• Title/Summary/Keyword: 65 nm

Search Result 689, Processing Time 0.027 seconds

Inactivation influences on Escherichia coli DS5α by irradiation with 405 nm violet-light

  • Young-Sun Kim;Mun-Jin Choi;Dae-Young Lee;Sang-Ook Kang;Geung-Joo Lee
    • Korean Journal of Agricultural Science
    • /
    • v.50 no.3
    • /
    • pp.417-425
    • /
    • 2023
  • Because an irradiation of 405 nm violet light could have a strong energy, it was used to be sterilized against various microbes in the indoor air condition or fresh food. Escherichia coli is a representative bio-pollutant in the indoor air-borne bacteria, and a hygienic microbe in the horticultural food. This study evaluated the inactivation influences on E. coli DS5α after exposure to 405 nm violet-light (VL) by investigating irradiating time, and the vertical and horizonal distance from light source. The illumination of 405 nm VL was inversely proportional to the distance from the VL source. E. coli DS5α on nutrient agar (NA) was inactivated approximately 50% more than the control when irradiated at 65 cm from 405 nm VL for 3 hours. When compared to the control, E. coli DS5α was inactivated approximately 50% within 70 cm from 405 nm VL for 3 hours. As it was irradiated for 3 hours 70 cm away from 405 nm VL, the horizonal distance from the point was negatively correlated to the inactivation of E. coli DS5α. These results indicated that the inactivation of E. coli DS5α grown on NA medium needs to be irradiated with 405 nm within 70 cm from the light source for 3 hours.

Studies on reactive ion etching of GaN using BCl$_{3}$ (BCl$_{3}$를 이용한 GaN계 질화합물 반도체의 RIE에 관한연구)

  • 윤관기;최용석;이일형;유순재;이진구;김송강
    • Proceedings of the IEEK Conference
    • /
    • 1998.06a
    • /
    • pp.409-412
    • /
    • 1998
  • BCl/sub 3/ 및 Cl/sub 2/ 반응가스를 사용하여 RIE 장치로 GaN의 건식식각을 연구하였다. RF 전력, 반응가스의 유량 및 반응가스의 혼합비 등의 변화에 따른 최적의 식각공정 조건 및 결합특성을 연구하였다. RF 전력에 따른 GaN의 식각율은 챔버압력 25mTorr, BCl/sub 3/ 유량 40 sccm의 조건에서 RF 전력이 100W일때 17nm/min을 얻었다. BCl/sub 3/의 유량에 따른 식각율은 RF 전력 100W 챔버압력 20mTorr, Cl/sub 2/ 유량 5sccm의 조건에서 BCl/sub 3/ 유량이 40 sccm일때 65nm/min을 얻었다. Cl/sub 2//BCl/sub 3/ 혼합가스 비율에 따른 식각율은 Cl/sub 2/ 유량을 5sccm으로 고정하고 BCl/sub 3/ 유량을 변화시켰을때 RF 전력 100W 및 챔버압력 20mTorr의 조건에서 혼합비가 0.25일때 50nm/min을 얻었다. RF 전력에 따른 PR의 식각율은 챔버압력 25mTorr, Cl/sub 2/ 유량 0 sccm 및 BCl/sub 3/ 유량 40 sccm의 조건에서 RF 전려이 100W일때 15nm/min을 얻었다. 또한, 챔버압력 20mTorr, Cl/sub 2/ 유량 5 sccm 및 BCl/sub 3/ 유량 20sccm의 조건에서 RF 전력이 100W 일때 82nm/min을 얻었다.

  • PDF

Simultaneous Determination of Tar Color Additives in Cold Syrups by Ion Pair-high Performance Liquid Chromatography (이온쌍-고성능 액체크로마토그래피에 의한 감기약 시럽에서 타르색소 첨가물의 동시분석)

