• Title/Summary/Keyword: 3Cr-1Mo

Search Result 314, Processing Time 0.032 seconds

On the Statistical Properties of the Parameters B and q in Creep Crack Growth Law, da/dt=B(C*)q, in the Case of Mod. 9Cr-1Mo Steel (Mod. 9Cr-1Mo강의 크리프 균열 성장 법칙의 파라메터 B와 q의 통계적 성질에 관한 연구)

  • Kim, Seon-Jin;Park, Jae-Young;Kim, Woo-Gon
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.35 no.3
    • /
    • pp.251-257
    • /
    • 2011
  • This paper deals with the statistical properties of parameters B and q in the creep crack growth rate (CCGR) law, da/dt=B$(C^*)^q$, in Mod. 9Cr-1Mo (ASME Gr.91) steel which is considered a candidate materials for fabricating next generation nuclear reactors. The CCGR data were obtained by creep crack growth (CCG) tests performed on 1/2-inch compact tension (CT) specimens under an applied load of 5000N at a temperature of $600^{\circ}C$. The CCG behavior was analyzed statistically using the empirical equation between CCGR, da/dt and the creep fracture mechanics parameter, $C^*$. The B and q values were determined for each specimen by the least-squares fitting method. The probability distribution functions for B and q were investigated using normal, log-normal, and Weibull distributions. As far as this study is considered, it can be appeared that B and q followed the log-normal and Weibull distributions. Moreover, a strong positive linear correlation was found between B and q.

The Solidification Microstructure of X%C-5%Cr-5%V-5%Mo-5%W-5%Co Multi-Component White Cast Iron (X%C-5%Cr-5%V -5%Mo-5%W-5%Co 다합금계백주철의 응고조직에 관한 연구)

  • Yu, Sung-Kon;Yasuhiro Matsubara
    • Korean Journal of Materials Research
    • /
    • v.11 no.6
    • /
    • pp.472-476
    • /
    • 2001
  • Type and three-dimensional morphology of carbides precipitated in the X(X= 1.70, 1.92, 2.21, 2.50, 2.86)%C-5%Cr-5%V-5%Mo-5%W-5%Co multi-component white cast iron were investigated using an optical microscope and SEM. The types of carbides precipitated were MC, M$_2$C and M$_{7}$C$_{3}$. Morphology of the MC carbide took three forms, that it petal-like, nodular and coral-like. MC carbide seemed to change its morphology from petal-like through nodular, and finally to coral-like with an increase in carbon content. M7C carbide was classified into lamellar and plate-like type. The lamellar M$_2$C arbide precipitated in the iron with low molybdenum and tungsten contents, and higher contents of both elements in the iron were needed to form the plate-like M$_2$C carbide. The morphology of M$_{7}$C$_{3}$ was rod-like similar to that observed in high chromium white cast iron. However, cobalt does not affect the type and morphology of precipitated carbides.des.

  • PDF

Effects of Heat-Treatments on Transformation Behavior of Matrix Structures in High Alloyed White Cast Iron (고합급백주철에 있어서 열처리가 기지조직의 변태에 미치는 영향)

  • Shin, Sang-Woo;Ryu, Seong-Gon
    • Korean Journal of Materials Research
    • /
    • v.10 no.6
    • /
    • pp.409-414
    • /
    • 2000
  • Three different white cast irons alloyed with Cr, V, Mo and W were prepared in order to study their transformation behavior of matrix structures in heat-treated conditions. The specimens were produced using a 15kg-capacity high frequency induction furnace. Melts were super-heated to $1600^{\circ}C$, and poured at $1550^{\circ}C$ into Y-block pepset molds. Three combinations of the alloying elements were selected so as to obtain the different types of carbides and matrix structures : 3%C-10%Cr-5%Mo-5%W(alloy No. 1), 3%C-10%V-5%Mo-5%W(alloy No. 2) and 3%C-17%Cr-3%V(alloy No. 3). The heat-treatments were conducted as follows: frist of all, as-cast specimens were homogenized at $950^{\circ}C$ for 5h under the vacuum atmosphere. Then, they were austenitized at $1050^{\circ}C$ for 2h and followed by air-hardening in air. The air-hardened specimens were tempered at $300^{\circ}C$ for 3h. The observation of morphology of the matrix structures was carried out in the states of as-cast(AS), air-hardened(AHF) and tempered(AHFT). The matrix structures of each alloy were almost fully pearlitic in the as-cast state but it was transformed to martensite, tempered martensite and retained austenite by the heat-treatments such as air-hardening and tempering.

