• Title/Summary/Keyword: Abnormal grain growth

Search Result 132, Processing Time 0.037 seconds

Effects of $SiO_2$ and Seed on Ba-ferrite Synthesized by Molten Salt (용융염법으로 합성한 Ba-ferrite의 $SiO_2$ 및 Seed 첨가 효과)

  • 김영근;이승관;김현식;오영우
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1996.11a
    • /
    • pp.326-329
    • /
    • 1996
  • In order to synthesize Ba-ferrite fine particles by molten salt method and inhibit the abnormal grain growth of sintered specimen, KCI anti NaCl were added to basic composition to 50% by weight, and added 1 male% of $SiO_2$ to control the shape of Ba-ferrite particles. $H_{c}$ and $M_{r}$ were decreased when F $e^{3+}$ was substituted with $Co_{2+}$ and $Ti_{4+}$ from x=0 to x=1.0 in $BaFe_{12-2x}$ $Ti_{x}$ $Co_{x}$ $O_{19}$ , and 1 mole% $SiO_2$ increased the size but shortened c-axis of hexagonal ferrite. Seeds added in Ba-ferrite particle effected inhibition of abnormal grain growth during sintering.ing.g.

  • PDF

CuO의 첨가량에 따른 Ni-Zn 페라이트의 소결 및 자기적 특성 변화

  • Kim, Seong-Tae;Kim, Jin-Ho
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.11a
    • /
    • pp.216-216
    • /
    • 2009
  • $(Ni_{1-x-y}Zn_xCu_y)Fe_2O_4(x=0.45,\;0{\leq}y{\leq}0.3)$ was synthesized by conventional ceramic processing, and the sintering behavior and the magnetic properties of which were studied as functions of CuO content and sintering temperature. Both the densification and the grain growth rates were significantly enhanced with the increase of CuO content, while abnormal grain growth occurred when the samples of $y{\geq}0.2$ were sintered above $950^{\circ}C$. Saturation magnetization and coercive field were mainly influenced by the densification and grain growth of the specimens, respectively.

  • PDF

Growth Behavior of (Ti,W)(C,N) and WC grains in a Co Matrix (Co 액상 내에 공존하는 (Ti,W)(C,N)과 WC입자의 성장 거동)

  • 이보아;윤병권;강석중
    • Journal of Powder Materials
    • /
    • v.11 no.2
    • /
    • pp.165-170
    • /
    • 2004
  • Growth behavior of two different types of grains, faceted and rounded, in a liquid matrix has been studied in the (75WC-25TiCN)-30Co system. Powder samples were sintered above the eutectic temperature for various times under a carbon saturated condition. (Ti,W)(C,N) grains with a rounded shape and WC grains with a faceted shape coexisted in the same Co based liquid. With increasing sintering time, the average size of (Ti.W)(C,N) grains increased continuously and very large WC grains appeared. The growth of rounded (Ti,W)(C,N) grains followed a cubic law, r^3-r^3_0$=kt, where r is the average size of the grains, $r_0$ the initial average size, k the proportionality constant and t the sintering time. indicating a diffusion-controlled growth. On the other hand, the growth of the faceted WC grains resulted in a bimodal grain size distribution, showing an abnormal grain growth. These observations show that the growth behavior of different types of grains is governed by their shape, faceted or rounded, even in the same liquid matrix.

Sintering Behavior of M-type Sr-Hexaferrite by MnCO3 Addition (M-type Sr-Hexaferrite에서 MnCO3 첨가에 따른 소결 거동)

  • Jeong, MinSeok;You, Changjae;Cho, Jung Young;Moon, Kyoung-Seok
    • Journal of Powder Materials
    • /
    • v.27 no.2
    • /
    • pp.126-131
    • /
    • 2020
  • The grain growth behavior of M-type Sr hexaferrite (SrM) grains is investigated with the addition of MnCO3. First, the SrM powder is synthesized by a conventional solid-state reaction. The powder compacts of SrM are sintered at 1250℃ for 2 h with various amounts of MnCO3 (0, 0.5, 1.0, and 4.0 mol%). There is no secondary solid phase in any of the sintered samples. Relative density increases when MnCO3 is added to the SrM. Obvious abnormal grain growth does not appear in any of the SrM samples with MnCO3. The average grain size increases when 0.5 mol% MnCO3 is added to the SrM. However, as the amount of MnCO3 increase to over 0.5 mol%, the average grain size decreases. These observations allow us to conclude that the growth of SrM grains is governed by the two-dimensional nucleation grain growth mechanism, and the critical driving force for the growth of a grain decreases as the amount of MnCO3 increases.

