• 제목/요약/키워드: AAO(Anodic aluminum oxidation)

검색결과 17건 처리시간 0.019초

AAO를 이용한 나노 패턴 마스터 제작에 관한 연구 (Study on Fabrication of Highly Ordered Nano Patterned Master by Using Anodic Aluminum Oxidation)

  • 신홍규;권종태;서영호;김병희
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 춘계학술대회 논문집
    • /
    • pp.368-370
    • /
    • 2007
  • AAO(Anodic Aluminum Oxidation) method has been known that it is practically useful for the fabrication of nano-structures and makes it possible to fabricate the highly ordered nano masters on large surface and even on the 2.5 or 3D surface at low cost comparing to the expensive e-beam lithography or the conventional silicon processing. In this study, by using the multi-step anodizing and etching processes, highly ordered nano patterned master with concave shapes was fabricated. By varying the processing parameters, such as initial matter and chemical conditions; electrical and thermal conditions; time scheduling; and so on, the size and the pitch of the nano pattern can be controlled. Consequently, various alumina/aluminum nano structures can be easily available in any size and shape by optimized anodic oxidation in various aqueous acids. The resulting good filled uniform nano molded structure through hot embossing molding process shows the validity of the fabricated nano pattern masters.

  • PDF

AAO를 이용한 나노 마스터 제작에 관한 연구 (Study on Fabrication of Highly Ordered Nano Master by Using Anodic Aluminum Oxidation)

  • 권종태;신홍규;서영호;김병희
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 추계학술대회 논문집
    • /
    • pp.162-165
    • /
    • 2007
  • AAO(Anodic Aluminum Oxidation) method has been known that it is practically useful for the fabrication of nano-structures and makes it possible to fabricate the highly ordered nano masters on large surface and even on the 2.5 or 3D surface at low cost comparing to the expensive e-beam lithography or the conventional silicon processing. In this study, by using the multi-step anodizing and etching processes, highly ordered nano patterned master with concave shapes was fabricated. By varying the processing parameters, such as initial matter and chemical conditions; electrical and thermal conditions; time scheduling; and so on, the size and the pitch of the nano pattern can be controlled. Consequently, various alumina/aluminum nano structures can be easily available in any size and shape by optimized anodic oxidation in various aqueous acids. In order to replicate nano patterned master, the resulting good filled uniform nano molded structure through electro-forming process shows the validity of the fabricated nano pattern masters.

  • PDF

실리콘 및 사파이어 기판을 이용한 알루미늄의 양극산화 공정에 관한 연구 (Fabrication of Anodic Aluminum Oxide on Si and Sapphire Substrate)

  • 김문자;이진승;유지범
    • 한국재료학회지
    • /
    • 제14권2호
    • /
    • pp.133-140
    • /
    • 2004
  • We carried out anodic aluminum oxide (AAO) on a Si and a sapphire substrate. For anodic oxidation of Al two types of specimens prepared were Al(0.5 $\mu\textrm{m}$)!Si and Al(0.5 $\mu\textrm{m}$)/Ti(0.1 $\mu\textrm{m}$)$SiO_2$(0.1 $\mu\textrm{m}$)/GaN(2 $\mu\textrm{m}$)/Sapphire. Surface morphology of Al film was analyzed depending on the deposition methods such as sputtering, thermal evaporation, and electron beam evaporation. Without conventional electron lithography, we obtained ordered nano-pattern of porous alumina by in- situ process. Electropolishing of Al layer was carried out to improve the surface morphology and evaluated. Two step anodizing was adopted for ordered regular array of AAO formation. The applied electric voltage was 40 V and oxalic acid was used as an electrolyte. The reference electrode was graphite. Through the optimization of process parameters such as electrolyte concentration, temperature, and process time, a regular array of AAO was formed on Si and sapphire substrate. In case of Si substrate the diameter of pore and distance between pores was 50 and 100 nm, respectively. In case of sapphire substrate, the diameter of pore and distance between pores was 40 and 80 nm, respectively

나노 광소자 응용을 위한 알루미늄 양극산화박막 공정 (Thin film process of anodic aluminum oxidation for optoelectronic nano-devices)

  • 최재호;백하봉;김근주
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.106-107
    • /
    • 2007
  • We fabricated anodic aluminium oxides (AAO) on Si and sapphire substrates from the electrochemical reactions of thin AI films in an aqueous solution of oxalic acid. The thin AI films have deposited on Si and Sapphire substructure by using E-beam evaporation and thermal evaporation, respectively. The formation of AAO structures has investigated from FE-SEM measurement image and showed randomly distributed phase of nanoholes instead of the periodic lattice of photonic crystals. The AAO structure on sapphire shows the double layers of nanoholes.

