탄화규소 휘스커의 합성(I) : 반응기구의 율속반응 (Synthesis of Silicon Carbide Whiskers (I) : Reaction Mechanism and Rate-Controlling Reaction)

  • 최헌진;이준근
    • 한국세라믹학회지
    • /
    • 제35권12호
    • /
    • pp.1329-1336
    • /
    • 1998
  • A twt -step carbothermal reduction scheme has been employed for the synthesis of SiC whiskers in an Ar or a H2 atmosphere via vapor-solid two-stage and vapor-liquid-solid growth mechanism respectively. It has been shown that the whisker growth proceed through the following reaction mechanism in an Ar at-mosphere : SiO2(S)+C(s)-SiO(v)+CO(v) SiO(v)3CO(v)=SiC(s)whisker+2CO2(v) 2C(s)+2CO2(v)=4CO(v) the third reaction appears to be the rate-controlling reaction since the overall reaction rates are dominated by the carbon which is participated in this reaction. The whisker growth proceeded through the following reaction mechaism in a H2 atmosphere : SiO2(s)+C(s)=SiO(v)+CO(v) 2C(s)+4H2(v)=2CH4(v) SiO(v)+2CH4(v)=SiC(s)whisker+CO(v)+4H2(v) The first reaction appears to be the rate-controlling reaction since the overall reaction rates are enhanced byincreasing the SiO vapor generation rate.

  • PDF

알루미나 또는 카본 코팅 SiC 휘스커의 코팅층 두께 및 형상에 미치는 코팅조건의 영향 (Effects of Coating Conditions on the Thickness and Morphology of Alumina- or Carbon-Coated Layers on SiC Whiskers)

  • 배인경;장병국;조원승;최상욱
    • 한국세라믹학회지
    • /
    • 제36권5호
    • /
    • pp.513-520
    • /
    • 1999
  • Alumina-coated SiC whiskers wee prepared by the calcination (1150$^{\circ}C$, 1h, Ar) of the alumina hydrate layer which was precipitated homogeneously on whisker surface from a solution of Al2(SO4)3 and urea as a precipitant. In addition carbon coated SiC whiskers were prepared by the pyrolysis (1000$^{\circ}C$, 4h Ar) of phenolic resin coated whisker. The effects of coating conditions on the thickness and morphology of the coated layers were examined by SEM and TEM. It was found that Al2O3-coating layers become thinner and more uniform with decreasing the Al2(SO4)3 concentration. Thin (0.075-0.1$\mu\textrm{m}$) and uniformly alumina-coating layers were obtained at the Al2(SO4)3 concentration 0.010mol/l. On the other han carbon-coating layers were uniform but very thin (5-16 nm) in thickness. For thicker carbon-coating layers ethanol as a disperse medium was found to be more efficient compared tousing acetone.

  • PDF

ZnO 나노휘스커 소재를 이용한 MEMS가스센서의 소비전력과 메탄 감응 특성 연구 (Methane sensing characteristics and power consumption of MEMS gas sensor based on ZnO nanowhiskers)

  • 문형신;박성현;김성은;유윤식
    • 센서학회지
    • /
    • 제19권6호
    • /
    • pp.462-468
    • /
    • 2010
  • A low power gas sensor with microheater was fabricated by MEMS technology. In order to heat up the gas sensing material to a operating temperature, a platinum(Pt) micro heater was built on to the micromachined Si substrate. The width and gap of microheater were $20\;{\mu}m$ and $4.5\;{\mu}m$, respectively. ZnO nanowhisker arrays were fabricated on a sensor device by hydrothermal method. The sensor device was deposited with ZnO seeds using PLD systems. A 200 ml aqueous solution of 0.1 mol zinc nitrate hexahydrate, 0.1 mol hexamethylenetetramine, and 0.02 mol polyethylenimine was used for growthing ZnO nanowhiskers. The power consumption to heat up the gas sensor to a operating temperature was measured and temperature distribution of sensor was analyzed by a Infrared Thermal Camera. The optimum temperature for highest sensitivity was found to be $250^{\circ}C$ although relatively high(64 %) sensitivity was obtained even at as low as $150^{\circ}C$. The power consumption was 72 mW at $250^{\circ}C$ and was only 25 mW at $150^{\circ}C$.

