• Title/Summary/Keyword: 5-Layers

Search Result 3,621, Processing Time 0.034 seconds

Effect of Columnar Structures on Exchange Anisotropy Field in Magnetoresistive NiO/NiFe Bilayers

  • Jai-Young Kim;Gyeong-Su Park;Jae-Chul Ro;Su-Jeong Suh
    • Journal of Magnetics
    • /
    • v.4 no.3
    • /
    • pp.88-91
    • /
    • 1999
  • A series of NiO/NiFe bilayer films are deposited with the variation of Ar sputtering pressure for the NiO layers only. As the pressure for the NiO layers increases, the exchange anisotropy field (HEX) decreases gradually and becomes extinct at 2.5 mTorr, at which the maximum coercive force (HC) in the NiO/NiFe films is obtained. Randomly oriented columnar structures with HEX a few tens of Oe and oriented columnar structures with zero HEX are observed in the NiP layers by highvoltage hihg-resolution transmission electron microscopy. The vanishing of the HEX in the oriented structures is attributed to the lack of exchange anisotropy energy (EEX) between NiO and NiFe layers, which results in little contribution of interfacial unidirectional pinning anisotropy to the interface of NiO/NiFe bilayer.

  • PDF

Cross-Layer and End-to-End Optimization for the Integrated Wireless and Wireline Network

  • Gong, Seong-Lyong;Roh, Hee-Tae;Lee, Jang-Won
    • Journal of Communications and Networks
    • /
    • v.14 no.5
    • /
    • pp.554-565
    • /
    • 2012
  • In this paper, we study a cross-layer and end-to-end optimization problem for the integrated wireless and wireline network that consists of one wireline core network and multiple wireless access networks. We consider joint end-to-end flow control/distribution at the transport and network layers and opportunistic scheduling at the data link and physical layers. We formulate a single stochastic optimization problem and solve it by using a dual approach and a stochastic sub-gradient algorithm. The developed algorithm can be implemented in a distributed way, vertically among communication layers and horizontally among all entities in the network, clearly showing what should be done at each layer and each entity and what parameters should be exchanged between layers and between entities. Numerical results show that our cross-layer and end-to-end optimization approach provides more efficient resource allocation than the conventional layered and separated optimization approach.

PERFORMANCE OF MULTILAYER CERAMIC ACTUATOR BY CONSIDERING THE SHAPE EFFECT

  • Wee, S.B.;Jeong, S.J.;Song, J.S.
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.11a
    • /
    • pp.594-597
    • /
    • 2003
  • In the present study, the piezoelectricity and polarization of multilayer ceramic actuator, being designed to stack PMN-PZ-PT ceramic layers and Ag-Pd electrode layers alternatively, were investigated under a consideration of geometric factor, the volume ratio of the ceramic to the electrode layers. The actuators were fabricated by tape casting of 0.2Pb(Mg1/3Nb2/3)O3-0.38PbZrO3-0.42PbTiO3 followed by lamination and burnout & co-firing processes. The actuators of 10 10 0.62 nm3 in size were formed in a way that 60 200 m thick ceramics were stacked alternatively with 5 m thick electrode layer. Increases in polarization and electric field-induced displacement with thickness of the ceramic layer were attributed to change of 90o/180o domain ratio, which was affected by interlayer internal stress. The piezoelectricity and actuation behaviors were found to depend upon the volume ratio (or thickness ratio) of ceramic to electrode layers.

