Azomethine Yilde Forming Photoreaction of N-(Tributylstannyl)methylphthalimide (N-(트리부틸스탄일)메틸프탈이미드의 아조메틴 일리드 형성 광화학 반응)

  • Jeong, Ho-Cheol;Park, Ki-Hyun;Park, Hea-Jung;Cho, Dae-Won;Yoon, Ung-Chan
    • Journal of the Korean Chemical Society
    • /
    • v.53 no.3
    • /
    • pp.302-307
    • /
    • 2009
  • Investigation was conducted to examine whether photochemical reaction of N-(tributylstannyl)- methylphthalimide generates an azomethine ylide intermediate in its excited state as its silyl derivative N-(trimethylsilyl)methylphthalimide which has been observed to form an azomethine ylide. The irradiation of N-(tributylstannyl)methylphthalimide in $D_2O-CH_3$CN generates mono-deuterated N-methylphthalimide as an exclusive product which supports the efficient generation of azomethine ylide intermediate and its trapping by water molecule through a proto-destannylation pathway. However the generated tributylstannyl subsitiuted ylide was not observed to be trapped with a dipolarophile such as methyl acrylate and acrylonitrile present in the reactions which is in contrast with the ylide from N-(trimethylsilyl)methylphthalimide.

Synthesis and Optical Properties of Acrylic Copolymers Containing AlQ3 Pendant Group for Organic Light Emitting Diodes

  • Kim, Eun-Young;Myung, Sung-Hyun;Lee, Young-Hee;Kim, Han-Do
    • Clean Technology
    • /
    • v.18 no.4
    • /
    • pp.366-372
    • /
    • 2012
  • Three acrylic copolymers containing tris(8-hydroxyquinoline) aluminum (AlQ3) pendant group (25 wt%), acrylateco-HEMA-$AlQ_3$ (25 wt%), were successfully synthesized by free radical polymerization from acrylates [methyl methacrylate (MMA), acrylonitrile (AN) or 2-hydroxyethyl methacrylate (HEMA)] with HEMA functionalized with AlQ3 pendant groups (HEMA-p-$AlQ_3$). The glass transition temperatures ($T_g$) of MMA-co-HEMA-p-$AlQ_3$ (copolymer 1), AN-co-HEMA-p-$AlQ_3$ (copolymer 2) and HEMA-co-HEMA-p-$AlQ_3$ (copolymer 3) were found to be 158, 150 and $126^{\circ}C$, respectively. They have good thermal stability: a very desirable feature for the stability of OLEDs. Their solubility, thermal properties, UV-visible absorption and photoluminescence behaviors were investigated. They were found to be soluble in various organic solvents such as tetrahydrofuran (THF), dimethylformamide (DMF), toluene and chloroform. It was also found that the UV-visible absorption and photoluminescence behaviors of these copolymers were similar to those of pristine $AlQ_3$. Green organic light-emitting diodes (OLEDs) have also been fabricated using these copolymers as light emission/electron transport components obtained easily by spin coating, and their current density voltage (J-V) curves were compared. The OLED device of the copolymer 3 had the lowest turn-on voltage of about 2 V compared to other copolymer types devices.

Studies on the Separation of Uranium from Seawater by Composite Fiber Adsorbents(2)(Characterization of Adsorption-Desorption) (복합재료 섬유흡착제를 이용한 해수로부터 우라늄 분리에 관한 연구(2)(흡-탈착 특성))

  • Hwang, Taek-Seong;Park, Jeong-Gi;Hong, Seong-Gwon;Sin, Hyeon-Taek;No, Yeong-Chang
    • Korean Journal of Materials Research
    • /
    • v.6 no.8
    • /
    • pp.761-767
    • /
    • 1996
  • The composite fiber adsorbents containing amidoxime group were prepared and separation properties of uranium ion from seawater were investigated. The amount of uranium adsorption was increased with an increase in adsorption time. When the mole ratio of monomer and comonomer, such as acrylonitrile (AN), tetraethyleneglycol dimethacrylate(TEGMA), and divinylbenzene (DVB), were 1 :0. 1 :0.003, this resin showed the maximum adsorption ability for uranium at a level of pH 8. The amount of uranium adsorption was also increased linearly to one hour with an increase in the content of adsorbent which was added in the composite fiber adsorbents(CFA). The maximum adsorption for uranium of CF A showed at $25^{\circ}C$. Hence, the adsorption ability of CF A for calcium and magnecium ions were increased gradually by the recycling of adsorption and disorption, the adsorption content of their on were 0.3, 0.9mmole/g-adsorbents, respectly. It also showed that the adsorption contents of Ca and \1g ions were much lower than them of uranium. The desorption of uranium on the CF A was carried out , bout 100% within 30min, and the desorption rate of various CF A were equalled.

