• 제목/요약/키워드: AISI

검색결과 404건 처리시간 0.033초

304 스테인리스강의 점소성 특성에 관한 연구 (The Rate Dependent Deformation Behavior of AISI Type 304 Stainless Steel at Room Temperature)

  • 호광수
    • 소성∙가공
    • /
    • 제16권2호
    • /
    • pp.101-106
    • /
    • 2007
  • Uniaxial displacement controlled tests were performed on annealed Type 304 stainless steel at room temperature. A servo-controlled testing machine and strain measurement on the gage length were employed to measure the response to a given input. The test results exhibit that the flow stress increases nonlinearly with the strain rate and the relaxed stress at the end of the relaxation periods depends strongly on the strain rate preceding the relaxation test. The rate-dependent inelastic deformation behavior is simulated using a new unified viscoplasticity model that has the rate-dependent format of nonlinear kinematic hardening rule, which plays a key role in modeling the rate dependence of relaxation behavior. The model does not employ yield or loading/unloading criteria and consists of a flow law and the evolution laws of two tensor and one scalar-valued state variables.

레이저 메탈 디포지션 변수에 의한 표면경도 특성 분석 (Surface Hardness as a Function of Laser Metal Deposition Parameters)

  • 김원혁;정병훈;박인덕;오명환;최성원;강대민
    • 소성∙가공
    • /
    • 제24권4호
    • /
    • pp.272-279
    • /
    • 2015
  • The characteristics of the laser metal deposition parameters were studied to enhance the deposition efficiency using a diode pumped disk laser. STD61 hot tool steel plate and Fe based AISI M2 alloy were used as a substrate and powder for the laser metal deposition, respectively. Among the laser metal deposition parameters the laser power, track pitch and powder feed rate were used to estimate the deposition efficiency. From the experimental results, the deposition efficiency was shown to be excellent when 1.8kW laser power 500um track pitch and 10g/min of the powder feed rate were used. For this optimal condition the average hardness of the deposition track was approximately 830HV, and this value is 30~50% better than the hardness of the commercially produced tool steel after heat treatment.

고체윤활용 $MoS_2$Bonded Film의 마찰마모 특성에 관한 실험적 고찰 (Experimental Studies on Friction and Wear of the Solid Lubricating $MoS_2$ Bonded Films)

  • 공호성;윤의성;한홍구;권오관
    • Tribology and Lubricants
    • /
    • 제12권1호
    • /
    • pp.15-21
    • /
    • 1996
  • Friction and wear properties of MoS$_2$ bonded films were studied using the Falex testing machine, and their properties were evaluated in terms of the life and the load carrying capacity of the films. MoS$_2$ bonded films were formulated from the mixtures of MoS$_2$ solid particles and epoxyphenol resin, and they were applied onto AISI 4130 steel surface by dipping method to form lubricating bonded films. The results of the life and the load carrying capacity of the films showed that films were mainly affected by the surface temperature arisen from the frictional heat at the contact surface. To obtain enhanced tribological properties of the films, various combinations of solid lubricants and additives with a basic polymer resin were attempted and evaluated. The effects of surface pretreatment, such as sand blast or Zn-phosphating, were also investigated.

아크 용접에서 구동력에 따른 열 및 물질 유동에 관한 연구

  • 김원훈;나석주
    • 한국추진공학회:학술대회논문집
    • /
    • 한국추진공학회 1996년도 제7회 학술강연회논문집
    • /
    • pp.27-41
    • /
    • 1996
  • In this study the heat transfer and fluid flow of the molten pool in stationary gas tungsten arc welding using argon shielding gas were investigated. Transporting phenomena from the welding arc to the base material surface, such as current density, heat flux, arc pressure and shear stress acting on the weld pool surface, were taken from the simulation results of the corresponding welding arc. Various driving forces for the weld pool convection were considered, self-induced electromagnetic, surface tension, buoyancy, and impinging plasma arc forces. Furthermore, the effect of surface depression due to the arc pressure acting on the molten pool surface was considered. Because fusion boundary has a curved and unknown shape during welding, a boundary-fitted coordinate system was adopted to precisely describe the boundary for the momentum equation. The numerical model was applied to AISI 304 stainless steel and compared with the experimental results.

  • PDF

유동제어 성형기술을 이용한 자동차 허브클러치의 실험적 연구 (A Experimental Study of Automobile Hub Clutch used Flow Control Forming Techniques)

  • 박종남;계중읍;김병민
    • 한국정밀공학회지
    • /
    • 제19권12호
    • /
    • pp.142-149
    • /
    • 2002
  • In this paper, the metal forming process is caused of rise of the unit cost of production in increase of the lead-time and cost because of manufacturing final product through a few the number of processes. Flow control complex forming is proposed to put into formulation in order to apply cold forging from conventional approximate similarity theory, and the forming loads of the real material(AISI 1008) can be calculated by put at the new similarity formula the load by plasticine model material experiment through hub clutch. In order to reduce lead-time and cost the technology is used to manufacture with lower die of this product. By the application synthetic resin as the raw material, it is have the merit such short lead-time, low cost, good surface finish etc., as compared with the machine work.