Line-Focus-Beam 초음파 현미경을 이용한 금속복합재료의 피로손상에 관한 연구 (Evaluation of Fatigue Damage of Metal Matrix Composite by LFB Acoustic Microscopy)

  • 이준현
    • 비파괴검사학회지
    • /
    • 제13권2호
    • /
    • pp.40-47
    • /
    • 1993
  • 분말 야금법에 의해 제조된 SiC휘스커 강화 2124알루미늄 복합재료(SiCw/2124 Al)에 피로하중이 작용할 경우 복합재료의 계면에 있어서의 전위의 집적현상으로 인해 피로손상에 매우 민감하다. 그러나 이와같은 계면에 있어서의 전위의 집적현상으로 발생하는 피로미소균열의 검출 및 그 특성 평가에 대해서는 종래의 초음파 기술로서는 많은 문제점이 지적되고 있다. 본 논문은 SiC 휘스커 강화 알루미늄 복합재료에 있어서의 초기 피로손상을 평가하기 위하여 최근 새로운 비파괴 기법인 선집속 빔초음파 현미경의 적용 가능성에 대하여 연구하였다. 이를 위해 SiCw/2124 Al 복합재료 시험편에 대해 하중제어하에서 누설표면파와 누설유사표면파의 속도를 V(z)곡선으로 부터 FFT해석으로 구해 그 특성에 대하여 검토하였다. 또 주파수 5MHz에 대한 종래의 표면파 기법에 의하여 얻어진 결과와 고주파 초음파 현미경에 의하여 구해진 결과를 비교 검토 하였다.

  • PDF

자전연소합성법에 의한 여러 가지 섬유상 및 입상 탄화물의 제조 (Fabrication of Various Carbides with Fibrous and Particulate Shapes by Self-Propagating High Temperature Synthesis Method)

  • 방환철;윤존도
    • 한국재료학회지
    • /
    • 제10권5호
    • /
    • pp.343-349
    • /
    • 2000
  • 자전연소합성(SHS)법을 이용하여 탄소섬유와 티타늄, 지르코늄, 니오븀, 규소, 붕소, 중석, 몰리브덴의 분말로부터 여러 가지 섬유상 탄화물의 합성을 시도하였다. 티타늄과 지르코늄은 예열없이, 그 이외의 경우는 전기로 또는 화학로를 사용하여 예열하여 반응을일으킨 결과, TiC, ZrC, NbC, SiC, $B_4$C, WC,$ Mo_2$C 의 순수한 탄화물의 형성되었다. TiC, ZrC, NbC 및 $B_4$C 탄화물의 형상은 속의 빈 섬유상이었고, SiC는 보다 작은 입자와 미세 휘스커로 이루어진 섬유상을 하고 있었고 WC와 $Mo_2$C 는 비섬유상을 하고 있었다. 여러 가지 형상의 원인에 대하여 합리적 설명을 시도하였으며 정성적 메카니즘을 제안하였다.

  • PDF

$Al_{18}B_4O_{33}$휘스커 강화 금속기 복합재료의 파괴인성에 관한 연구 (A Study on Fracture Toughness of Metal Matrix Composites Reinforced with $Al_{18}B_4O_{33}$)

