• Title/Summary/Keyword: AFM roughness

Search Result 524, Processing Time 0.019 seconds

The improvement of electrical properties of InGaZnO (IGZO)4(IGZO) TFT by treating post-annealing process in different temperatures.

  • Kim, Soon-Jae;Lee, Hoo-Jeong;Yoo, Hee-Jun;Park, Gum-Hee;Kim, Tae-Wook;Roh, Yong-Han
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.08a
    • /
    • pp.169-169
    • /
    • 2010
  • As display industry requires various applications for future display technology, which can guarantees high level of flexibility and transparency on display panel, oxide semiconductor materials are regarded as one of the best candidates. $InGaZnO_4$(IGZO) has gathered much attention as a post-transition metal oxide used in active layer in thin-film transistor. Due to its high mobility fabricated at low temperature fabrication process, which is proper for application to display backplanes and use in flexible and/or transparent electronics. Electrical performance of amorphous oxide semiconductors depends on the resistance of the interface between source/drain metal contact and active layer. It is also affected by sheet resistance on IGZO thin film. Controlling contact/sheet resistance has been a hot issue for improving electrical properties of AOS(Amorphous oxide semiconductor). To overcome this problem, post-annealing has been introduced. In other words, through post-annealing process, saturation mobility, on/off ratio, drain current of the device all increase. In this research, we studied on the relation between device's resistance and post-annealing temperature. So far as many post-annealing effects have been reported, this research especially analyzed the change of electrical properties by increasing post-annealing temperature. We fabricated 6 main samples. After a-IGZO deposition, Samples were post-annealed in 5 different temperatures; as-deposited, $100^{\circ}C$, $200^{\circ}C$, $300^{\circ}C$, $400^{\circ}C$ and $500^{\circ}C$. Metal deposition was done on these samples by using Mo through E-beam evaporation. For analysis, three analysis methods were used; IV-characteristics by probe station, surface roughness by AFM, metal oxidation by FE-SEM. Experimental results say that contact resistance increased because of the metal oxidation on metal contact and rough surface of a-IGZO layer. we can suggest some of the possible solutions to overcome resistance effect for the improvement of TFT electrical performances.

  • PDF

Effects of 1 keV $Ar^+$ ion irradiation on Au films on glass (1 keV $Ar^+$ 이온의 조사가 유리기판위의 금 박막의 미치는 영향)

  • Jang, H. G.;Kim, H. S.;Han, S.;Choi, W. K.;Koh, S. K.;Jung, H. J.
    • Journal of the Korean Vacuum Society
    • /
    • v.5 no.4
    • /
    • pp.371-376
    • /
    • 1996
  • Au films with a thickness around 1600 $\AA$ were deposited onto glass at room temperature by ion beam sputtering with a 5 cm cold-hollow ion gun at pressure $1\times 10^{-6}-1\times 10^{-5}$ Torr. Irradiation of the Au deposited samples was carried out at pressure of $7\times 10^{-6}$ Torr. For the sputter depositions, $Ar^+$ ion energy was 1 keV, and the current density at the substrate surface was 15 $\mu$A/$\textrm{cm}^2$. Effects of 1 keV $Ar^+$ ion dose($I_d$) between $1\times 10^{16}\; and\;2\times 10^{17}\;Ar^+\textrm{cm}^{-2}$on properties such as crystallinity, surface roughness and adhesion, etc. of the films have been investigated. The Au films sputtered by $Ar^+$ ion beam had only (111) plane and the X-ray intensity of the films decreased with increase of $I_d$. The thickness of Au films reduced with Id. $R_{ms}$ surface roughness of the films increased from 16 $\AA$ at as-deposited to 1118 $\AA$ at ion dose= $2\times 10^{17}\;Ar^+\textrm{cm}^{-2}$. Adhesion of Au film on sputtered at $I_d$= $2\times 10^{17}\;Ar^+\textrm{cm}^{-2}$ was 9 times greater than that of Au film with untreated, as determined by a scratch test.

