• Title/Summary/Keyword: 316 Stainless Steel

Search Result 458, Processing Time 0.024 seconds

Effects of Microstructural Change in Joint Interface on Mechanical Properties of Si3N4/S.S316 joint with Ni Buffer layer (Ni buffer layer를 사용한 Si3N4/S.S316 접합체에서 접합계면의 미세구조 변화가 접합체의 기계적 특성에 미치는 영향)

  • 장희석;박상환;권혁보;최성철
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.4
    • /
    • pp.381-387
    • /
    • 2000
  • Si3N4/stainless steel 316 joints with Ni buffer layer were fabricated by direct active brazing method (DIB) using Ag-Cu-Ti brazing alloy only and double brazing method (DOB) using Ag-Cu brazing alloy with Si3N4 pretreated with Ag-Cu-Ti brazing alloy. For the joint brazed by DIB method, Ti was segregated at the Si3N4/brazing alloy interface, but was not enough to form a stable joint interface. In addition, large amounts of Ni-Ti inter-metallic compounds were formed in tehbrazing alloy near the joint interface, which could deplete the contents of Ti involved in the interfacial reaction. However, for the joint brazed by DOB method, segregation of Ti at the joint interface were enough to enhance the formation of stable interfacial reaction products such as TiN and Ti-Si-Ni-N-(Cu) multicompounds, which restricted the formation of Ni-Tio inter-metallic compounds in the brazing alloy during brazing with Ni buffer layer. Fracture strength of Si3N4/S.S 316 joints with Ni buffer layer was much improved by using DOB method rather than DIB method. It could be deduced that the differences of fracture strength of the joint with Ni buffer layer depending on brazing process adapted were directly affected by the formation of stable joint interface and the change in microstructure of the brazing alloy near the joint interface. It was found that fracture strength of Si3N4/S.S 316 joints with Ni buffer layer was gradually reduced as the thickness of interface. It was found that fracture strength of Si3N4/S.S 316 joints with Ni buffer layer was gradually reduced as the thickness of Ni buffer layer in the joint was increased from 0.1 mm to 10 mm. It seems to due to the increased residual stress in the joint as the thickness of Ni buffer layer is increased. The maximum fracture strength of Si3N4/S.S 316 joints with Ni buffer layer was 386 MPa, and the fracture of joint was originated at Si3N4/brazing alloy joint interface and propagated into Si3N4 matrix.

  • PDF

Catalytic CVD-Kinetics of Pyrolytic Carbon and SiC on the Stainless Steel Stent (Stainless Steel Stent에 Pyrolytic Carbon과 SiC의 촉매적 CVD-Kinetic연구)