  • PDF

Influence of Ag thickness on properties of AZO/Ag/AZO Multi-layer Thin Films (AZO/Ag/AZO 다층박막의 Ag두께에 따른 특성 연구)

  • Yeon, Je ho;Kim, Hong Bae
    • Journal of the Semiconductor & Display Technology
    • /
    • v.16 no.2
    • /
    • pp.27-31
    • /
    • 2017
  • AZO/Ag/AZO multi-layer films deposited on glass substrate by RF magnetron sputtering and thermal evaporator have a much better electrical properties than Al-doped ZnO thin films. The multi-layer structure consisted of three layers, AZO/Ag/AZO, the electrical and optical properties of AZO/Ag/AZO were changed mainly by thickness of Ag layers. The optimum thickness of Ag layers was determined to be $90{\AA}$ for high optical transmittance and good electrical conductivity. The Ag layers thickness $90{\AA}$ is an optical transmittance greater than 80% of visible light and the obtained multilayer thin film with the low resistivity of $8.05{\times}10-3{\Omega}cm$ and the low sheet resistance $5.331{\Omega}/sq$. Applying to TCO and Solar electrode will improve efficiency.

  • PDF

The Effect of Finger Length on Bending Strength Properties in Laminated Wood (집성재의 정거길이가 휨강도성능에 미치는 영향)

  • 홍병화;변희섭;김종만
    • Journal of the Korea Furniture Society
    • /
    • v.11 no.2
    • /
    • pp.7-12
    • /
    • 2000
  • This paper describes the bending strength properties of laminated woods which had three kinds of specimens according to finger length-12, 4.5 mm and butt joint and the acoustic emissions (AEs) generated during the test. 3-ply laminated wood beams were tension side layers (lower layers) composed of one middle lamina and two side-jointed laminae, with one butt joint ($_1BJ$), one finger joint (12mm, $_1FJ_{12}$) or one finger joint (4.5mm, $_1FJ_{4.5}$) in the middle lamina of tension side layer. And 3-ply laminated wood beams were tension side layers (lower layers) also composed of one lamina, with one butt joint (BJ), one finger joint (12mm, $FJ_{12}$) or one finger joint (4.5mm, $FJ_{4.5}$/) in tension side layer. Cryptomelia pieces were cut for butt and two finger types and glued with resorcinol-phenol resin adhesive. The results were as follows It was not effective in the bending modulus of elasicity (MOE) with IFJL type and had no difference from finger length. The bending modulus of rupture (MOR) of laminated wood beams including finger joint was the same values as that including butt feint and had no difference from finger length. It was effective in MOE with FJL type and had no difference from finger length. The effect of finger joint on MOR was much higher than that of butt joint but had no difference from finger length. The AE generation time of IFJL type was earlier than that of the control wood and the number of AE count was much more than that of the control wood. However, the AE generation time of FJL type was earlier than that of the control wood and the number of U count was much fewer than that of the control wood.

  • PDF

Effect of Steel-fiber Distribution on Flexural Strength and Toughness of Shotcrete-mimicked Concrete Specimen (숏크리트 모사 콘크리트 공시체에 혼합된 강섬유의 분산도가 휨강도 및 인성에 미치는 영향)

  • Park, Sung-Sik;Kim, Sang-Jung
    • Journal of the Korean Geotechnical Society
    • /
    • v.29 no.6
    • /
    • pp.53-62
    • /
    • 2013
  • A 5-20 cm thick shocrete has been routinely constructed for NATM tunneling method to stabilize and confine the excavated rock of tunnel construction site. A $40kg/m^3$ of steel fibers are usually mixed into such shotcrete but these steel fibers may not be evenly distributed depending on shotcrete machines, mixing ratios and excavated rock conditions. In this study, square column shotcrete-mimicked concrete specimens of $15cm{\times}15cm{\times}55cm$ were prepared with 5 equal layers and 5 or 20% cement ratio. The specimens were prepared with different reinforced-patterns: non-reinforced, middle layer-reinforced, 1, 3, and 5 layers-reinforced, or all layers reinforced. The specimens were air-cured for 7 days and tested for flexural strength. The influence of steel-fiber distribution on flexural strength and toughness of shotcrete-mimicked concrete specimens was investigated. In the case of a specimen with cement ratio of 20%, a flexural strength increased as a number of fiber-reinforced layer increased. The flexural strength of one-layer reinforced specimen showed 20% less than that of evenly fiber-distributed specimen. On the other hand, a specimen with cement ratio of 5% decreased as the number of fiber-reinforced layers increased. A toughness index increased as the number of fiber-reinforced layers increased, regardless of cement ratios. The toughness index of evenly fiber-distributed specimen showed 2-3 times as large as that of one-layer reinforced specimen.

