• Title/Summary/Keyword: Al6061 alloy

Search Result 176, Processing Time 0.037 seconds

Mechanical and Electrochemical Characteristics in Welding with Robot on 6061-T6 Al Alloy for Al Ship (로봇으로 용접한 알루미늄 선박용 6061-T6 합금의 기계적, 전기화학적 특성)

  • Kim, Seong-Jong;Jang, Seok-Ki
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.33 no.2
    • /
    • pp.313-321
    • /
    • 2009
  • The construction of fiber-reinforced plastic (FRP) boats is decreasing trend since the application of international regulations on the control of marine environmental pollution, which recommended the use of environmentally friendly materials. The aluminum alloy used with material for ship is a superior to FRP. It is environmental friendly, easy to recycle, and provides a high added value to fishing boats. However, the welding for Al alloy materials have many problems, such as deformation by welding heat and effect of the working environment. In this paper, it was carried out welding by robot with welding material of ER5183 and ER5556 on 6061-T6 Al alloy for ship. The mechanical and electrochemical characteristics evaluated for specimen welded by robot. The cathodic polarization trend for the base metal and welding metal showed the effects of concentration polarization due to oxygen reduction and activation polarization due to hydrogen generation. The hardnesses of welding zone and heat affected zone are lower than that of base metal. At the result of tensile test, the specimen welded with ER5183 presented excellent property compared with ER5556.

A Study on the Mechanical Properties of Spray-cast Al 6061 Alloy with Variation of Mg/Si Content (분사주조한 Al 6061 합금의 Mg/Si 첨가량의 변화에 따른 기계적 특성 고찰)

  • Lee, Jae-Sung;Kim, Myung-Ho
    • Journal of Korea Foundry Society
    • /
    • v.28 no.4
    • /
    • pp.179-183
    • /
    • 2008
  • Mechanical properties of the spray-cast Al 6061 alloy with variation of Mg/Si addition were investigated. After spray-cast, hot extrusion was performed at $460^{\circ}C$ then followed ageing treatment to the T6 condition. SEM, EDX, and XRD were used to characterize a ${\beta}(Mg_{2}Si)$ precipitate. The amount of ${\beta}$ precipitate was calculated from the XRD measurements. Hardness, ultimate tensile strength and elongation were tested then compared with those of the Al 6061 alloys made by ingot metallurgy (I/M) and powder metallurgy (P/M). The ultimate tensile strength and elongation of the spray-cast Al 6061 alloy were 318MPa and 16.5%, respectively. These properties were improved in the 2.2 wt%Mg and 1.3wt%Si addition up to 349MPa of UTS and 12.5% of elongation, mainly due to increased amount of a fine supersaturated ${\beta}(Mg_{2}Si)$ precipitate.

Interfacial and Tensile Properties of TiNi Shape Memory Alloy reinforced 6061 Al Smart Composites by vacuum casting (진공주조법에 의한 TiNi 형상기억합금 강화 6061Al 지적 복합재료의 계면 및 인장 특성)

  • Park, Gwang-Hun;Park, Seong-Gi;Sin, Sun-Gi;Park, Yeong-Cheol;Lee, Gyu-Chang;Lee, Jun-Hui
    • Korean Journal of Materials Research
    • /
    • v.11 no.12
    • /
    • pp.1057-1062
    • /
    • 2001
  • We investigated the change of mechanical properties for TiNi shape memory alloy by heat treatment. 6061Al matrix composites with TiNi shape memory alloy as reinforcement were fabricated by vacuum casting. TiNi alloy has the maximum tensile strength at 673K treated and there is no change of tensile strength and hardness at 448K treated. The composites, prepared by vacuum casting, showed good interface bonding by vacuum casting. It was about 3$\mu\textrm{m}$ of thickness of the diffusion layer. Tensile strength of the composite was in higher than that of 6061Al alloy as increased value of about 70MPa at room temperature and about 110MPa at 363K. We thought that the increase of the tensile strength at 363K was due to reverse transformation of the TiNi shape memory alloy.

  • PDF

The Basic Study on Fatigue Crack Growth Behavior of SiC Whisker Reinforced Aluminium 6061 Composite Material (SiC 휘스커 보강 Al 6061 복합재료의 피로균열진전 특성에 관한 기초 연구)

  • 권재도;안정주;김상태
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.18 no.9
    • /
    • pp.2374-2385
    • /
    • 1994
  • SiCw/Al composite material is especially attractive because of their superior specific strength, specific stiffness, corrosion fatigue resistance, creep resistance, and wear resistance compared with the corresponding wrought Al alloy. In this study, Fatigue crack growth behavior and fatigue crack path morphology(FCPM) of SiC whisker reinforced Al 6061 alloy with 25% SiC volume fraction and Al 6061 allay were performed. Result of the fatigue crack growth test sgiwed that fatigue crack growth rate of SiCw/Al 6061 composite was slower than that of Al 6061 matrix therefore it was confirmed that Sic whisker have a excellent fatigue resistance. And Al 6061 matrix had only FCPM perpendicular to loading direction. On the other hand SiCw/Al 6061 composite had three types in fatigue crack path morphology. First type is that both sides FCPM of artificial notch are perpendicular to loading direction. Second type is that a FCPM in artifical notch has slant angle to loading direction and the other side FCPM is perpendicular to loading direction. Third type is that both sides FCPM of notch have slant angle to loading direction. It was considered that this kinds of phenomena were due to non-uniform distribution of SiC whisker and confirmed by SEM observation for fracture mechanism study.

