Effect of Cryogenic Treatment on Wear Resistance of STD 11 Steel (STD 11강 마모특성에 미치는 서브제로처리의 영향)

  • Hong, Young Hwan;Song, Keun
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.16 no.3
    • /
    • pp.134-140
    • /
    • 2003
  • Effects of cryogenic treatment and tempering temperature on the amount of retained austenite, hardness and wear properties has been investigated using alloy tool steel, STD 11. Cryogenic treatments were performed at the temperatures of $-100^{\circ}C$, $-150^{\circ}C$ and $-196^{\circ}C$, and tempering were performed at $200^{\circ}C$ and $530^{\circ}C$. It was shown that lower hardness value was obtained on high temperature ($530^{\circ}C$) tempering even after cryogenic treatment. And retained austenite was not entirely transformed to martensite after cryogenic treatment even at $-196^{\circ}C$, which was not consistent with the belief that $-80^{\circ}C$ was sufficient to entirely transform any austenite retained in the quenched microstructure. Austenite retained in cryogenic treated condition was completely transformed to martensite only after tempering at $530^{\circ}C$. As far as wear test conditions in this investigation, it was found that cryogenic treatments improved the sliding wear resistance, but improvement of wear resistance was not directly related with retained austenite contents. And it was found that predominent wear mechanisms of STD 11 steel were oxidation wear and adhesive wear In sliding wear conditions.

Effect of Solution Treatment on Corrosion Behavior of AZ91-2%Ca Magnesium Casting Alloy (주조용 AZ91-2%Ca 마그네슘 합금의 부식 거동에 미치는 용체화처리의 영향)

  • Moon, Jung-Hyun;Jun, Joong-Hwan
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.28 no.4
    • /
    • pp.190-199
    • /
    • 2015
  • The study is intended to investigate the effect of solution treatment on microstructure and corrosion behavior of AZ91(Mg-9%Al-1%Zn-0.3%Mn)-2%Ca casting alloy. In as-cast state, the AZ91-2%Ca alloy consisted of intermetallic ${\beta}(Mg_{17}Al_{12})$, $Al_8Mn_5$ and $Al_2Ca$ phases in ${\alpha}-(Mg)$ matrix. After the solution treatment, Al within the ${\alpha}-(Mg)$ matrix was distributed more homogeneously, along with the slight decrease in the total amount of intermetallic compounds. The corrosion resistance of the AZ91-2%Ca alloy was improved after the solution treatment. The microstructural examinations for the solution-treated samples revealed that the better corrosion resistance may well be related to the incorporation of more oxides and hydroxides such as $Al_2O_3$, $Al(OH)_3$, CaO and $Ca(OH)_2$ into the surface corrosion product without dissolution of the intermetallic phases along the grain boundaries.

Study of wastewater-treatment's efficiency using Bacillus subtilis: with an effect of ozonation (Bacillus subtilis를 이용한 폐수처리 효과연구: 오존의 영향을 중심으로)

  • 박영규
    • Journal of environmental and Sanitary engineering
    • /
    • v.17 no.4
    • /
    • pp.29-38
    • /
    • 2002
  • Advanced oxidation of wastewater was studied with a purpose to remove TOC and color by the ozone-assisted Fenton reaction. The optimal conditions were determined by hydrogen peroxide and ozone concentrations. Experimental results indicate that the ozone treatment after Fentons process was found to provide very efficient removal efficiency in the process, avoiding the exclusive ozone treatment. The combined process of ozone in the Fenton oxidation respectively was increased removal efficiences of 10.7% in comparison with exclusive Fenton oxidation. Also, the treatments of ozone after Fenton's oxidation respectively had increased the removal efficiences of 16.%. As a result, the treatment of ozone after Fentons oxidation had the best removal efficiency of approximately 96%. Removal efficiency of color was significantly increased as mush as 26% by the advanced Fenton's oxidation in comparison with exclusive Fenton's oxidation. The removal efficiencies in the biological treatment using Bacillus subtilis after Fenton's oxidation and after Fenton's and ozone's oxidation were increased by 14% and 19% respectively. Although these combined Bacillus subtilis-assisted Fenton's oxidation was determined to be effective method to treat the dyeing wastewater in an economic point of view, the choice of wastewater treatment can be varied depending on water quality.

A Study on the Advanced Treatment Process Improvement through the Dewatering Application an Expressway Rest Area Individual Sewage Treatment Plant (휴게소 개인하수처리시설의 슬러지 탈수공정 적용에 통한 고도처리 개선 연구)

  • Choi, Yoo Hyun;Joo, Hyun Jong
    • Journal of Korean Society on Water Environment
    • /
    • v.33 no.1
    • /
    • pp.63-69
    • /
    • 2017
  • Small size privately owned wastewater treatment plants have been difficult to treat their wasted sludge and maintain steady effluent quality compared with publicly owned wastewater treatment plants. Therefore, this study has focused on treatment efficiency enhancement, specially nitrogen removal efficiency by recycling dewatering filtrate as an alkalinity additive from filter press using $CaCO_3$. As the result, it was found that the optimal mixing ratio between the excess sludge and $CaCO_3$ was 1:2. The major operation parameters such as specific substrate utilization rate, specific nitrification rate, and specific denitrification rate were also improved 64% ($0.048-0.079mg\;BOD_5/mg\;MLVSS{\cdot}day$), 35% ($0.020-0.027mg\;NH_3-N/mg\;MLVSS{\cdot}day$) and 68% ($0.051-0.086mg\;NO_3{^-}-N/mg\;MLVSS{\cdot}day$), respectively, after the adoption of new methods. Therefore, both the problem of sludge treatment at small scale plants and the need for efficiency improvement could be solved.

