Journal of the Korean Crystal Growth and Crystal Technology
/
v.6
no.4
/
pp.584-594
/
1996
For the separation and purification of aluminium chloride hexahydrate crystals from kaolin leaching solution the effects of crystallization conditions, such as crystallization temperature, concentration of aluminium chloride concentration in the leaching solutin and gas flow rate of HCl into the leaching solution, on purity of the aluminium chloride hexahydrate crystals were investigated. The supersaturation level of aluminium chloride in the leaching solution gave great influence on the purity of the crystals. When supersaturated concentration of the aluminium chloride in the leaching solution was generated in low level, the aluminium chloride hexahydrate crystals were produced with high purity ; that is, the crystals hving a low Fe-ion concentration. The supersaturation level of aluminium chloride in the leaching solution was mainly determined by crystallization temperature, concentrations of aluminium chloride and hydrochloric acid in the solution. However, in spite of changes of the above crystallization coditions, a needle shape morphology of aluminium chloride hexahydrate crystals did not modified. To measure hydrochloric acid concentration in the kaolin leaching solution, we applied the oxalate titration method, which was suggested by shank [9] and it was prove that this method could titrate hydrochloroic acid concentration in multi-component ionic solution such as kaolin leaching solution.
The $3{\times}3{\times}30$ ($cm^3$) sized lumbers of Populus alba-grandulosa L. were treated with four fire-retardant solutions of ammonium sulfate, monoammonium phosphate, diammonium phosphate and aluminium chloride for 1, 15, 30, and 60 minutes and 1, 3, and 7 days. Thereafter they were air-dried and burned at high temperature about $1,800^{\circ}C$ and for short time of five minutes. This study estimated the relationship between absorbed chemical amounts and rate of weight loss or residual bending strength of these burned lumbers. The results were as follows: 1) In absorption amount of fire-retardant chemicals, diammonium phosphate showed the largest, aluminium chloride the smallest, but monoammonium phosphate and ammonium sulfate showed similar level. 2) The absorption amount of chemicals was decreased with the increase of specific gravity in the same species except aluminium chloride. 3) The rate of weight loss was decreased as the absorption amount of chemicals increased, especially monoammonium phosphate was most effective. 4) The MOR value of the residual bending strength was increased as the absorption amount of chemicals increased and especially monoammonium phosphate showed the most efficient effect. 5) Aluminium chloride showed more striking increase of MOR value of residual bending strength with the increase of absorption amount than any other chemical, therefore its MOR value was similar to the maximum MOR value of the most effective monoammonium phosphate. 6) The correlation between weight loss and MOR value of the residual bending strength was negative and aluminium chloride showed the most striking negative relation, but the others showed similar trends. 7) The correlation between work to proportional limit and absorption amount of chemicals was positive and the degree of increase in work to proportional limit was most in aluminium chloride, and the next, in monoammonium phosphate and diammonium phosphate in turn. 8) The correlation between work to maximum load and absorption amount of chemicals showed positive and diammonium phosphate revealed the best result and aluminium chloride showed better results than other two chemicals.
International Journal of Advanced Culture Technology
/
v.3
no.1
/
pp.39-45
/
2015
This research aims to study an effect of sodium chloride solution concentration on the corrosion rate of AA1100 aluminium alloy and SGACD zinc coated steel lap joint with a test duration of 30 days and a test temperature of $45^{\circ}$. The summarized results are as follows. Increase of the NaCl solution concentration increased the weight loss of Al, corrosion rate of Al, weight loss of Fe and also decreased the corrosion rate of Fe. Increase of the test duration affected to increase the weight loss and corrosion rate of Al and also decrease the weight loss and corrosion rate of Fe. The corrosion that was formed in a lap joint consisted of the uniform corrosion on the surface of the metals and the galvanic corrosion in the lap area of the joint. The maximum weight loss of AA 1100 aluminium and SGACD zinc coated steel that was occurred in the sodium chloride with 3.25% was 2.203% and 3.208%, respectively.. The maximum corrosion rate of AA 1100 aluminium and SGACD zinc coated steel that was occurred in 4.00% and 3.5% sodium chloride solution was 0.156 mm/year and 0.479 mm/year, respectively.
A study on the cementation for the recovery of tin with aluminium in the hydrochloric acid solution was carried out. Parameters, such as aluminium metal equivalent, pH, reaction time, reaction temperature and the concentration of chloride ions were investigated. The experimental results showed that the cementation rate of Sn(II) ions increased with increase of the addition amount of aluminium powders, temperature, pH and the concentration of chloride ions in hydrochloric acid solution. From the results, the optinum conditions for recovery of metallic tin by cementation with aluminium metal powders were proposed.
