• Title/Summary/Keyword: Aging Condition

검색결과 828건 처리시간 0.029초

초내열합금 Haynes 282 주조합금의 크리프강도에 미치는 시효처리의 영향 (Effect of Aging Time on Creep Property of Cast Haynes 282 Superalloy)

  • 김영주;안용식
    • 동력기계공학회지
    • /
    • 제21권6호
    • /
    • pp.13-20
    • /
    • 2017
  • Ni-base superalloy Haynes 282 was developed as a gas turbine material for use in the ultra-super-critical stage (USC) of next-generation coal-fired power plants. Temperatures in the USC stage exceed $700^{\circ}C$ during operation. In spite of its important role Haynes 282 in increasing the performance of high-pressure turbines, as a result of its high-temperature capability, there is little information on the microstructure, deformation mechanism, or mechanical properties of the cast condition of this alloy. The aim of present study is to examine the creep properties of cast alloy and compare with wrought alloy. The ${\gamma}^{\prime}-precipitates$ were coarsen with the increase of aging time ranging from 8 to 48 hrs. A creep test performed at $750^{\circ}C$ showed faster minimum creep rate and shorter rupture lifetime with the aging time. A creep test performed showed only a slight difference in the rupture life between cast and wrought products. Based on the creep test results, the deformation mechanism is discussed using fractographs.

플라스틱 포장재의 잔존 인쇄 용제 감소 방안 (Study about decreasing methods of printing ink solvents residue amounts on plastic food package materials)

  • 안덕준;조훈일
    • 한국포장학회지
    • /
    • 제10권1호
    • /
    • pp.1-6
    • /
    • 2004
  • Amount of residual ink solvent on the packaging materials from Korea, Japan and Europe was measured and compared. The amount of packaging materials from Korea was much higher than that of Japan and Europe. To reduce the residual amounts of ink solvent, aging condition of printed packaging materials including aging time and temperature was modified and evaluated. Aging with high temperature and short time ($60^{\circ}C$ and 24 hours) was more effective for reduction of residual amount of ink solvent than that with low temperature and long time. To find out change of reduction pattern of residual amount of solvent according to plastic packaging material, several monolayer and multilayer packaging materials were selected. Among the monolayer packaging materials, the amount of EVOH and PET was lower than that of polyolefin plastic film including PE and PP. PP/EVOH/PET among the selected multilayer film showed the lowest amount of residual ink solvent on food packaging materials. Result of this research revealed that the residual amount of ink solvent can be reduced by proper selection of aging condition with and by appropriate application of mutilayer plastic film.

  • PDF

비정질 $Fe_{78}B_{13}Si_9$ 합금의 자기적 특성의 경년 열화 (Aging Effect of Magnetic Properties in Amorphous $Fe_{78}B_{13}Si_9$ Alloy)

  • 김기욱;민복기;송재성;홍진완;조현진;이동희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1988년도 춘계학술대회 논문집
    • /
    • pp.49-51
    • /
    • 1988
  • The heat treatment condition and aging behavior of melt spun amorphous $Fe_{78}B_{13}Si_9$(Metglas 26058-2) were studied with investigating its magnetic properties, i.e., Br, $B_l$, Hc. The optimum heat treatment condition was $400^{\circ}C$, 1 hour under the external field of 200e, and aging was due to the surface oxidation and the appearance of local CSRO (chemical short lange order) with time and temperature. In addition. we investigated the effects of the thickness of the amorphous ribbons on the magnetic properties and aging effect of them.

