• 제목/요약/키워드: Al matrix composites

검색결과 319건 처리시간 0.018초

Saffil/SiCp을 이용한 금속 복합재료의 상온 마모 거동 (Wear Behavior of Saffil/SiCp reinforced Metal Matrix Composites at the room temperature)

  • 조종인;한경섭
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 2003년도 춘계학술발표대회 논문집
    • /
    • pp.46-49
    • /
    • 2003
  • Aluminum based metal matrix composites(MMCs) are well known for their high specific strength, stiffness and hardness. They are gaining further importance because of their high wear resistance. In this study, Al/Saffil-20%, Al/Saffil-5%/Al2O3(particle type)-15% and Al/Saffil-5%/SiC(particle type)-15% hybird MMCs' wear behavior were characterized by the pin-on-disk test under various normal load The superior wear resistance was exhibited at Al/Saffil-5%/SiC(particle type)-15% MMCs. And this MMCs' predominant wear mechanism is subsurface cracking in the low load wear regime. Others(Al/Saffil-20%, Al/Saffil-5%/Al2O3(particle type)-15%) showed the similar wear resistance with each other at the same test condition. In the low load & room temperature condition, the wear resistance was improved due to the high hardness of the ceramic reinforcements. As the test load increased, the wear properties were governed by the wear properties of matrix.

  • PDF

반응결합법에 의한 TiC-Ni/Al 복합체의 미세구조 및 기계적 특성 (Microstructure and Mechanical Properties of TiC-Ni/Al Composites by the Reaction-Bonding Method)

  • 한인섭;우상국;김흥수;양준환;정윤중
    • 한국세라믹학회지
    • /
    • 제33권5호
    • /
    • pp.536-546
    • /
    • 1996
  • The TiC-Ni/Al reaction-bonding composites were prepared by the infiltration of Ni/Al melt into the TiC preforms. The microstructure the reaction composition crystalline phase and the mechanical properties of the composites were investigated. During the reaction-bonding Ni/Al mixture had a good wettability and per-meability with TiC preform and pore-free and fully dense sintered bodies were produced. In the case of the Ni/Al atomic ratio of 0.3 and 0.5 TiC raw particle shape was changed to irregular particles because of the decomposition in the liquid matrix and its phenomena was more distinguished in the Al-rich liquid matrix. With increasing more than 1 of the Ni/Al atomic ratio the sample of TiC grain shape was changed from spherical to palatelet particles. Also with increasing the atomic ratio of Ni/Al bending strength and fracture spherical to palatelet particles. Also with increasing the atomic ratio of Ni/Al bending strength and fracture toughness were increased and its maximum value was 1073 MPa and 11 MPa.m1/2 respectively.

  • PDF

용탕단조법으로 제조된 AC4C 합금기 세라믹강화 복합재료의 특성연구 (Characterization of the Ceramic Reinforced AC4C Matrix Composites Processed by Squeeze Casting)

  • 김억수
    • 한국주조공학회지
    • /
    • 제25권2호
    • /
    • pp.88-94
    • /
    • 2005
  • The microstructure and mechanical property of the ceramic reinforced AC4C matrix composites processed by squeeze casting were investigated. In this study Kaowool and Saffil fiber which are ceramic reinforcements are used as preform materials. As a matrix material, Al-7wt.%Si-0.3wt.%Mg(AC4C) has been used. In case of Kaowool and Saffil/AC4C composites, 7.5 MPa squeezing pressure and minimum 7.0% binder amount are needed to produce sound composite materials. The tensile strength of Kaowool/ AC4C composite is lower than the matrix metal and this can be explained by the melt unfilling due to formed cluster of Kaowool reinforcements. But the mechanical properties of hardness, wear resistance and thermal expansion are better than the matrix materials due to the strengthening effect of ceramic reinforcements.

Al$_2$O$_3$/LaAl$_{11}$O$_{18}$ 복합재료의 인성증진 (Toughening of $Al_2$O$_3$/LaAl$_{11}$O$_{18}$ Composites)

  • 장병국;우상국
    • 한국세라믹학회지
    • /
    • 제35권12호
    • /
    • pp.1266-1273
    • /
    • 1998
  • Al2O3/(5~20vol%)LaAl11O18 composites in which the second phase was dispersed with a elongated grain shape were fabricated using Al2O3 and La2O3 composition by hot-pressing. In order investigate the in-fluence of LaAl11O18 on the toughening of LaAl11O18 on the toughening of Al2O3 matrix composites AE(acoustic emission) analysis was con-ducted together with an evaluation of fracture toughness using of SEPB technique. The degree of AE events occurred in composites were more than those in monolithic alumina. The occurrences of AE event increased with increasing the amount of LaAl11O18 phase in the Al2O3/LaAl11O18 composite is two times higher compared to monolithic alu-mina. The main toughening mechanism was attributed to the bridging of LaAl11O18 grains at tip of pro-pagating crack.