  • 박성호;최용범;박원조;허선철;윤한기
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2002년도 추계학술대회 논문집
    • /
    • pp.335-340
    • /
    • 2002
  • In recent years, the study of metal matrix composite has increased specially, aluminum alloy, research and development are briskly progress to find new metal matrix composite. this study is following the this purpose; This study is used metal matrix composite that was produced by matrix, AC4CH. and reinforcement $A_{18}B_4O_{33}$ metal matrix composite to add $Al_2O_3,\;TiO_2$ for strengthen of binding together among the Whisker. Each Metal matrix composite is produced using the squeeze casting method. Fracture tounghness test was in accordance with the provisions of ASTM E399; Specimen was produced half-size CT specimen W=25mm, B=12.5mm, Cross head speed 0.05mm/min in room temperature. The plane strain fracture toughness $K_{IC}$ is $8.7MPa-m^{0.5}$ for $Al_{18}B_4O_{33}$/AC4CH., $9.28MPa-m^{0.5}$ for $Al_{18}B_4O_{33}$/AC4CH added $TiO_2$. and $Al_2O_3$ but AC4CH alloy was violated the critical stipulated by ASTM standard for a valid measurement of $K_{IC}$. In case of, it was performed $I_{IC}$ test instead of $K_{IC}$ based on ASTM E 1820

  • PDF

3차원 Unit Cell 모델을 이용한 알루미늄 보레이트 휘스커 강화 Mg 복합재료의 유효 탄성계수 및 계면강도의 분석 (Analysis of Effective Elastic Modulus and Interfacial Bond Strength of Aluminum Borate Whisker Reinforced Mg Matrix Composite by Using Three Dimensional Unit Cell Model)

  • 손재형;이욱진;박용하;박용호;박익민
    • 대한금속재료학회지
    • /
    • 제48권5호
    • /
    • pp.469-475
    • /
    • 2010
  • In this study, the interfacial bond strength of a squeeze infiltrated $Al_{18}B_{4}O_{33}$/AS52 Mg composite was investigated by using a finite element method. Three types of Mg composites with volume fractions of 15, 25 and 35% were fabricated. Three-dimensional models of the composite were developed by using a unit cell model in order to determine the effective elastic modulus of the metal matrix composite and the interfacial bond strength between the whisker and magnesium matrix. After modeling, numerical results were compared with the experimental tensile test results of $Al_{18}B_{4}O_{33}$/AS52 Mg composites. The results showed that the effective modulus of the composite strongly depended on the interfacial strength between the matrix and reinforcement. Based on the numerical and experimental findings, it was found that the strong interfacial bond was achieved by the interfacial reaction product of 30 nm thick MgO, which led to an improvement in the mechanical properties of the $Al_{18}B_{4}O_{33}$/AS52 Mg composites.

석탄재를 이용한 뮬라이트 휘스커 고다공성 세라믹 제작 (Fabrication of High Porous Ceramic with Mullite Whisker from Fly Ash)

  • 신철;황광택;김응수;한규성;최정훈;김진호
    • 한국재료학회지
    • /
    • 제32권5호
    • /
    • pp.258-263
    • /
    • 2022
  • Porous ceramics have the advantages of low density, low thermal conductivity, and excellent mechanical properties. Among porous ceramic manufacturing methods, the replica template method allows the easy manufacturing of porous filters with the highest porosity and pores of the desired size, but it also has the disadvantage that the resulting filters have low mechanical strength. To overcome this shortcoming, mullite (3Al2O3·2SiO2) whiskers, which have excellent thermal stability and high mechanical strength, were introduced in porous ceramic structure. The mullite whiskers were synthesized using a composition of Al2O3, flyash and MoO3. The morphologies and crystal structures of the mullite whiskers with MoO3 contents were investigated in detail. When the porous ceramic with mullite whiskers was fabricated using 20 wt% MoO3 catalyst the most uniform microstructure was obtained, and the mullite whiskers showed the highest aspect ratio of 47.03. The porosity and compressive strength of the fabricated porous ceramic were 82.12 % and 0.83 MPa, respectively.

