• 제목/요약/키워드: 450 nm wavelength continuous laser

검색결과 3건 처리시간 0.022초

Deposition of Fine Linewidth Silver Layer using a Modified Laser-induced Forward Transfer Technique

  • Cheon, Jonggyu;Nguyen, Manh-Cuong;Nguyen, An Hoang-Thuy;Choi, Sujin;Ji, Hyung-Min;Kim, Sang-Woo;Yu, Kyoung-Moon;Kim, Jin-Hyun;Cho, Seong-Yong;Choi, Rino
    • Journal of the Korean Physical Society
    • /
    • 제73권9호
    • /
    • pp.1279-1282
    • /
    • 2018
  • This paper reports the deposition of a metal line using a multilayer stack and laser-induced forward transfer (LIFT) using a low cost continuous wave blue laser with a wavelength of 450 nm. The donor structure was composed of a light-to-heat (LTH) layer, a release layer, and a transfer layer in series. Amorphous silicon as the LTH layer absorbs photon energy and converts it to heat. A release layer was melted so that a silver transfer layer would be transferred to the receiver substrate. The transferred silver layer showed reasonable physical and electrical characteristics. A low cost fine linewidth metal layer could be achieved using this modified LIFT technique and blue laser.

적외선 영역에서 광대역으로 파장 가변되는 연속 발진 $Cr^{4+}$:YAG 레이저 개발 (Development of the continuous-wave $Cr^{4+}$: YAG laser with a broad tunability in the infrared region)

  • 추한태;이봉연;양준묵;이동한;임기수;이치원
    • 한국광학회지
    • /
    • 제10권3호
    • /
    • pp.226-232
    • /
    • 1999
  • 연속 발진 Nd: YAG 레이저를 펌핑 광원으로 하여 보다 조밀하고 견고하며, 안정된 연속 발진 파장 가변 Cr4+ : YAG 레이저를 개발하여 레이저 출력 특성, 파장 가변성 및 발진 레이저 선폭 등을 조사하였다. 공진기 구조는 공진기 안정 조건을 계산하여 비점수차가 보상된 Z 자형 접힘 공진기를 구성하였다. 공진기 출력 거울의 투과율이 1%일 때, 결정의 온도를 2$0^{\circ}C$로 유지하며 6W로 펌핑하였을 경우, 중심 파장이 1.45$\mu\textrm{m}$에서 최대 400 mW의 평균 출력을 갖는 매우 안정된 연속 발진 Cr4+ : YAG 레이저를 얻을 수 있었으며, 출력 기울기 효율은 8%였다. 또한 공진기 내에 복굴절 필터를 삽입하여 1.399 $\mu\textrm{m}$에서 1.532 $\mu\textrm{m}$까지의 파장 가변 영역을 얻었고, 1.4903 $\mu\textrm{m}$에서 최대 340 mW의 평균 출력을 얻을 수 있었으며, 이때의 레이저 발진 선폭은 0.21 $\mu\textrm{m}$였다.

  • PDF

열처리 조건에 따른 Ag-In-Sb-Te 상변화 기록 박막의 미세 조직과 반사도의 관계 (Dependence of Microstructure and Optical Properties of Ag-In-Sb-Te Phase-Change Recording Thin Firms on Annealing Heat-Treatments)

  • 서훈;박정우;최우석;김명룡
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1996년도 춘계학술대회 논문집
    • /
    • pp.9-14
    • /
    • 1996
  • The dependence of microstructural and optical properties of Ag-In-Sb-Te thin films on annealing heat-treatments was studied. It was found from the present work that the increase of reflectance after annealing heat-treatment is related with phase change of Ag-In-Sb-Te thin film from amorphous state to crystalline phases which involve Sb crystalline phase and AgInTe$_2$ stoichiometric phase. On the other hand, the reflectance is decreased after high temperature annealing (above 450$^{\circ}C$), due to the morphology .mange of film surface. For the purpose of practical application(erasable optical disk), we fabricated quadrilayered Ag-In-Sb-Te alloy disk, and annealed it with continuous laser beam. As result of this laser\ulcorner annealing treatment, we found that the increment of reflectance is 9.3% at 780nm wavelength. It might be considered that Ag-In-Sb-Te alloy optical disk is the big promising candidate for the erasable optical memory medium.

  • PDF