  • 이보성;이무용
    • Proceedings of the KAIS Fall Conference
    • /
    • 2000.10a
    • /
    • pp.30-33
    • /
    • 2000
  • 최근 국내에서도 관 동맥 질환 환자의 수가 급증하고 있으며, 관 동맥 질환의 치료 방법인 관 동맥 성형 술은 관 동맥 stent의 도입에 의하여 보편화되어 국내에서 년간 5000개 이상의 stent가 시술되고 있다. 그러나 stent는 고가(1,200천원/개)로 전량 수입에 의존하고 있으며, 시술 후 사망까지 이를 수 있는 혈전에 의한 급성 페쇠와 재 협착이 문제점이다. 이를 위한 한가지 방법이 생체 적합성이 뛰어난 복합 stent의 개발인데 SiC나 Carbon을 coating한 stent는 시술 후 혈전 형성을 억제하는 것으로 알려져 있다. 특히 가장 순수한 Pyrolytic carbon은 hemocompatibility가 탁월하고 기밀 성이기 때문에 본 연구에서 그의 CVB-Kinetics를 연구코저 하는 것이다. methane으로부터 pyrolytic carbon의 CVD는 온도에 따라서 다양한 구조를 가지며 따라서 그의 mechanism도 다양하다는 것은 잘 알려져 있다. 더구나 광간(균질)반응과 표면(불균질)반응의 정량적 관계에 따라서도 다르다는 것도 확인되었다. 그러나 stainless steel 316L로 만든 stent는 12 - 15 %의 Ni과 2%의 Mo을 함유해서 금속성을 잃지 않는 저온(600℃)에서도 pyrolytic carbon의 속매적 CVD가 가능함을 그리고 SiC의 코팅에 적합한 buffer layer 역할을 함을 확인하였다. 그리하여 본 연구는 반응기 설계에 필요한 저온 촉매적 pyrolytic carbon의 CVD-kinetics의 연구결로 그의 mechanism과 함께 rate law 식을 유도, 확인하였으며 600℃, 90kPa에서 P/sub ch4//P/sub H2/=5:1과 체류시간 1.8 sec가 최적임을 발견하였다. 이때 석출속도 11.2 g-mol/g-cat.h 혹은 두께속도로 73 nm/sec를 나타내었다.메타놀-물 (1 : 1) 유출액에서 $(0.80\;{\mu}g)$ 검출되었다. 하면 morey eel내장에서 얻은 독물질도 DEAE-셀루로즈에서 ST-1 과 ST-2로 나누어지며, 이 ST-1의 TLC, HPLC 및 알루미나 컬럼상의 거동이 파랑비늘돔에서 얻은 ST-1의 그것과 같으므로 scaritoxin으로 보고한 ST-1은 ciguatoxin의 형태인 less polar cigutoxin (LPCTX) 으로 생각된다.에서 각각 대조구의 57, 413 및 315% 증진되었다. 거품의 열안정성은 15분 whipping시, pH 4.0(대조구, 30.2%) 및 5.0(대조구, 23.7%)에서 각각 $0{\sim}38.0$$0{\sim}57.0%$이었고 pH 7.0(대조구, 39.6%) 및 8.0(대조구, 43.6%)에서 각각 $0{\sim}59.4$$36.6{\sim}58.4%$이었으며 sodium alginate 첨가시가 가장 양호하였다. 전체적으로 보아 거품안정성이 높은 것은 열안정성도 높은 경향이며, 표면장력이 낮으면 거품형성능이 높아지고, 비점도가 높으면 거품안정성 및 열안정성이 높아지는 경향이 있었다.protocol.eractions between application agents that are developed using different languages. Dynamic agent invocation is accomplished by Java Native Interface(JNI) that links two heterogeneous methods, and by KQML language interface that facilitates the communications between heterogeneous agents. This scheme of dyna

Detection of Thermal Ratcheting Deformation for Cylindrical Shells by Ultrasonic Guided Wave (유도초음파를 이용한 원통형 쉘의 열 라체팅 변형 탐지)

  • Joo, Young-Sang;Lee, Hyeong-Yeon;Kim, Jong-Bum;Park, Chang-Gyu;Lee, Jae-Han
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.26 no.5
    • /
    • pp.297-305
    • /
    • 2006
  • The thermal ratcheting deformation at the reactor baffle and upper internal structure of the liquid metal reactor (LMR) can occur due to movement of the hot sodium free surface. In in-service inspection of reactor internals of LMR, a new inspection technique should be developed for the detection of the thermal ratcheting damage. In this study, an inspection technique using ultrasonic guided wave is proposed for the detection of the thermal ratcheting damage of cylindrical vessels. A 316L stainless steel cylindrical shell specimen has been prepared. The thermal ratchet structural tests were cyclically performed by heat-up up to $550^{\circ}C$ with steep temperature gradients along the axial direction after cool-down by cooling water. Ultrasonic guided wave propagation has been characterized by analysis of dispersion curve of the stainless steel plate. The zero-order antisymmetric $A_0$ guided wave has been selected as the optimal mode for detection of the ratcheting deformation. It is confirmed that the thermal ratcheting deformation can be detected by the measurement of transit time difference of circumferentially propagated $A_0$ guided waves.