Evaluation of Electrochemical Characteristic and Investigation on Optimum Condition in Friction Stir Welding for 6061-T6 Al Alloy (6061-T6 합금의 최적 마찰교반 용접 조건 규명 및 전기화학적 특성 평가)

  • Kim, Seong-Jong;Jang, Seok-Ki
    • Journal of the Korean institute of surface engineering
    • /
    • v.41 no.6
    • /
    • pp.341-350
    • /
    • 2008
  • In friction stir welding for 6061-T6 with various traveling speed and rotation speed conditions, the best mechanical characteristics presented in traveling speed of 507 mm/min and rotation speed of 1100RPM. The maximum tensile strength and yield strength increased with the increasing of traveling speed. The result of the electrochemical characteristic evaluation in friction stir welding at optimum conditions for 6061-T6 Al alloy presented a good characteristics compare to base metal.

The Characteristic Evaluation of Electron Beam Welding for Al 6061 alloy with thick-thickness plate (후판 Al 6061합금의 전자빔용접 특성 평가)

  • Jeong In-Cheol;Sim Deok-Nam;Kim Yong-Jae
    • Proceedings of the KWS Conference
    • /
    • 2006.05a
    • /
    • pp.68-70
    • /
    • 2006
  • For the aluminum material of the thick-thickness more than 100mm Penetration depth Electron beam welding is effectively applicable with a characteristic of high energy intensity. But Al 6061 alloy has high crack sensitivity due to minor alloys, which are silicon, magnesium, copper etc. With a sample block of 135mm thickness EBW test was performed in vertical position. As tensile strength has $210{\sim}220N/mm^2$ with weld area broken. Bend test shows low ductility with fracture of partly specimens. Chemical contents of alloys show no difference between weld and base metal. Defect in middle weld area figures out typical hot crack due to low melting materials. Micro structure of weld area has some difference compare to HAZ and base metal. As a result of EBW test for Al 6061 alloy, it shows that weld defect could be occurred even though establishing of optimum weld parameter condition.

  • PDF

Effects of Na3PO4 Concentration on the Porosity of Plasma Electrolytic Oxidation Coatings Surface on the 6061 Al Alloy, and Subsequent-NaAlO2 Sealing (6061 알루미늄 합금의 플라즈마 전해산화 피막의 표면기공율 및 부식특성에 미치는 Na3PO4 농도 및 NaAlO2 봉공처리의 영향)

  • Song, Euiseok;Kim, Yong-Tae;Choi, Jinsub
    • Journal of the Korean institute of surface engineering
    • /
    • v.52 no.3
    • /
    • pp.117-122
    • /
    • 2019
  • In this study, surface porosity and corrosion resistance of PEO coatings prepared on the 6061 Al alloy were investigated in terms of sodium phosphate ($Na_3PO_4$) concentrations in an alkaline solution and $NaAlO_2$ sealing. The surface morphologies of the PEO coatings clearly show that the coatings film formed in $9g\;L^{-1}$ had the lowest porosity. The $NaAlO_2$ sealing was found to remove micropores and cracks existing on the surface of PEO coatings. As a result, the $NaAlO_2$ sealing resulted in the movement of corrosion potential toward more positive value and lower corrosion current density.

Comparison of chemical resistance properties of anodized film according to anodized sealing treatment method of Al6061 alloy (Al6061 합금의 양극산화 봉공 처리 방법에 따른 양극산화 피막의 내화학 특성 비교)

  • Young Uk Han;Sang Sub Lee;Jun Seok Lee;Gibum Jang;Sung Youl Cho
    • Journal of the Korean institute of surface engineering
    • /
    • v.57 no.3
    • /
    • pp.201-207
    • /
    • 2024
  • This study compared the chemical resistance properties according to various sealing treatment methods for the anode film formed during the anodization process of Al6061 alloy. Al6061 aluminum was used in four different sealing treatment methods: boiling water sealing, lithium sealing, nickel sealing, and pressurized sealing, and each sample was evaluated for corrosion resistance through a 5% HCl bubble test and the microstructure was observed through a scanning electron microscope(SEM). According to the results, corrosion resistance increased as time and temperature increased in all sealing treatment methods. Relatively, corrosion resistance was high in the order of boiling water sealing, lithium sealing, nickel sealing, and pressure sealing, and the best corrosion resistance was found in pressure sealing. These research results can be helpful in selecting a process necessary to improve the efficiency and performance of anodizing process in the industrial field using aluminum alloys.