• 제목/요약/키워드: 5G welding

검색결과 51건 처리시간 0.024초

Ni기 초합금 용접부의 열처리에 따른 미세조직 변화와 미세경도 (Microstructural Evolutions and Microhardness of the Heat Treated Ni-base Superalloy Weldment)

  • 김광수;지정훈
    • 열처리공학회지
    • /
    • 제18권5호
    • /
    • pp.297-304
    • /
    • 2005
  • This study was performed to determine the repair weldability of the damaged Ni type superalloy used for gas turbine blade. The experimental works included the evaluation of the microstructures of the damaged blade, selection of the repair welding procedure, characterization of repair weldment and finding the heat treatment procedures for repaired weldment. The morphology of the microstructure for the base metal was composed of austenite matrix with cubical ${\gamma}^{\prime}$ phase, MC type coarse precipitates located within grain and fine $M_{23}C_6$ type precipitates decorated at grain boundaries. The repair welding process using 90 amp current exhibited the best weld properties showing no weld microcracks. The solution and aging heat treatments of the repaired weldment could recover the original service properties of the damaged blade.

Nd:YAG 레이저빔을 이용한 SCP 강판과 STS304강판 용접시 오프셋(off-set) 위치 결정에 관한 연구 (A study of the determination of off-set position for Nd:YAC laser welding between SCP steel sheet and STS304 sheet)

  • 윤부선;김도훈;박기영;이경돈
    • 한국레이저가공학회지
    • /
    • 제7권2호
    • /
    • pp.1-10
    • /
    • 2004
  • This work was attempted to join SCP sheet and STS304 sheet by using Nd:YAC laser beam. SCP sheet has good formability and low cost, while STS304 has excellent corrosion resistance and mechanical properties in high temp. In this experiment, butt joint type was used to develop the tailored blank welding for dissimilar steel. Sheets which have different thermal properties. Computer simulation was conducted to obtain the off-set position for efficient welding by considering laser power, scanning speed, focal length and basic properties. The result showed that the optimum thermal distribution was obtained when the laser beam was irradiated at $0.05{\sim}0.1$ mm off-set toward the SCP sheet side. The experiment was conducted based on the result of computer simulation to show the same optimum conditions. Optimum conditions were 3KW in laser beam power, 6m/min in scanning speed, -0.5mm in focal position, 0.1mm off-set toward SCP. Microhardness test, tensile test, bulge test, optical microscopy, EDS, and XRD were performed to observe the microstructure around fusion zone and to evaluate the mechanical properties of optimum conditions, The weld zone had high microhardness values by the formation of the martensitic structure. Tensile test measured the strength of welded region by vertical to strain direction and the elongation of welded region by parallel to strain direction. Bulge test showed $52\%$ formability of the original materials. Bead shape, grain size, and martensitic structure were observed by the optical microscopy in the weld zone. Detailed results of EDS, XRD confirmed that the welded region was connected of martensitic structure.

  • PDF

플라스마 아크 紛體肉盛法에 의한 Al 合金의 硬化厚膜 合金化層의 形成 (Formation of Thicker hard Alloy Layer on Aluminum Alloy by PTA Overlaying with Metal Powders)

  • 박성두;이영호
    • Journal of Welding and Joining
    • /
    • 제11권2호
    • /
    • pp.74-85
    • /
    • 1993
  • Effect of Si metal powders addition with the plasma transferred arc(PTA) overlaying process on characteristics of the alloyed layer in aluminum alloy(A5083) has been investigated. The overlaying conditions were 175-250A in plasma arc current, 500mm/min in travel speed, the 5-20g/min in powder feeding rate. Main results obtained are summarized as follows. 1)Sufficient size of molten pool on surface of base metal was required for forming an alloyed layer; in a fixed travel, the formation of alloyed layer with clear and beautiful surface depend upon the plasma arc current and powder feeding rate; the greater plasma arc current and the smaller powder feeding rate were, the better bead was formed. Optimum alloyed conditions by which an excellent alloyed bead obtained was 225A in plasma arc current. PTA process made it possible to form an alloyed layer with up to 67wt% Si. 2)Microstructure in the alloyed layer was in accord with prediction from the Al-Si phase diagram 3)The hardness of the alloyed layer increased in proportion to Si content. 4)As volume fraction of primary Si increased, the specific wearness of the alloyed layer was significantly improved. However, no further improvement was found when the volume fraction was greater than about 30%. 5)Utilizing the PTA process, a crack free alloyed layer with maximum hardness of about Hv 310 could be obtained.

