• 제목/요약/키워드: Arc plasma

검색결과 556건 처리시간 0.03초

Low & Intermediate Level Radioactive Waste Vitrification Using Plasma Arc Melting Technology

  • Min Byeong-Yeon
    • Nuclear Engineering and Technology
    • /
    • 제35권5호
    • /
    • pp.482-496
    • /
    • 2003
  • effectiveness of the PAM graphite-electrode technology for the treatment of many types of low-level radioactive waste including : combustible material, solidified resins in cement, inorganic materials, steel, glass, and solidified boric acid cement. The objectives of PAM-200 evaluation were to verify that 1) the facility meets air emission regulations, 2) the facility can be safely operated when processing hazardous and radioactive materials and 3) satisfactory final waste forms can be produced. Results, derived from KAERI's(Korea Atomic Energy Research Institute) analyses for samples of vitrified product, scrubbing solution and offgas collected during test period, show that PAM-200 can treat radioactive wastes as well as hazardous wastes with toxic constituents and radionuclides contained in the offgas exiting from the stack to the environment controlled to be far lower than the limit regulated by air conservation law and atomic law.

Comparison of light transmittance in different thicknesses of zirconia under various light curing units

  • Cekic-Nagas, Isil;Egilmez, Ferhan;Ergun, Gulfem
    • The Journal of Advanced Prosthodontics
    • /
    • 제4권2호
    • /
    • pp.93-96
    • /
    • 2012
  • PURPOSE. The objective of this study was to compare the light transmittance of zirconia in different thicknesses using various light curing units. MATERIALS AND METHODS. A total of 21 disc-shaped zirconia specimens (5 mm in diameter) in different thicknesses (0.3, 0.5 and 0.8 mm) were prepared. The light transmittance of the specimens under three different light-curing units (quartz tungsten halogen, light-emitting diodes and plasma arc) was compared by using a hand-held radiometer. Statistical significance was determined using two-way ANOVA (${\alpha}$=.05). RESULTS. ANOVA revealed that thickness of zirconia and light curing unit had significant effects on light transmittance ($P$ <.001). CONCLUSION. Greater thickness of zirconia results in lower light transmittance. Light-emitting diodes light-curing units might be considered as effective as Plasma arc light-curing units or more effective than Quartz-tungsten-halogen light-curing units for polymerization of the resin-based materials.

농업기계의 내마모 특성 개선을 위한 PTA 표면 개질법의 적용 (An Application of PTA Method for the Endurance and Wear Surface Characteristics of Agricultural Implements)

  • 김창수;최중섭
    • Journal of Biosystems Engineering
    • /
    • 제24권6호
    • /
    • pp.473-478
    • /
    • 1999
  • Recently, it is necessary fir surface materials to be low cost and to keep well endurable and wear in machinery field. Since most good materials with endurance and wear are expensive, they are being studied hard to modify to surface materials with endurance and wear, which overlay with the surface membrane completely. One of them is PTA(Plasma Transferred Arc Overlaying Process) method, which gets into the spotlight. It is thought to be an optimum method, since this method of overlays properly materials with about 3∼5cm surface membrane. It is necessity for the modified materials with endurance and wear to improve within the agricultural environment. Therefore, this research was used the PTA method to endure and wear a material. This method proved to be a reliable method for overlaying the membrane on the materials of an economical agricultural machinery.

  • PDF

INVESTIGATION OF MULTI-ARC PLASMA PLATING FILM EQUIPMENT BULAT-6 AND ITS TECHNICAL CHARACTERISTICS

  • Wen Xueya;Ma Te2ngcai;Hu Shejun
    • 한국진공학회지
    • /
    • 제6권S1호
    • /
    • pp.133-136
    • /
    • 1997
  • In this paper multi-arc plasma plating film equipment Bulat-6 and its technical characteristics were analyzed in detail. This machine is the first of its kind in China. Influential factors and reducing methods on microdroplets of titanium were investigated. By method of electromagnetic field control and ion beam enhanced deposition excellent titanium nitride film could be obtained. Bicrohardness and adhesion were 250Mpa and 6.5Kg respectively.

  • PDF

A Study on the Surface Modification of the Super Alloy by Plasma Transferred Arc Overlay Welding Method

  • Kim, Young-Sik;Lim, Chang-Hoon;Hwang, Won-Seok;Choi, Young-Gook
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제31권7호
    • /
    • pp.852-856
    • /
    • 2007
  • The Plasma Transferred Arc(PTA) overlay welding method is lately introduced as one of the most useful surface overlay method of the engine component. In this paper, the overlay welding method on the Nimonic super alloy was established by the PTA overlay welding process using the same super alloy powder. The characteristics of the Co-base and Ni-base super alloy overlay layers were investigated through the metallurgical, abrasive and cavitation erosion test. The abrasive and cavitation characteristics were investigated at room and high temperature.

