• 제목/요약/키워드: AZ91

검색결과 130건 처리시간 0.027초

미량 Sn을 함유한 AZ91 마그네슘 합금의 미세조직 및 기계적 특성 (Microstructure and Mechanical Properties of AZ91 Magnesium Alloy Containing a Small Amount of Sn)

  • 전중환
    • 열처리공학회지
    • /
    • 제27권3호
    • /
    • pp.115-120
    • /
    • 2014
  • Microstructural features were comparatively investigated in AZ91 (Mg-9%Al-1%Zn) and AZ91-0.5%Sn alloys, in order to clarify the reason for the enhancement in room temperature tensile properties by the addition of small amount of Sn in Mg-Al-based alloy. In as-cast state, the Sn-containing alloy showed increased YS, UTS and elongation than the Sn-free alloy. The microstructural examination revealed that various factors including finer cell size, reduction of lamellar (${\alpha}+{\beta}$) phase and morphological change of bulky ${\beta}$ phase from partially divorced shape to fully divorced shape, are likely to be responsible for the improvement in tensile properties for the Sn-containing alloy. It is noted that two alloys showed similar tensile properties after solution treatment. This implies that microstructural evolution related to the ${\beta}$ phase plays a key role in better tensile properties in the Sn-containing alloy.

AZ91-5wt.%Sn 마그네슘 합금의 열처리의 특성 (Heat Treatment of AZ91-5wt.%Sn Magnesium Alloy)

  • 김대환;임수근
    • 한국주조공학회지
    • /
    • 제37권1호
    • /
    • pp.14-20
    • /
    • 2017
  • The microstructure, electrical conductivity and hardness variation of an AZ91-5wt%Sn Mg alloy sample during a solid-solution and aging heat treatment were instigated by optical microscopy, scanning electron microscopy, X-ray diffraction and by Rockwell hardness techniques in this study. The XRD result shows that the main phases in the as-casted alloy are ${\alpha}$-Mg, $Mg_{17}Al_{12}$ and $Mg_2Sn$. From the SEM images of the AZ91-5wt%Sn Mg alloy after the solution treatment, the $Mg_{17}Al_{12}$ phases in the alloy were found to have dissolved into the matrix with an increase in the holding time during the solution treatment, but $Mg_2Sn$ phases were clearly observable. The highest peak hardness of the AZ91-5wt%Sn Mg alloy is 82HRE at an aging temperature of $200^{\circ}C$.

주조용 AZ91-2%Ca 마그네슘 합금의 부식 거동에 미치는 용체화처리의 영향 (Effect of Solution Treatment on Corrosion Behavior of AZ91-2%Ca Magnesium Casting Alloy)

  • 문정현;전중환
    • 열처리공학회지
    • /
    • 제28권4호
    • /
    • pp.190-199
    • /
    • 2015
  • The study is intended to investigate the effect of solution treatment on microstructure and corrosion behavior of AZ91(Mg-9%Al-1%Zn-0.3%Mn)-2%Ca casting alloy. In as-cast state, the AZ91-2%Ca alloy consisted of intermetallic ${\beta}(Mg_{17}Al_{12})$, $Al_8Mn_5$ and $Al_2Ca$ phases in ${\alpha}-(Mg)$ matrix. After the solution treatment, Al within the ${\alpha}-(Mg)$ matrix was distributed more homogeneously, along with the slight decrease in the total amount of intermetallic compounds. The corrosion resistance of the AZ91-2%Ca alloy was improved after the solution treatment. The microstructural examinations for the solution-treated samples revealed that the better corrosion resistance may well be related to the incorporation of more oxides and hydroxides such as $Al_2O_3$, $Al(OH)_3$, CaO and $Ca(OH)_2$ into the surface corrosion product without dissolution of the intermetallic phases along the grain boundaries.

