세열전소자의 형성공정 및 열전발전특성)

  • Kim, Min-Young;Park, Kyung-Won;Oh, Tae-Sung
    • Korean Journal of Metals and Materials
    • /
    • v.47 no.4
    • /
    • pp.248-255
    • /
    • 2009
  • A micro thermoelectric device was processed by electroplating the n-type Bi-Te nanowires and ptype Sb-Te nanowires into an alumina template with 200 nm pores. Power generation characteristics of the micro devices composed of the Bi-Te nanowires, the Sb-Te nanowires, and both the Bi-Te and the Sb-Te nanowires were analyzed with applying a temperature difference of $40^{\circ}C$ across the devices along the thickness direction. The n-type Bi-Te and the p-type Sb-Te nanowire devices exhibited thermoelectric power outputs of $3.8{\times}10^{-10}W$ and $4.8{\times}10^{-10}W$, respectively. The output power of the device composed of both the Bi-Te and the Sb-Te nanowires decreased to $1.4{\times}10^{-10}W$ due to a large electrical resistance of the Cu electrode connecting the Bi-Te nanowire array with the Sb-Te nanowire array.