Dielectric and Pyroelectric Properties of Y-modified PSS-PT-PZ Ceramics

  • Lee, Sung-Gap
    • Transactions on Electrical and Electronic Materials
    • /
    • v.6 no.3
    • /
    • pp.119-123
    • /
    • 2005
  • $0.10Pb(Sb_{1/2}Sn_{1/2})O_3-0.25PbTiO_3-0.65PbZrO_3$ specimens doped with $ MnO_2\;(0.18\;mol\%)$ and $Y_2O_3\;(0\~0.4\;wt\%)$ were fabricated by the mixed-oxide method. All specimens showed the typical XRD patterns of a perovskite polycrystalline structure and the lattice constant decreased with increasing amount of $Y_2O_3$. The relative dielectric constant and the dielectric loss of the specimens doped with $0.2\;wt\%\;Y_2O_3$ were 704 and 0.0201, respectively. The remanent polarization, the coercive field and the pyroelectric coefficient of the specimen doped with $0.2\;wt\%\;Y_2O_3$ were $10.88\times10^{-2}Cm^{-2},\;11.12\times10^2kVm^{-1}$ and $5.03\times10^{-4}Cm^{-2}K^{-1}$ at $25^{\circ}C$, respectively. The figures of merit, $F_V$ for the voltage responsivity and $F_D$ for the specific detectivity, of the specimen doped with $0.2\;wt\%\;Y_2O_3$ were the good values of $3.04\times10^{-2}\;m^2C^{-1}\;and\;1.50\times10^{-5}\;Pa^{-1/2}$, respectively.

Electrical Characteristics of MIS Type $Pb_{1-x}Sn_xTe$ (MIS형 $Pb_{1-x}Sn_xTe$ Diode의 전기적 특성에 관한 연구)

  • Kim, Tae-Seoung;Park, Jong-Kun;Yeo, In-Seon;Lee, Jin;You, Rim
    • Proceedings of the KIEE Conference
    • /
    • 1987.11a
    • /
    • pp.187-190
    • /
    • 1987
  • This paper is for the charge storage effect and C-V characteristics of MIS type diode which is the basic structural unit of charge-coupled device after growing the $Pb_{1-x}Sn_xTe$ crystal. $Pb_{1-x}Sn_xTe$ singlecrystal dbtained from the horizental furnace using Bridgman method. To judge whether the grown singlecrystal is suitable for specimen or not, it was investigated by X-ray diffraction analysis, thermogravimetry and differential thermal analysis. The C-V characteristics of the specimen caused to anodic oxidation was the best when the insulator film's depth was 250[$\AA$]. Measuring the C-V characteristics aftermanufacturing MIS type diode resulted that the whole capacitance was the largest when the supply voltage was low, 0.3[V] and the capacitance also varied according to the variance frequence when the supply voltage is over 0.5[V]. From the above result, even if the supply voltage is low, the $Pb_{1-x}Sn_xTe$ also have a good charge storage effect.

  • PDF

Effects of $Ba(La_{1/2}Nb_{1/2})O_3$ content and Zr/Ti composition ratio on electrooptic properties of the $Ba(La_{1/2}Nb_{1/2})O_3-Pb(Zr, Ti)O_3$ ceramics ($Ba(La_{1/2}Nb_{1/2})O_3$의 고용량과 Zr/Ti 조성비가 $Ba(La_{1/2}Nb_{1/2})O_3-Pb(Zr, Ti)O_3$ 세라믹의 전기광학 특성에 미치는 영향)

  • 류기원;이성갑;배선기;이영희
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.44 no.5
    • /
    • pp.644-648
    • /
    • 1995
  • Transparent xBa(La$_{1}$2/Nb$_{1}$2/)O$_{3}$-(1-x)Pb(Zr, Ti)O$_{3}$ (x=8.5, 9.0[mol.%], Zr/Ti=70/30~40/60) ceramics were fabricated by the two-stage sintering method, the electrooptic properties were investigated with Ba(La$_{1}$2/Nb$_{1}$2/)O$_{3}$ content and Zr/Ti composition ratio. Decreasing the Zr/Ti ratio, the electrooptic property was changed from a quadratic electrooptic effect to a linear electrooptic effcet. In the BLN-PZT 9.0/50/50 specimen having the tetragonal structure, the linear electrooptic coefficient had the highest value of 6.01*10$^{-10}$ [m/V] and in the BLN-PZT 9.0/55/45 specimen which located near the MPB region, the quadratic electrooptic coefficient had the highest value of 10.53*10$^{-16}$ [m$^{2}$/V$^{2}$].