Effect of Power Mode of Plasma Anodization on the Properties of formed Oxide Films on AZ91D Magnesium Alloy

  • Lee, Sung-Hyung;Yashiro, Hitoshi;Kure-Chu, Song-Zhu
    • 한국재료학회지
    • /
    • 제28권10호
    • /
    • pp.544-550
    • /
    • 2018
  • The passivation of AZ91D Mg alloys by plasma anodization requires deliberate choice of process parameters due to the presence of large amounts of structural defects. We study the dependence of pore formation, surface roughness and corrosion resistance on voltage by comparing the direct current (DC) mode and the pulse wave (pulse) mode in which anodization is performed. In the DC plasma anodization mode, the thickness of the electrolytic oxide film of the AZ91D alloy is uneven. In the pulse mode, the thickness is relatively uniform and the formed thin film has a three-layer structure. The pulse mode creates less roughness, uniform thickness and improved corrosion resistance. Thus, the change of power mode from DC to pulse at 150 V decreases the surface roughness (Ra) from $0.9{\mu}m$ to $0.1{\mu}m$ and increases the corrosion resistance in rating number (RN) from 5 to 9.5. Our study shows that an optimal oxide film can be obtained with a pulse voltage of 150 V, which produces an excellent coating on the AZ91D casting alloy.

마그네슘 합금제 휠 제조에 관한 연구 (A Study of Manufacturing AZ91D Mg Alley Wheel)

  • 김정구;신일성;금동화
    • 한국재료학회지
    • /
    • 제9권7호
    • /
    • pp.715-723
    • /
    • 1999
  • 마그네슘은 20여년간 자동차 산업에서 휠소재로 사용되어 왔다. 마그네슘 휠은 무게가 알루미늄 휠보다 25% 가벼워서 주행성이 우수하다. 이 연구의 목적은 사형주조 및 영구금형주조 공정에 의한 AZ91D 합금제 췰을 개발하는 것이다 보호개스$(SF_6+CO_2)$를 사용하는 비플럭스 용해기술을 적용하여 용탕의 산화와 불순물의 유입을 배제하였다 마그네슘 용탕은 가압식 펌프시스템을 사용하여 가열된 파이프를 통하여 모울드에 자동으로 공급된다. 열처리 및 인고트의 조성에 따른 AZ91B 합금제 휠의 기계적 특성을 조사하였다.

  • PDF

금형 주조한 GZ21 합금과 AZ91 합금의 부식특성 비교 (Comparison of Electrochemical Corrosion Properties of Permanent Mold Casting GZ21 Alloy and AZ91 Alloy)

  • 김대한;김병호;박경철;장인기
    • 한국주조공학회지
    • /
    • 제36권2호
    • /
    • pp.60-66
    • /
    • 2016
  • In this study, comparison of corrosion properties of the Mg-1.5Ge-1Zn (GZ21) alloy and Mg-9Al-1Zn (AZ91) alloy were investigated. The studied alloys were fabricated by permanent mold casting method. And the potentiodynamic test, hydrogen evolution test, immersion test and A.C Impedance test were carried out in a 3.5% NaCl solution with pH7.2 at room temperature to measure the corrosion properties. The microstructure of GZ21 alloy was composed of ${\alpha}-Mg$ and $Mg_2Ge$ phases and AZ91 alloy was composed of ${\alpha}-Mg$ and $Mg_{17}Al_{12}$ phases. From the test results, the corrosion property was improved by adding Ge. It seemed that the corrosion mechanism was changed from galvanic corrosion (AZ91) to filiform corrosion (GZ21).

플라즈마 전해 산화처리한 AZ91 주조마그네슘합금의 기계적 및 부식 특성에 미치는 전해질의 영향 (Effect of Electrolyte on Mechanical and Corrosion Properties of AZ91 Cast Magnesium Alloy Coated by Plasma Electrolytic Oxidation Method)

  • 김보식;이두형;장시영
    • 한국주조공학회지
    • /
    • 제29권5호
    • /
    • pp.233-237
    • /
    • 2009
  • The effect of electrolyte on mechanical and corrosion properties of AZ91 magnesium alloy by plasma electrolytic oxidation (PEO) method was investigated. The coating layers formed in the silicate and the aluminate electrolytes showed porous structures. The small pores were randomly distributed on the coatings formed in aluminate electrolyte while the coatings formed in silicate electrolyte showed much bigger pores. In the aluminate electrolyte, the coatings were composed of Mg, MgO and $MgAl_2O_4$, whereas Mg, MgO, $MgAl_2O_4$ and $Mg_2SiO_4$ were identified in the coatings formed in silicate electrolyte. The hardness of coatings in the silicate electrolyte was higher than that of coating grown in the aluminate electrolyte. The AZ91 alloy coated in the silicate electrolyte had higher tensile strength and elongation than that coated in the aluminate electrolyte. In addition, the coatings formed in the silicate electrolyte showed much better corrosion resistance compared to the coatings formed in the aluminate electrolyte.