  • PDF

양극산화를 이용한 알루미나 나노세공 멤브레인의 제조 (Fabrication of Alumina Membrane Using Anodic Oxidation Process)

  • 임완순;조경철;조유석;최규석;김도진
    • 한국재료학회지
    • /
    • 제13권9호
    • /
    • pp.593-597
    • /
    • 2003
  • Anodic aluminum oxide (AAO) membrane was made of aluminum sheet (99.6%, 0.2 mm thickness). The regular array of hexagonal nano pores or channels were prepared by two step anodization process. A detail description of the AAO fabrication is presented. After the 1st anodization in oxalic acid (0.3 M) at 45 V, The formed AAO was removed by etching in a solution of 6 wt% $H_3$$PO_4$+1.8 wt% $H_2$$CrO_4$. The regular arrangement of the pores was obtained by the 2nd anodization, which was carried out in the same condition as the 1st anodization. Subsequently, the alumina barrier layer at the bottom of the channel layer was removed in phosphoric acid (1M) after removing of aluminum. Pore diameter, density, and thickness could be controlled by the anodization process parameters such as applied voltage, anodizing time, pore widening time, etc. The pore diameter is proportional to the applied voltage and pore widening time. The pore density and thickness can be controlled by anodization temperature and voltage.

양극산화를 이용한 나노템플레이트 기공 크기 제어에 관한 연구 (A study on the pore size control of nano template by anodic aluminum oxidation)

  • 이수호;서문수;유현민;이재형;정연호;임동건;황현석
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2011년도 제42회 하계학술대회
    • /
    • pp.1495-1496
    • /
    • 2011
  • Anodic aluminum oxide (AAO) nanotemplates for nano electronic device applications have been attracting increasing interest because of ease of fabrication, low cost process, and possible fabrication in large area. The size and density of the nanostructured materials can be controlled by changing the pore diameter and the pole density of AAO nanotemplate. In this paper, AAO nanotemplate was fabricated by second anodization method. In addition, effects of electrolyte and anodization voltate on the microstructure of porous alumina films were investigated. Vertically well aligned pores had the average pore sizes of 15-70 nm and the length of approximately 40 ${\mu}m$.

  • PDF

양극산화공정을 이용한 고세장비의 폴리머 마스터 제작 (Fabrication of Polymer Master with High Aspect Ratio by Using Anodic Aluminum Oxidation)

  • 권종태;신홍규;서영호;김병희
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 춘계학술대회 논문집
    • /
    • pp.285-287
    • /
    • 2008
  • AAO(Anodic Aluminum Oxidation) method has been known that it is practically useful for the fabrication of nano-structures and makes it possible to fabricate the highly ordered nano masters on large surface and even on the 2.5 or 3D surface at low cost comparing to the expensive e-beam lithography or the conventional silicon processing. In this study, by using the multi-step anodizing and etching processes, highly ordered nano patterned master with concave shapes was fabricated. By varying the processing parameters, such as initial matter and chemical conditions; electrical and thermal conditions; time scheduling; and so on, the size and the pitch of the nano pattern can be controlled. Consequently, various alumina/aluminum nano structures can be easily available in any size and shape by optimized anodic oxidation in various aqueous acids. In order to replicate nano patterned master, the resulting good filled uniform nano molded structure through electro-forming process shows the validity of the fabricated nano pattern masters.

