• Title/Summary/Keyword: Al합금

Search Result 2,431, Processing Time 0.032 seconds

Area Effect on Galvanic Corrosion of Condenser Materials with Titanium Tubes in Nuclear Power Plants (Titanium 전열관을 사용하는 원전 복수기 재료의 Galvanic Corrosion에 미치는 면적의 영향)

  • Hwang, Seong-Sik;Kim, Joung-Soo;Kim, Uh-Chul
    • Nuclear Engineering and Technology
    • /
    • v.25 no.4
    • /
    • pp.507-514
    • /
    • 1993
  • Titanium tubes have recently been used in condensers of nuclear power plants since titanium has very good corrosion resistance to seawater. However, when it is connected to Cu alloys as tube sheet materials and these Cu alloys are connected to carbon steels as water box materials, it makes significant galvanic corrosion on connected materials. It is expected from electrochemical tests that the corrosion rate of carbon steel will increase when it is galvanically coupled with Ti or Cu in sea water and the corrosion rate of Cu will increase when it is coupled with Ti, if this couple is exposed to sea water for a long time. It is also expected that the surface area ratios, R$_1$(surface area of carbon steel/surface area of Ti) and R$_2$(surface area of carbon steel/surface area of Cu) are very important for the galvanic corrosion of carbon steel and that these should not be kept to low values in order to minimize the galvanic corrosion on the carbon steel of the water box. Immersed galvanic corrosion tests show that the corrosion rate of carbon steel is 4.4 mpy when the ratio of surface area of Fe/ surface area of Al Brass is 1 while it is 570 mpy when this ratio is 10$^{-2}$ . The galvanic corrosion rate of this carbon steel is increased from 4.4 mpy to 13 mpy at this area ratio, 1, when this connected galvanic specimen is galvanically coupled with a Ti tube. This can be rationalized by the combined effects of R$_1$ and R$_2$ on the polarization curve.

  • PDF

The study on the quality characteristics factor of medium-sized orbit scroll (중형 선회 스크롤의 품질 특성 인자에 대한 연구)

  • Kim, Jae-Gi;Lim, Jeng-Taek;Kang, Soon-Kook;Park, Jong-Soon
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.17 no.9
    • /
    • pp.718-723
    • /
    • 2016
  • The use of the scroll compressor in the air conditioning of medium-sized vehicles has increased because of its low torque fluctuation, high energy efficiency and low noise. In addition, the main components of the compressor have been changed from steel to aluminum to reduce its weight, following studies on the constituent materials. The processing precision of the fixed scroll and orbiting involute scroll wrap of the scroll compressor must be below $10{\mu}m$. To ensure this, the surface roughness and contour tolerance are measured. To improve the hardness of the orbiting scrolls using aluminum subjected to anodizing treatment and as the base material, we used a sealing treatment and measured the resulting characteristics. The aluminum materials were made of an Al-Mg-Cu based alloy including small amounts of Ni, Fe, and Zn. The surface roughness was less than $3{\mu}m$ and the processing accuracy was within $10{\mu}m$. Also, the hardness of the nanodiamonds with CNTs used in the sealing treatment was more than 450. This was found to improve the hardness of the material by 50% or more compared to the water sealing treatment and there was little difference between the use of carbon nanotubes and nanodiamonds as sealing materials.

Basic Study for Solvent Extraction Separation of Mo from Synthetic Leaching Solution of Inconel713C by Alamine336 (Inconel713C 모사 용액으로부터 Alamine336을 통한 Mo의 용매추출분리를 위한 기초 연구)

  • Park, Sang-ryul;Ahn, Jong-gwan
    • Resources Recycling
    • /
    • v.27 no.4
    • /
    • pp.16-22
    • /
    • 2018
  • Inconel713C which of a commercial Ni super alloy have the compositions of 70 wt.% Ni, 12 wt.% Cr, 6 wt.% Al and 4 wt.% Mo. In this study, solvent extraction has been performed to separate Mo from the synthetic leaching solution, formation of Inconel713C alloy similarly and is found the optimum conditions of recovery of Mo from the leaching solution. The effects of some variables, such as the nature and concentration of the extractants, $H_2SO_4$ concentrations, and the presence of impurities were investigated. The extraction percentage of Mo by Cyanex272 is 96% in the condition of pH 1 and 4% of concentration of Cyanex272 but Alamine336 is 99% in the condition of the range of pH 1 to 4 and 1 wt.% of concentration of Alamine336. In the case of Alamine336, the extraction percentage of Mo is increased by increasing of the concentration of Alamine336. The optimum condition of this experiment is pH 1 in aqueous phase, 1% concentration of Alamine336 and activation ratio of $H_2SO_4$ 1:0.5.

