• Title/Summary/Keyword: Alkali treatment

Search Result 476, Processing Time 0.027 seconds

The Effect of Electrochemical Treatment in Lowering Alkali Leaching from Cement Paste to an Aquatic Environment: Part 1- Leachability of Alkali Ions (전기화학적 기법을 통한 시멘트페이스트의 수중노출에 따른 알칼리이온 침출저감 효과: Part 1- 알칼리이온의 침출능)

  • Bum-Hee Youn;Ki-Yong Ann
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.11 no.2
    • /
    • pp.138-144
    • /
    • 2023
  • In this study, the effect of electrochemical treatment in mitigating alkali leaching into an aquatic environment was investigated. To modify the surface of cement paste, 1000 mA/m2 of the direct current was passed through anodic graphite to the external mesh for 4 weeks. Then, the cement paste specimen was exposed to still water in air-tight condition to prevent natural healing of alkali leaching in the water. For 100 days of monitoring in water, the pH value was marginally increased at the electrochemical treatment, while control specimen ranked to the even higher pH accounting for 13.2 in the pH. Moreover, after the pH monitoring, the pH profile for the paste specimen indicated that the electrochemical treatment was effective in securing the higher alkalinity of cement matrix. The water obtained from alkali leaching process, was used to ecological test for Daphnia magna. It was evident that the electrochemical treatment had minimal adverse effect on ecological impact, while control specimen mostly immobilized the standard Daphnia magna.

Effects of Acid and Alkali Treatment for Chestnut Peeling and Its Physical Properties (밤의 박피를 위한 산 및 알카리 처리 효과와 물리적 특성)

  • 김영찬;홍순기;최종욱;이주백;정신교
    • Food Science and Preservation
    • /
    • v.6 no.3
    • /
    • pp.308-312
    • /
    • 1999
  • To develop the effective method for chestnut peeling, we examined the effect of peeling by acid and alkali treatment on their concentration, immersion temperature and time. Furthermore the physical properties of chestnut were investigated. In alkali treatment, 9% NaOH treated at 40$^{\circ}C$ for 9min was the most efficient for peeling outer peel, while acid treatment was less effective. But in the peeling of inner peel, acid treatment was more effective than alkali, especially, 3% HCIO$_4$ treated at 50$^{\circ}C$ for 30 min was the most effective. The correalation coefficient between weight and inner(outer) peel weight was higher than other physical properties, and multiple regression equation was established for predicting inner(outer) peel weight.

  • PDF

Cochineal natural dyeing of alkali-treated PET (II) - Color, Washfastness, Abrasion Resistance, Static Electricity Characteristics - (알칼리 감량(減量) PET의 코치닐 염색(染色) (II) - 색상(色相), 세탁견뢰도(洗濯堅牢度), 마찰견뢰도(摩擦堅牢度), 마찰대전압(摩擦帶電壓)을 중심(中心)으로 -)

  • Kim, Hyun-Su;Jeon, Dong-Won
    • Journal of Fashion Business
    • /
    • v.9 no.5
    • /
    • pp.122-135
    • /
    • 2005
  • It has been reported that natural dyeing is impossible without pre-treatment with metal mordanting agents. However, pre-treatment with chitosan, which has high affinity to natural dyes, could result in an excellent dyeing with various natural dyes. In this study, three treatment methods were employed; 1) Using PET without any pre-treatment (Method 1) 2) Using PET with chitosan acid solution pre-treatment (Method 2) 3) Using PET with chitosan pre-treatment and subsequent crosslinking using citric acid (Method 3) Method 2 and 3 enhanced the Cochineal dyeability remarkably compared to Mehod 1. Washfastness was also enhanced, and moisture content, static property, abrasion resistance, and fabric hand changes were investigated.