  • PDF

Study of Selective Etching of GaAs over AlGaAs and InGaP Semiconductors in High Density Planar Inductively Coupled BCl3/SF6 Plasmas (고밀도 평판형 유도결합 BCl3/SF6 플라즈마를 이용한 GaAs/AlGaAs와 InGaP 반도체의 선택적 식각에 관한 연구)

  • Yoo Seungryul;Ryu Hyunwoo;Lim Wantae;Lee Jewon;Cho Guan Sik;Jeon Minhyon;Song Hanjung;Lee BongJu;Ko Jong Soo;Go Jeung Sang;Pearton S. J.
    • Korean Journal of Materials Research
    • /
    • v.15 no.3
    • /
    • pp.161-165
    • /
    • 2005
  • We investigated selective dry etching of GaAs over AlGaAs and InGaP in high density planar inductively coupled $BCl_3/SF_6$ plasmas. The process parameters were ICP source power (0-500 W), RE chuck power (0-30W) and gas composition $(60-100\%\;BCl_3\;in\;BCl_3/SF_6)$. The process results were characterized in terms of etch rate, selectivities of GaAs over AlGaAs and InGaP, surface morphology, surface roughness and residues after etching. $BCl_3/SF_6$ selective etching of GaAs showed quite good results in this study. Selectivities of GaAs $(GaAs:AlGaAs\~36:1,\;GaAs:InGaP\~45:1)$ were superior at $18BCl_3/2SF_6$, 20 W RF chuck power, 300 W ICP source power and 7.5 mTorr. Addition of $(5-15\%)SF_6\;to\;BCl_3$ produced relatively high selectivities of GaAs over AlGaAs and InGaP during etching due to decrease of etch rates of AlGaAs and InGaP (boiling points of etch products: $AlF_3\~1300^{\circ}C,\;InF_3>1200^{\circ}C$ at atmosphere) at the condition. SEM and AFM data showed slightly sloped sidewall and somewhat rough surface$(RMS\~9nm)$. XPS study on the surface of processed GaAs proved a very clean surface after dry etching. It shows that planar inductively coupled $BCl_3/SF_6$ plasmas could be a good candidate for selective dry etching of GaAs over AlGaAs and InGaP.

Bias Voltage Dependence of Magnetic Tunnel Junctions Comprising Double Barriers and CoFe/NiFeSiB/CoFe Free Layer (CoFe/NiFeSiB/CoFe 자유층을 갖는 이중장벽 자기터널접합의 바이어스전압 의존특성)

  • Lee, S.Y.;Rhee, J.R.
    • Journal of the Korean Magnetics Society
    • /
    • v.17 no.3
    • /
    • pp.120-123
    • /
    • 2007
  • The typical double-barrier magnetic tunnel junction (DMTJ) structure examined in this paper consists of a Ta 45/Ru 9.5/IrMn 10/CoFe7/$AlO_x$/free layer/AlO/CoFe 7/IrMn 10/Ru 60 (nm). The free layer consists of an $Ni_{16}Fe_{62}Si_8B_{14}$ 7 nm, $Co_{90}Fe_{10}$ (fcc) 7 nm, or CoFe $t_1$/NiFeSiB $t_2$/CoFe $t_1$ layer in which the thicknesses $t_1$ and $t_2$ are varied. The DMTJ with an NiFeSiB-free layer had a tunneling magnetoresistance (TMR) of 28%, an area-resistance product (RA) of $86\;k{\Omega}{\mu}m^2$, a coercivity ($H_c$) of 11 Oe, and an interlayer coupling field ($H_i$) of 20 Oe. To improve the TMR ratio and RA, a DMTJ comprising an amorphous NiFeSiB layer that could partially substitute for the CoFe free layer was investigated. This hybrid DMTJ had a TMR of 30%, an RA of $68\;k{\Omega}{\mu}m^2$, and a of 11 Oe, but an increased of 37 Oe. We confirmed by atomic force microscopy and transmission electron microscopy that increased as the thickness of NiFeSiB decreased. When the amorphous NiFeSiB layer was thick, it was effective in retarding the columnar growth which usually induces a wavy interface. However, if the NiFeSiB layer was thin, the roughness was increased and became large because of the magnetostatic $N{\acute{e}}el$ coupling.