  • Jin, Jing-Yu;Huang, Hu;Lee, Beom-Gyu;Lee, Won-Jae
    • KSBB Journal
    • /
    • v.25 no.5
    • /
    • pp.459-465
    • /
    • 2010
  • A simple and efficient analytical method for the simultaneous determination of seven tar color additives was developed using ion pair high performance liquid chromatography. The conditions for HPLC analysis were as follows: column, ${\mu}$-Bondapak C18 (10 ${\mu}m$, 300 ${\times}$ 3.9 mm i.d.); gradient mobile phase, 0.025 mol/L ammonium acetate (containing 0.01 mol/L tetrabutylammonium bromide)-acetonitrile-methanol (65:25:10) as a mobile for fraction A and 0.025 mol/L ammonium acetate (containing 0.01 mol/L tetrabutylammonium bromide)-acetonitrilemethanol (40:50:10) as a mobile for fraction B; flow rate, 1.0 mL/ min; detection wavelength, 254/520/620 nm. We could attain to the detection limits as 0.01~0.05 ${\mu}$g/mL (254 nm) and 0.005~0.01 ${\mu}$g/mL (520 nm) for six red tar color additives, and 0.05 ${\mu}$g/mL (254 nm) and 0.002 ${\mu}$g/mL (620 nm) for Fast green FCF. This analytical method was applicable to determine the tar color additives contained in several commercial cold syrups.

Dielectrical and Electrical Characteristics of 9/65/35 PLZT Thin Films (9/65/35 PLZT 박막의 유전적, 전기적 특성)

  • Kang, Chong-Yun;Choi, Hyung-Wook;Paik, Dong-Soo;Yun, Hyun-Sang;Shin, Hyun-Yong;Park, Chang-Yub
    • Proceedings of the KIEE Conference
    • /
    • 1994.07b
    • /
    • pp.1305-1307
    • /
    • 1994
  • 9/65/35 PLZT thin films were prepared by sol-gel processing and annealed by direct insertion, 9/65/35 PLZT thin films were poly-crystallized after direct insertion at $750^{\circ}C$ for 3omin. The grain size of film was 50 nm, coercive field was 28.2 kV/cm and remnant polarization was $3.68 {\mu}C/cm^2$.

  • PDF

Photoluminescence properties of $CaS_{1-x}Se_x:Eu$ phosphors ($CaS_{1-x}Se_x:Eu$ 형광체의 발광 특성)

  • Ryu, Eun-Kyoung;Huh, Young-Duk
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.17 no.5
    • /
    • pp.204-209
    • /
    • 2007
  • We synthesized a series of $CaS_{1-x}Se_x:Eu$ red-emitting phosphors for application in phosphor-converted three-band white light emitting diode(LED). The photoluminescence and structural properties of $CaS_{1-x}Se_x:Eu$ were examined. The $CaS_{1-x}Se_x:Eu$ phosphors have a strong absorption at 455 nm, which is the emission wavelength of a blue LED. CaS:Eu has a red omission peak at 651 nm due to the $4f^65d^1(T_{2g}){\rightarrow}4f^7(^8S_{7/2})$ transition of the $Eu^{2+}$. The emission peak of $CaS_{1-x}Se_x:Eu$ is shifted from 651 to 598 nm with increasing Se content. $CaS_{1-x}Se_x:Eu$ can be used as wavelength-tunable red-emitting phosphors pumped by a blue LED. We also fabricated a three-band white LED by doping $SrGa_2S_4:Eu$ and $CaS_{0.50}Se_{0.50}:Eu$ phosphors onto a blue LED chip.

GOLDD 구조를 갖는 LTPS TFT 소자의 전기적 특성 비교분석

  • Kim, Min-Gyu;Jo, Jae-Hyeon;Lee, Jun-Sin
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.11a
    • /
    • pp.40-40
    • /
    • 2009
  • The electrical characteristic of the conventional self-aligned polycrystalline silicon (poly-Si) TFTs are known to present several undesired effects such as large leakage current, kink effect and hot-carrier effects. In this paper, LTPS TFTs with different GOLDD length were fabricated and investigated the effect of the GOLDD. GOLDD length of 1, 1.5 and $2{\mu}m$ were used, while the thickness of the gate dielectrics($SiN_x/SiO_2$) was fixed at 65nm(40nm/25nm). The electrical characteristics show that the kink effect is reduced at the LTPS TFTs, and degradation from the hot-carrier effect was also decreased by increasing GOLDD length.

