Search Result 412, Processing Time 0.03 seconds

Feasibility Analysis of Simulation on the Mechanical Properties of Neutron Irradiated Austenitic Stainless Steels by Cold-working (냉간가공을 통한 중성자조사된 오스테나이트 스테인리스강의 기계적물성 모사 타당성 분석)

  • Kim, Jin Weon;Kim, Yun Jae
    • Transactions of the Korean Society of Pressure Vessels and Piping
    • /
    • v.15 no.2
    • /
    • pp.9-18
    • /
    • 2019
  • The objective of this study is to investigate the feasibility of simulating the mechanical properties of irradiatied austenitic stainless steels by cold-working. In this study, the tensile properties, cyclic hardening behaviors and fracture toughness of cold-worked TP316L stainless steel were compared with those of austenitic stainless steels irradiated by neutrons. It showed that cold-working can properly simulate the increase in strength and the decrease in ductility and fracture resistance of austenitic stainless steels by neutron irradiation, even though it could not perfectly simulate the microstructures of irradiated austenitic stainless steels. Also, cold-working can appropriately simulate the hardening behaviors of neutron irradiated austenitic stainless steels under monotonic and cyclic loading conditions.

Cryogenic Fracture Toughness Evaluation for Austenitic Stainless Steels by Means of Unloading Compliance Method

  • Yu, Hyo-Sun;Kwon, Il-Hyun
    • Journal of Mechanical Science and Technology
    • /
    • v.15 no.1
    • /
    • pp.26-34
    • /
    • 2001
  • Most research to date concerning the cryogenic toughness of austenitic stainless steels has concentrated on the base metal and weld metal in weldments. The most severe problem faced on the conventional austenitic stainless steel is the thermal aging degradation such as sensitization and carbide induced embrittlement. In this paper, we investigate the cryogenic toughness degradation which can be occurred for austenitic stainless in welding. The test materials are austenitic stainless JN1, JJ1 and JK2 steels, which are materials recently developed for use in nuclear fusion apparatus at cryogenic temperature. The small punch(SP) test was conducted to detect similar isothermally aging condition with material degradation occurred in service welding. The single-specimen unloading compliance method was used to determine toughness degradation caused by thermal aging for austenitic stainless steels. In addition, we have investigated size effect on fracture toughness by using 20% side-grooved 0.5TCT specimens.

  • PDF

A study on the tensile property and corrosion resistance of austenitic stainless base and weld metal (오스테나이트계 스테인리스강 모재 및 용접부의 인장특성과 내식성에 관한 연구)

  • 정호신;김조권;엄동석
    • Journal of Welding and Joining
    • /
    • v.14 no.4
    • /
    • pp.71-78
    • /
    • 1996
  • The effect of chemical composition on mechanical properry and corrosion resistance of austenitic stainless steel was investigated. The main results obtained were as follows : 1. There was a linear relationship between the tensile strength of stainless steel and the $Cr_{eq}/Ni_{eq}$. The larger the $Cr_{eq}/Ni_{eq}$ was the higher the tensile strength of stainless steel. 2. There was a good correlationship between $Cr_{eq}/Ni_{eq}$ and intergranular, gerneral corrsion rate. 3. Intergranular corrosion rate decreased linearly with increasing Cr content. 4. General corrosion rate decreased linearly with increasing Ni content. 5. Logarithm corrosion rate of intergranular and general corrosion has a linear relationship with all of the factor of $Cr_{eq}/Ni_{eq}$, Cr and Ni content.

  • PDF

Effect of Tantalum and Lanthanum Addition on Electrochemical Property of Austenitic Stainless Steel in a Simulated PEMFC Environment

  • Kim, Kwang-Min;Koh, Seong-Ung;Kim, Kyoo-Young
    • Corrosion Science and Technology
    • /
    • v.7 no.6
    • /
    • pp.338-343
    • /
    • 2008
  • The electrochemical properties of W-modified austenitic stainless steels containing Ta and La were evaluated in a $H_{3}PO_{4}$ type PEMFC environment. Electrochemical test was conducted in 0.05 M $H_{3}PO_{4}$ solution at $80^{\circ}C$ and electrical property was conducted by contact resistance test. XPS was conducted to analyze the chemical elements consisting of passive film. Addition of La and Ta in W-modified austenitic stainless steel shows not only better corrosion resistance but also better electrical property.