  • PDF

해부생리학 해석을 통한 미용침의 연구 (A Study on Cosmetic Acupuncture Through Anatomy and Physiology Interpretation)

  • 김민식
    • Korean Journal of Acupuncture
    • /
    • 제30권3호
    • /
    • pp.171-177
    • /
    • 2013
  • Objectives : The purpose of this study is to investigate the mechanism of Cosmetic Acupuncture through reinterpretation of anatomy and physiology. Methods : The causes of wrinkle increases and rapid aging of facial skin were studied and the theoretical system of Cosmetic Acupuncture treatment was analyzed through anatomy and physiology reinterpretation. Results and Conclusions : An increase in wrinkles and rapid aging of facial skin is caused by xerosis. Skin condition represents the condition of subcutaneous muscle. The reason why skin becomes easily dry is the heat produced by craniofacial part. Craniofacial part always generates lot of physiological fever because of the muscles. This physiological fever is produced from the muscles that are responsible for maintaining skull suture, controlling the movement of temporomandibular joint, maintaining head and neck posture. Controlling this fever is the crux of Cosmetic Acupuncture mechanism. These muscles correspond to Foot Taeyang meridian-muscle, Foot Soyang meridian-muscle and Foot Yangmyung meridian-muscle. Cosmetic Acupuncture is effective for preventing facial skin from aging and wrinkle increase by mechanical stimulus on facial muscles, and for controlling craniofacial part meridian-muscle system producing the heat.

환경조건에 따른 EPDM 고분자 애자의 누설전류파형과 스펙트럼 분석 (Leakage Current Waveforms and Spectrum Analysis of EPDM Polymer Insulator according to Environment Condition)

  • 박재준;김정부;송영철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 춘계학술대회 논문집 방전 플라즈마 유기절연재료 초전도 자성체연구회
    • /
    • pp.82-86
    • /
    • 2004
  • This research is about the result of leakage current waveform about the situation of surface leakage current and environmental changes(Salt fog, clean fog and rain) by EPDM polymer insulators' amount of salt. The researcher presents the result of changing about fundamental harmonic, 3rd harmonic and 5th harmonic from starting point of supplying power to flashover. In this study, researched environmental affects (clean fog, salt fog and rain) about surface aging of polymer insulators and used frequency spectrum of leakage current waveform to develop the diagnostic technique of surface aging. When amount of salt contents changed, surface aging stage and the degree of aging (distortion factor) about 3rd and 5th harmonic waveform on low frequency harmonic wave. The distortion factor which is harmonic percentage about basic harmonic is important pointer to evaluate the surface condition of polymer insulators.

  • PDF

18 Ni 마르에이징 강의 기계적 성질에 미치는 시효처리의 영향 (Effect of Aging Treatment on the Mechanical Properties of a 18 Ni Maraging Steel)

  • 김학모;김인배;박세윤
    • 열처리공학회지
    • /
    • 제4권1호
    • /
    • pp.30-36
    • /
    • 1991
  • Effects of aging treatment on the mechanical properties of a 18 Ni maraging steel were investigated by considering the reverted austenite. Specimens were heat treated by austenitizing at $840^{\circ}C$ for 1 hr and then aged for various times at $480^{\circ}C$ and $520^{\circ}C$. The main results obtained are as follows : 1) The amounts of reverted austenite are increased up to about 4% at $480^{\circ}C$ and about 22% at $520^{\circ}C$ with 1 to 48 hrs aging time. 2) Decreasing tendencies of impact energy and fracture toughness with increasing aging time are diminished after aging for 2 hrs at two aging temperatures of $480^{\circ}C$ and $520^{\circ}C$. 3) Peak hardness and yield strength are obtained after aging for 4 hrs at $480^{\circ}C$ and 2 hrs at $520^{\circ}C$ respectively. From the above results, it was concluded that the optimum aging condition with which showed good strength and toughness combination are given to be $480^{\circ}C$ for 4 hrs and $520^{\circ}C$ for 2 hrs.