  • PDF

Dielectric and Piezoelectric Characteristics of PSS-PZT Piezoelectric Ceramics with CrS12TOS13t Addition (Cr2O3 첨가에 따른 PSS-PZT 압전 세라믹스의 유전 및 압전 특성)

  • 홍재일;이개명;윤석진;유주현;박창엽
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.41 no.6
    • /
    • pp.687-693
    • /
    • 1992
  • To improve dielectric, piezoelectric and temperature stability in 0.50Pb(SnS11/2TSbS11/2T)OS13T - 0.35PbTiOS13T - 0.60PbZrOS13T + 0.4[wt%]MnOS12T piezoelectric ceramics which is used for surface acoustic wave devices, CrS12TOS13T was added and the specimens were fabricated by Hot Press method, and their characteristics were measured with CrS12TOS13T addition. From the results, in the specimen added by 0.2[wt%]CrS12TOS13T, dielectric constant and mechanical quality factor were 380 and 2307, respectively, and it was suited for surface acoustic wave device and the temperature coefficient of the resonant frequency in the specimen added by 0.4[wt%]CrS12TOS13T was the least value of 74.96[ppm/$^{\circ}C$].

Structural and Electrical properties of MnO$_2$ added PbTiO$_3$system ceramics for Hydrophone (MnO$_2$가 첨가된 하이드로폰용 PbTiO$_3$계 세라믹스의 구조적 전기적 특성)

  • 홍재일;유주현;박정흠;이두희;박창엽
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1994.11a
    • /
    • pp.3-7
    • /
    • 1994
  • In this study, to improve sintering condition, anisotropic Property(k$\_$t//k$\_$p/) of electromechanical coupling coefficients, and hydrostatic piezoelerlric constants d$\_$h/ and g$\_$h/, MnO$_2$impurity was added to the (Pb$\_$0.76/Ca$\_$0.24)[(Co$\_$$\frac{1}{2}$W$\_$$\frac{1}{2}$/)$\_$0.04/Ti$\_$0.96/]O$_3$ System ceramics for hydrophone. And the structural, electrical properties of them were investigated. As a results. tetragonality was decreased with MnO$_2$ additives and density was the highest value of 7.06(g/㎤) at H2-3 specimen. Electromechanical coupling coefficients of H2-3 specimen were k$\_$t/=49 and k$\_$p/ 0, which exibited the hightest hydrostatic piezoelectric constants of d$\_$h/=64.52[10$\^$-1/C/N] and g$\_$h/=35.92[10$\^$-3/ Vm/N].

  • PDF

Temperature stability for length extensional vibration of $Pb(Zr_{0.56}Ti_{0.44}O_{3}+x[wt%]Cr_{2}O_{3})$ceramics ($Pb(Zr_{0.56}Ti_{0.44}O_{3}+x[wt%]Cr_{2}O_{3})$세라믹스의 길이진동에 대한 온도안정성)

  • 현덕수;한성훈;이개명
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.07a
    • /
    • pp.881-884
    • /
    • 2000
  • Recently mobile communication fields need piezoelectric ceramic resonators and filters as possible as small. The length-extensional vibration mode of a rectangular piezoelectric cesamic plate has the advantage of the small size, but the mode has not been studied sufficiently because it was not used extensively until now. In this paper, PZT + x[wt%l $Cr_20_3$ ceramics with rhombohedra1 phase were fabricated. And temperature stability for the mode of the ceramic specimen was investigated. Contrary to our expectations, addition of the stabilizer, $Cr_20_3$ did not promote the temperature stability for the mode in the PZT ceramic specimen with rhombohedra1 phase.

  • PDF

Effect of Excess MgO on Dielectric and Electrostrictive Properties of $0.99Pb(Mg_{1/3}Nb_{2/3})O_3-0.01Pb(Mn_{2/3}W_{1/3})O_3$ ($0.99Pb(Mg_{1/3}Nb_{2/3})O_3-0.01Pb(Mn_{2/3}W_{1/3})O_3$계의 유전 및 전왜 특성에 미치는 과잉 MgO의 영향)

  • 윤기현;김승연;남윤우;조용수;강동헌
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.8
    • /
    • pp.629-634
    • /
    • 1993
  • Dielectric and electrostrictive properties of 0.99Pb(Mg1/3Nb2/3)O3-0.01Pb(Mn2/3W1/3)O3 system using KCl-NaCl salts have been investigated as a function of the amount of excess MgO. For the specimens calcined at $700^{\circ}C$ for 1h and then sintered at 115$0^{\circ}C$ for 4h, the perovskite phase and the relative density were about 98% and 95%, respectively. With the addition of excess MgO up to 10mol%, the dielectric constant and the electrostrictive strain increased due to the increase of density and grain size, and these properties were degraded by the further addition of excess MgO. For the 10mol% excess MgO added specimen, the maximum electrostrictive strain, Xmax, and the electrostrictive coefficient, Q11, were 4.5$\times$10-4, 3.5$\times$10-2m4/C2, respectively. These results were correlated with the property of PMW and microstructure.

