• 제목/요약/키워드: Argon-welding

검색결과 45건 처리시간 0.025초

알루미늄 합금의 레이저 용접시 유기하는 플라즈마의 스펙트럼 분석 (Spectral Analyses of Plasma Induced by Laser Welding of Aluminum Alloys)

  • 김종도;최영국;김영식
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2001년도 추계학술대회 논문집
    • /
    • pp.292-300
    • /
    • 2001
  • The paper describes spectroscopic characteristics of plasma induces in the pulsed YAG laser welding of alloys containing a large amount of volatile elements. The authors have conducted the spectroscopic analyses of laser induced Al-Mg alloys plasma in the air and argon atmosphere. In the air environment, the identified spectra were atomic lines of Al, Mg, Cr, Mn, Cu, Fe and Zn, and singly ionized Mg lines, as well as the intense molecular spectra of A10 and Mg0 formed by chemical reactions of evaporated Al and Mg atoms from the pool surface with oxygen in the air. In argon atmosphere, Mg0 and AI0 spectra vanished, but AIH spectrum was detected. The hydrogen source was presumably hydrogen dissolved in the base metals, water absorbed on the surface oxide layer, or $H_2$ and $H_2O$ in the shielding gas. The resonant 1ines of Al and Mg were strongly self-absorbed, in particular, self-absorption of the Mg 1ine was predominant. These results show that the laser induced plasma was made of metal1ic vapor with relatively low temperature and high density.

  • PDF

펄스 YAG 레이저 용접시 유기하는 플라즈마의 스펙트럼선 동정과 발광특성 (Spectral Line Identification and Emission Characteristics of the Laser-Induced Plasma in Pulsed Nd:YAG Laser Welding)

  • 김종도
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제23권3호
    • /
    • pp.360-368
    • /
    • 1999
  • The paper describes spectroscopic characteristics of plasma induced in the pulsed YAG laser welding of alloys containing a large amount of volatile elements. The authors have conducted the spectroscopic analyses of laser induced Al-Mg alloys plasma in the air and argon atmosphere. In the air environment the identified spectra were atomic lines of Al, Mg, Cr, Mn, Cu, Fe and Zn and singly ionized Mg lines as well as the intense molecular spectra of ALO and MgO formed by chemi-cal reactions of evaporated Al and Mg atoms from the pool surface with oxygen in the air. In argon atmosphere MgO and AlO spectra vanished but AlH spectrum was detected. the hydrogen source was presumable hydrogen dissolved in the base metals water absorbed on the surface oxide layer or $H_2$ and $H_2O$ in the shielding gas. The resonant lines of Al and Mg were strongly self-absorbed in particular self-absorption of the Mg line was predominant. These results show that the laser induced plasma was made of metallic vapor with relatively low temperature and high density.

  • PDF

승합차의 램프 디자인과 제작을 위한 이종재료의 접합 (A Study on Welding of Dissimilar Materials for Van-Ramp Design and Production)

  • 이정현;김인철
    • 한국생산제조학회지
    • /
    • 제20권4호
    • /
    • pp.434-439
    • /
    • 2011
  • There are about 2.4million disabled in Korea, 2009. Also, Korean society entered into an aging society. Therefore disable and elderly are getting more involved in our society. This study proposes simple ramp design for wheel chair users and welding method and condition for manufacturing. In the middle of ramp, screw jack and motor are installed so that ramp can be moved left and right side. To make the ramp moves easily, ramp was fixed by installing LM guide on both sides. Ramp production for using Nd:YAG laser certain dissimilar welding in stainless steel sheet and cold reduced carbon steel. The output was fixed by 3kW, the speed was increased to 2~7m/min, Argon was used as shielding gas and the flow rate was changed to 10~30L/min. The proper welding condition is the output 3kW and welding speed 2~5m/min.