Effect of Re and Ru Addition on the Solidification and Solute Redistribution Behaviors of Ni-Base Superalloys (니켈계 초내열합금의 응고 및 용질원소의 편석 거동에 미치는 레늄 및 루테늄 첨가의 영향)

  • Seo, Seong-Moon;Jeong, Hi-Won;Lee, Je-Hyun;Yoo, Young-Soo;Jo, Chang-Yong
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.11
    • /
    • pp.882-892
    • /
    • 2011
  • The influence of rhenium (Re) and ruthenium (Ru) addition on the solidification and solute redistribution behaviors in advanced experimental Ni-base superalloys has been investigated. A series of model alloys with different levels of Re and Ru were designed based on the composition of Ni-6Al-8Ta and were prepared by vacuum arc melting of pure metallic elements. In order to identify the influence of Re and Ru addition on the thermo-physical properties, differential scanning calorimetry analyses were carried out. The results showed that Re addition marginally increases the liquidus temperature of the alloy. However, the ${\gamma}^{\prime}$ solvus was significantly increased at a rate of $8.2^{\circ}C/wt.%$ by the addition of Re. Ru addition, on the other hand, displayed a much weaker effect on the thermo-physical properties or even no effect at all. The microsegregation behavior of solute elements was also quantitatively estimated by an electron probe microanalysis on a sample quenched during directional solidification of primary ${\gamma}$ with the planar solid/liquid interface. It was found that increasing the Re content gradually increases the microsegregation tendency of Re into the dendritic core and ${\gamma}^{\prime}$ forming elements, such as Al and Ta, into the interdendritic area. The strongest effect of Ru addition was found to be Re segregation. Increasing the Ru content up to 6 wt.% significantly alleviated the microsegregation of Re, which resulted in a decrease of Re accumulation in the dendritic core. The influence of Ru on the microstructural stability toward the topologically close-packed phase formation was discussed based on Scheil type calculations with experimentally determined microsegregation results.

Effect of Alloying Elements on Particulate Dispersion Behavior and Mechanical Properties in TiC Particulate Reinforced Magnesium Matrix Composites (TiC 입자강화 Mg 복합재료에 있어서 입자 분산거동 및 기계적 성질에 미치는 합금원소의 영향)

  • Lim, Suk-Won;Choh, Takao;Park, Yong-Jin
    • Journal of Korea Foundry Society
    • /
    • v.14 no.3
    • /
    • pp.240-247
    • /
    • 1994
  • TiC particulate reinforced magnesium matrix composites were fabricated by melt stirring method. The effect of alloying elements on TiC particulate dispersion into molten magnesium and mechanical properties were investigated. The incorporation time is defined as the time required for dispersion of solid particles into molten metal. The incorporation time of TiC particles into molten pure magnesium was remarkably shorter and the particulated dispersion was more uniform than that of pure aluminum which was reported previously. The incorporation time was, prolonged by the addition of Al, Bi, Ca, Ce, Pb, Sn or Zn. The tensile strength increased and elongation decreased by the addition of Cu or Sn into the matrices and composites. Although, the tensile strength of the matrices and composites increased by alloying with Ca or Ce, the maximum elongation was observed at a content of about 1% for the matrices. By alloying with Zn, the tensile strength increased for the matrices and composites, but the elongation of the matrices increased. The pure magnesium and its alloy matrix composites reinforced with 20vol% TiC have the tensile strength of about 400MPa. This value is compared with the tensile strength of SiC whisker reinforced magnesium matrix composites fabricated by liquid infiltration method at the same volume fraction. There fore, the melt strirring method which has the advantages of simple process is considered to be efficient in fabricating magnesium matrix composites.

