• Title/Summary/Keyword: BSCCO 2223

Search Result 99, Processing Time 0.021 seconds

Transformation of the enthalpy and the entropy in BSCCO:2212-2223 (BSCCO:2212-2223 박막의 엔탈피와 엔트로피 변화)

  • Cheon, Min-Woo;Park, No-Bong;Park, Yong-Pil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.589-590
    • /
    • 2005
  • BSCCO:2212-2223 thin films were fabricated by using the ion beam sputter with a evaporation method at various substrate temperatures, $T_{sub}$, and ozone gas pressures, $pO_3$. The correlation diagrams of the BSCCO phases with Tsub and $pO_3$ are established in the 2212 and 2223 compositional films. In spite of 2212 compositional sputtering, Bi2201 and Bi2223 as well as Bi2212 phases come out as stable phases depending on Tsub and $pO_3$. From these results, the thermodynamic evaluation of ${\Delta}H$ and ${\Delta}S$, which are related with Gibbs' free energy change for single Bi2212 or Bi2223 phase, was performed.

  • PDF

The effect of step heat treatment in the critical current density of BSCCO 2223 tapes (BSCCO 2223선재의 임계전류밀도에 영향을 미치는 단계별 열처리의 효과)

  • 박성창;유재무;고재웅;김영국;김철진
    • Progress in Superconductivity
    • /
    • v.4 no.1
    • /
    • pp.90-93
    • /
    • 2002
  • The sintering process of BSCCO 2223 tapes is a complex process that is very sensitive to parameters, such as temperature, oxygen partial pressure, heating and cooling rate and holding time. During the first heat treatment, 2212 phase of precursor powder is partially transformed into 2223 phase and some residual secondary phases, such as $(Bi,Pb)_2$$Sr_2$CuO/sub y/(2201), $(Ca,Sr)_2$CuO/sub y/(2/1AEC), (Ca,Sr)/sub 14/Cu/sub 24/O/sub 41/(14/24 AEC) etc. The secondary phases are difficult to be removed from the BSCCO 2223 matrix on the heat treatment. These secondary phases degrade the critical current density. In order to minimize the amount and size of alkaline earth cuprate(AEC) particles step heat treatment is applied during the first heat treatment under the varying atmosphere. Experimental results showed that by adapting the step heat treatment process, the amount and particle size of the secondary phases in the final tapes are decreased. Consequently, the BSCCO 2223grain texture and Jc properties are improved.

  • PDF

Fabrication of fine BSCCO-2223 precursor powder by spray pyrolysis process (분무 열분해방법에 의한 미세 BSCCO-2223 전구분말의 제조)

  • 김성환;유재무;고재웅;김영국;박기호
    • Progress in Superconductivity
    • /
    • v.5 no.1
    • /
    • pp.65-69
    • /
    • 2003
  • Many researches on fabrication process for BSCCO precursor powders have been developed for high J$_{c}$ BSCCO-2223 tape. Spray pyrolysis method for fabrication of precursor powder has many advantages, such as high purity, fine particle size and low carbon content of BSCCO precursor powder. Fine, spherical powders were prepared by ultrasonic spray pyrolysis from the aqueous solution of metal nitrates. BSCCO precursor powders were synthesized with various solutes concentration and heat treatment conditions. Average particle size for spray pyrolysis powders was $1.5∼3\mu\textrm{m}$. Bi-2223/Ag tape was prepared by PIT method and followed by various sintering conditions. BSCCO precursor powders were characterized by XRD, SEM, EDS, Carbon content and particle size analysis.s.

  • PDF

The effect of the initial BSCCO 2212 grain size on the final grain size and the formation of BSCCO 2223

  • Yoo, Jai-Moo;Park, Myoung-Je;Kim, Hai-Doo;Chung, Hyung-Sik;Ko, Jae-Woong
    • 한국초전도학회:학술대회논문집
    • /
    • v.10
    • /
    • pp.285-288
    • /
    • 2000
  • The effect of the initial BSCCO 2212 grain size on the final gain size and the formation of the BSCCO 2223 was studied using a powder precursor synthesized by two-powder method. 2212 and CaCuO$_2$ tapes were prepared by dip coating and joined by pressing and then followed by the repeated thermo mechanical treatment. The samples were characterized by XRD and SEM analysis. The formation and grain size of the BSCCO 2223 depended on the initial BSCCO 2212 grain size.

  • PDF

Fabrication and microstructural development of BSCCO-2223 by modified two powder process (변형된 two powder 제조 공정법에 의한 BSCCO 2223 제조 및 미세구조발달)

  • Ko, Jae-Woong;Yoo, Jai-Moo;Park, Myoung-Je;Park, Sung-Chang;Kim, Hai-Doo;Chung, Hyung-Sik
    • 한국초전도학회:학술대회논문집
    • /
    • v.9
    • /
    • pp.397-400
    • /
    • 1999
  • We have fabricated BSCCO 2223 by modified two powder process and investigated 2223 phase formation and grain growth. Phase evolution and reactivity of 2223 were remarkably sensitive to size of 2212 grains and liquid phase. Larger size of 2212 phase increased liquid formation temperature. The Avrami relation was well suited for describing the kinetics of grain growth in BSCCO 2223.

