Kim, Byeong-Cheol;Gang, Gi-Won;Yeo, Jeong-Su;Song, Jin-Tae
Korean Journal of Materials Research
/
v.7
no.4
/
pp.287-294
/
1997
(NdㆍDy)-(FeㆍCoㆍAIㆍM)-B 합금에 Sn,Mo등을 첨가하여 그에 따른 미세구조와 열적안정성 및 자기적 특성 변화를 조사하였다. Sn과 Mo의 첨가는 (NdㆍDy)-(FeㆍCoㆍAIㆍM)-B 합금리본의 큐리온도를 크게 향상시켰으며 자기특성, 특히 보자력을 1KOe이상 증가시켰다. 그리고 이러한 현저한 보자력 증가는 입계형 defect인 disturbed grain boundary defect에 기인하는 것이라 판단되었다. 또한 Sn과 Mo 첨가원소는 irreversible loss를 각각 4%와 6% 감소시켜 리본자석의 열적안정성을 향상시켰다. 이는 Sn과 Mo의 첨가가 보자력을 크게 증가시켰기 때문이다. 한편 (NdㆍDy)-(FeㆍCoㆍAIㆍM)-B 리본자석들의 열저항온도(heat resistance temperature)는 irreversible loss와 직선관계를 이루었다.
Choi, Y.J.;Jang, S.J.;Kim, S.W.;Jeon, B.S.;Kim, S.M.;Song, C.B.;Kim, Y.C.;Namkung, J.
Journal of the Korean Magnetics Society
/
v.25
no.1
/
pp.4-9
/
2015
This study was carried out to investigate a influence of humidity variation (%) on the magnetic properties and the surface flaws in the fabrication of Fe-based $Fe_{78}Si_9B_{13}$ amorphous alloy ribbon by Planar Flow Casting process. As a result, the size of the air pocket and the droplet which is observed in the contact surface and the free face of the amorphous alloy ribbon becomes large when the humidity increases and the size highly increases with the surface roughness at the same time. Especially, the surface roughness value which is made in the 65 % of the humidity is the lowest in the contact surface ($Ra=0.60{\mu}m$, $Rz=3.11{\mu}m$) and the free face ($Ra=0.47{\mu}m$, $Rz=3.00{\mu}m$). Also, in case of the soft magnetic property of the magnetic core which is made with the toroidal core of $23(OD)^*20(ID)^*20(H)$ size, in the sample of the amorphous alloy ribbon which is made in 65% of the humidity, the most excellent value is gained as $B_s(B_{700})=1.055T$, $H_c=0.083Oe$, permeability = 1,197 and core loss = 0.276W/kg.
The thermal and magnetic properties of amorphous (FeCo)SiBNb ribbon alloys with high glass forming ability have been investigated. The glass forming ability was enhanced by Co substitution in amorphous ($Fe_{1-X}Co_X)_{72}Si_4B_{20}Nb_4$ alloys with the thickness of about $40{\mu}m$. With the increase in Co content, the temperature range of supercooled liquid phase increased indicating the high glass forming ability of the Co-added alloys. Further the ac permeability increased, and the core loss decreased considerably by Co substitution, while small change in $B_8$ (magnetic flux density at 800 A/m) was observed. The frequency characteristics of permeability deteriorated as compared to conventional amorphous ribbon alloys with the thickness of about $20\;{\mu}m$ due to the increased skin effect.
Amorphous FeBSiNb alloy ribbons having bulk glass forming ability and high saturation magnetic flux density were produced by single-roller melt spinning apparatus in the thickness range of 22∼102㎛. With the increase of thickness, the coercive force and squareness ratio decreased, while maximum permeability and AC permeability increased. However electrical resistivity was almost constant. Furthermore refined and complex magnetic domain structure was observed in thicker ribbons owing to the change in internal magnetic anisotropy. For the alloy with the thickness of 81㎛, small coercive force of 24 mOe and high effective permeability of 12,000 at 1㎑ were obtained, those are considered to be better comparing to the conventional soft magnetic amorphous alloys (∼20 ㎛). The good soft magnetic properties of the thick FeBSiNb amorphous alloys were attributed to the decrease in surface pinning effect during wall motion, appearance of perpendicular anisotropy and resulted domain refinement.
