The Strength Properties of Metal Matrix Composites by Binder Additives (금속기복합재료의 바인더 첨가제에 따른 강도 특성)

  • Park, Won-Jo;Huh, Sun-Chul
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.27 no.7
    • /
    • pp.1051-1057
    • /
    • 2003
  • This study is about controlled impurities, which make metal alloys, especially AC4CH alloy that is made by restraining 0.2% Fe and Aluminum to make a matrix material. A metal matrix composite is produced using the squeeze casting method. The first step in the squeeze casting method is to add some organic binder including aluminum borate whisker into the matrix. After the fabrication of a metal matrix composite, each is individually appended to an inanimate binder such as SiO$_2$, Al$_2$O$_3$, and TiO$_2$. Through experiments the mechanical property changes were investigated between the metal matrix composite and AC4CH alloy. This study proves the superiority of the mechanical property of a metal matrix composites over AC4CH according to the previous tests and results that were mentioned above. One excellent property of matrix material composites is the infiltrated TiO$_2$ reinforcement. This material is a good substitute for the existing materials that are used in the development of industries today.

The Strength Properties of Metal Matrix Composites by Binder Additives (금속기복합재료의 바인더 첨가제에 따른 강도 특성)

  • Park, Won-Jo;Lee, Kwang-Young;Huh, Sun-Chul;Choi, Yong-Bum
    • Proceedings of the KSME Conference
    • /
    • 2001.11a
    • /
    • pp.198-203
    • /
    • 2001
  • This study is about controlled impurities, which make metal alloys, especially AC4CH alloy that is made by restraining 0.2% Fe and Aluminum to make a matrix material. A metal matrix composite is produced using the squeeze casting method. The first step in the squeeze casting method is to add some organic binder including aluminum borate whisker into the matrix. After the fabrication of a metal matrix composite, each is individually appended to an inanimate binder such as $SiO_2,\;Al_2O_3$, and $TiO_2$. Through experiments the mechanical property changes were investigated between the metal matrix composite and AC4CH alloy. This study proves the superiority of the mechanical property of a metal matrix composites over AC4CH according to the previous tests and results that were mentioned above. One excellent property of matrix material composites is the infiltrated $TiO_2$ reinforcement. This material is a good substitute for the existing materials that are used in the development of industries today.

  • PDF

Selective Laser Sintering of Alumina Using an Inorganic Binder Monoclinic $HBO_2$ and Post-Processing

  • 이인섭
    • Journal of Powder Materials
    • /
    • v.5 no.3
    • /
    • pp.199-209
    • /
    • 1998
  • A new low melting inorganic binder, monoclinic $HBO_2$, has been developed for Selective Laser Sintering (SLS) of alumina powder by dehydration process of boron oxide powder in a vacuum oven at $120^{\circ}C$. It led to better green SLS parts and higher bend strength far green and fired parts compared to other inorganic binders such as aluminum and ammmonium phosphate. This appeared to be due to its low viscosity and better wettability of the alumina particle surface. A low density single phase ceramic, aluminum borate ($Al_{18}B_4O_{33}$), and multiphase ceramic composites, $A_{12}O_3-A_{14}B_2O_9$, were successfully developed by laser processing of alumina-monoclinic $HBO_2$ powder blends followed by post-thermal processing; both $Al_{18}B_4O_{33}$ and $A_{14}B_2O_9$ have whisker-like grains. The physical and mechanical properties of these SLS-processed ceramic parts were correlated to the materials and processing parameters. Further densification of the $A_{12}O_3-A_{14}B_2O_9$ ceramic composites was carried out by infiltration of colloidal silica, and chromic acid into these porous SLS parts followed by heat-treatment at high temperature ($1600^{\circ}C$). The densities obtained after infiltration and subsequent firing were between 75 and 80% of the theoretical densities. The bend strengths are between 15 and 33 MPa.

  • PDF

Fatigue Strength Characteristic of Metal Matrix Composite Material in $9Al_2\;.\;2B_2O_4$/ AC4CH ($9Al_2\;.\;2B_2O_4$/ AC4CH 금속기 복합재료의 피로강도 특성)

  • Park, Won-Jo;Lee, Kwang-Young;Huh, Sun-Chul
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.25 no.10
    • /
    • pp.1583-1589
    • /
    • 2001
  • Metal matrix composites with whisker reinforcements have significant potentials for demanding mechanical applications including defense, aerospace, and automotive industries. Especially metal matrix composites, which are reinforced with aluminum borate whisker, have been used leer the part of piston head in automobile because of good specific strength and wear resistance. In this study, AC4CH-based metal matrix composites with $Al_{18}$B$_{4}$ $O_{33}$ reinforcement have been produced using squeeze casting method, after T6 heat treatment, we evaluated fatigue life property of matrix and MMC composite and investigated fracture mechanism.m.