Development of Metallic Bipolar Plate Material with W-addition in Austenitic Stainless Steel for PEMFC Environment

  • Kim, Kwang Min;Koh, Sung Ung;Kim, Kyoo Young
    • Corrosion Science and Technology
    • /
    • v.5 no.5
    • /
    • pp.153-159
    • /
    • 2006
  • Austenitic stainless steels with addition of various amounts of Mo and W were evaluated in terms of corrosion and contact resistance to determine optimum alloy composition of metallic bipolar plate for PEMFC. The corrosion property was evaluated by both acid fume exposure test at $130^{\circ}C$ and by electrochemical polarization tests in $H_3PO_4$ solution at $80^{\circ}C$. Austenitic stainless steel with proper amount of Mo and W demonstrated not only good corrosion resistance but also low contact resistance. Analyses on the passive film show that partial substitution of Mo by W enhances passive film stability and repassivation property. Test results suggest that austenitic stainless steel with 2 wt%Mo and 4 wt%W has optimum composition for metallic bipolar plate used in PEMFC.

Press Formability of Austenitic AISI304 Stainless Steel (오스테나이트계 AISI304 스테인레스강판의 프레스 성형특성)

  • Nam, J.B.;Ryoo, D.Y.;Kim, Y.S.
    • Transactions of Materials Processing
    • /
    • v.3 no.1
    • /
    • pp.38-50
    • /
    • 1994
  • Fundamental deformation mechanism and plastic behavior of AISI304 austenitic stainless steel were investigated to evaluate press formability. Local and uniform deformation capacity of AISI304 steel were compared to those of ferritic AISI430 steel and Al killed low carbon steel. Nine kinds of austenitic stainless steels having different austenite stabilities were made in laboratory scale to examine the transformation behavior in various deformation mode and variation of mechanical properties. Deformation path and strain distributions along edge corner of commercial sink die were illustrated and effect of austenite stability on press forming of sink die was clarified with experiments using square cup drawing tools.

  • PDF

The Effect of Welding Method on the Electrochemical Behavior of Austenitic Stainless Steel Sheet

  • Kim, Young-Hune;Kim, Kyoo-Young
    • Corrosion Science and Technology
    • /
    • v.9 no.3
    • /
    • pp.122-128
    • /
    • 2010
  • The corrosion of the flexible tube in the automobile exhaust system is caused by the ambient water and chloride ions. Since welding is one of the key processes for the flexible tube manufacturing, it is required to select a proper welding method to prevent the flexible tube corrosion and to increase its lifetime. There are many studies about the efficiency of the welding method, but no systematic study is performed for the effect of welding method on the corrosion property of the austenitic stainless weldment. The aim of the present study is to provide information on the effect of two different welding methods of TIGW (tungsten inert gas welding) and PAW (plasma arc welding) on the corrosion property of austenitic stainless steel weldment. Materials used in this study were two types of the commercial austenitic stainless steel, STS321 and XM15J1, which were used for flexible tube material for the automotive exhaust system. Microstructure was observed by using optical microscopy (OM) and scanning electron microscopy (SEM). To evaluate the corrosion behavior, potentiodynamic and potentiostatic tests were performed. The chemical state of the passive film was analyzed in terms of XPS depth profile. Metallurgical analysis show that the ferrite content in fusion zone of both STS321 and XM15J1 is higher when welded by PAW than by TIGW. The potentiodynamic and potentiostatic test results show that both STS321 and XM15J1 have higher transpassive potential and lower passive current density when welded by PAW than by TIGW. XPS analysis indicates that the stable $Cr_2O_3$ layer at the outermost layer of the passive film is formed when welded by PAW. The result recommends that PAW is more desirable than TIGW to secure corrosion resistance of the flex tube which is usually made of austenitic stainless steel.

Effects of Heat Treatment on Corrosion Resistance Properties of Gas Nitrided Stainless Steels (스테인레스강의 가스질화 후 내식특성에 미치는 열처리조건의 영향)

  • Kim, H.G.;Kim, Y.H.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.22 no.5
    • /
    • pp.298-306
    • /
    • 2009
  • Gas nitriding and post oxidation were performed on stainless steels and SACM 645 steel. With increasing gas nitriding time, the increasing rate of nitrided layer was most rapid on SACM 645 steel and the nitriding depth of nitrided layer was most narrow on STS 304 steel among three steels. Corrosion resistance was increased with post oxidation on stainless steels and with increasing time the effect of corrosion resistance was decreased to compare with relatively short gas nitriding time. An improvement effect of corrosion resistance was consisted of predominantly on austenitic stainless steel by post oxidation after gas nitriding among three steels and it was relatively less influenced on martensitic stainless steel.