저탄소 박판 강재의 Nd:YAG 레이저 용접부 형성에 미치는 공정변수의 영향 (Effect of Process Parameters on Bead Formation in Nd:YAG Laser Welding of Thin Steels)

  • 김기철;허재협
    • Journal of Welding and Joining
    • /
    • 제19권3호
    • /
    • pp.317-324
    • /
    • 2001
  • This study deals with high power Nd:YAG laser welding of thin steels for small pressure vessels. Full penetration welding at the overlap joint was performed so as to assure sufficient weld strength. Results showed that mid-depth weld size reduced drastically with increasing the travel speed. Position of focus had little effect on the bead formation even though short focal system was used. However, the shape factor and the bead width had closely related with the position of focus. Based on the microstructural inspection, acceptable weld was obtained when the overlap clearance was controlled up to 20% of the base metal thickness. In the case that the joint contained more clearance than the critical value, both the tensile shear strength and the tear strength were reduced. Results also demonstrated that shielding gases were proved to play a key role as far as the bead formation characteristics was taken into consideration. Blowing dry air through 5mm in diameter nozzle produced narrower bead cross-section than that of argon or nitrogen shielding.

  • PDF

연속파형 Nd:YAG레이저를 이용한 Inconel 600와 STS 304의 이종금속용접 (Dissimilar Metal Welding of Inconel 600 and STS304 by a continuous wave Nd:YAG Laser)

  • 신호준;유영태;송성욱
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.1120-1125
    • /
    • 2004
  • Welding characteristics of STS304 stainless steel and Inconel 600 using a continuous wave Nd:YAG laser are experimentally investigated. Alloy 600 being used in steam generator tubing of pressurized water reactor(PWR) exposed to some corrosion environment, stress corrosion cracking can occur on this material. Presented here are the results from a series of experiments in which dissimilar metal welds were made using the gas tungsten arc welding process with pure argon shielding gas. But It is well known that solidification cracking susceptibility of austenitic alloys depends on the solidification temperature range and amount/distribution of solute rich liquid that exists at the terminal stages of solidification. An experimental study was conducted to determine effects of welding parameters and to optimize those parameters that have the most influence on eliminating or reducing the extent welding zone formation at dissimilar metal welds.

  • PDF

아크 용접에서 구동력에 따른 열 및 물질 유동에 관한 연구

  • 김원훈;나석주
    • 한국추진공학회:학술대회논문집
    • /
    • 한국추진공학회 1996년도 제7회 학술강연회논문집
    • /
    • pp.27-41
    • /
    • 1996
  • In this study the heat transfer and fluid flow of the molten pool in stationary gas tungsten arc welding using argon shielding gas were investigated. Transporting phenomena from the welding arc to the base material surface, such as current density, heat flux, arc pressure and shear stress acting on the weld pool surface, were taken from the simulation results of the corresponding welding arc. Various driving forces for the weld pool convection were considered, self-induced electromagnetic, surface tension, buoyancy, and impinging plasma arc forces. Furthermore, the effect of surface depression due to the arc pressure acting on the molten pool surface was considered. Because fusion boundary has a curved and unknown shape during welding, a boundary-fitted coordinate system was adopted to precisely describe the boundary for the momentum equation. The numerical model was applied to AISI 304 stainless steel and compared with the experimental results.

  • PDF

용접작업 형태별 공기중 용접흄 농도와 금속 성분에 관한 조사연구 (Airborne Concentrations of Welding Fume and Metal Components by Type of Welding)

  • 이권섭;백남원
    • 한국산업보건학회지
    • /
    • 제4권1호
    • /
    • pp.71-80
    • /
    • 1994
  • This study was conducted to evaluate worker exposure to welding fume in automobile body shop and to evaluate metal components by type of welding. The results are summarized as follows: 1. Average concentrations of total welding fume without and with ventilation were $5.2mg/m^3$ and $2.49mg/m^3$, respectively. Thus, the average reduction rate of total fume by ventilation was 52.1 %. 2. The highest fume concentration was indicated at shielded arc welding, followed by $CO_2$ gas welding, argon arc welding, and spot welding in order of decreasing concentration. 3. Average respirable fume concentrations without and with ventilation were $2.97mg/m^3$ and $1.64mg/m^3$, respectively. 4. Further analysis of welding fume indicated that total fume consisted of $Fe_2O_3$, ZnO, Mn, Pb, and CuO, in order of decreasing amount. Combined effect of metals was below the American Conference of Governmental Industrial Hygienists (ACGIH)Threshold Limit Values (TLVs).