  • PDF

Effects of Metal Oxide Addition on Co-pyrolysis of PVC and ABS Mixtures (PVC와 ABS 혼합물의 공열분해에 대한 금속산화물의 첨가 효과)

  • Kim, Hee Taik;Choung, Youn Wook;Lee, Hae Pyeong
    • Applied Chemistry for Engineering
    • /
    • v.16 no.2
    • /
    • pp.296-303
    • /
    • 2005
  • The co-pyrolysis characteristics of polyvinylchloride (PVC) and acrylonitrile butadiene styrene (ABS) mixtures with various mixing ratios and effect of addition of CaO and $Cu_2O$ have been studied using thermogravimetry (TG) and gas chromatograph-mass spectrometry (GC-MS). In an isothermal decomposition conducted at $500^{\circ}C$, the yields of styrene monomers and aromatic compounds increased as the mixing ratio of ABS increased, and the yield of BTX compounds reached its maximum (16.14%) when the mixing ratios of PVC and ABS was 4:1. In an isothermal decomposition added with metal oxides, the maximum yield of liquid product was 73% when CaO [CaO/(PVC+ABS)=0.4] was added and it was 70% when $Cu_2O$ [$Cu_2O$/(PVC+ABS)=0.4] was added, respectively, where HCl contained in the gaseous product was completely removed when added with CaO [CaO/(PVC+ABS)=0.5] and $Cu_2O$ [$Cu_2O$/(PVC+ABS)=1.0]. Therefore, to obtain the highest yield of liquid product it appears to be the reaction condition: the reaction temperature of $500^{\circ}C$ and mixing ratios of CaO and $Cu_2O$ are 0.5 and 1.0, respectively.

Obtaining Informed Consent Using Patient Specific 3D Printing Cerebral Aneurysm Model

  • Kim, Pil Soo;Choi, Chang Hwa;Han, In Ho;Lee, Jung Hwan;Choi, Hyuk Jin;Lee, Jae Il
    • Journal of Korean Neurosurgical Society
    • /
    • v.62 no.4
    • /
    • pp.398-404
    • /
    • 2019
  • Objective : Recently, three-dimensional (3D) printed models of the intracranial vascular have served as useful tools in simulation and training for cerebral aneurysm clipping surgery. Precise and realistic 3D printed aneurysm models may improve patients' understanding of the 3D cerebral aneurysm structure. Therefore, we created patient-specific 3D printed aneurysm models as an educational and clinical tool for patients undergoing aneurysm clipping surgery. Herein, we describe how these 3D models can be created and the effects of applying them for patient education purpose. Methods : Twenty patients with unruptured intracranial aneurysm were randomly divided into two groups. We explained and received informed consent from patients in whom 3D printed models-(group I) or computed tomography angiography-(group II) was used to explain aneurysm clipping surgery. The 3D printed intracranial aneurysm models were created based on time-of-flight magnetic resonance angiography using a 3D printer with acrylonitrile-butadiene-styrene resin as the model material. After describing the model to the patients, they completed a questionnaire about their understanding and satisfaction with aneurysm clipping surgery. Results : The 3D printed models were successfully made, and they precisely replicated the actual intracranial aneurysm structure of the corresponding patients. The use of the 3D model was associated with a higher understanding and satisfaction of preoperative patient education and consultation. On a 5-point Likert scale, the average level of understanding was scored as 4.7 (range, 3.0-5.0) in group I. In group II, the average response was 2.5 (range, 2.0-3.0). Conclusion : The 3D printed models were accurate and useful for understanding the intracranial aneurysm structure. In this study, 3D printed intracranial aneurysm models were proven to be helpful in preoperative patient consultation.

Polyacrylonitrile based Copolymer Synthesis and Precursor Fiber Spinning for Manufacturing High-performance Carbon Fiber (고성능 탄소섬유 제조를 위한 폴리아크릴로니트릴 기반 공중합 고분자 합성 및 전구체 섬유 방사)

  • Ju, Hyejin;Han, Minjung;Song, Kyunghyun;Jeon, Changbeom;Jeong, Hwakyung;Kim, Min Jeong;Chae, Han Gi
    • Composites Research
    • /
    • v.35 no.2
    • /
    • pp.115-119
    • /
    • 2022
  • The performance of carbon fiber is important for the production of these high-quality polymer composite materials such as CFRP (Carbon Fiber Reinforced Plastic). For this purpose, it is essential to use an optimized spinning process for improving the mechanical, physical, and structural properties of the precursor fiber, which greatly affects the properties of the carbon fiber, and the use of a suitable precursor polymer. In this study, the content of MAA (Methacrylic Acid), MAA injection time, and concentration of AIBN (2,2'-Azobis(2-methylpropionitrile)) were set as parameters for the polymer synthesis process, and Poly(AN-co-MAA) (poly(acrylonitrile-co-methacrylic acid)) was polymerized by solution polymerization. Poly(AN-co-MAA) with a molecular weight of 305,138 g/mol and an MAA ratio of 4.2% was dissolved in DMF (N,N-dimethylformamide) at a concentration of 16.0 wt%, and then a precursor fiber was prepared through dry-jet-wet spinning. The precursor fiber had a tensile strength of ~1.06 GPa and a tensile modulus of ~22.01 GPa, and no voids and structural defects were observed on the fiber.