  • PDF

Fabrication of Two-Layered $Al-B_4C$ Composites by Conventional Hot Pressing Uuder Nitrogen Atmosphere and Their Characterization

  • Bedir Fevzi
    • Journal of Mechanical Science and Technology
    • /
    • 제20권7호
    • /
    • pp.1002-1011
    • /
    • 2006
  • In this study, we describe the conventional hot pressing (CHP) of layered $Al-B_4C$ composites and their characterization. The matrix alloy Al-5 wt.%Cu was prepared from elemental powder mixtures. The metal and B4C powders were mixed to produce either $Al-Cu-10vol.%B_4C$ or $Al-Cu-30vol.%B_4C$ combinations. Then, these powder mixtures were stacked as layers in the hot pressing die to form a two-layered composite. Hot pressing was carried out under nitrogen atmosphere to produce $30\times40\times5mm$ specimens. Microstructural features and age hardening characteristics of composites were determined by specimens cut longitudinally. The flexural strength of both layered composites and their monolithic counterparts were investigated via three point bending tests. In the case of layered specimens of both $10vol.%B_4C$ and $30vol.%B_4C$ containing layers were loaded for three-point test. The results show that a homogeneous distribution of $B_4C$ particles in the matrix alloy which is free of pores, can be obtained by CHP method. The ageing behavior of the composites was found to be influenced by the reinforced materials, i.e. higher hardness values were reached in 8 hrs for the composites than that for the matrix alloy. Flexural strength test showed that two-layered composites exhibited improved damage tolerance depending on layer arrangement. Microstructural investigation of the fracture surfaces of the bending specimens was performed by means of scanning electron microscope (SEM). While layer with lower reinforcement content exhibited large plastic deformation under loading, the other with higher reinforcement content exhibited less plastic deformation.

Rheo-compocasting 및 Hot Pressing에 의하여 제조한 $Al-Si-Mg/Al_2O_3$ 단섬유강화 복합재료의 조직 및 인장특성 (Microstructures and Tensile Properties of $A_2O_3$ Short Fiber/Al-Si-Mg Alloy Composites Fabricated by Rheo-compocasting and Hot Pressing)

  • 곽현만;이학주
    • 한국주조공학회지
    • /
    • 제13권6호
    • /
    • pp.547-554
    • /
    • 1993
  • Aluminum alloy matrix composites reinforced with various amounts of $Al_2O_3$ short fibers have been produced by rheo-compocasting accompanied by hot pressing. When composites reinforced with fibers are produced by rheo-compocasting, S-L process is the most effective method for homogeneous dispersion of fibers. A sound composites with the improved orientation(3 dimension${\rightarrow}$2 dimension) of the fibers and increased volume fraction of them have been fabricated through the hot pressing of the casted composites. Fibers are broken down when rheo-compocasting, hot pressing, and $T_6$ treating. Among them fibers are broken down most heavily in the hot pressing. And even in the case of the composite reinforced with 30 vol% fibers, which showed the hardest fiber break down, aspect ratio(11.6) is higher than critical aspect ratio(10.7). The fiber strengthening effect in the composites has showed upto 573K. As the test temperature increases to the range of 573K, the effect has been higher. The fracture of composites is controlled by fiber from room temperature to 473K, but the fracture of composites is controlled by interface between fiber and matrix alloy above 473K.

  • PDF

Al/흑연 압출재를 이용한 Al-Si/흑연 복합재료 제조와 감쇠능 (Manufacturing and Damping Properties of Al-Si/Gr. Composite using extruded Al/Gr. Composite)

  • 박헌범;권혁무
    • 한국주조공학회지
    • /
    • 제21권2호
    • /
    • pp.119-126
    • /
    • 2001
  • Al/15%Gr. composite have been manufactured by mixing, compacting, and extruding aluminium powder and graphite powder. Then, Al-6%Si/x%Gr., Al-12%Si/x%Gr., and Al-18%Si/x%Gr.(x: 0, 2, 4, 6, 8) composites have been manufactured by remelting the extruded materials(Al/15%Gr.), Al-33.3%Si alloy, and Al ingot, etc. We conducted experiments to chracterize the microstructure, and damping properties and hardness. The result of microstructure experiment on Al-x%Si/y%Gr. composites reveals the good dispersion of graphite. As to Al-Si/y%Gr. composites, the more the graphite contents, the less the tensile strength. And the tensile strength varied according to contents of Si: with its highest value in Al-18%Si/y%Gr. composites and lowest in Al-6%Si/y%Gr. composites. As to Al-x%Si/y%Gr. composites, the more the contents of graphite, the more the vibration damping properties. And we can get the highest vibration damping rate in Al-12%Si/y%Gr. composites which matrix structure is an eutectic component.