Ni계 및 Co계 합금 PTA 오버레이용접층의 마모거동에 관한 연구 (Wear Behavior of Plasma Transferred Arc Deposited Layers for Ni - and Co - base Alloy)

  • 윤병현;이창희;김형준
    • Journal of Welding and Joining
    • /
    • 제19권5호
    • /
    • pp.540-547
    • /
    • 2001
  • This study has evaluated the wear behavior of PTA (Plasma Transferred Arc) Inconel 625 and Stellite 6 overlays on Nimonic 80A substrate. Nimonic 80A alloy was also included for comparison. In order to evaluate the wear performance, three-body abrasive wear test and pin-on-disk dry sliding wear test were performed. Microstructural development during the solidification of deposits is also discussed. Wear test results show that the wear rate of Stellite 6 deposit is lower than that of Inconel 625 deposit and Nimonic 80A. The sliding wear resistance of overlay deposits follows a similar trend to the abrasive wear resistance, but for Nimonic 80A. The main wear mechanisms were abrasive wear for Inconel 625 deposit, adhesive wear and delamination for Stellite 6 deposit in pin-on-disk dry sliding wear test and ploughing in three-body abrasive wear test. Cross sectional examinations of the worn surface of pin specimens after pin-on-disk dry sliding wear test implies that the plastic deformation near worn surface has occurred during the wear testing.

  • PDF

가변극성 플라즈마 아크용접을 이용한 알루미늄 합금의 키홀 용접 (Keyhole Welding of Aluminum Alloy by Variable Polarity Plasma Arc Welding)

  • 유준태;탁정수;윤종훈;장영순;이영무;강석봉
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2006년 추계학술발표대회 개요집
    • /
    • pp.72-74
    • /
    • 2006
  • The application of the variable polarity plasma arc welding process to A12219 is described. The thickness of aluminum alloy is 11.45mm and 5.08mm. 1-pass keyhole welding is applied to butt welding and 2-pass welding is also applied to thick material. During welding, all welding parameters are controlled by automated system and acquired by 10kHz rate. This paper covers the welding parameters, result of non-destructive test and tensile test.

  • PDF

플라즈마 화학증착법, 이온 플레이팅법 및 반응성 스퍼터링법에 의해 증착된 TiN 박막의 특성 비교 연구 (A Comparative Study on the Characteristics of TiN Films Deposited by Plasma-Assisted CVD, Ion Plating and Reactive Sputtering)

  • 안치범;정병진;이원종;천성순
    • 한국세라믹학회지
    • /
    • 제31권7호
    • /
    • pp.731-738
    • /
    • 1994
  • TiN films were deposited on high speed steels by plasma assisted chemical vapor deposition (PACVD), cathode arc ion plating (CAIP) and reactive magnetron sputtering (RMS). The properties of the films deposited by the three different methods were compared. The preferred oriented plane of PACVD-TiN is (200) and those of CAIP-TiN and RMS-TiN are (111). PACVD-TiN shows a dome surface and a microstructure having small grains. CAIP-TiN shows the highest microhardness and the best adhesion strength of the three because it has a dense microstructure and an ill-defined interface. But is shows the greatest surface roughness due to the Ti droplet created by the arc. RMS-TiN shows a microstructure having large voids so that its properties in microhardness and adhesion are the worst of the three.

  • PDF

RECOVERY OF METALS FROM EAF DUST WITH RAPID SYSTEM

  • Shin, Hyoung-ky;Moon, Seok-min;Jhung, Sung-sil
    • 대한전자공학회:학술대회논문집
    • /
    • 대한전자공학회 2001년도 The 6th International Symposium of East Asian Resources Recycling Technology
    • /
    • pp.381-386
    • /
    • 2001
  • The dust generated from the electric arc furnace steel making process is classified as hazardous material by Korean Environmental Protection Acts, mainly because of the existence of water teachable Pb, Zn and Cd. Thus the treatment of EAF dust is being carried out to fulfill both the environmental aspect and recovery of valuable metals. To establish the proper process for recovering the valuable metals (Fe, Zn, Pb and Cd) and producing the non-toxic slag from EAF dust, using RAPID-10 system, feasibility study have been carried out. To find out the scale-up factor for designing the commercial scale EAF dust treatment process(capacity 50,000 ton EAF dust per year) entitled RAPID-50 system. The design and construction of RAPID-50 (RIST Arc Plasma Industrial Device) system for treating 50,000 ton of EAF dust per year is now undergoing. Overall plan for treating EAF dust generated in KOREA will be setup after successful operation (December, 2002) of RAPID-50 system.

  • PDF

플라즈마 아크 용접에 의한 SUS 304L Lap 용접부형상이 강도에 미치는 영향 (Influence of Lap Weld Shapes on Shear Strength by Plasma Arc Welding of SUS 304L)

  • 문종현;윤동렬;김동철;이동우;장태원
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 춘계 학술발표대회 개요집
    • /
    • pp.129-130
    • /
    • 2004
  • The stainless steel sheet which is one of primary barrier components for membrane on LNG ship is ordinarily welded by either TIG or PAW. The weld shapes of acceptant tolerance for membrane construction are scripted by G.T.T.(Gaztransport & Technigaz)‘s rules such as penetration depth, weld throat and weld length etc. This paper presents relationship between weld metal shear strength and weld penetration formed with plasma arc welding. The results show penetration depth is not decisive factor on shear strength, but weld throat and length.

  • PDF