  • PDF

반구형 나노 패턴의 크기에 따른 PMMA기판의 광특성 평가 (Fabrication of nano-structured PMMA substrates for the improvement of the optical transmittance)

  • 박용민;신홍규;김병희;서영호
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 추계학술대회 논문집
    • /
    • pp.217-220
    • /
    • 2009
  • This paper presents fabrication method of nano-structured PMMA substrates as well as evaluations of their optical transmittance. For anti-reflective surface, surface coating method had been conventionally used. However, it requires high cost, complicated process and post-processing times. In this study, we suggested the fabrication method of anti-reflective surface by the hot embossing process. Using the nano patterned master fabricated by anodic aluminum oxidation process. Anodic aluminum oxide(AAO) is widely used as templates or a molds for various applications such as carbon nano tube (CNT), nano rod and nano dots. Anodic aluminum oxidation process provides highly ordered regular nano-structures on the large area, while conventional pattering methods such as E-beam and FIB can fabricate arbitrary nano-structures on small area. We fabricated a porous alumina hole array with various inter-pore distance and pore diameter. In order to replicate nano-structures using alumina nano hole array patterns, we have carried out hot-embossing process with PMMA substrates. Finally the nano-structured PMMA substrates were fabricated and their optical transmittances were measured in order to evaluate the charateristivs of anti-reflection. Anti-reflective structure can be applied to various displays and automobile components.

  • PDF

황산 용액에서 Al6061 합금의 아노다이징 피막 형성거동 (Formation Behavior of Anodic Oxide Films on Al 6061 Alloy in Sulfuric Acid Solution)

  • 문성모;정기훈;임수근
    • 한국표면공학회지
    • /
    • 제51권6호
    • /
    • pp.393-399
    • /
    • 2018
  • Formation behavior of aluminum anodic oxide (AAO) films on Al6061 alloy was studied in view of thickness, morphology and defects in the anodic films in 20 vol.% sulfuric acid solution at a constant current density of $40mA/cm^2$, using voltage-time curve, observation of anodized specimen colors and surface and cross-sectional morphologies of anodic films with anodization time. With increasing anodizing time, voltage for film formation increased exponentially after about 12 min and its increasing rate decreased after 25 min, followed by a rapid decrease of the voltage after about 28 min. Surface color of anodized specimen became darker with increasing anodizing time up to about 20 min, while it appeared to be brighter with increasing anodizing time after 20 min. The darkened and brightened surfaces with anodizing time are attributed to an increase in thickness of porous anodic oxide film and a chemical damage of the films due to heat generated by increased resistance of the film, respectively. Cross-sectional observation of AAO films revealed the formation of defects of crack shape at the metal/oxide interface after 15 min which prevents the growth of AAO films. Width and length of the crack-like defect increased with anodizing time up to 25 min of anodizing, and finally the outer part of AAO films was partly dissolved or detached after 30 min of anodizing, resulting in non-uniform surface structures of the AAO films.

AAO Template를 이용한 Au/TiO2 나노섬유 제조 및 응용에 관한 연구 (A Study on the Preparation and Application of Au/TiO2 Nanofiber from AAO Template)

  • 엄선미;박상선;김영덕;김용록;설용건
    • 전기화학회지
    • /
    • 제12권1호
    • /
    • pp.47-53
    • /
    • 2009
  • 본 연구에서는 불순물이 포함된 Al 기판으로부터 두 단계의 양극산화 (anodization) 법에 의해 균일한 나노기공을 갖는 AAO(Anodic Aluminum Oxide)을 제조하였다. 생성된 AAO템플릿 위에 Deposition-Precipitation(DP)방법을 사용하여 수직으로 형성된 $TiO_2$ 나노섬유에 Au를 첨가시켜 2 wt.% $Au/TiO_2$ 나노섬유룰 제조하였다. 두 단계의 양극산화를 통해 규칙적으로 배열된 AAO 기공 형상과 기판 위에 수직으로 배향된 $TiO_2$ 나노섬유의 형상을 SEM을 통해 확인하였다. 또한 $Au/TiO_2$ 나노섬유의 특성은 XRD와 Raman 분석을 통하여 $TiO_2$의 아나타제(anatase)와 루타일(rutile) 결정구조와 $TiO_2$ 나노섬유에 담지된 Au의 존재를 확인하였다. 또한 일산화탄소(CO) 산화반응을 통해 AAO(Anodic Aluminum Oxide)기판 위에 형성된 $TiO_2$와 2 wt% $Au/TiO_2$ 나노섬유의 광촉매적 활성을 비교하였다.