Effect of Mechanical and Toughening Characteristics of Epoxy/Carbon Fiber Composite by Polyamide 6 Particles, CTBN Addition Technology (Polyamide 6 입자 및 CTBN 첨가 기술에 따른 에폭시/탄소섬유 복합재의 강인화 효과 및 기계적 특성)

  • Sung-Youl Bae;Kyo-Moon Lee;Sanjay Kumar;Ji-Hun Seok;Jae-Wan Choi;Woo-Hyuk Son;Yun-Hae Kim
    • Composites Research
    • /
    • v.36 no.5
    • /
    • pp.355-360
    • /
    • 2023
  • Epoxy-based carbon fibers reinforced plastic (CFRP) exhibit limitations in their suitability for industrial applications due to high brittleness characteristics. To address this challenge, extensive investigations are underway to enhance their toughness properties. This research focuses on evaluating the toughening mechanisms achieved by Polyamide 6 particles(p-PA6) and Carboxyl-Terminated Butadiene-Acrylonitrile (CTBN) elastomer, with a specific emphasis on utilizing minimal additive quantities. The study explores the impact of varying concentrations of p-PA6 and CTBN additives, namely 0.5, 1, 2.5, and 5 phr, through comprehensive Mode I fracture toughness and tensile strength analyses. The inclusion of p-PA6 demonstrated improvements in toughness when introduced at a relatively low content of 1phr. This improvement manifested as a sustained fracture behavior, contributing to enhanced toughness, while simultaneously maintaining the material's tensile strength. Furthermore, the investigation revealed that the incorporation of p-PA6 affected in particle aggregation, thus influencing the overall toughening mechanism. Incorporation of CTBN, an elastomeric modifier, exhibited a pronounced increase in fracture toughness at higher concentrations of 2.5 phr and beyond. However, this increase in toughness was accompanied by a reduction in tensile strength, resulting in fracture behavior similar to conventional CFRP exhibiting brittleness. The synergy between pPA6, CTBN and CFRP appeared to marginally enhance tensile strength under specific content conditions. As a result of this study, optimized conditions for the application of the p-PA6, CTBN toughening technology have been identified and established.

Structure Analysis and Scale Model Test for Strength Performance Evaluation of Submersible Mooring Pulley Installed on Floating Offshore Wind Turbine (부유식 해상풍력발전기용 반잠수식 계류 풀리의 강도 성능평가를 위한 구조해석과 축소 모형시험)

  • Chang-Yong Song
    • Journal of the Korean Society of Marine Environment & Safety
    • /
    • v.29 no.5
    • /
    • pp.479-487
    • /
    • 2023
  • Recently, the destructive power of typhoons is continuously increasing owing to global warming. In a situation where the installation of floating wind turbines is increasing worldwide, concerns about the huge loss and collapse of floating offshore wind turbines owing to strong typhoons are deepening. A new type of disconnectable mooring system must be developed for the safe operation of floating offshore wind turbines. A new submersible mooring pulley considered in this study is devised to more easily attach or detach the floating of shore wind turbine with mooring lines compared with other disconnectable mooring apparatuses. To investigate the structural safety of the initial design of submersible mooring pulley that can be applied to an 8MW-class floating type offshore wind turbine, scale-down structural models were developed using a 3-D printer and structural tests were performed on the models. For the structural tests of the scale-down models, tensile specimens of acrylonitrile butadiene styrene material that was used in the 3-D printing were prepared, and the material properties were evaluated by conducting the tensile tests. The finite element analysis (FEA) of submersible mooring pulley was performed by applying the material properties obtained from the tensile tests and the same load and boundary conditions as in the scale-down model structural tests. Through the FEA, the structural weak parts on the submersible mooring pulley were reviewed. The structural model tests were conducted considering the main load conditions of submersible mooring pulley, and the FEA and test results were compared for the locations that exceeded the maximum tensile stress of the material. The results of the FEA and structural model tests indicated that the connection structure of the body and the wheel was weak in operating conditions and that of the body and the chain stopper was weak in mooring conditions. The results of this study enabled to experimentally verify the structural safety of the initial design of submersible mooring pulley. The study results can be usefully used to improve the structural strength of submersible mooring pulley in a detailed design stage.