• 제목/요약/키워드: Active alumina

검색결과 65건 처리시간 0.023초

활성 알루미나 겔을 혼입한 고로슬래그 경화체의 실내오염물질 흡착 특성 (Adsorption Properties of Indoor Air Pollutants in Blast Furnace Slag Matrix with Active Alumina Gel)

  • 박채울;이상수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2019년도 추계 학술논문 발표대회
    • /
    • pp.29-30
    • /
    • 2019
  • The indoor air quality of modern people who work indoors more than 80 percent a day has also become a very important factor in their lives. But most indoor air quality is highly polluted due to energy conservation and lack of ventilation. This can lead to pneumonia, asthma and even lung cancer, which can be fatal to children, the elderly and the elderly. Indoor pollutants are caused by boards, wallpaper, paint, etc. used in interior By producing indoor finishing materials using active alumina gel, which is used as dehumidifier, indoor pollutants will be reduced and the possibility of developing respiratory diseases and lung cancer will be reduced.

  • PDF

Fourier Transform Raman Studies of Methyl Red Adsorbed on γ-Alumina and Silica-Alumina

  • Park, Sun-Kyung;Lee, Choong-Keun;Min, Kyung-Chul;Lee, Nam-Soo
    • Bulletin of the Korean Chemical Society
    • /
    • 제25권12호
    • /
    • pp.1817-1821
    • /
    • 2004
  • Fourier transform Raman spectra of methyl red adsorbed on untreated and pretreated ${\gamma}$-alumina and silicaalumina calcined at 900 $^{\circ}C$ under 1 atm steam flowing were recorded. Spectral analysis shows that the active species adsorbed on ${\gamma}$-alumina was to be deprotonated methyl red, and on silica-alumina to be di-protonated. This indicates that ${\gamma}$-alumina adapted in this work holds Bronsted basicity, and silica-alumina Bronsted acidity. Raman intensities of methyl red on pretreated ${\gamma}$-alumina are about three times stronger than on untreated ${\gamma}$-alumina, while spectral features are unchanged. For silica-alumina, spectral features show modified vibrational characteristics upon surface hydroxylations generated from pretreatment. Consequently, the acidity loss for silica-alumina and the basicity gain for ${\gamma}$-alumina were observed by increasing the surface hydroxyl groups on the catalysts through pretreatment of the steam calcination.

낮은물/알루미나 비에서 비정질 알루미나 분말의 수화특성 (The Rehydration Properties of Amorphous Alumina Powder in Low Water/Alumina Ratio)

  • 박병기;서정권;이정민;서동수
    • 한국세라믹학회지
    • /
    • 제35권10호
    • /
    • pp.1085-1093
    • /
    • 1998
  • Amorphous alumina powder prepared by the fast calcination of aluminum trihydroxide(Al(OH)3 gibbsite) for 0.5 second at 580$^{\circ}C$ was investigated rehydration propeties. Phase composition crystal size and mor-phology surface area pore volume and pore size distribution of pesudo-boehmite and bayerite crystals changed with temperature time water/alumina ratio and particle size when amorphous alumina rehydrated with water. Phase compositions were examined with XRD and DTA and crystal sized morphologies were investigaed with SEM and TEM. Also rehydration properties of amorphous alumina were in-vestigated by measuring the surface area pore volume and pore size distribution.

  • PDF

알루미나에 생체유리의 코팅시 결합의 특성 (Bonding Behavior of Bioglass Coated Alumina)

  • 김정구;김철영
    • 한국세라믹학회지
    • /
    • 제27권7호
    • /
    • pp.925-933
    • /
    • 1990
  • The possible use of bioglass,, which is one of the surface active biomaterials, as implants materials has drawn great attention due to their ability to bond to human living tissue. In the present work, the investigation was carried out to find the bonding phenomena between alumina substrate and bioglass(45S5) or fluorine-containing bioglass(45S5$.$4F), and the properties of coated bioglass. The stable bonding between alumina and bioglass was formed when heat-treated at 1150$^{\circ}C$ for 120 minutes or at 1250$^{\circ}C$ for 30 minutes for the 45S5, and at 1150$^{\circ}C$ for 30 minutes for the 45S5$.$4F. When bioglass coated alumina was heat-treated, great amount of Al was diffused into bioglass from alumina substrate. More Al was diffused into fluorine-containing bioglass than into bioglass without fluorine. At early stage of heat-tretment, the diffused alumina content was increased with the square root of time and it was also increased with the thickness of coating layer and heat-treatment temperatures. The alumina content became constant after its saturation for longer heat-treatment time. Coated bioglasses were crystallized to Na2O$.$CaO$.$3SiO2 when heat-treated at lower temperature, and to CaO$.$SiO2 at higher temperature.