PMMA(Poly Methyl Methacrylate) 코팅층 두께 및 적용하중에 따른 마멸기구 분석 (Effects of thickness and applied load on wear mechanisms of PMMA (Poly Methyl Methacrylate) coating layers)

  • 강석하;김용석
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 춘계학술대회 논문집
    • /
    • pp.152-155
    • /
    • 2004
  • Effects of sliding speed, applied load, counterpart radius and thickness of PMMA (Poly Methyl Methacrylate) coating layers on their dry sliding frictional and wear behavior were investigated. Sliding wear tests were carried out using a pin-on-disk wear tester. The PMMA layer was coated on Si wafer by a sol-gel technique with two different thicknesses, $1.5{\mu}m\;and\;0.8{\mu}m$. AISI 52100 bearing steel balls were used as a counterpart of the PMMA coating during the wear. Normal applied load and sliding speed were varied. Wear mechanisms were investigated by examining worn surfaces by an SEM. Under most of sliding test conditions, the thicker layer with the thickness of $1.5{\mu}m$ showed lower fiction coefficient than the thinner layer. Effects of sliding speed and counterpart's radius on the frictional behavior were varied depending on the thickness of the coating layer.

  • PDF

TiN이 코팅된 316 스테인리스강 분리판을 이용한 고분자전해질 연료전지의 성능에 관한 연구 (A Study on the Performance of PEMFC Using the TiN-Coated 316 Stainless Steel Bipolar Plates)

  • 조은애
    • 한국수소및신에너지학회논문집
    • /
    • 제14권4호
    • /
    • pp.291-297
    • /
    • 2003
  • As an alternative bipolar plate material for polymer electrolyte membrane fuel cell (PEMFC), TiN-coated 316 stainless was evaluated in terms of electrical contact resistance and water contact angle. Performance and lifetime of the TiN-coated 316 bipolar plates were measured in comparison with those of graphite and bare 316 bipolar plates. At a cell voltage of 0.6 V, current density of the single cells using graphite, AISI 316, and TiN/316 bipolar plates was 996, 796, and $896mA/cm^2$, respectively. By coating 316 stainless steel with TiN layer, performance degradation rate determined to be the voltage degradation rate at a cell voltage of 0.6 V was reduced from 2.3 to 0.43 mV/h.

중절삭시 공구마모에 의한 절삭상태변수의 변화 (Cutting state parameter variations caused by tool wear in hard turning)

  • Jang, Dong-Young;Hsiao, Ya-Tsun;Kim, Il-Hae;Kim, Woo-Jung;Han, Dong-Chul
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2000년도 춘계학술대회 논문집
    • /
    • pp.653-657
    • /
    • 2000
  • Machining performance in hard turning of hardened AISI M2 steel has been studied. Ceramic tools were used in the cutting tests without coolants and workpiece was prepared by heat treatment to increase its hardness up to Rc 60. Cutting state parameters such as cutting forces, temperature, and tool wear were measured in the experiments and effects of tool wear on cutting states were investigated.

  • PDF

은 박막이 코팅된 베어링강의 마찰거동에 미치는 마모입자의 영향에 대한 실험적 고찰 (An Experimental Study on the Effect of Wear Particles on the Sliding Behavior of Silver-Coated Bearing Steels)

  • 양승호;공호성;윤의성;김대은
    • Tribology and Lubricants
    • /
    • 제17권3호
    • /
    • pp.221-227
    • /
    • 2001
  • The effect of silver particles on the sliding behavior of bearing steels was studied experimentally by using a ball-on-disk tribometer. Tests were performed in ambient air, dry air and vacuum. Disks of AISI 52100 were silver-coated by a thermal evaporation method, and the effects of silver particle transfer on friction were analyzed. In order to understand further the mechanism of silver particle transfer and its effect on friction and wear, pre-compressed silver particles were artificially introduced into the friction interface and the results were compared to those of silver-coated specimens. Results showed that the introduced silver particles produced transfer layers and resulted in low friction. It also showed that this low friction is closely related to the characteristic behavior of transfer layers. Shakedown occurred at the friction interface affected the friction and wear.

냉간 가공시 조질 및 비조질강의 성형성과 기계적성질의 비교 연구 (The Study on Mechanical Properties and Formability of Non-Heat-Treated and Heat-Treated Cold Forging Materials)

  • 이영선;이정환;이상용;강종훈;김주현
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1998년도 춘계학술대회논문집
    • /
    • pp.224-230
    • /
    • 1998
  • Non-heat-treated type material has been investigated for formability compared to heat-treated material. It is very important in automation of metal forming, since it has difficulties of controlling heat treating system by the computer and has bottle neck problem related with heat treatment. In this paper, we have concerned about mechanical properties of non-heat-treated material after the forging. To compare the characteristics between heat-treated material and non-heat-treated material, tensile, compression and fatigue test has been performed. Considering results of mechanical properites of non-heat-treated material, it can replace heat-treated material. Therefore non-heat-treated material may be applied to cold forging.

  • PDF