Synthesis and Characteristic of Novel Soluble Triazoleimide Oligomers with Terminated Arylacetylene

  • Zhou, Xiao'an;Du, Lei;Wan, Liqiang;Wang, Xiaofei;E, Yanpeng;Huang, Farong
    • Bulletin of the Korean Chemical Society
    • /
    • v.31 no.9
    • /
    • pp.2603-2606
    • /
    • 2010
  • Novel soluble triazoleimide oligomers terminated with arylacetylene terminated were synthesized by the Cu(I)-catalysed 1,3-dipolar cycloaddition polymerization of diazides and imide-containing dialkyne. Several molecular weight triazoleimide oligomers were prepared from diazide and dialkyne monomers with different stoichiometric combinations. The curing behaviors of the oligomers were tested by differential scanning calorimetry (DSC). The thermal properties of the cured products were evaluated by DSC and thermogravimetric analysis (TGA). These cured oligomers showed the glass transition temperature of about $225-235^{\circ}C$ and the decomposition temperature (at 5% weight loss) of about $385-393^{\circ}C$ in nitrogen.

Preparation and Properties of Modified Silicon-containing Arylacetylene Resin with Bispropargyl Ether

  • Zhang, Jian;Huang, Jianxiang;Yu, Xiaojiao;Wang, Canfeng;Huang, Farong;Du, Lei
    • Bulletin of the Korean Chemical Society
    • /
    • v.33 no.11
    • /
    • pp.3706-3710
    • /
    • 2012
  • A novel silicon-containing arylacetylene resin (MSAR) modified by dipropargyl ether of bisphenol A (DPBPA) and dipropargyl ether of perfluorobisphenol A (DPPFBPA) was prepared separately. The curing behaviors of modified resins, DPBPA/MSAR and DPPFBPA/MSAR, were characterized with differential scanning calorimeter (DSC). The kinetic parameters of modified resins were obtained by the Kissinger and Ozawa methods. The results of dynamic mechanical analysis (DMA) revealed that the glass transition temperature ($T_g$) of the cured DPBPA/MSAR reached $486^{\circ}C$. According to the thermogravimetric analysis (TGA), the decomposition temperature ($T_{d5}$) of the cured resins and char yield ($Y_c$, $800^{\circ}C$) decreased as the dipropargyl ether loadings increased, especially in air. With the same weight loading, thermal stability of DPBPA/MSAR was better than that of DPPFBPA/MSAR. The carbon fiber (T300) reinforced composites exhibited excellent flexural properties at room temperature with a high property retention at $300^{\circ}C$.

Synthesis and Properties of Arylacetylene Resins with Siloxane Units

  • Gao, Fei;Zhang, Lingling;Tang, Lemin;Zhang, Jian;Zhou, Yan;Huang, Farong;Du, Lei
    • Bulletin of the Korean Chemical Society
    • /
    • v.31 no.4
    • /
    • pp.976-980
    • /
    • 2010
  • A series of arylacetylene resins with siloxane units were synthesized by the condensation reactions of m-diethynylbenzene magnesium reagents with various $\alpha,\omega$-bis(chloro)dimethylsiloxanes. These resins are liquids and are miscible with common organic solvents at room temperature. The structures of the resins were characterized by FT-IR, $^1H$ NMR, $^{13}C$ NMR, $^{29}Si$ NMR, and gel permeation chromatography (GPC). The thermal behaviors of the resins were examined with differential scanning calorimetry (DSC). These resins have good processability. They can be thermally cross-linked through the ethynyl groups to produce cured resins. The thermal and thermooxidative stabilities of the cured resins were studied by thermogravimetric analysis (TGA). The cured resins possess high thermal and thermooxidative stability. Their decomposition occurs at above $500^{\circ}C$ in both $N_2$ and air. With increasing the length of siloxane units in the resins, the thermal stability of the cured resins decreases in $N_2$. When the cured resins were sintered above $1450^{\circ}C$ under argon, hard and glassy SiOC ceramics were obtained. These SiOC ceramics have the decomposition temperatures at 5% weight loss above $800^{\circ}C$ in air.