  • PDF

Bauxite로부터 습식 산처리법에 의한 알루미나 분체의 제조 및 그 이용에 관한 연구(III) : Aluminum Hydrate Gel의 분산에 의한 알루미나 분체의 소결성 향상 (A Study on the Preparation of Alumina Powders from Bauxite by Wet Acid Process and Their Utilization (III) : Effects of the Dispersion of Aluminum Hydrate Gel on the Sintering Behavior of Alumina Powder)

  • 조철구;정원도;배원태
    • 한국세라믹학회지
    • /
    • 제30권4호
    • /
    • pp.299-308
    • /
    • 1993
  • Dispersant was used to avoid the agglomeration of aluminum hydrate precipitate and improve the sinterability of calcined alumina powder. The mean particle size of the aluminum hydrate precipitates was 0.26${\mu}{\textrm}{m}$ and 0.44${\mu}{\textrm}{m}$ when ball-milled with and without dispersant, respectively. After calcination at 110$0^{\circ}C$ for 5 hours, the size of the alumina powder without dispersant increased to 0.84${\mu}{\textrm}{m}$, while with dispersant slightly decreased to 0.22${\mu}{\textrm}{m}$. The most thermally active alumina powder was obtained from the sample calcined at 110$0^{\circ}C$ for 5 hours with the 1% dispersant concentration. Using the calcined alumina powder at the above optimized condition, the specimen showed fired density of 3.94g/㎤, 4-point MOR of 364MPa, and KIC of 3.26MPam1/2 after sintered at 155$0^{\circ}C$ for 3 hours.

  • PDF

초미립 WC-Graphene-Al2O3 복합재료 소결 및 기계적 성질 (Mechanical Properties and Sintering of Ultra Fine WC-Graphene-Al Composites)

  • 손인진
    • 열처리공학회지
    • /
    • 제36권4호
    • /
    • pp.206-214
    • /
    • 2023
  • Tungsten carbide has many industrial applications due to its high electrical and thermal conductivity, high melting temperature, high hardness and good chemical stability. Because tungsten carbide is difficult to sinter, it is sintered with nickel or cobalt as a binder and is currently used in nozzles, cutting tools, and molds. Alumina is reported to be a viable binder for tungsten carbide due to its higher oxidation resistance and lower cost than nickel and cobalt. The ultrafine tungsten carbide-graphene-alumina composites were rapidly sintered in a high frequency induction heating active sintering unit. The microstructure and mechanical properties (fracture toughness and hardness) of the composites were investigated and analyzed by Vickers hardness tester and electron microscope. Since the high-frequency induction heating sintering method enables high-speed sintering, ultrafine composites can be prepared by preventing grain growth. In the tungsten carbide-graphene-alumina composites, the grain size of tungsten carbide increased with the amount of alumina participation. The hardness and fracture toughness of the tungsten carbide-5% graphene- x% alumina (x = 0, 5, 10,15) composites were 5.1, 8.6, 8.6, and 8.4 MPa-m1/2 and 2384, 2168, 2165, and 2102 kg/mm2, respectively. The fracture toughness increased without a significant decrease in hardness. Sinterability was improved by adding alumina to tungsten carbide-graphene.

알루미나에 코팅된 불화물 생체유리에의 수산화 아파타이트 형성 (Hydroxyapatite Formation on Fluoride Bioactive Glasses coated on Alumina)

  • 안현수;이은성;김철영
    • 한국세라믹학회지
    • /
    • 제36권10호
    • /
    • pp.1087-1093
    • /
    • 1999
  • Bioglass which is one of the surface active bionmaterials has a good biocompatibility but a poor mechanical strength, In the present work therefore two types of fluoride-containing bioglasses were coated on an alumina to improve mechanical strength. Crystallization of the coating layer and the hydroxyapatite formation on the bioactive glass coatings in tris-buffer solution were studied. When bioactive glass coated alumina was heat-treated Na2CaSi3O8 crystal was formed on the layer at lower temperature while wollastonite(CaSIO3) was obtained at higher temperature. Hydroxyapatite forming rate on the coating layer with Na2CaSi3O8 crystal was delayed with SiO2 contents in glass composition. However the hydroxyapatite was developed in 20minutes regardless SiO2 contents when the coating layer crystallized into wollastonite. More amount of P3+ ions were leached out of the coating layer with wollastonite than that with Na2CaSi3O8 crystal while Na+ and Ca2+ ions were leached out more easily from the Na2CaSi3O8 crystal containing coating layer.

