• Title/Summary/Keyword: Biaxial strain

Search Result 140, Processing Time 0.032 seconds

A Study on the Material Behavior of Glass Fiber Reinforced Thermoplastic Composite in Biaxial Stretch Forming (유리섬유 강화 열가소성 복합재료의 2축 인장성형시 재료거동에 관한 연구)

  • 이중희;류성기
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.17 no.2
    • /
    • pp.169-175
    • /
    • 2000
  • The object of this study was to investigate the feasibility of solid-phase forming of the composites and to characterize the material behavior in the biaxial stretch forming. The materials tested contained 20%, 30%, and 40% glass fibers by weight in a polypropylene matrix. Biaxial stretch forming tests were performed at three forming speeds of 10mm/sec, 1mm/sec, and 0.1mm/sec and at four forming temperatures of $75^{\circ}C, 100^{\circ}C, 125^{\circ}C, and 150^{\circ}C$ to investigate effects of forming speed and forming temperature. The microscopic observation of a formed part was conducted at various strain levels to characterize the material behavior. The strain distribution on a formed part was measured and displayed on the farmed geometry with a contour display The material behavior of the composite in the biaxial stretch forming was strongly influenced by the forming conditions.

  • PDF

Corrections for effects of biaxial stresses in annealed glass

  • Nurhuda, Ilham;Lam, Nelson T.K.;Gad, Emad F.;Calderone, Ignatius
    • Structural Engineering and Mechanics
    • /
    • v.39 no.3
    • /
    • pp.303-316
    • /
    • 2011
  • Experimental tests have shown that glass exhibits very different strengths when tested under biaxial and uniaxial conditions. This paper presents a study on the effects of biaxial stresses on the notional ultimate strength of glass. The study involved applying the theory of elasticity and finite element analysis of the Griffith flaw in the micro scale. The strain intensity at the tip of the critical flaw is used as the main criterion for defining the limit state of fracture in glass. A simple and robust relationship between the maximum principal stress and the uniaxial stress to cause failure of the same glass specimen has been developed. The relationship has been used for evaluating the strength values of both new and old annealed glass panels. The characteristic strength values determined in accordance with the test results based on 5% of exceedance are compared with provisions in the ASTM standard.

Cracking Behavior of RC Panels under Biaxial Tension (이축인장을 받는 철근콘크리트 패널의 균열 거동)

  • 곽효경;김도연
    • Proceedings of the Computational Structural Engineering Institute Conference
    • /
    • 2003.10a
    • /
    • pp.599-606
    • /
    • 2003
  • An analytical model which can simulate the post-cracking nonlinear behavior of reinforced concrete (RC) members such as bars and panels subjected to uniaxial and biaxial tensile stresses is presented. The proposed model includes the description of biaxial failure criteria and the average stress-strain relation of reinforcing steel. Based on strain distribution functions of steel and concrete after cracking, average response of an embedded reinforcement, a criterion to consider the tension-stiffening effect is proposed using the concept of average stresses and strains. The validity of the introduced model is established by comparing the analytical predictions for reinforced concrete tension members with results from experimental studies. Finally, correlation studies between analytical results and experimental data from biaxial tension test are conducted with the objective to establish the validity of the proposed models and identify the significance of various effects on the response of biaxially loaded reinforced concrete panels.

  • PDF

Stress-Strain Response of Polymer-Impregnated Concrete in Uniaxial and Biaxial Compression (일축 및 이축압축을 받는 폴리머침투콘크리트의 응력-변형률 특성)

  • 변근주;이상민;노병철;이용진
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1991.10a
    • /
    • pp.93-98
    • /
    • 1991
  • Polymer-Impregnated Concrete(PIC) can be considered composite material of concrete and polymer and has superior properties compared to conventional cement concrete, such as strength, stiffness, toughness, durability, water-proofing, chemical resistance. However, so far, the usage of PIC has been limited to repairing materials and non-structural applications, due to the lack of the design criteria and the analytical model to determine structural behavior. The objective of this study is to define the stress-strain response and strength characteristics of PIC in uniaxial and various biaxial compressive loading. On the bases of experimental results, general stress-strain relation, biaxial failure envelope and strength evaluation formular of PIC made with normal aggregate and methylmethacrylate(MMA) are proposed.

  • PDF

Time-dependent Analysis of Cracked Reinforced Concrete Sections with Biaxial Bending (2축휨을 고려한 철근콘크리트 균열단면의 장기거동 해석)

  • Yang, Joo Kyoung
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.28 no.2A
    • /
    • pp.243-247
    • /
    • 2008
  • An analytical approach to calculate time-dependent stresses and strains in initially cracked reinforced concrete section with biaxial bending was proposed. The method utilized the aging coefficient approach of Bazant and the linear creep theory. The position of neutral axis and strain and stress distributions of cracked section after creep and shrinkage were determined from the requirements of strain compatibility and equilibrium of a section. With this proposed algorithm, examples were given for rectangular section and a comparative analysis for stress and strain was also made.