Formation and Development of Abscission Layer between Pedicel and Rachilla, and Changes in Grain Shedding during Ripening in African Rice, Oryza glaberrima Steud (아프리카 벼 Oryza glaberrima의 종실 이층조직의 발달과정과 등숙기간 중 탈립성의 변화)

  • Il Doo, Jin;Yeong Hwan, Bae;Jun, Inouye
    • KOREAN JOURNAL OF CROP SCIENCE
    • /
    • v.40 no.1
    • /
    • pp.103-112
    • /
    • 1995
  • Six African rice varieties, two each from three types having the characteristics of partially, irregularly, and completely developed abscission layers, were selected and grown 1) to investi-gate the histological differences during the formation and development of the abscission layers and 2) to evaluate the changes in the breaking tensile strength required to detach a grain from its pedicel dur-ing ripening period in relation with developmental stage of the abscission layers. In African rice, the panicle and spikelet grew rapidly from 15 days before heading and almost completely grown in length at five days before heading. The abscission regions were recognized at 15 days before heading. However, any apparently developed abscission layers were not recognized in the lemma side for partially developed abscission layers. A group of parenchymatous cells could be observed sporadically in the abscission layers of the lemma side for irregularly developed ab-scission layers. At ten days before heading, abscission layers consisting of one or two layers of parenchymatous cells were clearly distinguished from neighboring cells due to thickened and lignified cell walls. There were a number of individual parenchymatous cells scattered sporadically in the lemma side of partially developed abscission layers, and a number of grouped parenchymatous cells scattered randomly in the lemma side of irregularly developed abscission layers. At two weeks after heading, the grains became almost fully filled. The cracking of abscission layers between rachilla and pedicel was observed, and the breaking tensile strength required to detach a grain from its pedicel was as low as that at harvest time.

  • PDF

Growth and Characteristics of Al2O3/AlCrNO/Al Solar Selective Absorbers with Gas Mixtures

  • Park, Soo-Young;Han, Sang-Uk;Kim, Hyun-Hoo;Jang, Gun-Eik;Lee, Yong-Jun
    • Transactions on Electrical and Electronic Materials
    • /
    • v.16 no.5
    • /
    • pp.264-267
    • /
    • 2015
  • AlCrNO cermet films were prepared on aluminum substrates using a DC-reactive magnetron sputtering method and a water-cooled Al:Cr target. The Al2O3/AlCrNO (LMVF)/AlCrNO (MMVF)/AlCrNO (HMVF)/Al/substrate of the 5 multi-layers was prepared according to the Ar and (N2 + O2) gas-mixture rates. The Al2O3 of the top layer is the anti-reflection layer of triple AlCrNO (LMVF)/AlCrNO (MMVF)/AlCrNO (HMVF) layers, and an Al metal forms the infrared reflection layer. In this study, the crystallinity and surface properties of the AlCrNO thin films were estimated using X-ray diffraction (XRD) and field-emission scanning electron microscopy (FESEM), while the composition of the thin films was systematically investigated using Auger electron spectroscopy (AES). The optical properties of the wavelength spectrum were recorded using UH4150 spectrophotometry (UV-Vis-NIR) at a range of 0.3 μm to 2.5 μm.

TENSILE BOND STRENGTH BETWEEN ELASTOMERIC IMPRESSION MATERIALS AND TRAY RESINS DEPENDING ON THE THICKNESS OF THE TRAY ADHESIVE

