Study on the material properties and heating efficiency according to the internal surface coating of the brazed plate heat exchanger (BPHE) (접합 판형 열교환기(BPHE)의 내부 코팅에 따른 소재 특성 및 성능 평가에 관한 연구)

  • Jung, Hangchul;Yang, Hyunseok;Kim, Hyunjong;Park, Jongpo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.30 no.6
    • /
    • pp.237-243
    • /
    • 2020
  • In this study, a silane-based coating was applied to improve corrosion resistance and thermal efficiency performance of a brazed plate heat exchanger (BPHE) composed of stainless plate and copper (Cu) brazing. Although the selected coating material was applied to the BPHE by evaluating the corrosion and contact angle according to the coating material, the result of the heat transfer performance evaluation showed that the thermal efficiency was lower than that of the uncoated BPHE. It was analyzed that the adhesion of the coating agent to the flow path inside the BPHE and the residual coating agent on the surface acted as heat resistance, preventing heat transfer. This is due to the structural characteristics of the BPHE in which a fine flow path exists inside, and it is believed that manufacturing after coating the surface of the flow path in advance in the manufacturing process of the BPHE can improve heat transfer performance.

니켈-흑연 복합분말의 니켈코팅층에 미치는 코팅 촉매제의 영향

  • Kim, Dong-Jin;Jeong, Heon-Saeng;Yun, Gi-Byeong
    • Korean Journal of Materials Research
    • /
    • v.3 no.5
    • /
    • pp.521-528
    • /
    • 1993
  • Ni-graphi~e composite powders were prepared by reduct ion of $Ni^{++}$ from arnmoniacal nickel sulfate solution on graphite core by hydrogen gas at elevated temperature and pressure. Effect of coating catalyst. Anthraquinone $(C_6H_4COC_6H_4 CO)$, on the reduction rate and the properties of nickel layer were investigated by SEM, X-ray, size and chemical analysis. 1nduct.ion period, a time lag between the ~njection of hydrogen gas and the start of the reduction, was 22 to 70 mins and was affected by the size and amount of Anthraquinone. Kickel layer deposited on the surface of graphite core material was composed of nickel nodules whose sizes were different with vari~ ous reduction conditions. Minimum diameter of nickel nodules was about 2-3$\mu \textrm m$.

  • PDF

The Evaluation of n-Octyl Ethoxy Silane as a Water Repellent of Concrete (콘크리트에서의 n-octyl ethoxy silane 발수제의 성능평가)

  • 황인동;이완조;염희남;정윤중
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.12
    • /
    • pp.1172-1177
    • /
    • 2000
  • 최근 콘크리트 보호 재료는 코팅을 이용하는 과거의 방법에서 함침을 이용하는 기법으로 전환하였다. 이중 발수제는 콘크리트의 표면의 특성을 변화시키는 것으로 친수성의 콘크리트를 소수성 물질을 결합시켜 물에 의한 젖음을 방어하는 것으로 콘크리트에 사용하였을 경우 콘크리트의 고유한 표면 장력을 작게 변화시키고 장력이 큰 물질 중의 하나인 물의 흡수를 방어하게 한다. 본 실험은 발수제의 성능 평가를 위하여 다공질의 재료인 콘크리트의 접촉각을 측정하여 그 변화를 관찰하였으며, 발수제들의 우수한 기능 중의 하나인 통기성을 시편의 중량 감소로 측정하였다. 발수제로 n-octyl ethoxy silane을 사용한 콘크리트 시편의 흡수 능력은 사용하지 않은 것의 약 10% 정도로 측정되었으며 시편의 수분 중량 감소는 7일 동안 90~130%로 관찰되어 통기성이 유지되어 콘크리트의 강도 유지에 효과적임을 알 수 있었다. 또한 겉보기 접촉각은 처리하지 않은 시편에서 24~33$^{\circ}$로 측정되었으나 처리된 시편의 최초면에서 130~141$^{\circ}$이었으며 2mm의 연마면에서는 127~132$^{\circ}$로 측정되어 콘크리트 표면 장력 변화가 유지되고 있음을 알 수 있었다.

