  • The whisker grows at the plating of a lead frame so that it causes the serious problem like the short. To prove this case, many people have studied the cause and influence of the tin whisker growth. This study explains the grain size affects the growth of the whisker in the lead frame. By these studies about the whisker, the whisker growth is discovered by stresses generated by the intermetallic compound and CTE mismatch in both plating and base metal. The stresses or lattice defect generated in the plating process changes grain structure of plating. Consequently, these various stresses are stabilized by forming unspecified whiskers through lots of grain boundaries. Because the grain boundary is the path of the whisker growth, the smaller grain size exists, the more whiskers grow.

  • PDF

순 Sn 도금에서의 Sn 휘스커 성장제어 기술 (Mitigation Methods of Sn Whisker Growth on Pure Sn Plating)

  • 김근수
    • Journal of Welding and Joining
    • /
    • 제31권3호
    • /
    • pp.17-21
    • /
    • 2013
  • Sn whiskers are one of the serious causes of the failure of electronics. Sn whiskers grow spontaneously from Sn-based, lead-free finished surfaces, even at room temperature. A primary factor of these Sn whiskers growth is compressive stress, which enhances the diffusion of Sn or other elements. The sources of compressive stress are the growth of non-uniform large intermetallic compounds along the interface between the Sn grain boundary and Cu substrate. Recent studies revealed the methods for reducing Sn whisker growth. This paper gives an overview about recent researches for mitigation methods of Sn whisker growth during nearly room temperature storage.

알루미나 분말의 선택적 레이저 소결을 하기 위한 새로운 무기 접착제의 개발 (Development of a New Inorganic Binder for Selective Laser Sintering of a Alumina Powder)

  • 이인섭
    • 한국재료학회지
    • /
    • 제6권12호
    • /
    • pp.1170-1178
    • /
    • 1996
  • 저용융점을 가진 새로운 무기 접착제인 단사정 HBO2가 알루미나 분말의 선택적 레이저 소결을 하기 위한 접착제로서 개발되었다. 이것을 이용하여 만들어진 green body는 현재까지 알루미나 분말의 선택적 레이저 소결을 위하여 개발된 다른 무기 접착제들인 알루미늄(Ai)과 Ammonium Phosphate(NH4H2PO4)을 이용하여 제조된 것에 비교하여 훨씬 높은 굽힘 강도를 가지고 있고 또 정밀도가 우수하였다. Green Body는 후속의 열처리를 받음으로써 저밀도 단상 세라믹 AI18B4O33과 다상 세라믹 복합재료 AI2O3-AI4B2O9으로 된다. AI18B4O33과 AI4B2O9의 결정립의 모양은 휘스커 구조와 유사하였다. 재료인자와 가공변수가 이 세라믹의 기계적 및 물리적 성질에 미치는 영향이 조사되었다.

  • PDF

플라이 애쉬로부터 뮬라이트 휘스커의 합성 (Synthesis of Mullite Whisker from Fly Ash)

  • 김성환;방희곤;박상엽
    • 한국세라믹학회지
    • /
    • 제42권11호
    • /
    • pp.753-757
    • /
    • 2005
  • In this study, we attempted to recycle the fly ash as a mullite whisker with addition of $Al_{2}O_{3}$ to obtain the high yield of mullite whisker. During the reaction process, mullite whisker was formed with the reaction of amorphous $\alpha$-Cristobalite and Anorthite above $1350^{\circ}C$. With increasing the heat treatment temperature and time, the mean length and aspect ratio of mullite whiskers was gradually increased.

휘스커상을 함유한 수산화아파타이트시멘트 경화체의 미구조-강도 특성 (Microstructure and Mechanical Strength of Hardened Paste of Hydroxyapatite Cement Containing Whisker Phase)

  • 손영도;송태웅
    • 한국세라믹학회지
    • /
    • 제36권12호
    • /
    • pp.1342-1349
    • /
    • 1999
  • In order to improve the density and the mechanical strength without change in chemical composition the hardened pastes of hydroxyapatite cement were reinforced with powders and/or whiskers of hydroxyapatite. The powders behaved as a seed of hydroxyapatite formation rather than a filler while the whiskers were mrerly dispersed in matrix and capillary pores of the hardened bodies leading to increase in mechanical strength. But the increase in strength But the increase in strength was nnt enough owing to the lack of homogeneous dispersion of the fibers. The highest diametral tensile strength of 18.5 MPa was measured at the hardened hydroxyapatite body in which well-dispersed whisker phase formed uniformly during hydro-thermal curing of power-added and dry-formed hydroxyapatite cement.