Microstructural Characterization of Hot Extruded Al-Zn-Mg-Cu Alloys Containing Sc (Sc을 첨가한 Al-Zn-Mg-Cu 합금 압출재의 열처리에 따른 미세구조 변화)

  • 이혜경;서동우;이상용;이경환;임수근
    • Transactions of Materials Processing
    • /
    • v.13 no.1
    • /
    • pp.53-58
    • /
    • 2004
  • The microstructural changes of Al-Zn-Mg-Cu alloy containing Sc during hot extrusion and post heat treatment were investigated. Two kinds of Al-Sc alloys with different alloying elements (B1, B2) were hot extruded to make T-shape bars at extrusion temperature of $380^{\circ}C$, then the bars were solution treated at $480^{\circ}C$ for 2hrs followed by artificial aging at $120^{\circ}C$ for 24hrs. The interior microstructure of as extruded bar consisted of elongated grains, however, fine equiaxed grains were also observed around surface. The microstructural gradient suggested that different restoration process could proceed during the hot extrusion. For B1 and B2, different grain growth behaviors were found around the surface during the post heat treatment. Rapid grain growth behavior was observed for B1 around the surface, however, it was not observed for B2. Orientation pinning, which was related with the evolution of preferred orientation, and precipitation were thought to be responsible for the rapid grain growth.

Effect of Co additive on the Abnormal Grain Growth of WC (Co첨가에 의한 WC의 비정상입성장)

  • 이동범;채기웅
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.2
    • /
    • pp.131-135
    • /
    • 2004
  • The effect of Co additive on the microstructural evolusion of WC was investigated. A small amount of Co powder was placed on the top-center of the pure WC powder compact and then sintered at 1950$^{\circ}C$. During sintering some abnormally large WC grains of different size and shape observed depending on the distance from the liquid source. However, in the region far away from Co liquid source, it showed low densification and the grains of WC were very small and uniform in size. A small amount of Co liquid phase has a remarkable influence on the AGG of WC and it has been explained in terms of 2-D nucleation and growth mechanism.

Effects of ZnO and PbO on the Magnetic Properties of Sr-ferrite (ZnO와 PbO가 Sr-페라이트의 자기적 특성에 미치는 영향)

  • 김정훈;김동엽;김동진;정완배;오재현
    • Journal of the Korean Ceramic Society
    • /
    • v.28 no.6
    • /
    • pp.471-477
    • /
    • 1991
  • Effects of ZnO, PbO and SiO2 on the grain growth and magnetic properties of Sr-ferrite were investigated. (1) Addition of ZnO to Sr-ferrite increased remanence, but decreased coercivity and maximum energy product. (2) Addition of PbO up to 0.5 wt% increased (B$.$H)max of Sr-ferrite, but addition more than 0.5 wt% decreased (B$.$H)mzx (3) SiO2 addition to the 0.5 wt% PbO doped Sr-ferrite decreased remanence and increased coercivity. The coercivity increase in due to the grain refinement effect of SiO2. But addition of SiO2 more than 0.5 wt% invoked a decrease of coercivity and (B$.$H)max of Sr-ferrite due to abnormal grain growth. Sr-ferrite magnet having maximum energy product of 3.7MGOe was fabricated by using the roasting product of Pyrrhotite.

  • PDF

The Effect of CuO and SiO2 on the Magnetic Properties of Sr-Ferrite (CuO와 SiO2가 Sr-페라이트의 자기적 특성에 미치는 영향)

  • 김동식;김동엽;정원용;오재현
    • Journal of the Korean Ceramic Society
    • /
    • v.26 no.6
    • /
    • pp.747-754
    • /
    • 1989
  • The effects of CuO and SiO2 on the sintered density, grain growth and magnetic properties of Sr-ferrite were investigated. The sintered density of Sr-ferrite is increased with increasing the amount of CuO or SiO2 addition. The grain of Sr-ferrite grow uniformly with the addition of CuO, so remanence increases and coercivity decreases. The addition of SiO2 increase coercivity but does not affect remanence prominently. The sintering temperature above 125$0^{\circ}C$ and SiO2 addition above 0.8wt% causes abnormal grain growth in Sr-ferrite. When CuO and SiO2 are added simultaneouly, remanence does not decrease but coercivity shows low value.

  • PDF