  • PDF

Convergence Study on the Development and Material Property of Wax for Surface Conservation of Iron Alloy Outdoor Sculpture (야외 철제 조각 작품 표면 보존용 왁스의 개발 및 재료 특성에 관한 융합 연구)

  • Oh, Seung-Jun;Wi, Koang-Chul
    • Journal of the Korea Convergence Society
    • /
    • v.9 no.4
    • /
    • pp.151-160
    • /
    • 2018
  • Waxes currently used as a coating material to preserve surfaces of outdoor iron sculptures tend to face lower coating strength and efflorescence due to the aging from air pollution and acid rains. Consequently, they are subjected to repeated corrosions shortly after the treatment. And the sculptures face the problem losing their original nature because of the changes of colors and lusters, so this convergence study aims at developing wax with better performance than the existing materials. For this reason, the study identified the effects of physical property using the environmental experiments such as the tests of salt spray and gas corrosion as well as the analysis of luster level and thermo-gravimetry. As this study result, the developed ISC wax showed the excellent blocking effect from salt water and coating durability more than five times compared with the existing waxes, better acid resistance by two-four times, sun block effect by 2-10 times, improved luster variance by 3-16 times, improved thermo-stability and durability by 0.5-5 times, and therefore demonstrating far better coating effect than the existing waxes. In the light of these findings, this study contributes for this new development which can replace the existing waxes used so far in order to preserve the outdoor iron sculptures.

Evaluation of Hydrophobic Performance and Durability of Concrete Coated with Cellulose Nanofiber Mixed Antifouling Coating Agent (셀룰로오스 나노섬유 혼합 방오코팅제가 도포된 콘크리트의 소수성능과 내구성능 평가)

  • Nak Sup Jang;Chi Hoon Nho;Hongseob Oh
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.27 no.5
    • /
    • pp.1-8
    • /
    • 2023
  • Marine and hydraulic structures are subject to durability damage not only due to the penetration of sea water but also due to the attachment of marine organisms. Therefore, in this study, we tried to develop an antifouling coating agent with self-cleaning function for marine concrete. It was confirmed that the antifouling coating agent mixed with AKD, cellulose nanofibers and BADGE had sufficient antifouling performance at a well hydrophobicity of around 140° in contact angle and an inclination angle of 15°. In the abrasion resistance test of the surface, only a maximum loss of 0.015 g occurred. In the durability test, as a result of the chloride ion permeation test, almost no chloride ion permeation occurred in the variable where the coating agent was applied, and carbonation and freeze-thaw damage also rarely occurred, so it was analyzed that it was effective in securing durability of concrete.

An Analysis of Hydrophobic Characteristics of Concrete Surfaces by Antifouling Coating Agent using Cellulose Nonofiber and Alkyl Ketene Dimer (셀룰로오스 나노 섬유와 AKD를 활용한 방오 코팅제에 의한 콘크리트 표면의 소수 특성 분석)

  • Nag-Seop Jang;Chi-Hoon Noh;Hongseob Oh
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.11 no.2
    • /
    • pp.120-129
    • /
    • 2023
  • Marine structures are subject to damage not only from sea salt but also from the adhesion of marine microorganisms and suspended particles, which cause additional damages. In order to prevent this, periodic coating is employed in the case of vessels to maintain the necessary performance. However, it is true that periodic coating is difficult for concrete or steel support structures, and there is a risk of marine environmental pollution. In this study, authors developed an anti-fouling coating agent using eco-friendly materials that possess hydrophilic cellulose nanofibers and AKD(alkyl ketene dimer). To achieve a homogeneous mixture, the content of cellulose nanofibers was fixed at 1 %, and AKD, distilled water, and waste glass were mixed using a digital mixer and homogenizer. The contact angle of the prepared coated surface was observed to be over 130°, indicating sufficient performance even in a water droplet flow test with a 15° slope, suggesting self-cleaning capability. Furthermore, through the analysis of viscosity characteristics at different temperatures, it was confirmed that the application is feasible at room temperature. Microstructure analysis also verified that the coating agent is uniformly applied to the concrete surface.