  • PDF

Single crystal growth of synthetic emerald by flux method of Vandadium - Molybdenum - Lithium oxide system (산화 바나디움, 몰리브데늄, 리티움계 융제법에 의한 합성 Emerald 단결정 육성)

  • 최의석;김무경;이종민;안영필;서청교;안찬준
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.6 no.1
    • /
    • pp.44-55
    • /
    • 1996
  • Emerald (3BeO{\cdot}Al$_{2}$O_{3}{\cdot}6SiO_2 : Cr^{3+}$) single crystals were grown by flux method of $Li_2O-MoO_3 - V_2O_5$ system. The composition of starting materials were 1, 3, 5 mole ratio of $MoO_3 - V_2O_5/$Li_2O$, 20 - 15% of emerald content to flux composition and 1% of $Cr_2O_3$ colordopant to emerald composition. After mixing those were melted at $1100^{\circ}C$ in Pt crucible of electric furnace. Single crystal growth was cooled down slowly rate of $3^{\circ}C$/hr from $1100^{\circ}C$ to $650^{\circ}C$, for the cooling period it was controlled and prevented the nucleation of microcrystallite from variation of each thermal fluctuation range. Specially it has been obtained plenty of large emerald single crystal when thermal fluctuation was treated for cooling period at $1050 ~ 950^{\circ}C$, in 3 mole ratio of $V_2O_5 - MoO_3/Li_2O$ flux. Emerald single crystal growing effect and $Cr_{+3}$ ion of substitutional solid solution effect for $Al_{+3}$ ion was good than mole ratio of 5. Emerald single crystals were c (0001) hexagonal rystal face of preferencial direction and m (1010) post side. Emerald was hexagonal columnar greenish transparent and 2.65 ~ 2.66 of specific gravity.

  • PDF

Effect of Welding Condition on Microstructure of Transient Zone in Overlay Weld of 3Cr-1Mo Steel/STS-309L (3Cr-1Mo강/STS-309L 오버레이 용접부의 천이영역 조직에 미치는 용접조건의 영향)

  • 김동진;김병훈;지병하;김정태;김성곤;강정윤;박화순
    • Journal of Welding and Joining
    • /
    • v.18 no.2
    • /
    • pp.176-176
    • /
    • 2000
  • Recently developed Austenite stainless steel,309L was to overlay on 3Cr-1Mo-V-Ti-B steels, using Electroslag welding process, which wide electrodes were adopted. Transition region in welding interlayer relating to disbonding crack was investigated. Also. the effect of welding condition on the width of transition region and coarsening grains of the austenite were studied.1) With increasing welding speed the width of martensite at transient region was increased, but the amount of delta ferrite in weld metal was reduced, being fine grained.2) The form of martensite at the transition region was occured by reversible transition region, leading to increasing Ms point.3) With increasing welding speed, the grain of austenite formed at the welding interface was finer. With increasing welding current under the same welding speed, the grain size of the austenite was finer. At high current, original grain size of the austenite is coarse, but the austenite has fine grains because the austenite was transformed to martensite during cooling.4) In the case of high welding speed, the width of martensite at the welding interface was increased, but the grain size of austenite at the welding interface was finer. This indicates that the inhibition of disbonding crack may be achieved through dispersening fine carbides in the grain boudary.(Received August 3, 1999)

Dietary intakes of Fe, Zn, Cu, Mn, Se, Mo, and Cr of Korean adult women - Comparison between the data from analyzed and calculated - (성인 여성의 미량무기질(Fe, Zn, Cu, Mn, Se, Mo 및 Cr) 섭취량 - 분석치와 계산치의 비교 -)