Studies on Negative Thermal Expansion in $SrA1_2(BO_3)_2O$ Compound ($SrA1_2(BO_3)_2O$ 화합물에 있어서 열적 수축성 연구)

  • 장기석;이영건;오원균;한범수;더글라스케슬러
    • Korean Journal of Crystallography
    • /
    • v.14 no.1
    • /
    • pp.7-12
    • /
    • 2003
  • The compound SrA1₂(BO₃)₂O is a good host lattice for negative thermal expansion. We have measured thermal expansion over the limited temperature range by X-ray diffraction and ceramic dilatometry. In the aluminum borate compound, a thermal contraction is observed with a coefficient -1.64×10/sup -4/ Å/℃ on the c axis in the temperature range 23∼215℃ and with a maximum change -1.75㎛ in length of a ceramic bar of 20㎜ in the temperature range 110∼170℃, respectively.

A Fundamental Study of Eu2+ Luminescence in Aluminum Borate Compounds (Aluminum Borate 화합물에 있어서 EU2+이온의 발광성)

  • Chang, Ki-Seog
    • Journal of the Korean Chemical Society
    • /
    • v.44 no.4
    • /
    • pp.350-355
    • /
    • 2000
  • The compounds, CaAl$_2$(BO$_3$)$_2$O, SrAl$_2$(BO$_3$)$_2$O and BaAl$_2$(BO$_3$)$_2$O, are good host lattices for highly efficient $Eu^{2+}$ luminescence. The europium emission peaks at 450 nm in $Eu^{2+}$:CaAl$_2$(B0$_3$)$_2$O, 411 nm in $Eu^{2+}$: SrAl$_2$(BO$_3$)$_2$O and 375 nm in $Eu^{2+}$: BaAl$_2$(BO$_3$)$_2$O. The $Eu^{2+}$: CaAl$_2$(BO$_3$)$_2$O Phosphor shows a high output and should be a good maintenance in VUV Xe lamps. It is ideally suited for use in PDP phosphors. The $Eu^{2+}$ ion is interesting because the Stokes shift emission is a strong host dependent. The difference in the Stokes shift is oneimportant factor leadingto a difference in wavelength. If the 5d level of $Eu^{2+}$ ion is lower in energy,according to a decrease in the doping lattice size, then the emission wavelength will be longer and the Stokes shift will be smaller. Therefore, a knowledge of the relationship between the crystal lattice size and the Stokes shift. (orthe energy of the 5d level),is essential for beingable to predict $Eu^{2+}$ emission properties.

  • PDF

Growth Behavior of Aluminum Borate Whisker under 2.45 GHz Electromagnetic Irradiation (2.45 GHz 전자기파 조사하에서 Aluminum Borate Whisker의 성장 거동)

  • 김성완;이상근;김지경;이창희;안진모;신준식;박성수;박희찬
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.10
    • /
    • pp.998-1004
    • /
    • 2003
  • With starting materials of two different powder mixtures, $Al_2$(S $O_4$)$_3$+xNa$_2$B$_4$ $O_{7}$$.$10$H_2O$(㏖ ratio; x=0.1, 0.7) and ${\gamma}$-Al$_2$ $O_3$+xNa$_2$B$_4$ $O_{7}$$.$10$H_2O$(㏖ ratio; x=0.1, 0.7), whisker-type $Al_{18}$B$_4$ $O_{33}$ particles were synthesized by using conventional and microwave heat-treatment. The effects of microwave, amount of flux and temperature on the growth of whisker-type $Al_{18}$B$_4$ $O_{33}$ particles were investigated by using X-Ray Diffractometry (XRD) and Scanning Electron Microscopy (SEM). With increase of heat-treatment temperature and amount of flux, the size of whisker-type $Al_{18}$B$_4$ $O_{33}$ particles increased in both conventional and microwave heat-treated samples. However, compared to the conventional heat-treated samples, whisker-type $Al_{18}$B$_4$ $O_{33}$ particles were well grown for the microwave heat-treated samples.ted samples.

