• Title/Summary/Keyword: 6 mm steel plate

Search Result 108, Processing Time 0.021 seconds

A Study of Weldability and Welded Joint Performance on the Gas Shield Arc Welding (FCAW) of SM490TMC Steel Plate (120mm) (SM490TMC 극후판(120mm) 강재의 가스실드아크용접(FCAW)을 이용한 용접성 및 이음성능에 관한 연구)

  • Kim, Sung Bae;Hong, Hyung Ju;Choi, Young Han;Kim, Sang Seup
    • Journal of Korean Society of Steel Construction
    • /
    • v.29 no.6
    • /
    • pp.455-465
    • /
    • 2017
  • To figure out the weldability and welded joint performance on the FCAW of SM490TMC 120mm, several specimens were manufactured and 10 kinds of experiments were implemented. The result of the weld zone chemical composition test, weld metal tensile test, weld zone tensile test, and weld zone impact test has satisfied the KS. Especially, the weld zone tensile test result shows the base metal fracture, which means the weld zone performs enough required performance. In addition, the results of the weld zone bending test, hardness test, macroscopic test, microscopic test, and the maximum hardness in HAZ were showing that the FCAW weld zone has fine quality.

Residual Stress and Displacement Analysis of Thick Plate for Partial Penetration Multi-Pass Weldment (후판의 부분용입 다층용접에 대한 잔류음력 및 변형해석)

  • Kim, Seok;Bae, Sung-In;Song, Jung-Il
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.25 no.11
    • /
    • pp.1813-1819
    • /
    • 2001
  • Partial penetration welding Joint defines that groove welds without steel backing, welded from on side, and groove weeds welded from both sides but without back gouging, that is. it has an unwelded portion at the root of the weld. In this study we analysed fur residual stress and displacement distribution on partial penetration welding condition of thick plate metal. For 25.4mm thick plate, theoretical residual stress and displacement analysis by finite element method using ABAQUS was carried out and compared with the experimental result using hole-drilling method. In results of the condition of partial penetration, it appeared that longitudinal stress at welding area was a little difference and transverse stress did not have any effect by partial penetration multi-pass welding. From a point of welding distortion in partial penetration multi-pass welding, it seemed to be better to control root face smaller than 6.35mm.

A Study on the Damage Design of Military Aircraft Structure Material by Armor Piercing Bullet Hit (철갑탄 피격에 의한 군용 항공기 구조재료의 손상설계에 관한 연구)

  • Hur, Jang-Wook;Hyun, Young-Jin
    • Journal of the Korea Institute of Military Science and Technology
    • /
    • v.13 no.6
    • /
    • pp.1051-1057
    • /
    • 2010
  • Database for the damage reference by armor piercing bullet test was established for both tube and plate specimens having a range of thickness. As the inclined angles of hit are increasing, it has been found that penetration damage diameter tends to increases accordingly in both specimen of the tube and plate, and such penetration damage diameter on the rear side becomes bigger than those on the front side. The tube specimen showed that the damage becomes bigger when central areas rather than the peripheral were hit. Through the plate test, it also has been found that the penetration ballistic limit for Al alloy is about 25.4mm and that of stainless steel about 12.7mm. From the fatigue analysis results using the database for damage reference, it has been identified whether the safety requirements of military aircraft could be met.

Effect of chitosan/carbon nanotube fillers on vibration behaviors of drilled composite plates

  • Demir, Ersin;Callioglu, Hasan;Sayer, Metin;Kavla, Furkan
    • Steel and Composite Structures
    • /
    • v.35 no.6
    • /
    • pp.789-798
    • /
    • 2020
  • The effect of Chitosan (CS), Carbon Nanotube (CNT) and hybrid (CS-CNT) fillers on the natural frequency of drilled composite plate is investigated by experimentally in this study. The numerical validation is also made with a program based on Finite Element Method (SolidWorks). Nine types filled and one neat composite plates are used in the study. The fillers ratios are 1% CS, 2% CS, 3% CS, 0.1% CNT, 0.2% CNT, 0.3% CNT, 1% CS+0.3% CNT, 2% CS+0.3% CNT, 3% CS+0.3% CNT. The specimens cut to certain sizes by water jet from the plates 400 mm × 400 mm in dimensions. Some of them are drilled in certain dimensions with drill. The natural frequency of each specimen is measured by the vibration test set up to determine the vibration characteristic. The vibration test set up includes an accelerometer, a current source power unit, a data acquisition card and a computer. A code is written in Matlab® program for the signal processing. The study are investigated and discussed in four main points to understand the effect of the fillers on the natural frequency of the composite plate. These are the effect of fillers contents and amounts, orientation angles of fibers, holes numbers and holes sizes. As results, the natural frequency of the plate with 1% CS and 0.1% CNT hybrid filler is lower than those of the plates with other fillers ratios for 45° orientation angle. Besides, in the composite plate with 0° orientation angle, the natural frequency increases with increasing the filler ratio. Moreover, the natural frequency increases until a certain hole number and then it decreases. Furthermore, the natural frequency is not affected until a certain hole diameter but then it decreases.