EFFECT OF CHEMICAL TREATMENT ON THE BIOACTIVITY OF TITANIUM (화학적 처리가 티타늄의 생체활성도에 미치는 영향)

  • Min Kwan-Sik;Lee Min-Ho;Ahn Seung-Geun;Park Charn-Woon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.43 no.4
    • /
    • pp.562-572
    • /
    • 2005
  • Statement of problem : Titanium is widely used as an implant material lot artificial teeth. Also, studies on surface treatment to form a fine passive film on the surface of commercial titanium or its alloys and improving bioactivity with bone have been carried out. However, there is insufficient data about the biocompatibility of the implant materials in the body. Purpose: The purpose of this study was to examine whether the precipitation of apatite on titanium metal is affected by surface modification. Materials and methods: Specimens chemically washed for 2 minute in a 1:1:1.5 (in vol%) mixture of 48% HF 60% $HNO_3$ and distilled water. Specimens were then chemically treated with a solution containing 97% $H_2SO_4$ and 30% $H_2O_2$ at $40^{\circ}C$S for 1 hour, and subsequently heat-treated at $400^{\circ}C$ for 1 hour. All specimens were immersed in the HBSS with pH 7.4 at $36.5^{\circ}C$ for 15 days, and the surface were examined with TF-XRD, SEM, EDX and XPS. Also, commercial purity Ti specimens with and without surface treatment were implanted in the abdominal connective tissue of mice for 4 weeks. Conventional aluminium and stainless steel 316L were also implanted for comparison. Results and conclusions : The results obtained were summarized as follows. 1. An amorphous titania gel layer was formed on the titanium surface after the titanium specimen was treated with a $H_2SO_4$ and $H_2O_2$ solution. The average roughness was $2.175{\mu}m$ after chemical surface treatment. 2. The amorphous titania was subsequently transformed into anatase by heat treatment at $400^{\circ}C$ for 1 hour. 3. The average thickness of the fibrous capsule surrounding the specimens implanted in the connective tissue was $46.98{\mu}m$ in chemically-treated Ti, and 52.20, 168.65 and $100.95{\mu}m$ respectively in commercial pure Ti, aluminum and stainless steel 316L without any treatment.

Study on VHCF Fatigue Behaviors and UNSM Effects of Hydrogen Attacked STS 316L (수소취화된 스테인리스강 316L의 VHCF(Very High Cycle Fatigue) 피로특성과 UNSM 효과에 관한 연구)

  • Nahm, Seung-Hoon;Baek, Un-Bong;Suh, Chang-Min;Pyun, Young-Sik
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.41 no.11
    • /
    • pp.1011-1020
    • /
    • 2017
  • This study was conducted to investigate the material properties of stainless steel 316L specimens of untreated and UNSM treated material, hydrogen attacked material(100 bar, $300^{\circ}C$ at 120 h) and UNSM treated hydrogen attacked material at room temperature. Results demonstrated that the hydrogen attacked materials showed a tendency toward a slightly decreased fatigue strength, while the hydrogen embrittlement effect was smaller than the S-N curve of conventional untreated material. As compared to untreated material, the fatigue limit of the UNSM treated material increased by 43.8%, while it was 57.1% higher in the UNSM treated hydrogen attacked material than in untreated hydrogen attacked material. The plastic deformation layer was ${\sim}152{\mu}m$ thick, as confirmed by maps showing the level of local plastic deformation affected by the UNSM treatment in three ways: an image quality map, inverse pole figure map, and kernel average misorientation map captured via electron back scatter diffraction. Owing to hydrogen embrittlement, about 90% of surface cracks were smaller than the average grain size of $35{\mu}m$.