  • PDF

Corrosion Analysis and Apatite Forming Ability of Ti and Ti-Alloys in SBF Solution (Ti과 Ti합금의 SBF에서 Apatite 형성 관찰 및 부식거동 테스트)

  • Lee Seung-Woo;Kim Yun-Jong;Choi Je-Woo;Park Joong-Keun;Kim Won-Soo;Kim Taik-Nam
    • Korean Journal of Materials Research
    • /
    • v.15 no.10
    • /
    • pp.671-677
    • /
    • 2005
  • Ti and Ti alloys are known to have excellent corrosion properties, which is an important aspect for biocompability of these implants in human body. In our study, four types of samples (Cp-Ti, Ti-6Al-4V, $0.5wt.\%$ Fe-Ti and ECAP Ti) were tested for their apatite forming ability and corrosion properties. The micropolished samples were treated with 5M NaOH solution at $60^{\circ}C$ for 24 hours. Each samples was gently washed with distilled water and heat-treated at 600"C for 1 hour. The heat-treated samples were soaked in Simulated Body Fluid (SBF) solution at $36.5^{\circ}C$ in an incubator for different period of time. The test revealed that $0.5 wt.\%$ Fe-Ti showing faster apatite growth on the surface (7th day) compared to other samples. Polarization curve test (PCT) was also carried out to determine the corrosion resistance of each samples in SBF solution. ECAP-Ti showed highest corrosion resistance compared to any other samples. $0.5wt.\%Fe-Ti$ showed higher corrosion potential and corrosion current compared to other samples.

Micro-deformation behavior of Brittle Hf-based Metallic Glass during Mechanical Milling (기계적 합금화 공정에 의한 Hf계 비정질 분말의 미세변형거동 관찰)

  • Kim, Song-Yi;Lee, A-Young;Cha, Eun-Ji;Kwon, Do-Hun;Hong, Sung-Uk;Lee, Min-Woo;Kim, Hwi-Jun;Lee, Min-Ha
    • Journal of Powder Materials
    • /
    • v.25 no.3
    • /
    • pp.246-250
    • /
    • 2018
  • In this study, we investigate the deformation behavior of $Hf_{44.5}Cu_{27}Ni_{13.5}Nb_5Al_{10}$ metallic glass powder under repeated compressive strain during mechanical milling. High-density (11.0 g/cc) Hf-based metallic glass powders are prepared using a gas atomization process. The relationship between the mechanical alloying time and microstructural change under phase transformation is evaluated for crystallization of the amorphous phase. Planetary mechanical milling is performed for 0, 40, or 90 h at 100 rpm. The amorphous structure of the Hf-based metallic glass powders during mechanical milling is analyzed using differential scanning calorimetry (DSC) and X-ray diffraction (XRD). Microstructural analysis of the Hf-based metallic glass powder deformed using mechanical milling reveals a layered structure with vein patterns at the fracture surface, which is observed in the fracture of bulk metallic glasses. We also study the crystallization behavior and the phase and microstructure transformations under isothermal heat treatment of the Hf-based metallic glass.

Fabrication Process and Reliability Evaluation of Shape Memory Alloy Composite (형상기억복합재료의 저조공정 및 신뢰성 평가)

  • Lee, Jin-Kyung;Park, Young-Chul;Lee, Kyu-Chang;Choi, Il-Kook;Lee, Joon-Hyun
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.21 no.6
    • /
    • pp.634-641
    • /
    • 2001
  • Shape memory alloy has been used to improve the tensile strength of composite by the occurrence of compressive residual stress in matrix using its shape memory effect. In order to fabricate shape memory alloy composite, TiNi alloy and A16061 were used as reinforcing material and mix, respectively. In this study, TiNi/A16061 shape memory alloy composite was made by using hot press method. However, the specimen fabricated by this method had the bonding problem at the boundary between TiNi fiber and Al matrix when the load was applied to it. A cold rolling was imposed to the specimen to improve the bonding effect. It was found that tensile strength of specimen subjected to cold rolling was more increased than that of specimen which did not underwent cold rolling. In addition, acoustic emission technique was used to quantify the microscopic damage behavior of cold rolled TiNi/A16061 shape memory alloy composite at high temperature.

