Under W/O emulsion method using a homogenizer, ${\alpha}$-alumina powder was prepared to evaluate the effects of experimental conditions on its properties, such as particle shape, extent of aggregation, average particle size and distribution. The experimental parameters were the change of type, quantity and composition of emulsifiers as well as the change of O : W volumetric ratio and agitation rate. As results, in the case of the use of single surfactant of SP80, sphere-like particles could be prepared and the average particle size was hardly affected by the agitation speed more than 16000 rpm regardless of SP80 quantity used. When the extent of aggregation among sphere-like particles prepared using $HLB_m$ = 5 of [SP80 & TW80] was compared with that prepared using SP80 at the same vol% surfactant and agitation speed, the former showed more or less low aggregation phenomena and average particle size was slightly reduced. In addition, the fraction of nano-sized particles with low aggregation was increased by the use of 0.1 vol% n-butanol, as a co-surfactant, with $HLB_m$ = 5 of [SP80 & TW80].
Kim, Myeongja;Lim, Jeongsik;Lee, Jinbok;Lee, Jeongsoon
Analytical Science and Technology
/
v.30
no.5
/
pp.240-251
/
2017
1,1,1,2-Tetrafluoroethane (HFC-134a), which is used as refrigerant in air conditioners, has been recently regulated as a greenhouse gas and is recommended for reuse by refining. It is very important to quantitatively analyze trace impurities present in the refrigerant to evaluate the criteria for reuse. In this study, trace impurities including C, H, Cl, and F, which are difficult to quantify because there are no reference materials, were quantitatively analyzed by a gas chromatograph-atomic emission detector (GC/AED); for this analysis, this was preceded by a qualitative analysis with a GC-mass selective detector (GC/MSD). In addition, the AED response was investigated using a hydrocarbon mixed reference material, which was proportional to the number of atoms in the component. Fifteen refrigerant components were detected as trace impurities in HFC-134a by qualitative analysis of trace impurities including C, H, Cl, and F in the samples. Based on the results of the qualitative analysis, quantitative analysis of trace impurities using AED showed that the highest mole fractions were for the $CHClF_2$ component ($45438.38{\mu}mol/mol$) in one sample and for the $C_2H_2ClF_3$ component ($1311.47{\mu}mol/mol$) in another sample. From this study, it has been shown that it is possible for this analytical method to be applied to the qualitative and quantitative analysis of trace compounds in refrigerants, which are difficult to quantify because of the absence of reference materials.
Some iron(III)porphyrin complexes were prepared, and identified by the spectroscopic methods. Elution behavior of iron(III)porphyrin complexes was investigated by reversed-phase HPLC. The optimum conditions for the separation of iron(III)porphyrin complexes were examined with respect to flow rate and mobile phase strength. These complexes were successfully separated on NOVA-PAK $C_{18}$ column using methanol / water(95/5) for $[T_pCF_3PP)Fe(R)]$ and methanol / water (98/2) for $[(P)Fe(C_6F_5)]$ as a mobile phase. It was found that these complexes were largely eluted in an acceptable range of capacity factor value ($0{\leq}logk'{\leq}1$). The dependence of the capacity factor (k') on the volume fraction of water in the binary mobile phase as well as the dependence of k' on the liquid-liquid extraction distribution ratio$(D_c)$ in methanol-water / n-pentadecane extraction system showed a good linearity. It means that the retention of iron(III)porphyrin complexes on NOVA-PAK $C_{18}$ column is largely due to the solvophobic effect. Also, there was a good linear dependence of the capacity factor(k') on the column temperature and enthalpy calculated by van't Hoff plot. From these results, it was confirmed that the retention mechanism of iron(III)porphyrin complexes in reversed-phase liquid chromatography was invariant under the condition of various temperature, and the solvophobic binding process exhibited isoequilibrium behavior.