Extraction Yield and Quality Attributes of Agar from Domestic Seaweeds According to Various Pretreatments (국산원조(國産原藻)의 전처리(前處理)과정에 따른 한천(寒天)의 수율(收率) 및 품질특성(品質特性))

  • Lee, Su-Rae;Cho, Han-Ok;Park, Sang-Ki
    • Korean Journal of Food Science and Technology
    • /
    • v.7 no.3
    • /
    • pp.109-114
    • /
    • 1975
  • Domestic seaweeds Gracilaria verrucosa collected from coastal areas of Namhae, Wando and Yeosoo, Korea were subjected to the examination of yield and quality of agar prepared according to various pretreatment conditions. In alkali treatment at high temperature, higher alkali concentration for one-hour period at $90^{\circ}C$ gave rise to higher yield of agar. In acid treatment, higher yield was obtained by higher acid concentration and longer treating period. Alkali treatment at room temperature gave rise to a slightly decreased yield at higher alkali concentration and longer treating time. Total nitrogen and crude ash of agar samples were greatly decreased by pretreatments. Jelly strength, gelation ability, gelation point and viscosity of agar samples tended to increase as the alkali-treating condition of seaweed became stronger. It was shown that sulfur content of agar had a high negative correlation with jelly strength of its gel. Various alkali treatments of seaweed at room temperature showed no marked difference in agar quality and did not exhibit any good effect comparable to alkali treatment at high temperature.

  • PDF

Hydrolysis of Silk Fibroin on Alkali Conditions (견 피브로인의 알칼리 가수분해)

  • 김남정;배도규
    • Journal of Sericultural and Entomological Science
    • /
    • v.39 no.2
    • /
    • pp.197-202
    • /
    • 1997
  • To hydrolyze silk fibroin was treated with NaOH solution on various concentrations and times. And it was examined that the addition effects of NaHSO3 solution on the solubility and colouring of silk fibroin. As obtained results are as follows; The more increasement of concentration and time of NaOH treatment, the more increasement of solubility but solubility was slight above 3% concentration of NaOH. Fibroin yield was decreased above 3% concentration. This was due to formation of peptide or amino acids below molecular weight 3,000. Most of molecular weight distribution came out to be under 3,000 in 2% concentration and 4hrs of NaOH treatment. The more increasement of adding concentration and 4hrs of NaOH treatment. The more increasement of adding concentration of NaHSO3, the more reduction of solubility but white index of powder increased. In the results of FT-IR spectras of silk fibroin powder obtained by various concentrations of NaHSO3 treatment, the absorbent peak at 3,400 cm-1 which was considered as -CH=N- (azomethine) was disappeared by the more addition of NaHSO3. It showed that absorbent peak of $\beta$-fibroin moved into low temperature region and transferred to $\alpha$- and random coil structure through the DSC experiment. In the results of amino acid analysis, alkali hydrolysis reduced the oxy amino contents acid like serine and tyrosine, but increased the glycine content by the more addition of NaHSO3.

  • PDF

Change of Dispersibility and Refractive Index of Zirconia Suspension Depending on Alkali Treatment Time (염기처리시간에 따른 지르코니아 현탁액의 분산성과 굴절율 변화)

  • Jo, Choong Hee;Ham, Dong Seok;Lee, Jae Heung;Ryu, Juwhan;Lee, Kee-Yoon;Cho, Seong Keun
    • Korean Journal of Materials Research
    • /
    • v.27 no.1
    • /
    • pp.1-7
    • /
    • 2017
  • Zirconia nanoparticles were widely used as filler in order to get high refractive index layer. However, dispersion of nanoparticles is difficult due to their agglomeration in solvent. In this study, the dispersibility of the zirconia suspension is promoted by controlling the steric hindrance and electrostatic interactions through the adsorption of PEI according to alkali treatment time. Also, to induce improved dispersibility on suspension, we changed the dispersion conditions variously and fabricated an ink formulation method for the coating layer. Zirconia suspension was characterized by dynamic light scattering (DLS), Zeta potential measurement, Transmission Electron Microscope (TEM) and FT-IR. We were able to confirm that good dispersion of zirconia suspension by alkali treatment and PEI led to high refractive index.