  • PDF

용탕단조한 $Al/Al_2O_3$ 복합재료에서의 예비성형체 변형 및 섬유열처리 영향 (Preform Deformation and Fiber Heat-Treatment Effect in Squeeze Cast $Al/Al_2O_3$ Metal Matrix Composites)

  • 지동철;정성실;조경목;박익민;김진
    • 한국주조공학회지
    • /
    • 제13권1호
    • /
    • pp.62-70
    • /
    • 1993
  • This study presents the effect of applied pressure on the preform deformation during squeeze casting of $Al_2O_3$ short fiber reinforced aluminum alloy (AC8A) metal matrix composites. A preliminary model based on the general beam theory is suggested for the prediction of the preform deformation. Two different commercially available $Al_2O_3$ short fiber (Saffil, Kaowool) were used to study the influence of the fibers on the microstructure and mechanical properties of the squeeze cast $Al/Al_2O_3$ composites. The composites were fabricated with the applied pressure of 75 MPa which was found to be the optimum condition for the squeeze casting of the composites in this study. For the amorphous Kaowool fiber, hard crystalline Mullite phase was formed with heat treatment. Both of amorphous and the crystallized Kaowool fibers were used to fabricate $Al/Al_2O_3$ composites. Microhardness of crystallized Kaowool fiber revealed higher than that of the amorphous Kaowool fiber in the squeeze cast composites. It was also found that the wear resistance of Kaowool fiber reinforced composites increased with the amount of Mullite.

  • PDF

SiCp입자강화 Al 복합재료에 대한 합금원소의 영향과 시효특성에 관한 연구 (A Study on Ageing Characteristics and Alloy Elements of SiCp Reinforced Al Matrix Composites)

  • 김석원;이의종;우기도;김동건
    • 한국주조공학회지
    • /
    • 제21권1호
    • /
    • pp.7-14
    • /
    • 2001
  • The research on new DRA(discontinuous reinforced alloy) and CRA(continous reinforced alloy) composites has been carried out to improve the properties of ceramic fiber and particle reinforced metal matrix composites(MMCs). Effects of alloying elements and aging conditions on the microstructures and aging behavior of Al-Si-Cu-Mg-(Ni)-SiCp composite have been examined. The specimens used in this study were manufactured by duplex process. The first squeeze casting is the process to make precomposite and the second squeeze casting is the process to make final composite. The hardening behavior was accelerated with decreasing the size of SiCp particle in the composites. It is considered that the dislocation density increased with increasing SiCp size, due to the different thermal deformation between Al matrix and SiCp during quenching after the solution treatment. Peak aging time to obtain the maximum hardness in 3 ${\mu}m$ SiCp reinforced Al composite was reduced than that in large size(5, 10 ${\mu}m$) of SiCp because of difference in dislocation density. Aging hardening responce(${\Delta}H$ = $H_{Max}.-H_{S.T}$) of composites was greater than that of unreinforced Al alloy because of higher density of second phases in matrix.

  • PDF

용융가압함침공정을 이용한 세라믹 입자 강화 철강복합재료의 제조성 검증 (Fabrication of Ceramic Particulate Reinforced Steel Composites by Liquid Pressing Infiltration Process)

  • 조승찬;이영환;고성민;박현재;이동현;신상민;조일국;이상관;이상복
    • Composites Research
    • /
    • 제31권4호
    • /
    • pp.117-121
    • /
    • 2018
  • 본 연구에서는 용융가압함침 공정을 이용하여 TiC, $TiB_2$, $Al_2O_3$ 세라믹 입자가 분산된 SUS431 금속복합재료를 제조하고 미세조직을 분석하여 세라믹 입자에 따른 제조성에 대해 검토하였다. 젖음성이 나쁜 $Al_2O_3$의 경우 내부에 결함이 다수 존재함을 알 수 있었으며, $TiB_2$ 및 TiC 입자 강화 복합재의 경우 상대적으로 결함이 적고 강화재가 균일 분산되었음을 확인하였다. 특히, TiC-SUS431 복합재료의 경우 TiC와 Fe계 기지합금의 우수한 젖음성 및 용융가압함침공정 적용으로 우수한 계면 특성을 가지며 결함이 적고 균일한 미세조직을 가지는 것을 확인하였다.