Characterization of Microbial Fermented Cellulose Porous Foam Prepared by Radiation Treatment (방사선 이용 미생물 발효 셀룰로오스 다공성 폼 제조 및 특성)

  • Gwon, Hui-Jeong;Shin, Young Min;Choi, Jong-Bae;Lim, Jong-Young;Jeong, Jin-Oh;Jeong, Sung In;Park, Jong-Seok;Kim, Jin Kyu;Lim, Youn-Mook;Choi, Young-Hun;Kim, Sang-Suk
    • Korean Journal of Environmental Biology
    • /
    • v.31 no.4
    • /
    • pp.302-307
    • /
    • 2013
  • Microbial fermented cellulose gel, citrus gel (CG), was successfully fabricated to porous foam by radiation treatment and freeze drying. The chemically induced radiation was used to create highly porous foam and further freeze drying of the CG produced tough foams with interconnected open pores for use in tissue engineering. The microstructure of the CG foam was controlled by varying the irradiation dose and quenching temperature with pore size ranging from several microns to a few hundred microns. Tensile strength and Gurley value of the CG foam were influenced by irradiation dose. These radiation induced CG foams are promising scaffolds for tissue engineering.

Study on the Detoxification of Asbestos-Containing Wastes (ACW) Using SiC Plate (SiC 플레이트를 이용한 석면 함유 폐기물의 무해화 연구)

  • Hong, Myung Hwan;Choi, Hyeok Mok;Joo, So Young;Lee, Chan Gi;Yoon, Jin-Ho
    • Resources Recycling
    • /
    • v.29 no.1
    • /
    • pp.35-42
    • /
    • 2020
  • Even asbestos-containing waste (ACW) are highly harmful to humans, it continues being produced due to the massive disposal of asbestos-containing products. A development of asbestos detoxification and recycling technologies is required. Heat treatment using microwave is the most efficient method for ACW detoxification. However, microwave heat treatment method has the limitation that asbestos does not absorb microwave at room temperature. That is why, in this study, ACW was detoxified by microwave heat treatment adding the ACW between SiC plates, which are inorganic heating elements that absorb microwaves at room temperature. In order to improove the heat transfer, ACW was crushed and pulverized and then heated using microwave. Microwave heat treatment temperature and time variables were adjusted to investigate the detoxification properties according to heat treatment conditions. After heat treatment, treated ACW was analyzed for detoxification properties through crystal structure and microstructure analysis using X-ray diffraction (XRD) and scanning electron microscopy (SEM). Microwave heat treatment method using SiC plate can be heated up to the target temperature within a short time. Finally, complete asbestos detoxification was confirmed from the crystal structure and the microstructure when the microwave heat treatment was performed at 1,200℃ for at over 60 minutes and at 1,300℃ for at over 10 minutes.

Effect of Post Heat Treatment Temperature on Interface Diffusion Layer and Bonding Force in Roll Cladded Ti/Mild steel/Ti Material (압연 클래드된 Ti/Mild steel/Ti 재의 계면확산층과 접합력에 미치는 후열처리온도의 영향)

  • Lee, Sangmok;Kim, Su-Min;We, Se-Na;Bae, Dong-Hyun;Lee, Geun-An;Lee, Jong-Sup;Kim, Yong-Bae;Bae, Dong-Su
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.4
    • /
    • pp.316-323
    • /
    • 2012
  • The aim of this study is to investigate the effect of post heat treatment on bonding properties of roll cladded Ti/MS/Ti materials. First grade Ti sheets and SPCC mild steel sheets were prepared and then Ti/MS/Ti clad materials were fabricated by a cold rolling and post heat treatment process. Microstructure and point analysis of the Ti/MS interfaces were performed using the SEM and EDX Analyser. Diffusion bonding was observed at the interfaces of Ti/MS. The thickness of the diffusion layer increased with post heat treatment temperature and the diffusion layer was verified as having $({\epsilon}+{\zeta})+({\zeta}+{\beta}-Ti)$ intermetallic compounds at $700^{\circ}C$ and an $({\zeta}+{\beta}-Ti)$ intermetallic compound at $800^{\circ}C$, respectively. The micro Knoop hardness of mild steel decreased with post heat treatment temperature; however, those of Ti decreased at a range of $500{\sim}600^{\circ}C$ and showed a uniform value until $800^{\circ}C$ and then increased rapidly up to $900^{\circ}C$. The micro Knoop hardness value of the diffusion layer increased up to $700^{\circ}C$ and then saturated with post heat treatment. A T-type peel test was used to estimate the bonding forces of Ti/Mild steel interfaces. The bonding forces decreased up to $800^{\circ}C$ and then increased slightly with post heat treatment. The optimized temperature ranges for post heat treatment were $500{\sim}600^{\circ}C$ to obtain the proper formability for an additional plastic deformation process.