  • PDF

Luminescent properties of magnesium thiogallate phosphor with green emission for LEDs

  • Kim, Kyung-Nam;Kim, Jae-Myung;Choi, Kyoung-Jae;Park, Joung-Kyu;Kim, Chang-Hae
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2005.07b
    • /
    • pp.1331-1333
    • /
    • 2005
  • A magnesium thiogallate phosphor doped with europium was prepared by solid-state method. This phosphor has green emission near 535 nm due to the allowed transition from $4f^65d$ at an excitation state $(T_{2g})$ to $4f^7 (^8S_{7/2}) at a ground state of $Eu^{2+}$ ion. This phosphor shows a wide excitation spectrum from ultra violet (300 nm) to bluish green (515 nm).

  • PDF

A Study on the Mechanism of Photoluminescence in Poly(3-hexylthiophene) (Poly(3-hexylthiophene)의 PL 발광 메카니즘에 관한 연구)

  • 김주승;서부완;구할본
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.14 no.2
    • /
    • pp.133-138
    • /
    • 2001
  • We studied the optical properties of poly(3-hexylthiophene) for applying to the emitting material of organic electro luminescent device. The infrared spectrum and NMR of synthesized polymer gave good evidence for the conjugation of 3-hexylthiophene monomer unit. We confirmed that poly(3-hexylthiophene) contains the HT(head-to-tail)-HT(head-to-Tail) linkage larger than 65% based on NMR analysis. FTIR and raman spectroscopy show that poly(3-hexylthiophene) has two main vibration levels which have an energy about 0.18eV and 0.36eV. Electronic absorption spectra shifted to the shorter wavelength with increasing temperature, which is related to a conformational transition of the polymer. Photoluminescence spectrum generated at low temperature(10K) is separated at 669nm, 733nm and 812nm that it's because of phonon energy generated from the lattice vibration.

  • PDF

An Electron Microscopic Structure of Rotavirus by Negative Stain (Negative stain을 이용한 Rotavirus의 투과전자현미경적 구조)

  • Kwon, Jung-Kyun
    • Applied Microscopy
    • /
    • v.24 no.4
    • /
    • pp.107-114
    • /
    • 1994
  • The Rotaviruses are members of the family Reoviridae and are the major cause of severe childhood gastroenteritis worldwide. Recently, electron microscopy has been used to detect non-group A rotaviruses to determine a relatively high resolution structure of the rotavirion. Mature, infectious virions(double-shelled particles) have a diameter of approximately 70nm, and have a capsid structure composed of two concentric protein layers. We have studied patient's stool specimen by negative staining technique complete removal of sucrose suspension. This negative staining technique that could be carried out in about 30 minutes and that could be used with crude stool specimen was an advantage of major significance. Removal of sucrose in the sample by has been completed washing with distilled of sucrose and by washing with distilled water. Ultrastructurally, typical feature of rotavirus has a double capsid construction with an inner capsid of 55nm and on outer 65-70nm diameter can be clearly demonstrated.

  • PDF

Formation and Thermal Decomposition of a Quasicrystalline Phase in Al-Fe-Mo Alloys (Al-Fe-Mo 합금에서 준결정상의 생성 및 열분해에 관한 연구)

  • Kim, Suk Hwan
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.18 no.6
    • /
    • pp.362-368
    • /
    • 2005
  • Formation and thermal stability of a quasicrystalline phases in Al-Fe-Mo alloys were investigated by means of melt-spinning process and subsequent heat treatment test. Thermal decomposition and phase transformation process of the as-spun alloys were studied using X-ray diffraction and electron microscopy. The melt-spun Al-Fe-Mo alloys contained an icosahedral quasicrystalline phase with a quasilattice constant of 0.457 nm. Icosahedral phase formed at a composition of $Al_{82.5}Fe_{14}Mo_{3.5}$ as a metastable phase during rapid solidification was transformed into the stable crystalline phases, cubic 1/0 approximant and monoclinic ${\lambda}$-phase, upon heating. A metastable icosahedral and cubic(a = 0.93 nm) phases in as-spun $Al_{65}Fe_{20}Mo_{15}$ alloy were decomposed into two cubic(a = 0.62, 0.31 nm) phases by heat treatment.