  • PDF

Vapor-Phase Chlorination of Chlorobenzene over Solid-Acid Catalysts

  • 장향자;최평호;박상언
    • Bulletin of the Korean Chemical Society
    • /
    • 제16권6호
    • /
    • pp.507-511
    • /
    • 1995
  • Catalytic chlorination of chlorobenzene was studied in vapor phase using various solid-acid catalysts such as silica-alumina, alumina, zeolite and a modified clay prepared by impregnating bentonite with ferric chloride. The conversions of both chlorine gas and chlorobenzene showed high over silica-alumina, alumina and modified clay catalysts. However relatively large amounts of polychlorinated benzene derivatives were also observed. The active species of catalytic activity in chlorination of chlorobenzene in vapor phase were proved to be as Lewis acid sites by in-situ IR experiments. The strength of Lewis acid sites which were effective for the vapor-phase chlorination seemed to be having Hammett acidity Ho >-3.0. The selectivity to dichlorobenzenes was proved to be high over the zeolite catalyst due to their shape-selective properties. p-Dichlorobenzene or dichlorobenzene selectivities were improved more or less by changing the reaction conditions.

수열법에 의한 Fe2O3 담지 감마알루미나 촉매제조 (Preparation of Fe2O3 Supported γ-alumina Catalyst by Hydrothermal Method)

  • 박병기;이정민;서동수
    • 한국세라믹학회지
    • /
    • 제40권7호
    • /
    • pp.683-689
    • /
    • 2003
  • 비정질알루미나와 기공형성제를 물과 혼합하여 원통형으로 성형하고 수화, 건조 및 소성하여 ${\gamma}$-alumina pellet을 제조하였다. 이를 Fe(NO$_3$)$_3$.9$H_2O$$CH_3$COOH, HNO$_3$ 또는 $CH_3$COOH와 HNO$_3$의 혼합용액에 침척시켜 20$0^{\circ}C$ 온도로 3시간 수열처리 한 다음 결정의 형태 및 변화, 기공특성, $N_2$ 흡/탈착특성, 산점변화 및 기계적 강도 등을 조사하였다. 제조방법에 따라서 0.1~0.3 $mu extrm{m}$ 크기의 작은 결정이 0.5~2 $\mu\textrm{m}$ 길이의 큰 침상결정으로 형태가 변했고, 결정구조는 의사베마이트 또는 ${\gamma}$-alumina 구조를 나타냈다. ${\gamma}$-alumina pellet에 Fe(NO$_3$)$_3$.9$H_2O$$CH_3$COOH 용액을 침적시켜 수열처리 했을 때 촉매와 반응물간의 물질전달이 용이한 100~1000 $\AA$ 사이의 기공부피가 0.34 ㏄/g에서 0.86 ㏄/g으로 크게 증가하였다. 기공크기의 증가로 인해 질소 흡.탈착이 원활히 이루어짐을 알 수 있었으며, C-H 그룹의 관능기를 흡착할 수 있는 새로운 활성점이 형성되었다. 또한 촉매의 기계적 강도도 1.06 ㎫에서 1.36 ㎫로 증가하였다.

Catalytic Dehydration of Methanol to Dimethyl Ether (DME) over Solid-Acid Catalysts

  • Jun, Ki-Won;Lee, Hye-Soon;Rho, Hyun-Seog;Park, Sang-Eon
    • Bulletin of the Korean Chemical Society
    • /
    • 제23권6호
    • /
    • pp.803-807
    • /
    • 2002
  • The conversion of dimethyl ether(DME) has been carried out over $\gamma-alumina$, silica-alumina, and modified $\gamma-aluminal$ catalysts. Especially, the water effect has been investigated on purpose to develop a suitable catalyst for one-step synthesis of DME from $CO_2$ hydrgenation, The $\gamma-Al_2O_3$ modified with 1 wt% silica is more active and less deactivated by water than unmodified one. $CO_2has$ no effect on catalytic dehydration of methanol to DME.