  • PDF

폭발접합된 열교환기류 튜브와 튜브시트의 계면 특성에 관한 고찰 (A Study on the Tube/tubesheet Interface in the Heat Exchangers Jointed by Explosive Bonding)

  • 이병일;공창식;이상철
    • Journal of Welding and Joining
    • /
    • 제18권4호
    • /
    • pp.38-47
    • /
    • 2000
  • Characteristics of the interface between tube and tube sheet which were formed by explosive expansion and roll expansion, have been studied in the research. The results are as follows: Optimum amounts of explosives for the expansion of Alloy 600 (19.05mm and 15.88mm) were found to be RDX 3.5-8.5g/m. Because explosive expansion caused les strain hardening and increased bounding strength, characteristics of the explosively expanded were better than those of mechanically expanded. As the transition region of the explosive expansion is inactive, the resistance to the stress corrosion cracking increases by 30∼40% compared to the roll and hydraulic expansion.

  • PDF

ʼn-BGA에서 Sn-Ag-Cu 솔더의 도금층에 따른 솔더링성 연구 (A Study on Solderability of Sn-Ag-Cu Solder with Plated Layers in ʼn-BGA)

  • 신규식;정석원;정재필
    • Journal of Welding and Joining
    • /
    • 제20권6호
    • /
    • pp.59-59
    • /
    • 2002
  • Sn-Ag-Cu solder is known as most competitive in many kinds of Pb-free solders. In this study, effects of solderability with plated layers such as Cu, Cu/Sn, Cu/Ni and Cu/Ni/Au were investigated. Sn-3.5Ag-0.7Cu solder balls were reflowed in commercial reflow machine (peak temp. : 250℃ and conveyer speed : 0.6m/min). In wetting test, immersion speed was 5mm/sec., immersion time 5sec., immersion depth 4mm and temperature of solder bath was 250℃. Wettability of Sn-3.5Ag-0.7Cu on Cu, Cu/Sn (5㎛), Cu/Ni (5㎛), and Cu/Ni/Au (5㎛/500Å) layers was investigated. Cu/Ni/Au layer had the best wettability as zero cross time and equilibrium force, and the measured values were 0.93 sec and 7mN, respectively. Surface tension of Sn-3.5Ag-0.7Cu solder turmed out to be 0.52N/m. The thickness of IMC is reduced in the order of Cu, Cu/Sn, Cu/Mi and Cu/Ni/Au coated layer. Shear strength of Cu/Ni, Cu/Sn and Cu was around 560gf but Cu/Ni/Au was 370gf.

조선업 용접공진폐증에서 용접 흄 폭로력에 따른 방사선 소견의 경시적 변화양상 (Chest Radiological Changes after Cessation and Decrease of Exposure to Welding Fume in Shipyard Welders)