  • PDF

철강재료 용접에서 보조가스가 레이저플라즈마와 용입특성에 미치는 영향 (Effect of Assist Gas on Laser Induced Plasma and Bead Formation in Welding of Structural Steel by CW Nd:YAG Laser)

  • 김기철;신현준
    • Journal of Welding and Joining
    • /
    • 제20권3호
    • /
    • pp.109-115
    • /
    • 2002
  • In this study high power Nd:YAG laser welding of structural steel was investigated. For the test steel blocks of $50{\times}50{\times}200mm$ were cut and machined, and bead-on-plate weld was made on the machined surface. Argon, nitrogen, helium, dry air or mixed gases were used to find the effect of shielding conditions on the bead formation. Results demonstrated that there were Fe I rich region and Fe II rich region in the laser induced plasma column based on the spectral analysis with S-2000 field spectrometer The Fe I region was located at the root of the column near keyhole opening. On the other hand, Fe II region was found at the middle of the plasma column. In the Nd:YAG laser welding, Fe I region emitted continuum which had peak value at wave length of around 710nm, and Fe II region had the peak at 580nm. In the welding of steel by $CO_2$ laser, however, no continuum was observed. There showed two groups of strong spikes in the $CO_2$ laser welding; the first group was displayed at the wave band of 450-560nm. This spike group emitted stronger intensity of light and sharper peaks than those group at 680-800nm.

ENHANCING TIG WELD PERFORMANCE THROUGH FLUX APPLICATION ATIG AND FBTIG PROCESSES

  • Marya, S.
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.70-75
    • /
    • 2002
  • The penetration potential of TIG welding in one single run is limited, though the process itself generates high quality welds with good weld cosmetics. This is one of the main reasons, which has contributed to its development in high duty applications such as those encountered in aeronautical, aerospace, nuclear & power plant applications. For these applications, stainless steels, titanium k nickel based alloys are most often used. As these materials remain very sensible to weld heat input k atmospheric pollution, stringent processing conditions are imposed. For example welding of titanium alloys requires argon shielding of weld zone and for 5 mm thick plates multi-pass runs & filler additions are required. This multi-run operation not only raises the welding cost, but also increases defect risks. In recent years, extensive interest has been raised by the possibility to increase weld penetrations through flux applications & the process is designated ATIG-activated TIG, or FBTIG-flux bounded TIG. The improved welding performance of such flux assisted TIG is related to arc constriction and surface tension effects on weld pool. The research work by authors has lead to the formulation of welding fluxes for stainless steels k titanium alloys with TIG Process. These fluxes are now commercialized & some applications in industry have already been carried out. FBTIG for aluminum has been proposed with silica application for AC mode TIG welding. The paper highlights the fundamentals of flux role in TIG welding and illustrates some industrial applications.

  • PDF

슈퍼듀플렉스 스테인리스강의 TIG 용접에서 질소 침투 모델에 관한 연구 (A study of model for nitrogen permeation in TIG welding of super duplex stainless steel)

  • 이재형;정병호;조상명;전재호
    • Journal of Welding and Joining
    • /
    • 제33권3호
    • /
    • pp.68-74
    • /
    • 2015
  • Superduplex stainless steels are important materials to the oil and gas industry, especially for off-shore production. TIG welding of super duplex stainless steels to obtain the optimal phase balance between austenite and ferrite is mainly achieved by controlling the cooling rate and the weld chemistry. The latter depends on the filler wire chosen and the shielding gas used. If TIG welding of superduplex stainless steels is performed with argon shielding gas only, then nitrogen gets lost from the weld pool, which can result in a ferrite-rich weld metal, with an inferior corrosion resistance than parent metal. In the present study, nitrogen permeation model from the shield gas which gets into the weld metal in DCEN-TIG welding has suggested. This plasma stream model shows characteristics of permeation of nitrogen ions into the molten metal due to the strong physical effect of plasma stream which formed by the arc pressure rather than the permeation of nitrogen ions caused by electric effect.