$Nd_{14}Fe_{80}B_6$ ribbon alloy was manufactured with using melt-spinning method and analyzed the magnetic properties according to the manufacturing conditions. The microstructure and magnetic properties of melt-spun ribbons are sensitively dependent on the quench rate and annealing conditions. As-quenched $Nd_{14}Fe_{80}B_6$ ribbons with optimum magnetic properties are obtained at wheel speed($v_s$) of about 20m/sec and over quenched ribbons show optimum magnetic properties at $v_s$=22m/see when annealed for 30 minutes at $600^{\circ}C$ under vacuum. The crystallization temperature($T_k$) of $Nd_2Fe_{14}B$ phase is about $595^{\circ}C$ in the DTA analysis.
높은 포화자속밀도와 낮은 철손을 갖는 Fe/aub 80/B$_{12}$Si$_{8}$ 비정질합금을 일반열처리, 자장열처리시켜 그의 자기적특성과 자구구조와의 관계를 조사하였다. 이를 위하여 Fe$_{80}$B$_{12}$Si$_{8}$ 비정질리본을 단롤법으로 제작하여 결정화온도를 측정하였으며 측정된 결정화온도 이하의 여러 온도에서 30분간 Ar-gas 분위기하에서 일반열처리, 자장열처리를 행하였다. 이와같이 하여 준비된 시료의 자기적특성을 조사하기 위하여 D.C., A.C. Recorking Fluxmeter를 이용하였으며 자구구조는 Bitter method로 관찰하였다. as-cast 상태의 시료를 일반열처리함에 따라 내부응력이 완화되면서 maze자구가 점차 사라지고 wave형태의 180.deg.자구가 관찰되었다. 동시에 자화과정에 있어서 자기이력곡선은 Barkhausen jump가 없어 smooth하였다. 그리고 자장열처리시에는 as-cast 상태나 일반열처리에 비해 자기적특성이 현저하게 향상되었으며 이는 열처리를 행함에 따라 내부응력이 완화되면서 maze 자구가 없어지고 일축자기 이방성으로 리본길이방향에 평행하게 형성된 180.deg.자구에 기인하는 것이라 사료된다. 그리고 자장열처리의 경우, 폭방향으로 열처리한 리본의 자구폭은 길이방향으로 열처리한 리본의 폭보다 미세하였으며 전자의 이력손실이 후자의 것보다 더 컸다.다.
Change in phases, microstructures, and magnetic properties by the variation of quench rate and heat treatment were investigated for melt-spun $Fe_{77}Pr_{15}C_8$ ribbons. The amorphization of as-spun ribbons increased as the quench rate increased. As a result, the ribbon quenched at 40 m/s was almost entirely amorphous. Similarly to cast alloys, the primary phase in crystalline ribbons quenched at 10 m/s was $\alpha$-Fe followed by the secondary $Fe_{17}Pr_2C_x$. Crystalline phases were still dominant in the ribbon spun at 20 m/s, but in this case crystallization of $Fe_{17}Pr_2C_x$ was remarkable with a little suppression of $\alpha$-Fe. At 30 m/s an amorphous phase obviously dominated in the as-spun ribbons with small fraction of crystals. Therefore, substantial amount of hard magnetic $Fe_{14}Pr_2C$ was not obtained from the as-spun state but, as in cast alloys, produced only by a solid-state transformation. Within a few minutes fine grains of $Fe_{14}Pr_2C$ were easily obtained at relatively low temperature when the degree of amorphization of as-spun ribbons was higher. The grain size of $Fe_{14}Pr_2C$ was well less than 1${\mu}{\textrm}{m}$. The ribbons quenched at 20 or 30 m/s yielded higher coercivities after heat treatment.
In order to investigate the origin of the asymmetric magnetization reversal effect, we studied the variation of magnetic hysteresis loops with the alloy composition in amorphous ferromagnetic alloy ribbons of ${(Fe_{1-x}Co_{x})}_{75}Si_{10}B_{15}$ system annealed at $380^{\circ}C$ for 16 hours in a zero field condition. The asymmetric magnetization reversal effect developed more strongly in amorphous ribbons having two metallic components than in ribbons having a single metallic component. The effect developed more strongly in ribbons showing a smaller value of the saturation mag¬netostriction. The development of the asymmetric magnetization reversal effect was affected by the ratio of two metallic components as well as the magnitude of the saturation magnetostriction.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.