• 제목/요약/키워드: AE counts

검색결과 122건 처리시간 0.025초

ENF 시험편을 이용한 평직 CFRP의 층간파괴인성 및 AE 특성 평가 (The Evaluation of Interlaminar Fracture Toughness and AE Characteristics in a Plain Woven CFRP Composite with ENF Specimen)

  • 윤유성;권오헌
    • 동력기계공학회지
    • /
    • 제10권2호
    • /
    • pp.117-123
    • /
    • 2006
  • Woven fabrics composites are used as primary structural components in many applications because of their superior properties that offer high specific strength and stiffness. However, the complexity of the fabric structure makes understanding of their failure behavior very difficult. Also, laminate woven fabrics CFRP have unique failure mechanisms such as fiber bridging, fiber/matrix crack and so on. In particular, the delamination phenomenon of the composite materials is one of the most frequent failure mechanisms. So, we estimated interlaminar fracture and damage in composites using as ENF specimen by a 3 point bending test. And AE characteristics were examined for crack propagation on plain woven CFRP. We obtained the following conclusions from the results of the evaluation of the 3 point bending fracture test and AE characteristic estimation. AE counts of maximum crack length were obtained as $85.97{\times}10^4\;and\;93{\times}10^3\;for\;a_0/L=0.3$ and 0.6, respectively. Also the maximum amplitudes were over 80dB at both $a_0/L=0.3\;and\;0.6$. $G_{IIc}$ at that's $a_0/L$ ratio were obtained with $1.07kJ/m^2\;and\;3.79kJ/m^2$.

  • PDF

원공결함을 갖는 SM45C 인장시험편의 강도해석과 음향방출에 관한 사례연구 (Case Study on the Load-Deflection and Acoustic Emission Analysis of SM45C Coupons with a Circular Hole Defect under Tensile Loading)

  • 우창기;이장규
    • 한국공작기계학회논문집
    • /
    • 제17권1호
    • /
    • pp.50-58
    • /
    • 2008
  • The SM45C metallic coupons have been tested under static tensile loading with acoustic emission (AE) as the load-deflection curve mainly. In this study, we used AE to detect the yielding of material and AE techniques was applied to rapidly estimate the mechanical characteristics of a material. First, coupons without an artificial defect were tested at different cross-head speed. For all cases in this analysis, yielding point of SM45C coupons did not appear definitely compared to mild steel, whereas coupons start to generate AE counts upon yielding. So all cases are normalized to know the possibility of accelerated life test of a material. And next, coupons with different from sizes of circular hole defects were tested at the same cross-head speed of 5 mm/min. Results were classified into 3 classes and analyzed by AE amplitude & signal strength as a function of time. Summarizing the specific conclusions, we need to additional research considering plate with width-ratio in order to estimate the fracture mechanism.

304 스테인레스 강의 부식 손상 중 발생하는 음향방출신호 분석 (Detection of Acoustic Signal Emitted during Corrosion of 304 Stainless Steel)

  • 우카이거;최찬양;변재원
    • 비파괴검사학회지
    • /
    • 제33권5호
    • /
    • pp.409-414
    • /
    • 2013
  • 음향방출법을 이용하여 304 스테인레스 강의 부식 손상 과정을 평가하였다. 스테인레스 강의 가속부식시험을 수행하면서 음향방출신호를 수집할 수 있는 측정 시스템을 구성하였다. 양극분극시험에서 공식부식(pitting corrosion)이 발생하는 시점 이후부터 음향방출(AE)신호가 검출되기 시작함을 확인하였다. 부식 실험 후 시편 표면을 광학현미경으로 관찰하여 다수의 공식부식이 발생하였음을 검증하였다. 부식 시간의 증가에 따른 AE 누적카운트 증가율과 AE 신호 진폭의 변화는 3단계로 구분되는 특징을 보였다. 이러한 AE 신호 발생 특징을 스테인레스 강의 부식 발생 과정의 단계별 변화와 관련하여 고찰하였다. AE 신호를 이용하여 금속 소재의 부식 손상 정도 및 부식 과정의 평가 가능성을 제시하였다.