Journal of Korean Society of Environmental Engineers
/
v.31
no.10
/
pp.933-940
/
2009
To evaluate characteristics in spray flame, laminar counterflow is investigated on the effects of equivalence ratio and fuel by a two-dimensional DNS (direct numerical simulation). For the gaseous phase, Eulerian mass, momentum, energy, and species conservation equations are solved. For the disperse phase, all individual droplets are calculated by the Lagrangian method without the parcel model. n-Decane ($C_{10}H_{22}$) and n-heptane ($C_7H_{16}$) is used as a liquid spray fuel, and a one-step global reaction is employed for the combustion reaction model. As equivalence ratio increases, the fuel ignites early and the high temperature region spreads wider. The peak value of temperature, however, tends to once increase and then decreases with increasing equivalence ratio. The decrease in the peak value of temperature for the higher equivalence ratio condition is caused by the cooling effect associated with droplet group combustion. Since the evaporation of n-heptane is early, the high temperature region spreads wider than ndecane, but the peak values of temperature for both n-heptane and n-decane is almost same.
Journal of the Institute of Electronics Engineers of Korea SD
/
v.37
no.8
/
pp.17-27
/
2000
This paper presents deposition and characterization of hydrogenated microcrystalline silicon (${\mu}c$ -Si:H) films on low cost glass substrate by Hot Wire CVD(HWCVD). The HWCVD ${\mu}c$ -Si:H films had deposition rates ranging from 2${\AA}$/sec to 35${\AA}$/sec with the variations of preparation conditions, which was 10 times higher than that of the films obtained from the conventional PECVD method. From the Raman spectroscopy, the prepared silicon films were found to be composed of the mixture of crystalline and amorphous phases. The crystalline volume fraction and average crystallite size, obtained from the Raman To mode peak near 520cm$^{-1}$, were 37-63% and 6-10 nm, respectively. The conductivity activation energy($E_a$) of the ${\mu}c$ -Si:H films, representing the difference of conduction band and Fermi level in an intrinsic semiconductors, increased from 0.22eV to 0.68eV with increasing pressure from 30mTorr to 300mTorr. The increase of $E_a$ with pressure indicates that the deposited films have properties close to intrinsic semiconductors, which is also proved with low dark conductivity of the ${\mu}c$ -Si:H deposited at 300mTorr. The tungsten concentration incorporated into films was about $6{\times}10^{16}atoms/cm^3$ in the samples prepared at wire temperature of 1800$^{\circ}C$.
The effect of sub-grid turbulence and combustion models on the mean flame height in a heptane pool fire according to the Fire Dynamics Simulator (FDS) version (5 and 6) based on Large Eddy Simulation (LES) was examined. The heat release rate for the fire simulation was provided through experiments performed under identical conditions and the predictive performance of the mean flame height according to FDS version was evaluated by a comparison with the existing correlation. As a result, the Smagorinsky and Deardorff turbulence models applied to FDS 5 and 6, respectively, had no significant effects on the mean flow field, flame shape and flame height. On the other hand, the difference in pool fire characteristics including the mean flame height was due mainly to the difference in the mixture fraction and Eddy Dissipation Concept (EDC) combustion models applied to FDS 5 and 6, respectively. Finally, compared to FDS 6, FDS 5 provided the predictive result of a significantly longer flame height and more consistent mean flame height than the existing correlation.
In this work, $Fe_3O_4$ (magnetite), conductive filler was prepared from $FeCl_2{\cdot}4H_2O,\;(CH_2)_6N_4$ (hexamethylene tetramine), and $NaNO_2$, followed by mixing with crystallizable chloroprene rubber(CR). The influence of conductive filler content on the properties of the conductive composite was studied and temperature dependence of the electrical conductivity (${\sigma}$) was also investigated. It is found that the percolation threshold concept holds true for the conductive particle-filled composite where ${\sigma}$ indicates a nearly sharp increase when the fraction of magnetite in the mixture exceeds 27%. The temperature dependence of ${\sigma}$ is thermally activated blelow or at the $P_c$. Magnetite acts as reinforcement and conductive filler for CR rubber. Moreover, it is shown that the composite with magnetite of 50 phr gives the most significant mechanical properties for tensile strength and elongation at break, which is due to the formation of optimum physical interlock and crosslinking. The results of 100%, 200%, and 300% moduli suggest that the moduli are related with reinforcement effect of magnetite and viscosity of the blend.