Evaluation of Mechanical Properties of Alloy 82/182 Weld Joint Between SA508 Gr.3 Nozzle and F316L Safe-End (SA508 Gr.3 노즐과 F316L 안전단 사이의 Alloy 82/182 용접부에 대한 기계적물성치 평가)

  • Kim, Jin-Weon;Lee, Kyung-Soo;Park, Chi-Yong
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.34 no.3
    • /
    • pp.333-340
    • /
    • 2010
  • This paper presents the distributions of the tensile and fracture properties of an alloy 82/182 dissimilar weld joint between an SA508 Gr.3 nozzle and F316L SS safe-end at ambient temperature. Tensile and J-R tests were conducted using specimens extracted from base metals, heat-affected zones (HAZs), buttering regions, and various regions of the weld metal. The results show that the root region of the weld has higher strength than the upper region. The yield and tensile strengths vary considerably within the root region of the weld. The buttering region had the lowest strengths. The strengths gradually increased as the F316L stainless steel weld boundary was approached. The variation of the strengths within the upper region of the weld is insignificant. The fracture toughness of the alloy 82/182 weld metal is less than those of both the base metals and both HAZs. Within the alloy 82/182 weld, the center of weld has a slightly lower fracture toughness than the weld boundary and buttering region, and the root region has greater toughness than the upper region of the weld.

Effect of Micro-grooves Manufactured via Ultrasonic Nanocrystalline Surface Modification on Sliding Friction (초음파나노표면개질기술로 제작된 마이크로 그루브가 미끄럼 마찰 특성에 주는 영향)

  • Ro, Junsuek;Amanov, Auezhan
    • Tribology and Lubricants
    • /
    • v.37 no.1
    • /
    • pp.25-30
    • /
    • 2021
  • The surface texture produced via surface texturing is an important approach for controlling the tribological behavior of friction behavior of mechanical devices. The purpose of this study is to investigate the effect of grooves generated via ultrasonic nanocrystal surface modification (UNSM) technology on the tribological performance of AISI 4150 steel against stainless steel 316L. In the study, tribological tests are performed under two different regimes, namely mixed and hydrodynamic lubrication, by varying the applied normal load and reciprocating speed during the tests. According to the test results, the friction coefficient decreases as static load (10 N, 30 N, and 50 N) of UNSM technology increases in the mixed lubrication regime. Conversely, the friction coefficient increases as the static load (10 N, 30 N, and 50 N) of UNSM technology increases in the hydrodynamic lubrication regime. Hence, the results indicate that micro-grooves generate hydrodynamic pressure in the outlet, which increases the oil film thickness between the two mating surfaces. This potentially leads to a reduction in friction in the mixed lubrication regime due to the prevention of contact of asperities and debris. However, the results indicate an adverse effect in the hydrodynamic lubrication regime. In this regard, additional experiments should be performed to investigate the effect of grooves generated by UNSM technology at varying conditions on the friction behavior of AISI 4150 steel, which in turn can be controlled by the generated pressure and oil film thickness at the contact interface.

Dose modeling and its Application of Ir-192 for substitution of Ralstron Brachytherapy source (Ralstron 선원대체형 Iridium-192 선원의 선량모델링과 응용)

  • 김옥배;최태진;김진희;이호준;박정호;김성규;조운갑;한현수
    • Progress in Medical Physics
    • /
    • v.11 no.2
    • /
    • pp.131-139
    • /
    • 2000
  • We designed high dose rate Ir-192 source which was prepared for substitute the Co-60 source in Ralstron unit (Simatsu, Japan) which is supplied for cervical cancer treatment. The source dimension is 1.5 mm in a diameter and 1.5mm thickness of cylinder and encapsulated with 3 mm diameter of stainless steel(SUS316L) to substituted for the Co-60 source size. The Ir-192 source was prepared the dose model for tissue dose computation through the experimental determination of apparent activity and applied the empirical tissue correction factors extended to 20cm distance. The tissue dose model was applied the 4.69 R/cm-mCi-hr gamma constant and the ratio of energy absorption coefficient of water to that of air showed 1.112 include filteration of the self-absorptions. In this experiments, we prepared the dose computation software to clinical usefulness.