냉동 냉면류의 제조공정별 미생물학적 위해요소 평가 (Microbial Hazard Analysis of the Manufacturing Processes for Frozen Korean Cold Noodle, Naengmyeon)

  • 김유정;김혜진;임영은;양혜걸;박슬기;정진숙;엄애선
    • 급식외식위생학회지
    • /
    • 제3권1호
    • /
    • pp.38-44
    • /
    • 2022
  • This study investigated the microbiological hazards in the manufacturing processes of Naengmyeon. Sanitary indicative bacteria, such as aerobic plate counts and coliforms as well as pathogenic bacteria, were examined from raw materials, manufacturing processes, working area, 17 utensils and equipment. The aerobic plate counts for raw materials and arrowroot starch estimated as 0.77±0.68~5.02±0.28 and 5.02±0.28 log CFU/g, respectively. Coliforms were detected from wheat flour, buckwheat flour, and potato starch. Staphylococcus aureus was detected to be 0.61±1.06 log CFU/g in wheat flour and 0.20±0.35 log CFU/g in buckwheat flour. During the manufacturing process, aerobic plate counts for kneading process were 4.54±0.34 log CFU/g. But after the press out and heat process, contamination of aerobic plate counts and coliforms decreased and remained at a low level until the release process. Aerobic plate counts before washing disinfection of screw were 3.28±0.62 log CFU/100 cm2, the level of which was high in utensils and equipment that had contact with employees or water. These results represent not only an important indicator for the hygienic level but also a scientific basis for analyzing biological hazards, which lead to the introduction of HACCP for the production of safe and hygienic cold noodles processed by manufacturers.

자동차 크랭크 軸用 鋼材의 棒對棒 同種材 摩擦熔接의 疲勞强度 特性 및 AE 評價 (Optimization of Bar-to-Bar Similar Friction Welding of Crank Shaft for Motor Vehicle and the Weld Fatigue Strength Properties and its AE Evaluation)

  • 오세규;양형태;김헌경
    • 한국해양공학회지
    • /
    • 제13권2호통권32호
    • /
    • pp.74-82
    • /
    • 1999
  • Nowadays, the crank shaft motor vehicle has become essential as the important component. The machining precision was asked for manufacturing the shaft. They could be unstable in the quality by the conventional are welding. Both in-process quailty control and high reliability of the weld are the major concerns in applying friction wlding to the economical and qualified mass-production. No reliable nondestructive monitoring method is avaliable at present to determine the real-time evaluation of automatic production quality control for bar-to-bar friction welding of the crank shaft of O.D 24mm for motor vehicle. This paper, so that, presents the experimental examinations and statistical quantitative analysis of the correlation between the cumulative counts of acoustic emission(AE) during plastic deformation periods of the welding and the tensile strength and other properties of the bar-to-bar welded joints of O.D. 24mm shaft as well as the various welding variables, as a new approach which attempts finally to develop real-time quality monitoring system for friction welding, resulting in practical possiblility of real-time quality control more than 100% joint efficiency showing good weld with no micro structural defects.

  • PDF

해수 열화 및 원공 손상 CF/Aramid 복합재의 패치 부착이 굽힘거동에 미치는 영향 (The Patch Attachment Effect for Bending Behavior on the CF/Aramid Composites with Seawater Aging and Hole Damage)

  • 권우덕;권오헌;윤유성
    • 한국안전학회지
    • /
    • 제38권3호
    • /
    • pp.20-26
    • /
    • 2023
  • Fiber-reinforced composite materials with carbon, glass, and aramid fibers are widely applied to industrial field structures due to their excellent properties. However, carbon fibers are vulnerable to external impacts, whereas aramid fibers degrade when exposed to water. This study evaluated carbon/aramid fiber composites degraded and damaged by high-temperature saline environments using acoustic emission (AE). The test specimen was molded using an autoclave and immersed in seawater at 70 ℃ for 224 days. In order to imitate the damage, a 3-mm-diameter hole was drilled using a diamond drill. Additionally, the specimen with the perforation was repaired by patch attachment processing. Three-point bending was used to conduct the flexural experiment, and an AE sensor with a 150-kHz resonance frequency was attached to evaluate the damage and the effect of patch attachment. AE accumulative counts obtained at the maximum load were 69.2, 67.1, and 91.2 for a high-temperature seawater deteriorated condition, a hole specimen, and a repaired patch specimen, respectively. Furthermore, the maximum amplitude of AE was detected at low values of 28 dB, 31.3 dB, and 30.3 dB.