This study evaluates the potential of various coagulants to enhance the efficiency of total phosphorus removal facilities in a sewage treatment plant. After analyzing the existing water quality conditions of the sewage treatment plant, the coagulant of poly aluminium chloride was experimentally applied to measure its effectiveness. In this process, the use of poly aluminium chloride and polymers in various ratios was explored to identify the optimal combination of coagulants. The experimental results showed that the a coagulants combination demonstrated higher treatment efficiency compared to exclusive use of large amounts of poly aluminium chloride methods. Particularly, the appropriate combination of poly aluminium chloride and polymers played a significant role. The optimal coagulant combination derived from the experiments was applied in a micro flotation method of real sewage treatment plant to evaluate its effectiveness. This study presents a new methodology that can contribute to enhancing the efficiency of sewage treatment processes and reducing environmental pollution. This research is expected to make an important contribution to improving to phosphorus remove efficiency of similar wastewater treatment plant and reducing the ecological impact from using coagulants in the future.
Cho Deug-Hee;Han Jeong-Sik;Choi Myong-Jae;Cho Joon-Hyun;Lee Ho-Jin;Kim Young-Youn
Proceedings of the Korean Society of Propulsion Engineers Conference
/
2006.05a
/
pp.193-196
/
2006
This paper presents the results of catalytic endo- to exo- isomerization of saturated poly cyclic compound. Several zeolites were tested and influences of, Si/Al ratio and Structures of the zeolites on the reaction were investigated. The results showed that Y zeolites were more active than other zeolites, because of its large pore size and relative strong acidity. In all Y zeolites with different Si/Al, Y-5.4 is best. In all the zeolites tested, Y calcined at $450^{\circ}C$ was favorable. Still now the aluminium chloride catalyst is more active than zeolites. However, considering of environmental problems, corrosion, and treatment can make the zeolite catalyst substitute the aluminium chloride catalyst.
Park, Hyung-Kyu;Choi, Young-Yoon;Eom, Hyoung-Choon;Bae, Dong-Su
Resources Recycling
/
v.15
no.5
s.73
/
pp.52-56
/
2006
Waste aluminum dross was leached with hydrochloric acid to prepare PAC, poly aluminium chloride, used as water treatment chemicals. Metallic aluminum remained in the waste aluminum dross was dissolved into the hydrochloric acid solution. The solution could be used as PAC after adjusting the required alumina concentration and the basicity. Comparing to the conventional method far preparation of PAC using aluminum hydroxide, material cost could be saved in this method. Also, there is an additional merit in view of recycling of the waste aluminum dross by reducing the amount of waste dross to be landfilled.
Increasing water consumption produced sludge problems of the water treatment plants. The objective of this study is to investigate aluminium coagulants recovery n acidic and alkaline conditions. Water treatment plant sludge produced in Pusan Metropolitan City were tested for the aluminium extraction process. Experiment samples were obtained in summer from water treatment plants of Deoksan and Myongjang. Aluminium coagulants used in these plants during the test period were polyaluminium chloride(PAC), polyaluminium sulfate organic(PSO), polyaluminium sulfate silicate(PASS). Aluminium contents of water treatment sludge were in the range of 7.2~10.9% of the total solids. The recovery percentages for aluminium and iron by acidic extraction method was evaluated to 88% and 42% respectively. Extracted mass variation for other materials such as iron, manganese, total organic carbon was observed during the extraction operation. Alkaline extraction produced more than two times amount of total organic carbon than that in the acidic extraction process.
Synthesis of aluminium nitride has been studied by using the starting materials such as-alumina which was prepared at the lowest temperature from AlO(OH), anhydrous aluminium chloride and metallic aluminium powders. For the synthesis of aluminium nitride, the reaction temperature was carefully controlled and the reaction conditions were determined and discussed with the results. Reaction of metallic aluminium powder and nitrogen gas was taken place at relatively low temperature. The reaction parameters were determined kinetically.
The Zn-Al composite electroplating was studied by using chloride zinc bath containing metal hydroxides $(Zn(OH)_2,\;Al(OH)_3))$ and aluminium powder. The size of Al powder codeposited in the beaker bath with Al powder of-400 mesh was under 10${\mu}m$. The Zn-Al composite was electro-deposited at 40$^{\circ}C$ in the ranges of current density of 5-50 A/$dm^2$ in the flowing electrolyte. The content of aluminium particles codeposited increased slightly with increasing flow rate of electrolyte from 0.5 m/sec to 1.0 m/sec, and decreased with increasing current density from 5 A/$dm^2$ to 50 A/$dm^2$. The content of aluminium particles codeposited by using the electrolyte containing zinc hydroxide(0.1M) was 2~4 wt%. The Al powder was codeposited mainly near the surface layer of the electrodeposits. The dissolution rate of aluminium particles in the electrolyte containing 0.1M $Zn(OH)_2$ and Boric acid was 0.41 g/l. day in comparison with 1.5 g/l. day dissolution rate in pure chloride bath.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.