  • Kim, Tae-Won;Moon, Hong-Seok;Lee, Keun-Woo;Chung, Moon-Kyu
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.44 no.6
    • /
    • pp.699-711
    • /
    • 2006
  • Statement of problem. Elastomeric impression materials have been widely used to obtain an accurate impression. However there have not been enough studies on the influence of the thickness of the tray adhesives on the bonding strength between the trays and the elastomeric impression materials. Purpose. In order to understand the relationship between the thickness of the tray adhesive and the tensile bond strength and to suggest the thickness at which the bonding strength is strongest, tensile bond strength related to the thickness of adhesives of 3 different elastomeric impression materials were tested. Materials and methods. 3 impression materials, $Permlastic^{(R)}$. Regular Set(Kerr Corp., Romulus, Michigan, U.S.A.), $Impregum^{TM}$ $Penta^{TM}$(3M ESPE, Seefeld, Germany), and Aquasil Ultra Monophase Regular Set Smart Wetting.(Dentsply Caulk, Milford, Delaware, U.S.A.), were used in this study, and tray adhesives from the same manufacturers of the impression materials were used, which were Rubber Base Adhesive, Polyether Adhesive, and Silfix, respectively. The tray specimens were prepared by autopolymerizing the tray material(Instant Tray Mix, Lang, Wheeling, Illinois, U.S.A.), and a PVC pipe was used to house the impression material. In group A, tray adhesives were applied in multiple thin layers of 1 to 5 and in group B, adhesives were applied only once, in the thickness equivalent to several applications. Lightness($L^*$) of the adhesion surface was measured with a spectrophotometer(CM-3500d, Konica Minolta, Sakai, Osaka, Japan). The tensile bond strength of the elastomeric impression material and the tray resin was measured with universal materials testing machines(Instron, Model 3366, Instron Corp, Nowood, Massachusetts, U.S.A.). A formula between the number of adhesive application layers and the lightness of the adhesion surface was deduced in group A, and the number of adhesive layers in group B was estimated by applying the lightness($L^*$) to the deduced formula. Results. 1. In group A, a statistically significant increase in tensile bond strength appeared when the number of application layers increased from 1 to 2 and from 4 to 5, and no significant difference was present between 2, 3, and 4 layers in Permlastic. In Impregum, the tensile bond strength was significantly increased when the number of adhesive layers increased from 1 to 3, but no significant difference after 3 layers. In Aquasil, the tensile bond strength significantly increased as the number of application layers increased up to 4 but showed no significant difference between 4 and 5. 2. In group B, the tensile bond strength was decreased when the thickness of the adhesive increased in Permlastic. Impregum showed an increased tensile bond strength when the thickness of the adhesive was increased. In Aquasil, the tensile bond strength increased as the number of adhesive application layers increased up to approximately 2.5 layers but it sharply decreased after approximately 4.5. Conclusion. From the study, the common idea that it is better to apply a thin and single coat of tray adhesive needs correction in more detailed ways, and instructions on some of the tray adhesives should be reconsidered since there were several cases in which the tensile bond strength increased according to the increase in the thickness of the adhesives.

Development of Wireless Monitoring System for Layers Rearing in Multi-tier Layers Battery by Machine Vision (기계시각을 이용한 고단 직립식 산란계 케이지의 무선 감시시스템 개발)

  • Lim, Song-Su;Chang, Dong-Il;Lee, Seung-Joo;So, Jae-Kwang
    • Journal of Biosystems Engineering
    • /
    • v.32 no.3
    • /
    • pp.173-178
    • /
    • 2007
  • This research was conducted to develop and analyze a wireless monitoring system for judging if sick or dead layers (SDL) exist in multi-tier layers battery (MLB) by machine vision, and to evaluate the performance between a wired monitoring system and it. This study used the AP (Access Point), the RS-285 to RS-232 converter, RS-232 to Ethernet converter, PICBASIC board and upgraded lump image processing method to change wired monitoring system into wireless monitoring system. The system was tested at a pilot farm and farm layer house. Results showed that monitoring judgement success rate at a pilot farm on normal cage (without SDL) was 82.3% and that on abnormal cage (with SDL) was 87.5%, respectively. And communication performance test results showed at farm layer house was $700{\sim}900$ kbps while equipments operated. There were dropped slightly than performance of wired monitoring system, however, the quantity was too small to make a significant difference of performance of the controling system developed for wireless communication.