A Study on Weldability and Prediction of Nugget Shape in Dissimiar Metal Arc Spot Weld (이종 금속의 아크 스폿 용접성 및 접합부 형상 예측에 관한 연구)

  • Kim, Gi Sun;Jang, Gyeong Bok;Gang, Seong Su
    • Journal of Welding and Joining
    • /
    • v.18 no.2
    • /
    • pp.184-184
    • /
    • 2000
  • In this study, the lap welding between austenitic stainless steel and carbon steel was carried out using arc spot welding process and weldability of welded specimens was estimated. From the tensile-shear strength test, micro Vickers hardness test, and microstructure observation, specimen of 6.5mm(hole of upper plate) showed the best results in terms of tensile-shear strength and nugget shape. And there was an unmixed zone in fusion boundary between the carbon steel base metal and bulk weld metal. This zone had very thin width with the hard microstructure. The shape of weld nugget in arc spot welding of dissimilar metal welds was predicted by searching thermal history of a weld joint through a three-dimensional finite element model. From the numerical analysis, predicted the shape of weld nugget showed good agreement with the experiment(Received August 24, 1999)

A Study on Weldability and Prediction of Nugget Shape in Dissimilar Metal Arc Spot Weld (이종 금속의 아크 스폿 용접성 및 접합부 형상 예측에 관한 연구)

  • 김기순;장경복;강성수
    • Journal of Welding and Joining
    • /
    • v.18 no.2
    • /
    • pp.57-63
    • /
    • 2000
  • In this study, the lap welding between austenitic stainless steel and carbon steel was carried out using arc spot welding process and weldability of welded specimens was estimated. From the tensile-shear strength test, micro Vickers harness test, and microstructure observation, specimen of $psi6.5mm$(hole of upper plate) showed the best results in terms of tensile-shear strength and nugget shape. And there was an unmix zone in fusion boundary between the carbon steel base metal and bulk weld metal. This zone had very width with the hard microstructure. The shape of weld nugget in arc spot welding of dissimilar metal melds was predicted by searching thermal history of a weld joint through a three-dimensional finite element model. From the numerical analysis, predicted the shape of weld nugget showed good agreement with the experiment.

  • PDF

Biomechanical Testing of Anterior Cervical Spine Implants: Evaluation of Changes in Strength Characteristics and Metal Fatigue Resulting from Minimal Bending and Cyclic Loading

  • Kim, Sung-Bum;Bak, Koang-Hum;Cheong, Jin-Hwan;Kim, Jae-Min;Kim, Choong-Hyun;Oh, Seong-Hoon
    • Journal of Korean Neurosurgical Society
    • /
    • v.37 no.3
    • /
    • pp.217-222
    • /
    • 2005
  • Objective: To achieve optimal fit of implant, it is necessary to bend the implant during spine surgery. Bending procedure may decrease stiffness of plate especially made of titanium and stainless steel. Typically titanium suffers adverse effects including early crack propagation when it is bent. We investigate whether 6 degree bending of titanium plates would decrease the stiffness after full cyclic loading by comparing with non-bending titanium plates group. Methods: Authors experimented 40 titanium alloy plates of 57mm in length, manufactured by 5 different companies. Total 40 plates were divided into two groups (20 bent plates for experimental group and 20 non-bent plates for control group). Twenty plates of experimental group were bent to 6 degree with 3-point bending technique and verified with image analyzer. Using the electron microscope, we sought for a initial crack before and after 3-point bending. Mechanical testing by means of 6000 cyclic axial-compression loading of 35N in compression with moment arm of 35mm-1.1 Nm was conducted on each plate and followed by the electron microscopic examination to detect crack or fissure on plates. Results: The stiffness was decreased after 6000 cyclic loading, but there was no statistically significant difference in stiffness between experimental and control group. There was no evidence of change in grain structure on the electron microscopic magnification. Conclusion: The titanium cervical plates can be bent to 6 degree without any crack or weakness of plate. We also assume that minimal bending may increase the resistance to fatigue fracture in cervical flexion-extension movement.

