  • Failure phenomena in uni-axial tension test were experimentally and numerically investigated for AA6111-T4, AA5083-H18 and DP-Steel, which were friction-stir welded with the same and different thicknesses. Forming limit diagram(FLD) was measured using hemispherical dome stretching tests for base materials and also predicted by Hill's bifurcation and M-K theories for welded areas. Finite element simulations well predicted hardening behaviors, failure locations as well as failure patterns for the uni-axial tension tests especially utilizing very fine meshes and FLD along with stress softening.

마찰교반용접(FSW) 된 알루미늄 합금(AA6111-T4, AA5083-H18) 및 DP강 판재의 인장 실험시 파단 현상 해석 (Analysis of Failure Phenomena in Uni-axial Tension Tests of Friction Stir Welded AA6111-T4, AA5083-H18 and DP-Steel)

  • 박상준;엄기문;마닝;안강환;정경환;;;;정관수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 춘계학술대회 논문집
    • /
    • pp.258-261
    • /
    • 2007
  • Failure phenomena in uni-axial tension test were experimentally and numerically investigated for AA6111-T4, AA5083-H18 and DP-Steel, which were friction-stir welded with the same and different thicknesses. Forming limit diagram(FLD) was measured using hemispherical dome stretching tests for base materials and also predicted by Hill's bifurcation and M-K theories for welded areas. Finite element simulations well predicted hardening behaviors, failure locations as well as failure patterns for the uni-axial tension tests especially utilizing very fine meshes and FLD along with stress softening.

  • PDF

모재의 방향성에 따른 마찰교반용접 판재의 성형성에 관한 실험적 연구 (Experimental Formability Investigation for FSW Sheets with Respect to Base Material's Directional Combination)

  • 김대용;이원오;김준형;;정관수
    • 소성∙가공
    • /
    • 제18권1호
    • /
    • pp.73-79
    • /
    • 2009
  • In order to investigate the formability of friction stir welded(FSW) tailor welded blanks(TWB) with respect to the base material's directional combination, aluminum alloy AA6111-T4 sheets were welded with three different conjoining types: RD-RD, TD-RD and TD-TD. Here, RD and TD represent rolling and transverse directions, respectively. For experimental formability study, three tests with gradual complexity were performed: the simple tension test with various weld line directions for uni-axial elongation, the hemisphere dome stretching test for biaxial stretching and the cylindrical cup deep drawing test. As a result, all three forming tests showed that RD-RD type samples exhibited the best formability, while TD-TD type sheets showed the least formability performance.

Hot wall epitaxy법에 의한 MgGa2Se4 단결정 박막 성장과 광학적 특성 (Growth and optical properties for MgGa2Se4 single crystal thin film by hot wall epitaxy)

  • 문종대;홍광준
    • 한국결정성장학회지
    • /
    • 제21권3호
    • /
    • pp.99-104
    • /
    • 2011
  • 단결정 성장을 위한 $MgGa_2Se_4$ 다결정은 수평 전기로에서 합성하였으며, 결정구조는 rhombohedral이고 격자상수 $a_0$는 3.953 ${\AA}$, $c_0$는 38.890 ${\AA}$였다. $MgGa_2Se_4$ 단결정박막은 HWE(Hot Wall Epitaxy) 방법으로 반절연성 GaAs(100)기판에 성장시켰다. 단결정박막의 성장 조건은 증발원의 온도 $610^{\circ}C$, 기판의 온도 $400^{\circ}C$에서 진행되었으며 성장 속도는 0.5 ${\mu}m/h$였다. 단결정박막의 결정성은 이중 결정 x-선 회절곡선의 반폭치와 X-선 회절무늬의 ${\omega}-2{\theta}$로부터 구하여 최적 성장 조건을 알 수 있었다. Hall 효과는 van der Pauw 방법에 의해 측정되었으며, 온도에 의존하는 운반자 농도와 이동도는 293 K에서 각각 $6.21{\times}10^{18}/cm^3$, 248 $cm^2/v{\cdot}s$였다. $MgGa_2Se_4$/SI(Semi-Insulated) GaAs(100) 단결정 박막의 광흡수 스펙트럼을 10 K에서 293 K까지 측정하였다. 광흡수 스펙트럼으로부터 구한 에너지 갭 $E_g(T)$는 varshni 공식 $E_g(T)=E_g(0)=({\alpha}T^2/T+{\beta})$을 잘 만족함을 알 수 있었다. 여기서 $E_g(0)=2.34\;eV$, ${\alpha}=8.81{\times}10^{-4}\;eV/K$, ${\beta}=251\;K$였다.