  • PDF

SiC 휘스커 보강 알루미나 복합재료에서 Slow Crack Growth 현상의 직접관찰 연구 (In Situ Observation of Slow Crack Growth in a Whisker-Reinforced Alumina Matrix Composite)

  • 손기선;김우상;이성학
    • 한국세라믹학회지
    • /
    • 제33권2호
    • /
    • pp.203-213
    • /
    • 1996
  • In this study the subcritical crack growth behavior in an Al2O3-SiCw composite has been investigated using in situ fracture technique of applied moment double cantilever beam (AMDCB) specimens indside an SEM. This technique allows the detailed observation of whisker and grain bridging in the crack wake region. The experimental results indicated that the KI-a curve was deviated from the conventional powder law form and that the existed a region where the rate of microcrack growth was decreased with increasing the externally applied stress intensity factor. This behavior could be explained by arising crack growth resistance i.e. R-curve behavior which was associated with crack shielding due to whisker and grain bridging. The R-curve was also analyzed from the KI-a curve data in order to quantify the bridging effect in the Al2O3-SiCw composite.

  • PDF

카올린의 환원 열탄화법에 의한 베타 탄화규소 휘스커의 합성 (Synthesis of $\beta$-SiC Whiskers by the Carbothermal Reduction of Kaolin)

  • 오세정;류종화;조원승;최상욱
    • 한국세라믹학회지
    • /
    • 제35권12호
    • /
    • pp.1249-1256
    • /
    • 1998
  • ${\beta}$-Silicon carbide(${\beta}$-SiC) whiskers could be synthesized by the carbothermal reduction of kaolin at tem-peratures between 1400 and 1500$^{\circ}C$. The whiskers were grown up to about 1150 of aspect ratio by VS mechanism (showing tapering tips) and to about 45 of that by VLS mechanism (showing round droplet tips) respectively. Hydrocarbon like methane in the reaction atmosphere promoted the formation of gaseous il-icon monoxide(SiO) from silicon dioxide(SiO2) and subsequently reacted with it to form whiskers. The for-mation of ${\beta}$-SiC whiskers increased with increasing carbon content(to 30 wt%) and reaction temperatures. The max. yield of ${\beta}$-SiC whiskers was 15% at 1500$^{\circ}C$ under 20%CH4/80%H2.

  • PDF

Al(OH)3-SiO2-AlF3 조성으로 합성된 뮬라이트 휘스커의 특성평가 (Characterization of Mullite Whiskers Synthesized with Compostion of Al(OH)3-SiO2-AlF3)

  • 이홍림;강종봉
    • 한국세라믹학회지
    • /
    • 제43권5호
    • /
    • pp.320-326
    • /
    • 2006
  • Mullite whiskers were synthesized by a vapor-solid reaction with $Al(OH)_3-SiO_2-AlF_3$. The heat treatment temperature did not affect the shape of mullite whisker but the composition change resulted in different sizes. The first one was $30-50{\mu}m$ in size with the aspect ratio of 60 and above, and the second one was $600{\mu}m$ and below in size with the aspect ratio of 15 and below. The $Al_2O_3$ content in formed mullite whisker was 73.57-80.29 wt%, which is high $Al_2O_3$ content composition. The Young's modulus and the hardness measured by nano-indentation method were 136.7 GPa and 19.81 GPa, respectively.

SiC 휘스커 보강 $Al_2$O$_3$-SiC 복합체의 열간특성 (Thermal Characteristics of SiC Whisker Reinforced $Al_2$O$_3$-SiC Composite)

  • 김윤주;나용한
    • 한국세라믹학회지
    • /
    • 제35권1호
    • /
    • pp.1-4
    • /
    • 1998
  • SiC whisker reinforced Al2O3-SiC composite was fabricated by reaction synthesis method whish is cost ef-fective and allows good dispersion of whiskers. Fracture strength at room temperature showed the highest value with 150$0^{\circ}C$ reaction temperature because a lot of SiC whiskers was formed. Fracture strength at 135$0^{\circ}C$ did not show big differences with reaction temperature due to agglomeration of whiskers and formation of sil-icon oxynitride during hot MO(modulus of rupture) test probably promoting grain boundary sliding.

  • PDF

콜로이드 혼합법 및 Sol-Gel 법에 의해 제조한 SiC 휘스커 강화 LAS 기지 복합체의 특성 (Characteristics of SiC Whisker-Reinforced LAS Matrix Composites Fabricated by the Mixed Colloidal Route and the Sol-Gel Process)

  • 김광수;장현명;정창주;백용기
    • 한국세라믹학회지
    • /
    • 제28권12호
    • /
    • pp.1012-1018
    • /
    • 1991
  • SiC whisker-reinforced LAS matrix composites were developed by a mixed colloidal processing route. An optimization of processing conditions was made using the zeta potential data of silica, boehmite, and SiC whisker dispersions. Similarly, the SiC whisker-reinforced composites were also fabricated by the conventional sol-gel process using the hydrolysis-condensation reaction of relevant metal alkoxides. The composites fabricated by the mixed colloidal processing route were characterized by a uniform spatial distribution of SiC whisker throughout the matrix. The fracture toughness increased from 1.3 MPa.m1/2 for the LAS specimen to 5.0 Mpa.m1/2 for the hot-pressed composite (95$0^{\circ}C$ and 20 MPa for 20 min) containing 20 wt% SiC whisker. The increase in fracture toughness appears to result mainly from the crack deflection and the crack bridging by whiskers with some additional toughenings from the whisker pullout and the matrix prestressing mechanisms.

  • PDF