응력확대계수와 음향방출 변수를 이용한 피로균열 거동 연구 (Study on the Fatigue Crack Behavior by the Stress Intensity Factor and AE Parameters)

  • 윤동진;정중채;박휘립;김기복;이승석
    • 비파괴검사학회지
    • /
    • 제20권5호
    • /
    • pp.412-423
    • /
    • 2000
  • 응력확대계수와 음향방출 발생 관계를 이용해 균열 길이 및 균열 검출 능력을 평가할 수 있는 새로운 접근 방법을 파괴역학적인 관점에서 제시하였다. 이를 위해 강 교량 부재인 SWS 490B 강의 피로 균열 활동도를 음향방출 시험을 통해 관찰하였다. 표준 CT 시편에 대한 피로균열 진전 시 AE 특성을 관찰하는 실험을 진행하였으며, 기존의 AE 파라미터 분석은 물론 응력확대계수와 AE 발생거동 사이의 관계를 논의하였다. CT 시편 실험 결과에서 균열 성장 길이, AE 최대진폭, AE 에너지, AE hit 발생율 등과 같은 특정 변수들은 응력확대계수 값이 증가함에 따라 이들 값도 증가하는 경향을 나타내었다. 또한 피로사이클 수에 따른 AE 에너지의 변화는 균열진전에 대한 활동성을 평가하는데 사용되는 효과적인 변수중의 하나임을 보여 주었으며, AE 에너지 분석은 균열 활동도와 AE 변수 사이의 관계를 평가하는데 사용될 수 있을 것으로 판단된다.

  • PDF

산양유의 체세포수에 영향을 미치는 비병원성 요인 (Non-Pathogenic Factors Affecting Somatic Cell Counts of Goat Milk)

  • 김민경;최아리;한기성;정석근;오미화;장애라;설국환;함준상
    • Journal of Dairy Science and Biotechnology
    • /
    • 제28권2호
    • /
    • pp.1-5
    • /
    • 2010
  • Somatic cell counts (SCCs) of goat milk can vary widely depending on the counting methods used and non-pathogenic factors; the goat milk industry can be threatened by establishment of a legal standard based on the findings in cow milk. In Korea, SCCs have been excluded from the items that are analyzed under the "Livestock Products Processing and Composition Standards" in accordance with a recent NVRQS Notice amendment. From April to October, SCCs of 150 goat milk samples from 2 farms were analyzed using a Somascope calibrated with standard goat milk samples. Average SCCs of the samples was 598,000/mL, and significant differences were not found between farms and between breeds. SCCs increased from 3 to 8 months after delivery.

  • PDF

TiNi/A16061 형상기억복합재료의 미시적 손상거동과 손상위치측정에 관한 연구 (A Study on the Microscopic Damage Behavior and the Damage Position Evaluation of TiNi/Al6061 Share Memory Alloy Composite)

  • 이진경;박영철;구후택;이규창
    • 대한기계학회논문집A
    • /
    • 제26권9호
    • /
    • pp.1787-1794
    • /
    • 2002
  • TiNi alloy fiber was used to solve the problem of the tensile residual stress as the reinforced material. TiNi alloy fiber improves the tensile strength of composite by occurring compressive residual stress in the matrix using shape memory effect. In order to generate compressive residual stress in TiNi/Al6061 shape memory alloy(SMA) composite, 1, 3 and 5% pre-strains were applied to the composite in advance. It was also evaluated the effect of compressive residual stress corresponding to the pre-strain variation and the volume fraction of TiNi alloy. AE technique was used to clarify the microscopic damage behavior at high temperature and the effect of pre-strain in TiNi/Al6061 SMA composite. The results of the microscopic damage evaluation of TiNi/Al6061 SMA composite under various pre-strain using AE technique can be divided into three stage corresponding to the AE signals. AE counts and events were useful parameters to evaluate the fracture mechanism according to the variation of pre-strain. In addition, two dimensional AE source location technique was applied for monitoring the crack initiation and propagation in composite.

두께변화에 따른 엔지니어링 플라스틱의 파괴인성과 AE특성 (Fracture toughness and AE Characteristics of Engineering plastic according to thickness)

  • 남기우;김선진;안병현
    • 한국해양공학회지
    • /
    • 제10권4호
    • /
    • pp.51-57
    • /
    • 1996
  • A standard method for the evalution of the fracture toughness of the high polymer materials has not been fully developed in comparison with that for metallic materials, and has not yet established. In this paper, fracture toughness tests using polycarbonate specimens were carried out. The fracture thughness tests using polycabonate specimens were carried out. The fracture toughness of commercial polycarbonate were dependent on the specimen thickness. The specimen thickness is necessary above 8mm to obtain the valid $K_{IC}$. A cumulative counts were slightly dependent on specimen thickness.

  • PDF