  • PDF

A comprehensive study of the effects of long-term thermal aging on the fracture resistance of cast austenitic stainless steels

  • Collins, David A.;Carter, Emily L.;Lach, Timothy G.;Byun, Thak Sang
    • Nuclear Engineering and Technology
    • /
    • 제54권2호
    • /
    • pp.709-731
    • /
    • 2022
  • Loss of fracture resistance due to thermal aging degradation is a potential limiting factor affecting the long-term (80+ year) viability of nuclear reactors. To evaluate the effects of decades of aging in a practical time frame, accelerated aging must be employed prior to mechanical characterization. In this study, a variety of chemically and microstructurally diverse austenitic stainless steels were aged between 0 and 30,000 h at 290-400 ℃ to simulate 0-80+ years of operation. Over 600 static fracture tests were carried out between room temperature and 400 ℃. The results presented include selected J-R curves of each material as well as K0.2mm fracture toughness values mapped against aging condition and ferrite content in order to display any trends related to those variables. Results regarding differences in processing, optimal ferrite content under light aging, and the relationship between test temperature and Mo content were observed. Overall, it was found that both the ferrite volume fraction and molybdenum content had significant effects on thermal degradation susceptibility. It was determined that materials with >25 vol% ferrite are unlikely to be viable for 80 years, particularly if they have high Mo contents (>2 wt%), while materials less than 15 vol% ferrite are viable regardless of Mo content.

대용량 발전기 고정자 권선의 절연열화 특성 (Characteristics of Insulation Aging in Large Generator Stator Windings)

  • 김희동;이영준;주영호
    • 전기학회논문지
    • /
    • 제58권7호
    • /
    • pp.1375-1379
    • /
    • 2009
  • Insulation tests have been performed on two generator stator bars under accelerated aging under a laboratory environment. Electrical stress was applied to stator bar No.1, and electrical and thermal stresses were applied to stator bar No.2. Nondestructive stator insulation tests including the ac current, dissipation factor($tan{\delta}$), and partial discharge tests have been performed on both bars as the bars were aged for 11460 hours. Experimental test results show that ${\Delta}I$, ${\Delta}tan{\delta}$, and partial discharge of No. 1 and No.2 stator bars increased with increased in aging time. It has been concluded from the test that the stator insulation of the two generators are in good condition.

폴리머 피뢰기 가속열화 방법과 열화특성 분석 (Accelerated aging test method and characteristics analysis of polymer housed surge arresters)

  • 김주용;박철배;권태호;정연하
    • 한국조명전기설비학회:학술대회논문집
    • /
    • 한국조명전기설비학회 2007년도 춘계학술대회 논문집
    • /
    • pp.210-213
    • /
    • 2007
  • In this study accelerated aging test cycle and equipment was developed for aging test of polymer housed surge arresters under domestic weather condition In order to investigate aging characteristics of polymer surge arresters electrical and chemical analysis of the arresters which are used for accelerated aging test and outdoor exposure test were conducted. Through the analysis the capability of the proposed method was verified and characteristics data were presented for maintenance of domestic arresters. Based on these results long term reliability assessment method was proposed for polymer housed distribution surge arresters.

  • PDF

Effects of thermal aging on mechanical properties of laminated lead and natural rubber bearing

  • Kim, Dookie;Oh, Ju;Do, Jeongyun;Park, Jinyoung
    • Earthquakes and Structures
    • /
    • 제6권2호
    • /
    • pp.127-140
    • /
    • 2014
  • Laminated rubber bearing is very popular base isolation of earthquake engineering pertaining to the passive structural vibration control technologies. Rubber used in fabricating NRB and LRB can be easily attacked by various environmental factors such as oxygen, heat, light, dynamic strain, and organic liquids. Among these factors, this study carried out thermal aging test to investigate the effect of thermal aging on the mechanical properties of laminated rubber bearings in accelerated exposure condition of $70^{\circ}C$ temperature for 168 hours. The compressive-shear test was carried out to identify the variation of compressive and shear properties of the rubber bearings before and after thermal aging. In contrast to tensile strength and elongation tests, the hardness of rubber materials showed the increasing tendency dependent on exposure temperature and period. Based on the test results, the property changes of rubber bearing mainly aged by heat are quantitatively presented.