  • 손혜숙;이종태;신해림;이채언;배기택;박형종;김용완;윤임중
    • Journal of Preventive Medicine and Public Health
    • /
    • 제22권3호
    • /
    • pp.328-336
    • /
    • 1989
  • 27 shipyard welders were diagnosed as pneumoconiosis and suspected pneumoconiosis(1976-1988) by chest radiographs and were observed over three years. 27 welders were divided into three groups by the state of exposure to welding fume i.e. cessation, decresase or continuity of exposure. And we observed the changing pattern of the chest radiographs of 27 welders with the passage of time. The results were as follows; 1. Grour I (ceased exposure to welding fume) were 10 cases(3 cases: suspected pneumoconiosis,7 cases: pneumoconiosis). Chest radiographs of all cases were improved. The shape and size of small opacities was improved in 6 cases(85.7%) and did not changed in 1 case(14.3%) out of 7 pneumoconiosis welders. 2. Group II (decreased exposure to welding fume) were S cases(2 cases: suspected pneumoconiosis, 3 cases: pneumoconiosis). Chest radiographs were progressed in 2 cases(40%), did not changed in 1 case(20%), were improved in 2 cases(40%) out of 5 cases. The shape and size of small opacities was progressed in 1 case(33.3%) and was improved in 2 cases(66.7%) out of 3 pneumoconiosis welders. 3. Group III(continued expoxsure to welding fume) were 12 cases(1 case: suspected pneumoconiosis, 11 cases: pneumoconiosis). Chest radiographs were progressed in 9 cases(75%), did not changed in 3 cases(25%) out of 12 cases. The shape and size of small opacities was progressed in 1 case(9.1%) and did not changed in 10 cases(90.9%) out of 11 pneumoconiosis welders. 4. The average duration for development into suspected pneumoconiosis was 6.6 years and for progression of each one category after that was 2.2 years(p<0.01). The radiological appearance of pneumoconiosis had disappeared or decreased after cessation of exposure to the welding fume. So that, early detection and control e.g., change of department of pneumoconiosis of welders by screening program will be important for medical surveillance of welders.

  • PDF

AISI 316L 용접부의 시그마상 형성에 영향을 미치는 크롬/니켈 당량비 (The effect of sigma phases formation depending on Cr/Ni equivalent ratio in AISI 316L austenitic stainless steel weldments.)

  • 김연희;장아영;최창현;강동훈;전재혁;변지철;정광호;이상화;이해우
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2010년도 춘계학술발표대회 초록집
    • /
    • pp.21-21
    • /
    • 2010
  • AISI 316L 용접금속의 크롬/니켈 당량비에 따른 시그마상의 영향을 알아보기 위하여 응고모드가 다른 3종류의 플럭스 코어드 와이어를 제작하였다. AISI 316L 시편에 FCAW 프로세스를 적용한 용접재를 $650^{\circ}C$, $750^{\circ}C$, $850^{\circ}C$, $950^{\circ}C$에서 각 각 1H, 5H, 24H, 72H동안 열처리하였다. 크롬/니켈 당량비가 높을수록 즉, 크롬의 함량이 높아질수록 $\delta$-페라이트 함량은 증가하였으며, $\delta$-페라이트는 고온에서 시그마상으로 변태되었다. $\delta$-페라이트는 $650^{\circ}C$에서 가장 느리게 분해되었으며 $850^{\circ}C$에서 가장 활발히 분해되었다. 용접부의 특성상 크롬과 니켈 등의 합금원소에 의하여 응고온도범위가 넓어져 $950^{\circ}C$에서도 시그마상이 석출되었으며, 5시간 이상 유지 시 구형으로 존재하였다. 충격시험 시 시그마상에 의해 취약해진 inter-dendrite 를 따라 파면이 형성되었으며, $-100^{\circ}C$이하의 극저온에서는 시그마상의 양과 무관하게 충격흡수에너지는 0에 가까워졌다. 하지만 3%미만의 $\delta$-페라이트를 함유하는 AF모드에서 발생한 DDC와 미량의 시그마상은 충격흡수에너지에 결정적인 영향을 미치지 않았다.