Development of Inspection Technique for Filling or Unfilling of Containment Liner Plate Backside Concrete in Nuclear Power Plant (원전 격납건물 라이너플레이트 배면 콘크리트 채움 여부 점검 기술 개발)

  • Lee, Jeong Seok;Kim, Wang Bae;Kwak, Dong Ryul
    • Transactions of the Korean Society of Pressure Vessels and Piping
    • /
    • v.16 no.1
    • /
    • pp.37-41
    • /
    • 2020
  • The Nuclear containment building is a main safety-related structure that performs shielding and conservation functions to prevent highly radioactive materials from leakage to the outside environment in the case of various environmental conditions and postulated accidents. The containment building contains a reactor, steam generator, pressurizer, tank, reactor coolant system, auxiliary system and engineering safety system, and is designed so that highly radioactive materials above the limits specified in 10 CFR 100 do not escape to the outside environment in the case of LOCA(Loss of Coolant Accident) for instance. The containment metal liner plate(CLP) is a carbon steel plate with a nominal plate thickness of 6 mm, which functions as a mold for the wall and dome of the containment building when concrete is filled, fulfills airtightness to prevent leakage of seriously radioactive materials. In recent years, backside corrosion was found on the liner plate in some domestic nuclear power plants. The main cause of backside corrosion was unfilled concrete. In this paper, an inspection technique of assessing filling suitability for CLP backside concrete is developed. Results show that the validity of inspection technique for CLP backside concrete using vibration sensor is successfully verified.

A Study on the Fatigue Crack Growth Behaviour for the Welded Configuration in Pressure Vessel Stiffener (압력용기 보강재의 용접 형태에 따른 피로균열성장 거동에 관한 연구)

  • 차용훈;김하식;성백섭
    • Journal of the Korean Society of Safety
    • /
    • v.16 no.3
    • /
    • pp.1-6
    • /
    • 2001
  • The study is to investigate the influence on the fatigue crack growth behaviors for the welded configuration in pressure vessel stiffener. In order to perform this goal, the automatic welded specimens were prepared. The material is ASTM A516 grade 60 steel used in pressure vessel mainly. In skip welding of pad-on-plate, continuous fillet welding and PWHT specimen, fatigue crack is generally initiated at the starting and end old toe zone, and ruptured at the starting old toe zone. The fatigue life of pad-on-plate of the continuous fillet welding specimen is larger than that of pad-on-plate skip fillet welding specimen about 85% under low load, about 20% under high load and less than that of two-pad continuous fillet welding specimen about 85%. In da/dN-$\Delta$K curve under low load, skip fillet welding specimen of pad-on-plate showed retardation on the initial crack, and the fatigue crack growth rate at the low region of $\Delta$K greater specimen E($3.8 {\times} 10^{-6}mm/cycle$). And the fatigue life of welding specimen was smaller than that of PWHT specimen.

  • PDF

The Effects of Welding Clearance and bending moment on Spot Weldability (점용접 간극과 굽힘 모멘트가 용접성에 미치는 영향)

  • Lim, Jae-Kyoo;Song, Jun-Hee;Kuk, Jung-Ha;Yang, Seung-Hyon
    • Proceedings of the KSME Conference
    • /
    • 2001.11a
    • /
    • pp.55-60
    • /
    • 2001
  • The automobile is made up of thousands of parts. Some parts are formed by pressing and combined by spot welding. To find weldability conditions of spot welding, clearance between two welding plates was made and after spot welding, weldability is evaluated by means of tensile shear load, nugget size and shape. Specimen used in this study was a steel plate of 1.2mm thickness and electrode was Cu-Cr alloy of 6mm diameter. When spot welding started, the clearance of two specimens was changed 0mm, 3mm and 5mm and distance from vise to measure influence of bending moment 25mm, 45mm, 65mm step by step. The fractured surface of specimen after this test was observed by Optical Microscope to measure microstructure and nugget shape. When clearance of two specimen was 3mm and 5mm, strength and nugget size was decreased and nugget shape was not clear. The much bending moment and crosshead speed are the much tensile shear load is.

  • PDF