Plastic Deformation Characteristic of AZ31 Magnesium Alloy Sheet (AZ31 마그네슘 합금판재의 소성변형특성)

  • Park J. G.;Kuwabara T.;You B. S.;Kim Y. S.
    • Transactions of Materials Processing
    • /
    • v.14 no.6 s.78
    • /
    • pp.520-526
    • /
    • 2005
  • In recent years, there has been a growth of the manufacture and application of magnesium products because of its small specific gravity as well as its relatively high strength. However, there are so many studies to assure good formability because magnesium sheet alloy is difficult to form. In this study, uniaxial tensile and biaxial tensile tests of AZ31 magnesium sheet alloy with thickness of 1.2mm were performed at room temperature. Uniaxial tensile tests were performed until $7{\%}$ of engineering strain. Lankford values and stress-strain curve were obtained. Biaxial tensile tests with cruciform specimen were performed until the breakdown of the specimen occurs. The yield loci were calculated by application of plastic work theory. The results are compared with the theoretical predictions based on the Hill and Logan-Hosford model. In this study, Hill's 1979 yield function for the case of m=2.8 and Logan-Hosford yield function for the case of M=8 give good agreements with experimental results. However, next study will be performed at warm-temperature because the specimens are broken under the $0.5{\%}$ of equivalent strain at biaxial tensile test.

The effect of compressive strain rate on biaxial compressive deformation characteristics of Al circular pipe (AI 원형 관의 2축 압축 변형특성에 미치는 압축속도의 영향)

  • Won, S.T.;Jung, H.J.;Ahn, H.J.;Cho, H.H.;Yoo, C.K.
    • 한국금형공학회:학술대회논문집
    • /
    • 2008.06a
    • /
    • pp.23-26
    • /
    • 2008
  • In order to examine the deformation characteristics of Al circular pipe underthe biaxial compression, the horizontal biaxial compression die for the experiment was manufactured. From this, in the various compressive strain rate (1 mm/min. ${\sim}$ 400 mm/min.)conditions, the circular pipes, which were made by Al materials, were investigated based on the properties change of cross section area, punch load and deformation behavior. The tensile and compressive strains were evaluated from micro Vickers hardness tester. From these results, the punch load and deformation characteristic of Al circular pipes were highly changed in the compressive strain rate about 200 mm/min. The Al circular pipes had the tendency that the punch load decreased with increasing the compressive strain rate. In addition, following as the change of the shape and position of neutral axis due to the deformation proceeding of the circular pipe, the special point of the internal circular pipe at maximum load showed the maximum deformation strain and the maximum measured hardness value. The CAE (computer aided engineering) simulation using Deform-2D program was performed on the circular pipe in order to know and verify the exact compressive deformation behavior. From these results, the experimentally measured results were reasonably in good agreement with the simulation results.

  • PDF

The effect of strain on the electronic properties of MoS2 monolayers

  • Park, Soon-Dong;Kim, Sung Youb
    • Coupled systems mechanics
    • /
    • v.5 no.4
    • /
    • pp.305-314
    • /
    • 2016
  • We utilize first-principles calculations within density-functional theory to investigate the possibility of strain engineering in the tuning of the band structure of two-dimensional $MoS_2$. We find that the band structure of $MoS_2$ monolayers transits from direct to indirect when mechanical strain is applied. In addition, we discuss the change in the band gap energy and the critical stains for the direct-to-indirect transition under various strains such as uniaxial, biaxial, and pure shear. Biaxial strain causes a larger change, and the pure shear stain causes a small change in the electronic band structure of the $MoS_2$ monolayer. We observe that the change in the interaction between molecular orbitals due to the mechanical strain alters the band gap type and energy.

Experimental Study on Failure Behavior of Plain Concrete - Biaxial Stress Test (콘크리트 파괴거동특성의 실험적 연구I-이축응력시험)

  • 이상근;이상민;박상순;한상훈;송영철
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.05a
    • /
    • pp.315-320
    • /
    • 2003
  • Two different strength types of plain concrete plate specimens (200$\times$200$\times$60mm) were tested under different biaxial load combinations. The specimens were subjected to biaxial combinations covering the three regions of compression-compression, compression-tension, and tension-tension. The loading platens with Teflon pads were used to reduce a confining effect in boundary surface between the concrete specimen and the solid platen. The principal deformations in the specimens were recorded, and the failure modes along with each stress ratio were examined. Based on the strength data, the failure envelops were developed for each type of plain concrete. The biaxial stress-strain responses of concrete plate specimens for three biaxial loading regions were also plotted. The test data indicated that the strength of concrete under biaxial compression ($f_2 / f_1$$_1$=-1/-1) is about 17 percent larger than under uniaxial compression.

  • PDF