알루미늄 보레이트 나노휘스커를 이용한 향상된 절연성 및 기계적 특성을 가지는 고분자 복합체 제작 (Fabrication of Polymer Composite with Enhanced Insulation and Mechanical Properties using Aluminum Borate Nanowhiskers)

  • 최준혁;이상인;송기호;김태경;안창의
    • 한국분말재료학회지
    • /
    • 제30권4호
    • /
    • pp.356-362
    • /
    • 2023
  • Inorganic-organic composites find extensive application in various fields, including electronic devices and light-emitting diodes. Notably, encapsulation technologies are employed to shield electronic devices (such as printed circuit boards and batteries) from stress and moisture exposure while maintaining electrical insulation. Polymer composites can be used as encapsulation materials because of their controllable mechanical and electrical properties. In this study, we propose a polymer composite that provides good electrical insulation and enhanced mechanical properties. This is achieved by using aluminum borate nanowhiskers (ABOw), which are fabricated using a facile synthesis method. The ABOw fillers are created via a hydrothermal method using aluminum chloride and boric acid. We confirm that the synthesis occurs in various morphologies based on the molar ratio. Specifically, nanowhiskers are synthesized at a molar ratio of 1:3 and used as fillers in the composite. The fabricated ABOw/epoxy composites exhibit a 48.5% enhancement in mechanical properties, similar to those of pure epoxy, while maintaining good electrical insulation.

대전지역 민방위 비상급수용 지하수에 대한 수리화학과 질소 및 황 동위원소 연구 (Hydrochemistry and Nitrogen and Sulfur Isotopes of Emergency-use Groundwater in Daeieon City)

  • 정찬호
    • 지질공학
    • /
    • 제13권2호
    • /
    • pp.239-256
    • /
    • 2003
  • 이 연구에서는 대전지역 민방위 비상급수용 지하수의 수리화학적 특성을 밝히고 질소 및 황 동위원소를 분석하여 질산성 질소와 황산염의 기원을 해석하고자 하였다. 지하수의 수질화학적 특성은 전반적으로 약산성화 되어 있으며, 전기전도도 값은 $142~903{\;}\mu\textrm{S}/cm$의 범위로 평균 $352{\;}\mu\textrm{S}/cm$을 보인다. 지하수의 화학적 유형은 $Ca-HCO_3$ 형에서 Ca-Cl ($SO_4,NO_3$) 형까지 넓게 분포한다. 지하수의 $CO_2$ 함량과 pH에 의해 결정되는 $EpCO_2$ 값을 유기오염의 지수로 활용하였다. 지역별 지하수의 성분을 비교하고 성분별 농도분포를 알아보기 위하여 박스-휘스커(Box-Whisker) 다이아그램과 등치선도를 작성하였다. 수리화학적 자료를 종합하면 동구와 중구, 대덕구 일대 구도심권의 지하수가 약산성의 높은 전기전도도 특성과 높은 $NO_3$, $SO_4$, $EpCO_2$ 분포를 보여 서구와 유성구에 비해 오염이 많이 진행된 상태를 보인다. 지하수 22개 시료에 대한 ${\delta}^{15}N$ 분석 값은 서구와 유성구의 지하수에서 ${\delta}^{15}N$ 값이 $+7.4~+9.6{\textperthousand}$ 범위를 보여 지하수내 질산성질소 오염은 생활하수의 가능성이 높다. 그리고 동구, 중구, 대덕구 등 구도심권 지하수의 ${\delta}^{15}N$ 값은 $+10.2~+23.5{\textperthousand}$의 범위를 보여 정화조에서의 누출수가 주요 오염원일 가능성이 있다. 그리고 지하수의 ${\delta}^{34}S$ 값은 $+3~13.4{\textperthousand}$의 범위를 보인다. 일부 지하수 시료는 황산염 환원반응을 거쳐 $10{\textperthousand}$이상의 높은 ${\delta}^{34}S$ 값을 보이고, $7{\textperthousand}$ 내외의 ${\delta}^{34}S$ 값을 보이는 지하수는 황철석과 대기기원 외에도 인위적 오염에 의한 황 성분의 유입 가능성을 배제할 수 없다.