A Study on Fracture Toughness Properties of $Al_{18}B_4O_{33}/AC4CH$ by Binder Additives (바인더 첨가에 따른 $Al_{18}B_4O_{33}/AC4CH$의 파괴인성에 관한 연구)

  • Shin, Dong-In;Jung, Jae-Wook;Park, Won-Jo;Huh, Sun-Chul;Kim, Hyung-Jin
    • Proceedings of the KSME Conference
    • /
    • 2003.04a
    • /
    • pp.61-66
    • /
    • 2003
  • In this paper, the effect of binder additive on the fracture toughness was metal matrix composite produced by squeeze casting method. In this study using the matrix is AC4CH and reinforcement used Aluminum borate whisker. Each MMC was produced by add inanimate binder ($SiO_2,\;Al2O_3,\;TiO_2$) to whiskers for increase the binding together of whiskers. Fracture toughness test were carry out in accordance with the ASTM E-399 standard test method, W=25mm, b=12.5mm CT(half size) specimen. However Base metal AC4CH was not meet the qualification of $P_m/P_Q<1.1$, so that test were performed $J_{IC}$ test. $K_{J_{IC}}$ value was measuring by $J_{IC}$ value change into $K_{IC}$. $J_{IC}$ test was carry out in accordance with the ASTM 1820.

  • PDF

Effect of Matrix Microstructure on Creep Properties of Squeeze Cast Magnesium Matrix Composites (용탕 단조한 Mg복합재료의 크립특성에 미치는 기지조직의 영향)

  • Kim, Byeong-Ho;Son, Jae-Hyoung;Park, Kyung-Chul;Park, Yong-Ho;Park, Ik-Min
    • Journal of Korea Foundry Society
    • /
    • v.29 no.4
    • /
    • pp.176-180
    • /
    • 2009
  • Effect of matrix microstructure on creep behaviors of squeeze cast magnesium matrix composites was investigated. Aluminum borate whisker was used as reinforcement and AZ31, AS52 and Sr added AS52 Mg alloys were used for matrix alloys. The reinforcement was distributed homogeneously and defect-free composite was manufactured. Creep tests were carried out at the temperature of $150^{\circ}C$ under the applied stress of 50 and 100 MPa for Mg alloys and Mg MMCs, respectively. The creep resistance of Mg MMCs was in this order: AS52-Sr > AS52 AZ31 MMCs. Void initiation during creep mainly occurred at $Mg/Mg_{17}Al_{12}$ interface and propagation went along grain boundaries. On the other hand, $Mg_2Si$ phase was not attributed to the creep void initiation.

Effect of Boron Content on Atomic Structure of Boron-bearing Multicomponent Oxide Glasses: A View from Solid-state NMR (비정질 소듐 보레이트와 붕소를 함유한 다성분계 규산염 용융체의 붕소의 함량에 따른 원자 구조에 대한 고상 핵자기 공명 분광분석 연구)

  • Lee, A Chim;Lee, Sung Keun
    • Journal of the Mineralogical Society of Korea
    • /
    • v.29 no.3
    • /
    • pp.155-165
    • /
    • 2016
  • Understanding the effect of boron content on atomic structures of boron-bearing multicomponent silicate melts is essential to reveal the atomistic origins of diverse geochemical processes involving silica-rich magmas, such as explosive volcanic eruption. The detailed atomic environments around B and Al in boron-bearing complex aluminosilicate glasses yield atomistic insights into reactivity of nuclear waste glasses in contact with aqueous solutions. We report experimental results on the effect of boron content on the atomic structures of sodium borate glasses and boron-bearing multicomponent silicate melts [malinkoite ($NaBSiO_4$)-nepheline ($NaAlSiO_4$) pseudo-binary glasses] using the high-resolution solid-state NMR ($^{11}B$ and $^{27}Al$). The $^{11}B$ MAS NMR spectra of sodium borate glasses show that three-coodrinated boron ($^{[3]}B$) increases with increasing $B_2O_3$ content. While the spectra imply that the fraction of non-ring species decreases with decreasing boron content, peak position of the species is expected to vary with Na content. Therefore, the quantitative estimation of the fractions of the ring/non-ring species remains to be explored. The $^{11}B$ MAS NMR spectra of the glasses in the malinkoite-nepheline join show that four-coordinated boron ($^{[4]}B$) increases as $X_{Ma}$ [$=NaBSiO_4/(NaBSiO_4+NaAlSiO_4)$] increases while $^{[3]}B$ decreases. $^{27}Al$ MAS NMR spectra of the multicomponent glasses confirm that four-coordinated aluminum ($^{[4]}Al$) is dominant. It is also observed that a drastic decrease in the peak widths (full-width at half-maximum, FWHM) of $^{[4]}Al$ with an addition of boron ($X_{Ma}=0.25$) in nepheline glasses. This indicates a decrease in structural and topological disorder around $^{[4]}Al$ in the glasses with increasing boron content. The quantitative atomic environments around boron of both binary and multicomponent glasses were estimated from the simulation results of $^{11}B$ MAS NMR spectra, revealing complex-nonlinear variation of boron topology with varying composition. The current results can be potentially used to account for the structural origins of the change in macroscopic properties of boron-bearing oxide melts with varying boron content.