  • PDF

Dielectric and Piezoelectric Characteristics of PSN-PNN-PZT Ceramics with the Sintering Temperature (소성온도에 따른 PSN-PNN-PZT 세라믹스에 미치는 압전특성)

  • Nam, Seung-Hyon;Ryu, Ju-Hyun;Lee, Su-Ho;Park, Chang-Yub;Yoon, Hyun-Sang;An, Byung-Ryul
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.11a
    • /
    • pp.326-329
    • /
    • 2002
  • In this study, to develop the low temperature sintering ceramics for multilayer piezoelectric transformer, $0.02Pb(Sb_{1/2}Nb_{1/2})O_{3}-0.13Pb(Ni_{1/3}Nb_{2/3}O_3-0.85Pb(Zr,Ti)O_{3}$ system ceramics were manufactured with the variations of sintering temperature between 1,090 and $1240^{\circ}C$ and its dielectric and piezoelectric characteristics were investigated. With increasing the sintering temperature, electromechanical coupling factor (kp) and mechanical quality factor(Qm) were decreased. At $1,180^{\circ}C$ sintered specimen showed maximum value of 0.535 electromechanical coupling factor (kp). On the other hand,. The specimen sintered at $1,180^{\circ}C$ showed the maximum value of ${\varepsilon}r$=1,571, Qm=1,181 respectively.

  • PDF

A Study on the Dielectric and Pyroelectric Properties of the PSS-PT-PZ Ceramics Added $MnO_2$ ($MnO_2$가 첨가될 PSS-PT-PZ 세라믹의 유전 및 초전특성에 관한 연구)

  • Lee, Sung-Gap;Ryu, Ki-Won;Lee, Young-Hie;Bae, Seon-Gi;Park, Chang-Yub
    • Proceedings of the KIEE Conference
    • /
    • 1991.07a
    • /
    • pp.194-197
    • /
    • 1991
  • In this study, $(Pb_{0.99}La_{0.01})[(Sb_{1/2}Sn_{1/2})_{0.10}Ti_{0.25}Zr_{0.65}]O_3$, added $MnO_2$ (0-0.30[mol%]) ceramics were fabricated by the mixed oxide method. The sintering temperature and time were $1250[^{\circ}C]$, 2[hr], respectively. In the $(Pb_{0.99}La_{0.01})[(Sb_{1/2}Sn_{1/2})_{0.10}Ti_{0.25}Zr_{0.65}]O_3$ added $MnO_2$ (0.24[mol%]) specimens, relative dielectric constant and dielectric loss were minimum values 3.52, 0.003, respectively, and Curie temperature were highest values $256[^{\circ}C]$. Pyroelectric coefficient and voltage responsivity of the $(Pb_{0.99}La_{0.01})[(Sb_{1/2}Sn_{1/2})_{0.10}Ti_{0.25}Zr_{0.65}]O_3$, and added $MnO_2$ (0.24[mol%]) specimen were good values, $6.73{\times}10^{-8}[C/cm^2K],\;125[v/W]$, respectively. Figure of merit of pyroelectric current, voltage and detectivity of the specimen, $(Pb_{0.99}La_{0.01})[(Sb_{1/2}Sn_{1/2})_{0.10}Ti_{0.25}Zr_{0.65}]O_3$ added $MnO_2$ (0.24[mol%]) were good values $2.714{\times}10^{-8}[Ccm/J],\;7.706{\times}10^{-11}[Ccm/J],\;2.640{\times}10^{-8}[Ccm/J]$, respectively. Voltage responsivity of the $(Pb_{0.99}La_{0.01})[(Sb_{1/2}Sn_{1/2})_{0.10}Ti_{0.25}Zr_{0.65}]O_3$ added $MnO_2$ (0.24[mol%]) specimens were decreased with increasing the chopper frequency.

  • PDF

A Study on the Dielectric and Pyroelectric Properties of the $Pb({Sn}_{1/2}Nb_{1/2})O_3-PbTiO_3-PhZrO_3$ Ceramics ($Pb({Sn}_{1/2}Nb_{1/2})O_3-PbTiO_3-PhZrO_3$ 세라믹의 유전 및 초전특성에 관한 연구)

  • Ham, Young-Wook;Lee, Neung-Hun;Kim, Yong-Hyuk;Kim, Jin-Soo;Kim, Young-Il
    • Proceedings of the KIEE Conference
    • /
    • 1993.07b
    • /
    • pp.1119-1121
    • /
    • 1993
  • The PSN-PT-PZ ceramics doped with the Mn-oxide(0.5wt%) were fabricated by the mixed oxide method at 1250($^{\circ}C$) for 2(hr) and then the dielectric and pyroelectric properties were investigated with the compositions. In the 0.05PSN-0.4PT-0.55PZ specimen with 0.5(wt%) $MnO_2$, the pyroelectric coefficient was $6.6{\times}10^{-8}(C/Cm^2^{\circ}C)$, and the figure of merits for pyroelectric current and voltage were $27{\times}10^{-9},\;45{\times}10^{-12}$(C.Cm/J), respectibly.

  • PDF