  • PDF

The latest movement of PVD coating for industrial application (산업용 PVD코팅 기술 최근 동향)

  • Im, Sang-Won
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2016.11a
    • /
    • pp.33-55
    • /
    • 2016
  • PVD(Physical Vapour Deposition)코팅은 70년대 미국의 Multi-arc이란 기업에 의해 질화물계나 탄화물계 피막 증착이 가능한 아크이온플레팅(Arc Ion Plating) 기술이 산업에 소개되어, 주로 내마모나 내구성을 요구하는 금형, 절삭공구, 산업용 부품 분야 등에 적용되면서 꾸준한 성장세를 거듭해 왔다. 최근 들어 PVD기술은 그 수요의 급증과 더불어 보다 진화된 형태의 코팅장치 및 코팅피막들이 산업에 소개 되고 있다. 먼저 절삭가공분야에는 new composition, nano composite, multi-element composition, multi-layer, SML(Self Modification Layer)등의 코팅피막들이 단독 또는 조합된 형태로 개발되어 철계 소재를 대상으로 고경도 소재의 고속가공, 저경도~중경도 소재의 중속~고속 광범위영역에서 동시 절삭을 가능케 하였고, 비철.비금속 소재 절삭용으로 종전의 가스방식의 DLC(a-C:H)코팅을 훨씬 능가하는 ta-C Plus(Ultra super DLC) 코팅이 개발되어 고 Si함량의 Al-Si계 합금, Cu-W계, 고 섬유 CFRP, CFRM 및 반소결 상태의 세라믹 소재들을 황삭에서 정삭까지 단일 공정으로 절삭이 가능한 고성능 공구들이 개발보급되고 있다. 금속 성형분야에는 고장력 강판을 냉간에서 성형 가능한 Lubricative multi-layer coating, 열간 또는 고온에서 성형이 가능한 functional multi layer과 이형성이 더한층 개선된 dimpled(or embossed) functional multi layer 코팅들이 개발되어 산업현장에 빠르게 확산되고 있다. PVD 코팅의 또 다른 주요 적용분야로 의료분야를 들 수 있는데, 이는 코팅의 대다수가 고경도의 생체친화적인 특성을 가진데 착안되었으며, 흔히 현대성 질환이라 일컫는 과민성 체질, 과체중 및 허약체질 환자의 증가와 각종 재해 및 사고의 증가 및 인간 수명 증가에 따른 인공적인 시술의 요구증가에 편승하여 이 분야의 시장 또한 가파르게 성장하고 있다. 또한 대량으로 양산 적용단계에 접어든 자동차 핵심부품들을 비롯해서 각종 산업용, 방산용 기계 부품에도 성능 향상, 내구성 향상, 환경친화성 등 다양한 목적으로 확대 적용되고 있는 사례들을 본 발표를 통해 간략하게나마 소개하고자 한다.

  • PDF

Influences of Process Conditions on the Surface Expansion and Contact Pressure in Backward Can Extrusion of Al Alloys (알루미늄 합금을 이용한 후방압출에 의한 캔 성형시 성형 조건이 표면확장과 접촉 압력에 미치는 영향)

  • Min, K.H.;Seo, J.M.;Koo, H.S.;Vishara, R.J.;Tak, S.H.;Lee, I.C.;Hwang, B.B.
    • Transactions of Materials Processing
    • /
    • v.16 no.7
    • /
    • pp.521-529
    • /
    • 2007
  • This paper is concerned with the analysis on the surface expansion of AA 2024 and AA 1100 aluminum alloys in backward extrusion process. Due to heavy surface expansion appeared usually in the backward can extrusion process, the tribological conditions along the interface between the material and the punch land are very severe. In the present study, the surface expansion is analyzed especially under various process conditions. The main goal of this study is to investigate the influence of degree of reduction in height, geometries of punch nose, friction and hardening characteristics of different aluminum alloys on the material flow and thus on the surface expansion on the working material. Two different materials are selected for investigation as model materials and they are AA 2024 and AA 1100 aluminum alloys. The geometrical parameters employed in analysis include punch corner radius and punch nose angle. The geometry of punch follows basically the recommendation of ICFG and some variations of punch geometry are adopted to obtain quantitative information on the effect of geometrical parameters on material flow. Extensive simulation has been conducted by applying the rigid-plastic finite element method to the backward can extrusion process under different geometrical, material, and interface conditions. The simulation results are summarized in terms of surface expansion at different reduction in height, deformation patterns including pressure distributions along the interface between workpiece and punch, comparison of surface expansion between two model materials, geometrical and interfacial parametric effects on surface expansion, and load-stroke relationships.