Creep damage and life assessment of thick cylindrical pressure vessels with variable thickness made of 304L austenitic stainless steel

  • Kashkoli, Mosayeb Davoudi;Tahan, Khosro Naderan;Nejad, Mohammad Zamani
    • Steel and Composite Structures
    • /
    • v.32 no.6
    • /
    • pp.701-715
    • /
    • 2019
  • Using first-order shear deformation theory (FSDT), a semi-analytical solution is employed to analyze creep damage and remaining life assessment of 304L austenitic stainless steel thick (304L ASS) cylindrical pressure vessels with variable thickness subjected to the temperature gradient and internal non-uniform pressure. Damages are obtained in thick cylinder using Robinson's linear life fraction damage rule, and time to rupture and remaining life assessment is determined by Larson-Miller Parameter (LMP). The thermo-elastic creep response of the material is described by Norton's law. The novelty of the present work is that it seeks to investigate creep damage and life assessment of the vessels with variable thickness made of 304L ASS using LMP based on first-order shear deformation theory. A numerical solution using finite element method (FEM) is also presented and good agreement is found. It is shown that temperature gradient and non-uniform pressure have significant influences on the creep damages and remaining life of the vessel.

Development of a duplex stainless steel for dry storage canister with improved chloride-induced stress corrosion cracking resistance

  • Chaewon Jeong;Ji Ho Shin;Byeong Seo Kong;Junjie Chen;Qian Xiao;Changheui Jang;Yun-Jae Kim
    • Nuclear Engineering and Technology
    • /
    • v.56 no.6
    • /
    • pp.2131-2140
    • /
    • 2024
  • The chloride-induced stress corrosion cracking (CISCC) is one of the major integrity concerns in dry storage canisters made of austenitic stainless steels (ASSs). In this study, an advanced duplex stainless steel (DSS) with a composition of Fe-19Cr-4Ni-2.5Mo-4.5Mn (ADCS) was developed and its performance was compared with that of commercial ASS and DSS alloys. The chemical composition of ADCS was determined to obtain greater pitting and CISCC resistance as well as a proper combination of strength and ductility. Then, the thermomechanical processing (TMP) condition was applied, which resulted in higher strength than ASSs (304L SS and 316L SS) and better ductility than DSSs (2101 LDSS and 2205 DSS). The potentiodynamic polarization and electrochemical impedance spectra (EIS) results represented the better pitting corrosion resistance of ADCS compared to 304L SS and 316L SS by forming a better passive layer. The CISCC tests using four-point loaded specimens showed that cracks were initiated at 24 h for 304L SS and 144 h for 316L SS, while crack was not found until 1008 h for ADCS. Overall, the developed alloy, ADCS, showed better combination of CISCC resistance and mechanical properties as dry storage canister materials than commercial alloys.

Unified Constitutive Modeling for Low Temperature Austenitic Stainless Steel (저온용 스테인레스강의 통합 구성방정식)

  • Yoo, Seong-Won;Park, Woong-Sup;Lee, Jae-Myung
    • Proceedings of the Computational Structural Engineering Institute Conference
    • /
    • 2010.04a
    • /
    • pp.504-507
    • /
    • 2010
  • 본 논문에서는 저온용 오스테나이트계 스테인리스강(ASS)의 온도 및 변형률 속도의 영향을 고려한 통합 구성 방정식 및 손상 모델을 제안하였다. 저온 영역에서, 304L ASS의 온도 및 변형률 속도별 인장 실험을 시행하였다. 그 결과, 변형 유기 마르텐사이트 상변태에 의해 상변태 유기 소성(TRIP)이 저온에서 현저히 나타났으며 온도 및 변형률 속도의 영향이 지대하였다. 실험 결과를 바탕으로 ASS의 저온 거동 및 특성을 규명하여 수치 모델에 반영하였다. 저온에서 일어나는 2차 경화 현상을 표현하기 위해, Bodner/Partom 점소성 구성 방정식을 수정하고 Tomita/Iwamoto 변형 유기 상변태 모델을 구성 방정식에 적용시켰다. 저온 연성 파단 현상을 표현하기 위해, Bodner/Chan 손상모델을 수정하여 접목시켰다. 제안된 모델을 유한요소 프로그램에 탑재시키고, 온도 및 변형률 속도 의존 재료 정수를 결정하였다. 저온 영역에서, 온도 및 변형률 속도별 재료 거동을 시뮬레이션하고 이를 실험 결과와 비교 및 검증하였다.