  • PDF

고출력 $CO_2$레이저빔에 의한 구리, 청동/알루미늄 합금 클래딩 (Cladding of Cu and Bronze/Al Alloy by $CO_2$ Laser)

  • 강영주;김재도
    • Journal of Welding and Joining
    • /
    • 제15권4호
    • /
    • pp.109-115
    • /
    • 1997
  • Laser cladding is a technique for modification of metal surface. In this laser cladding experiment a metal powder feeding system was developed for more efficient laser cladding. This system can reduce processing time and be used simpler than the conventional method. The feeding of metal powder has given a rise to the process for sequential buildup of bulk rapidly solidified materials in the form of fine powder stream to the laser cladding process. The parameters of laser cladding have been investigated using this experimental equipment. Bronze on aluminum alloy and copper on aluminum alloy were experimented by using defocused beam, powder feeding system, and gas shielding. Good cladding was achieved in the range of beam travel speed of 2.25m/min. In the case of copper/aluminum and bronze/aluminum substrate, the absorption of laser beam was too high to produce low diluted clad. In the case of copper/1050 aluminum, the optimal laser cladding condition was of laser power of 2.8kW, powder feed rate of 0.31g/s and beam travel speed of 2.25m/min. In the case of bronze/aluminum the optimal condition is of laser power of 2.5kW, powder feed rate of 0.31g/s, and beam travel speed of 2.36m/min.

  • PDF

분말송급장치의 개조에 의한 미세$5\mu\textrm{m}$ $Al_2O_3$분말의 송급 특성개선 및 플라즈마 용사조건에 따른 코팅층의 특성분석 (Improvement of Powder Feeding Characteristics of Fine$5\mu\textrm{m}$ $Al_2O_3$ Powder by Modification of the Powder Feeding Systems and Characterization of the Coating Layer depending on Plasma Spraying Conditions)

  • 설동욱;김병희;정민석;임영우;서동수
    • Journal of Welding and Joining
    • /
    • 제15권1호
    • /
    • pp.116-124
    • /
    • 1997
  • A scope of this study is to establish the optimum plasma spray conditions for fine ($5\mu\textrm{m}$) $Al_2O_3$ powder. However, the flowability of the $Al_2O_3$ powder is not so good because of irregular particle shape and fine particle size. Therefore, powder feeding system was modified by 1) change of powder feeding line material from polymer to copper 2) shorten the powder feeding tube length 3) heating the powder feeding system to $80^{\circ}C$4) vibrating the powder feeding line continuously, in order to feed the fine powder homogeneously. The homogeneous powder feeding conditions were obtained with the modified powder feeding system by controlling the powder carrier gas flow and the powder flow rate indicator. The best plasma spraying conditions for the fine $Al_2O_3$ powder were found out as 40kw gun power, 80 g/min. powder feed rate and 50 mm working distance after characterizing the microstructure, hardness and wear loss of the $Al_2O_3$ coating layer.

  • PDF

초음파에 의한 필렛 용접힐부의 표면결함 검출능에 관한 실험적 검증 (Experimental Verification on the Detectability of Surface Flaws at Fillet Weld Hills by Ultrasonic Method)

  • 박익근;이철구
    • Journal of Welding and Joining
    • /
    • 제18권1호
    • /
    • pp.46-51
    • /
    • 2000
  • Ultrasonic nondestructive evaluation (UNDE) technique is commonly used for detecting inner defects in the materials. Recently, new methods are trying to apply for detecting surface and subsurface flaws using Rayleigh wave or creeping wave. These techniques, however, have following problems. Echo amplitude is remarkably affected by the surface conditions and discrimination of echo pattern is usually difficult because shear wave propagate in the material at the same time. We can apply surface SH-wave(which is horizontally polarized shear wave traveling along near surface layer) technique to detect surface flaws. In this paper, directivity, distance amplitude characteristics and detectability of surface flaws at fillet weld hills of the 5 MHz and 2 MHz surface flaws at fillet weld hills of the 5 MHz and 2 MHz surface Sh-wave are experimentally investigated. As a result of the study, it was found out that these techniques are valuable for the detection of fatigue cracks at fillet weld heels which can not be detected by other ultrasonic techniques such as angle beam technique and which are inaccessible for non-destructive testings e.g. MT(magnetic particle testing) or PT(liquid penetrant testing).

  • PDF