0.7wt% CaO 첨가 AZ91D Eco-Mg 다이캐스팅 부품의 미세조직 및 기계적 특성 (Microstructures and Mechanical Properties of Diecast 0.7wt% CaO added Eco-Mg Parts)

  • 서정호;임현규;김세광
    • 한국주조공학회지
    • /
    • 제30권6호
    • /
    • pp.224-230
    • /
    • 2010
  • To prevent oxidation of Mg melt, $SF_6$ gas has been generally used for Mg alloys during melting and casting as a cover gas. The use of $SF_6$ gas, however, will be restricted owing to its crucial impact on global warming. Non-$SF_6$ process during melting and casting in diecasting industry has been proved with Eco-Mg alloys by a simple addition of small amount of CaO into Mg alloys. This paper shows non-$SF_6$ diecasting procedures for 0.7wt% CaO added AZ91D Eco-Mg alloys. Cold-chamber diecasting was performed under $CO_2$ atmosphere without $SF_6$ gas. An increment of mechanical properties, especially strength and ductility of Eco-Mg alloys is, in part, due to high-quality melt, refined grain size and $Al_2Ca$ second phase strengthening. Microstructures and mechanical properties of 0.7wt% CaO added AZ91D Eco-Mg alloys are evaluated in comparison with those of conventional AZ91D Mg alloy.

Electrodeposition of Copper on AZ91 Mg Alloy in Cyanide Solution

  • Nguyen, Van Phuong;Park, Min-Sik;Yim, Chang Dong;You, Bong Sun;Moon, Sungmo
    • 한국표면공학회지
    • /
    • 제49권3호
    • /
    • pp.238-244
    • /
    • 2016
  • Copper electrodeposition on AZ91 Mg alloy was studied in views of preferential deposition on ${\alpha}$- or ${\beta}$- phases and how to achieve uniform deposition over the entire surface on ${\alpha}$- and ${\beta}$-phases in a cyanide solution. The inhomogeneous microstructure of AZ91 Mg alloy, particularly ${\alpha}$- and ${\beta}$-phases, was found to result in non-uniform deposition of zincate layer, preferential deposition of zincate on ${\beta}$-phases, which leads to non-uniform growth of copper layer during the following electrodeposition process. The preferential depositions of zincate can be attributed to higher cathodic polarizations on the ${\beta}$-phases. Pin-hole defects in the copper electrodeposit were observed at the center of large size ${\beta}$-phase particles which is ascribed to gas bubbles formed at the ${\beta}$-phases. The activation of AZ91 Mg alloy in hydrofluoric acid solution was used to obtain uniform growth of zincate layer on both the ${\alpha}$- and ${\beta}$-phases. By choosing an optimum activation time, a uniform zincate layer was obtained on the AZ91 Mg alloy surface and thereby uniform growth of copper was obtained in a cyanide copper electroplating solution.

AZ91 마그네슘합금 절분 및 스크랩의 재활용에 관한 연구 (The study on the recycle for machined chips and scraps of AZ91 magnesium alloy)

  • 이두면;이준서;이치환
    • 자원리싸이클링
    • /
    • 제3권1호
    • /
    • pp.25-31
    • /
    • 1994
  • AZ91 마그네슘합금 절분 및 스크램외 재활용을 목적으로 절분 및 스크랩을 상온가압하여 빌렛을 얻었다. 이 압출용 벨렛을 압축비율 25:1로 고정하고, 압출온도를 $300~380^{\circ}C$로 변화시켜 가면서 시편을 제조하였으며, 비교재로 마그네슘합금 주조재도 열간압출을 행하였다. 마그네숨합금 절분 및 스크랩을 열간압출함에 따라 매우 미세한 재설정 조직을 얻었으며, 인장강도 및 연산률은 각각 330 MPa, 10%로 주조재를 열간압층한 재료와 거의 비슷한 기계적 특성을 나타내었다.

  • PDF