  • Kim, Kyung-Hee;Lim, Hyeon-Sook
    • Korean Journal of Human Ecology
    • /
    • v.9 no.3
    • /
    • pp.69-79
    • /
    • 2006
  • The previous studies on the intake of trace elements performed in Korea were only concerned about major elements like Fe, Zn or Cu. There is little data about the intake of minor elements like Mn, Se, Mo or Cr. And most of the data were obtained by calculation using Food Composition Tables or by analysis using atomic absorption spectrophotometers (AAS). The purpose of this study, therefore, was to evaluate the dietary intake of seven trace elements, Fe, Zn, Cu, Mn, Se, Mo, and Cr of Korean adult wonmen and to compare the data between analyzed using ICP-MS (or ICP-AES) and calculated by the CAN-Pro (or Food Composition Table). A total of nineteen adult women participated voluntarily in this study and collected one-tenth of the foods that they consumed for three consecutive days. Analyzed intake of Fe of the subjects was $6.94{\pm}2.18$ (calculated, $18.87{\pm}4.50$) mg/day, that of Ze was $9.35{\pm}4.95$ (calculated, $8.35{\pm}2.87mg/day$), that of Cu was $1.18{\pm}0.26\;(1.11{\pm}0.32mg/day)$, that of Mn was $3.69{\pm}0.69\;(2.83{\pm}1.68mg/day)$, that of Se was $41.93{\pm}9.28$ (calculated, $27.58{\pm}6.97{\mu}g/day$), that of Mo was $134.0{\pm}49.1{\mu}g/day$, and that of Cr was $136.5{\pm}147.9{\mu}g/day$. The analyzed Fe intake of the subjects did not meet Estimated Average Requirement (EAR) nor Recommended Intakes (RI) for Korean women aged 20-29 years old. However, the analyzed intakes of the other six elements, Zn, Cu, Mn, Se, Mo, and Cr, seemed to meet each of the respective RIs. The analyzed Fe intake was significantly lower than the calculated one, in fact by 2.72 times, however, the analyzed intakes of the other elements, Mn and Se, were significantly higher and those of Zn and Cu were similar than each of the calculated ones. The difference of the data between analyzed and calculated intakes indicates that it is necessary to set up database on trace element contents of foods of the Food Composition Table and the CAN-Pro so as to have accuracy.

  • PDF

Optimization of Friction Welding of Cr-Mo Steels and Real-Time Nondestructive Evaluation by Acoustic Emission Method (Cr-Mo강의 마찰용접 최적화와 음향방출법에 의한 실시간 비파괴적 평가)

  • Oh, S.K.;Jang, J.H.;Chang, H.K.
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.15 no.4
    • /
    • pp.511-519
    • /
    • 1996
  • The purposes of this study are 1) to develop optimum FRW technique of SNCM220, SCM435, SACM645 and SCM415 bar-to-bar similar friction welding, 2) to develop in-process real-time weld quality nondestructive evaluation technique by acoustic emission method, and 3) to certify of weld quality by inspection of tensile fracture surface on friction welded joints.

  • PDF

Effect of Dissolved Oxygen on the Stress Cor rosion Cracking Behavior of 3.5NiCrMoV Steels in High Temperature Water

  • Lee, J.H.;Maeng, W.Y.;Kim, U.C.
    • Corrosion Science and Technology
    • /
    • v.2 no.4
    • /
    • pp.178-182
    • /
    • 2003
  • Slow Strain Rate Tests (SSRT) were carried out to investigate the effect of environmental factors on the Stress Corrosion Cracking (SCC) susceptibility of 3.5NiCrMoV steels used in discs for Low-Pressure (LP) steam turbines in electric power generating plants. The influences of dissolved oxygen on the stress corrosion cracking of turbine steel were studied, For this purpose, specimens were strained at variously oxygenated conditions at $150^{\circ}C$ in pure water. When the specimen was strained with $1{\times}10^{-7}s^{-1}$ at $150^{\circ}C$ in pure water, increasing concentration of dissolved oxygen decreased the elongation and the UTS. The corrosion potential and the corrosion rare increased as the amounts of dissolved oxygen increased. The increase of the SCC susceptibility of the turbine steel in a highly dissolved oxygen environment is due to the non protectiveness of the oxide layer on the turbine steel surface and the increase of the corrosion current. These results clearly indicate that oxygen concentration increases Stress Corrosion Cracking susceptibility in turbine steel at $150^{\circ}C$.