Kim, Hey-Suk;Shin, Mi-Soo;Jang, Dong-Soon;Lee, Dae-Geun
Journal of Korean Society of Environmental Engineers
/
v.29
no.1
/
pp.23-30
/
2007
The ultimate objective of this study is to develop oxygen-enriched combustion techniques applicable to the system of practical industrial boiler. To this end the combustion characteristics of lab-scale LNG combustor were investigated as a first step using the method of numerical simulation by analyzing the flame characteristics and pollutant emission behaviour as a function of oxygen enrichment level. Several useful conclusions could be drawn based on this study. First of all, the increase of oxygen enrichment level instead of air caused long and thin flame called laminar flame feature. This was in good agreement with experimental results appeared in open literature and explained by the effect of the decrease of turbulent mixing due to the decrease of absolute amount of oxidizer flow rate by the absence of the nitrogen species. Further, as expected, oxygen enrichment increased the flame temperatures to a significant level together with concentrations of $CO_2$ and $H_2O$ species because of the elimination of the heat sink and dilution effects by the presence of $N_2$ inert gas. However, the increased flame temperature with $O_2$ enriched air showed the high possibility of the generation of thermal $NO_x$ if nitrogen species were present. In order to remedy the problem caused by the oxygen-enriched combustion, the appropriate amount of recirculation $CO_2$ gas was desirable to enhance the turbulent mixing and thereby flame stability and further optimum determination of operational conditions were necessary. For example, the adjustment of burner with swirl angle of $30\sim45^{\circ}$ increased the combustion efficiency of LNG fuel and simultaneously dropped the $NO_x$ formation.
Two crystal structures of bromine sorption complexes of vacuum dehydrated Cd(ll)-exchanged zeolite A have been determined by single-crystal xray diffraction techniques in the cubic space group Pm3m at 21(1) ℃. Both crystals were ion exchanged in flowing streams of exchange solution In which mole ratio of Cd(NO3)2 and Cd(OOCCH3)B was 1:1 with a total concentration of 0.05 M. First crystal was dehydrated at 450℃ and 2 ×10-6 Torr for two days. Second crystal was dehydrated at 650℃ and 2 ×10-6 Torr for two days. Both crystals were then treated with 160 Torr for two days. Second crystal was dehydrated at 650℃ and 2 × 10-6 Torr for two days. Both crystals were then treated with 160 Torr of zeolitically dried bromine vapor at 24℃. Full-matrix least-squares refinements of toe first crystal(a: 12.250(1) A )· and the second crystal(a: 12.204(2) A ) have contecoed to final error indices, Rl:0.075 and Ra:0.079 with 212 reflections, and Rl : 0.089 and Ra = 0.078 with 128 reflections, respectively, for which I >3σ(I). Crystallographic analyses of both crystals show that six Cd2+ ions are located on two different threefold axes of unit cell associated with 6-ring oxygens. Each 4.5 Cd2+ ion is recessed ca.0. 441 A Into the large cavity to complex either with Brsor with Br3from the (111) plane of 0(3), whereas each 1.5 Cd2+ ions recessed ca. 0.678 A into we sodalite unit. Approximately 1.5 Br5-and 1.5 Br3-ions are sorbed per unit cell. Each Brsion interacts and stabilized by complexing with two Cd2+ ions and framework oxide ions, while each Br3ion interacts with one Cd2+ ion and framework oxide ions. Because of residual water molecules the following reactions may be occurred inside of zeolite cavity:
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.