  • PDF

Synethisis of fine BSCCO precursor powder by spray pyrolysis (분무 열분해에 의한 미세 BSCCO 전구체 분말의 합성)

  • 김성환;유재무;고재웅;김영국;박성창
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2003.10a
    • /
    • pp.99-102
    • /
    • 2003
  • Many researches on synthesis process for BSCCO precursor powders have been developed for high J$_{c}$ BSCCO-2223/Ag tape. Spray pyrolysis method for fabrication of precursor powder has many advantages, such as high purity, fine particle size of BSCCO precursor powder. Fine, spherical powders were prepared by ultrasonic spray pyrolysis from the aqueous solution of metal nitrates. BSCCO precursor powders were synthesized with 0.1 M concentration and heat treatment conditions. Average particle size for spray pyrolysis powders was 1.5 ~ 3 ${\mu}{\textrm}{m}$. BSCCO -2223/Ag tape was prepared by PIT method and followed by various sintering conditions. The critical current density of BSCCO-2223/Ag tape sintered in low oxygen partial pressure was ~ 23 kAcm$^{-2}$.

  • PDF

고온초전도 BSCCO 2223상 형성시 나타나는 여러 가지 이차상들이 선재의 임계전류에 미치는 영향(토요일)

  • 박성창;김철진;유재무;고재웅;김영국
    • Proceedings of the Korea Crystallographic Association Conference
    • /
    • 2003.05a
    • /
    • pp.24-24
    • /
    • 2003
  • 고온초전도 BSCCO 2223 ((Bi, Pb)₂Sr₂Ca₂Cu₃O/sub x/) 선재의 특성을 향상시키기 위해서는 반복적인 인발 및 압연과정을 통한 texturing향상, BSCCO 2223입자의 배향성 증대, 피복재내 초전도체의 충진율(밀도)향상, 이차상의 부피분율 감소등이 이루어져야 한다. 최적 열처리 조건을 통하여 열처리 시에 형성되는 이차상인 (Bi,Pb)₂Sr₂CuO/sub y/ (2201, amorphous phase)를 조절하면서, (Ca,Sr)₂CuO₃ (2/1 AEC), (Ca,Sr)/sub 14/Cu/sub 24/O/sub 41/ (14/24 AEC)와 같은 이차상들의 부피분율 및 크기를 감소시켜야만 한다. 본 실험에서는 BSCCO 2223 선재의 특성을 향상시킬수 있는 최적의 열처리 조건 확립 및 기계적 공정시 나타나는 여러 가지 문제점을 개선하여 높은 임계전류를 가지는 선재의 특성을 분석하고자 하였다. 최종적으로 제조된 선재는 2223상 결정이 피복재(Ag)와 평행하게 길게 성장하며, AEC상의 크기와 부피분율이 감소할수록 더 높은 임계전류특성을 나타내었다(I/sub c/~70A, J/sub c/~42,000 A/㎠). 또한 이 선재에서 나타나는 여러 가지 이차상들을 분석하기 위하여 XRD, SEM, EDS 분석을 행하였다.

  • PDF

Thermodynamics for Formation of Each Stable Single Phase in BSCCO Thin Films

  • Yang, Sung-Ho;Park, Yong-Pil;Kim, Gwi-Yeol
    • Proceedings of the Korean Institute of Navigation and Port Research Conference
    • /
    • 2000.11a
    • /
    • pp.104-105
    • /
    • 2000
  • High quality BSCCO thin films have been fabricated by means of an ion beam sputtering at various substrate temperatures, T$_{sub}$, and ozone gas pressures, PO$_3$. The correlation diagrams of the BSCCO phases appeared against T$_{sub}$ and PO$_3$are established in the 2212 and 2223 compositional films. In spite of 2212 compositional sputtering, Bi2201 and Bi2223 phases as well as Bi2212 one come out as stable phases depending on T$_{sub}$ and PO$_3$. From these results, the thermodynamic evaluations of ΔH and ΔS which are related with Gibbs'free energy change for single Bi2212 or Bi2223 phase are performed.ormed.i2212 or Bi2223 phase are performed.

  • PDF

Fabrication of Ultra Fine MgO Particles Added BSCCO 2223 Tapes with Different Precursor Phase Constituent

  • Ko, Jae-Woong;Yoo, Jai-Moo;Kim, Hai-Doo;Chung, Hyung-Sik
    • Progress in Superconductivity
    • /
    • v.1 no.1
    • /
    • pp.56-60
    • /
    • 1999
  • Ultra fine MgO particles added BSCCO tapes were fabricated by tape casting using Doctor Blade Method and enclosed by silver foil for different starting compositions (that is, 2223 major, 2212 major). In order to obtain optimum microstructure, thermomechanical treatment was done. Microstructure and phase were analyzed by XRD, SEM and DTA. The critical current density was measured under magnetic field at 77K. The tapes fabricated from the precursor powder with BSCCO-2223 phase (>90%) result in a microstructure with a larger grain size and higher transport critical current density value under magnetic field at given thermomechanical treatment conditions.

  • PDF

Thermodynamics for Formation of Each Stable Single Phase in BSCCO Thin Films

  • Yang, Sung-Ho;Park, Yong-Pil;Kim, Gwi-Yeol
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.11a
    • /
    • pp.104-107
    • /
    • 2000
  • High quality BSCCO thin films have been fabricated by means of an ion beam sputtering at various substrate temperatures, T$\_$sub/, and ozone gas pressures, PO$_3$. The correlation diagrams of the BSCCO Phases appeared against T$\_$sub/ and PO$_3$ are established in the 2212 and 2223 compositional films. In spite of 2212 compositional sputtering, Bi2201 and Bi2223 phases as well as Bi2212 one come out as stable phases depending on T$\_$sub/ and PO$_3$. From these results, the thermodynamic evaluations of ΔH and ΔS which are related with Gibbs' free energy change for single Bi2212 or Bi2223 phase are performed.

  • PDF