Electrical Conductivity of ${La_{2-x}}{Sr_x}{Mo_{2-y}}{Cr_y}{O_{9-\delta}}$Ionic Conductors (${La_{2-x}}{Sr_x}{Mo_{2-y}}{Cr_y}{O_{9-\delta}}$ 이온전도체의 전기전도도)

  • ;;Allan J. Jacobson
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.8
    • /
    • pp.693-697
    • /
    • 2001
  • 고상반응법으로 이론 밀도의 약 92%의 소결 밀도를 갖는 입방정계의 새로운 이온전도체 L $a_{2-x}$S $r_{x}$M $o_{2-y}$C $r_{y}$ $O_{9-{\delta}}$(x=0, 0.05, y=0, 0.1)를 제조하였다. 교류 복소임피던스는 3$50^{\circ}C$~90$0^{\circ}C$의 온도범위에서 공기중에서 측정하여, EQUIVCRT 모델링 소프트웨어로 해석하였다. 상 전이온도인 58$0^{\circ}C$ 전.후로 임피던스 스펙트럼에 큰 차이가 있었으며, 전기전도도는 L $a_2$M $o_2$ $O_{9}$ 시편의 경우 7$50^{\circ}C$에서 3$\times$$10^{-2}$ S$cm^{-1}$ /로 우수하였으며, 활성화 에너지는 고온 상 영역에서는 0.89 eV, 저온 상 영역에서는 1.12 eV이었다. 순수한 L $a_2$M $o_2$ $O_{9}$과 비교하여 Cr 치환효과는 크지 않았으나, Sr 치환 시에는 상 전이온도의 감소와 전기전도도의 증가 현상을 보였으며, 전이온도 부근에서의 전기전도도 변화 폭은 작았다.다.

  • PDF

Characteristics of Hydrogen Storage in Ti-Cr-Mo and Ti-Cr-V bcc Alloys (Ti-Cr-Mo계 및 Ti-Cr-V계 bcc 합금의 수소저장특성에 관한 연구)

  • You, J.H.;Cho, S.W.;Park, C.N.;Choi, J.
    • Journal of Hydrogen and New Energy
    • /
    • v.16 no.2
    • /
    • pp.122-129
    • /
    • 2005
  • The characteristics of hydrogen storage have been investigated in the Ti-Cr-Mo and Ti-Cr-V ternary alloys with bcc structure. The alloys were melted by arc furnace and remelted 4-5 times for homogeneity. The lattice parameters, microstructures and phases of the alloys were examined by SEM, EDX and XRD, and the Pressure-Composition isotherms of the alloys were measured. From these data the relationship of the maximum and effective hydrogen storage capacities vs. chemical composition, lattice parameter and the radius of tetrahedral site were analyzed and discussed. The results showed that all of these alloy, in the range of the this study, had mainly bcc solid solutions with small amount of Ti segregation due to a lower melting point of Ti compared with other elements. Lattice parameters of the alloys were very near to the atomic average values of lattice parameters of the constituent elements. It was also found that maximum hydrogen storage capacities of the Ti-Cr-Mo alloys increased with increasing Ti content and the radius of tetrahedral site but the effective hydrogen storage capacities decreased after showing the maximum. The hydrogen storage capacities of the Ti-Cr-V alloys were almost same even though the V contens were quite different from alloy to alloy and this could be attributed to the almost same Ti/Cr ratio of the alloys. The maximum effective hydrogen storage capacity of the Ti-Cr-Mo alloys was revealed at Ti content of about 40${\sim}$50 at% and radius of tetrahedral site of 0.43${\sim}$0.45 nm. The Ti-Cr-V alloys showed the hydrogen storage capacities of 3.0 wt% and effective hydrogen storage capacities of 1.5 wt%.