  • PDF

PWR 원전환경에서 오스테나이트 스테인리스강의 피로균열성장특성에 미치는 질소의 영향

  • Min, Gi-Deuk;Kim, Dae-Hwan;Lee, Bong-Sang;Kim, Seon-Jin
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.10a
    • /
    • pp.39.1-39.1
    • /
    • 2011
  • 가압경수로의 압력경계기기는 약 $300^{\circ}C$, 150기압의 고온고압수환경에서 가동되고 있다. 특히 가압기 밀림관은 고온수와, 저온수가 교차하는 부분으로 열성층 형성으로 열적, 기계적 피로 및 수화학환경이 더해진 부식피로 등에 의하여 손상을 받는다. PWR 원전에서 수화학환경은 대표적으로 용존산소(DO) 5ppb, pH 6~8, 용존수소(DH) <30 cc/kg, 온도 $316^{\circ}C$의 환경을 유지하게 된다. 가압기 밀림관에는 오스테나이트계 스테인리스강이 사용되는데, 오스테나이트계 스테인리스강은 고온 수화학환경에 민감한 것으로 알려져 있다. 따라서 오스테나이트계 스테인리강을 공기중에서의 기계적특성 및 피로특성을 향상시키기 위하여 질소를 첨가한 스테인리스강을 제조하여 PWR 원전환경에서의 피로균열성장특성을 평가하였다. 실험에 사용된 재료는 PWR 원전 가압기 밀림관 소재인 Type 347 스테인리스강에 0.0005 wt%가 첨가된 상용재와 0.11 wt% 질소가 첨가된 재료이다. 사용된 시편형상은 두께 5 mm, 폭 25.4 mm의 CT 시편이다. 수화학환경은 150기압, 온도 $316^{\circ}C$, 용존산소(DO) 5ppb, 용존수소(DH) 30 cc/Kg, pH는 약 7로 유지 하였으며, 응력비 0.1, 하중 반복속도 10Hz의 기계적 조건에서 하중제어로 시험을 진행하였다. 균열길이는 직류전위차법(Direct Current Potential Drop: DCPD)을 이용하여 측정하였다. 질소함량이 증가할수록 동일 사이클에서 균열길이가 늦게 성장하였고, 피로균열성장속도도 약간 늦어지는 것으로 나타났다. 각 스테인리스강의 피로파면 관찰결과 상용재는 약 1 ${\mu}m$의 산화물들이 생성되는 반면 질소첨가 스테인리스강은 약 0.1 ${\mu}m$정도 산화물이 생성되었다. 산화막의 두께도 질소가 첨가됨으로써 상용재에 비해 얇게 생성되었다. 따라서 질소가 첨가됨으로써 부식환경에서 내산화성이 향상되었으며, 이는 피로균열성장특성에 영향을 미치는 것으로 판단된다.

  • PDF

A Study on the Overlay Welding Process Optimization of GTAW by Double Torch (GTAW Double Torch의 육성용접 공정최적화에 관한 연구)

  • Lim, Byung-Chul;Son, Young-San
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.17 no.3
    • /
    • pp.73-78
    • /
    • 2016
  • In this study, GTAW was carried out on austenitic STS316 stainless steel. Overlay welding with the stellite-base filler metal was implemented using a double torch. The response variable was calculated on the measured Vickers hardness for process optimization using the Taguchi method and its response variable was then analyzed about effect on overlay welding characteristics. The optimal process design by the Taguchi method is extremely effective in the overlay welding process for the multiple response variables. In addition, the effects of contribution rate about each response variable was analyzed easily. The conditions of the optimal process were 105A, 18V, pre-heat treatment at $200^{\circ}C$, and post weld heat treatment at $100^{\circ}C$. The Vickers hardness of the specimens produced under the optimal condition of GTAW by the double torch was 8.19% higher than that by a single torch.