Effects of Solvent Treatment of Bamboo Fiber on Physical Properties of Polypropylene/Glass Fiber/Bamboo Fiber Composite (엔진커버용 폴리프로필렌/유리섬유/대나무섬유 복합체의 물리적 특성에 대한 대나무섬유의 용제 처리의 영향)

  • Lee, Su Kyoung;Lim, Sung Wook;Shin, Hyung Shik;Woo, Seung-Keon;Park, Eun Young
    • Textile Coloration and Finishing
    • /
    • v.31 no.1
    • /
    • pp.42-47
    • /
    • 2019
  • In this study, the effects of surface treatment of bamboo fiber on the physical properties of polypropylene(PP)/glass fiber(GF)/Bamboo fiber(BF) composite for engine cover were investigated. PP, GF and BF were fixed at 40%, 40% and 20% and the surface of bamboo fibers were treated to 0.5, 1.0 and 2.0% as an acid and alkali solution. PP/GF/BR composites using surface treated bamboo fibers were prepared and their tensile strength, bursting strength and impact strength were measured by universal testing machine(UTM). The composites with alkali treated bamboo fiber showed better mechanical properties than the acid treated composites. It was checked that the optimum alkali content was at 1.0% from the results of mechanical properties. The effect of surface treatment on the mechanical properties was confirmed by SEM images of fractured surface.

Preparations Purified Cellulose from Rice Hull (왕겨기반 고순도 셀룰로오스의 제조)

  • Lee, Young-Ju;Sung, Yong-Joo
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.44 no.3
    • /
    • pp.79-85
    • /
    • 2012
  • In this study, purified cellulose was prepared from rice husk which is one of the major agricultural residues in Korea. The various bleaching processes such as ozone bleaching, $ClO_2$ bleaching and $H_2O_2$ bleaching were applied to remove residual lignin and impurities. In order to increase the contents of ${\alpha}$-cellulose contents, the effects of acid and alkali treatments were evaluated. Although the multi stages of the bleaching processes resulted in less than 0.5 % residual lignin contents, the application of ozone leaded to the decrease in DP(degree in Polymerization) and ${\alpha}$-cellulose contents. The alkali treatment after bleaching processes resulted in pure cellulose which showed more than 98% of ${\alpha}$-cellulose contents.

Effect of NaOH Treatments on Jute and Coir Fiber PP Composites

  • Hai, Nguyen Minh;Kim, Byung-Sun;Lee, Soo
    • Advanced Composite Materials
    • /
    • v.18 no.3
    • /
    • pp.197-208
    • /
    • 2009
  • Changes occurring in jute and coir fiber composites with 2-8% concentration of a NaOH treatment for 24 h were investigated, respectively, for void content, microscopy images, mechanical properties and water absorption. The jute and coir fibers were vacuum dried before molding composite specimens. Mechanical properties indicated good adhesion between natural fibers and PP. Jute fibers, when alkali-treated with 2% concentration for 24 h, showed best improvement in tensile strength by 40% and modulus by 9%, respectively, while coir fibers, when alkali-treated with 6% concentration for 24 h, showed best improvement in tensile strengths by 62% and modulus by 17%, respectively. With 2% concentration of alkali-treatments, the elongation of jute and coir composites reached 8% and 13.5%, respectively. Moisture absorption for jute and coir composites are 50% and 60% lower than untreated fiber composites, respectively.

Disintegration of Flotation Scum in Food Wastewater Using Thermo-Alkaline Pretreatment (열-알칼리 전처리를 통한 음식물류 폐수 부상 스컴의 가용화)

  • Choi, Jae-Min;Lee, Chae-Young
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.26 no.1
    • /
    • pp.71-78
    • /
    • 2015
  • This study was performed to optimize the integrated thermal-alkali pre-treatment of flotation scum for the enhanced biodegradability. The optimum conditions of the integrated thermal-alkali pre-treatment were obtained using response surface methodology. The disintegration degree of carbohydrate (69.2%) and protein (57.3) were estimated under the optimum conditions. Although the optimum conditions were different, the disintegration degrees were similarly. A fermentative hydrogen batch test was conducted to evaluate the hydrogen production from scum with and/or without. The maximum hydrogen production from scum with pre-treatment was of 0.64 mol H2/mol hexoseadded, which about 1.4 times higher than without pre-treatment.