Surface Mmodification of Poly(DL-lactide-co-glycolide) Nanoparticle (Poly(DL-lactide-co-glycolide) 나노입자의 표면 수식)

  • Oh, Yu-Mi;Jung, Taek-Kyu;Chi, Sang-Cheol;Shin, Byung-Cheol
    • Journal of the Korean Chemical Society
    • /
    • v.47 no.6
    • /
    • pp.601-607
    • /
    • 2003
  • We studied on preparation of nanoparticles modified surface using biodegradable polymer, poly(DL-lactide-co-glycolide) (PLGA). Two kinds of PLGA nanoparticles were prepared by a spontaneous emulsification solvent diffusion (SESD) method using cetyltrimethylammonium chloride (CTAC) and tetradecyltrimethylammonium bromide (TTAB) as a cationic surfactant and polyethylene glycol-block-polypropylene glycol copolymer (Lutrol F68) as a nonionic surfactant. Model protein was coated on the surface of nanoparticles by the ionic complexation. The model protein was that influenza vaccine ($H_3N_2,\;H_1N_1$, B strain) labeled with NHS-fluorescein. The sizes of cationic nanoparticles were 140-160 nm and the surface charges were 50-60 mV. The sizes of nonionic nanoprticles were 80-90 nm and the surface charge was -10 mV. After coating vaccine on the surface of nanoparticles, the sizes of cationic nanoparticles were increased to 380-400 nm and the size of nonionic nanoparticles was not increased. The amount of coated vaccine on the cationic nanoparticles was 22.73 ${\mu}g$/mg.

고밀도 알루미늄 박막 코팅과 특성 분석

  • Yang, Ji-Hun;Jeong, Jae-In;Jang, Seung-Hyeon;Park, Hye-Seon
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2011.02a
    • /
    • pp.45-45
    • /
    • 2011
  • 알루미늄과 그 합금은 내부식성(corrosion resistance)이 좋고, 밀도가 낮아 높은 연료소비 효율을 필요로 하는 항공기와 자동차 같은 운송수단의 내-외장 소재로 사용되고 있다. 또한 알루미늄의 높은 내부식성을 이용하여 철강소재의 부식을 방지하는 보호막으로도 폭 넓게 사용된다. 물리기상증착(physical vapor deposition)으로 알루미늄을 코팅하면 박막 성장 초기단계에서 핵(nucleus)을 형성하고, 형성된 핵을 중심으로 주상 구조(columnar structure)로 박막이 성장하는 것이 일반적으로 알려진 방식이다. 주상 구조의 알루미늄 박막은 주상정과 주상정 사이에 필연적으로 공극(pore)이 존재하게 되어 부식을 일으키는 물질이 박막으로 침투하게 되고, 부식 물질과 모재가 반응하여 공식(pitting corrosion)이 발생한다. 본 연구에서는 스퍼터링(magnetron sputtering)을 이용하여 치밀한 조직을 갖는 알루미늄 박막을 코팅할 수 있는 공정을 개발하고, 치밀한 알루미늄 조직이 내부식성에 어떠한 영향을 미치는지 평가하였다. 기판은 냉연강판(cold rolled steel sheet)이 사용되었으며, 알루미늄 타겟의 순도는 99.999%, 크기는 직경 4"이었다. 냉연강판은 진공용기(vacuum chamber)에 장착하기 전에 계면활성제를 이용하여 표면에 존재하는 기름성분을 제거하였으며, 진공용기에 장착한 후에는 아르곤 가스를 이용하여 발생시킨 글로우 방전으로 표면에 존재하는 산화물을 제거하였다. 알루미늄 박막의 조직에 영향을 미치는 공정변수를 확인하기 위해서 스퍼터링 파워, 공정 온도, 공정 압력, 외부 자기장 세기 등의 공정 조건을 변화시켜 코팅을 실시하였다. 실험을 통해서 얻어진 최적 조건으로 알루미늄을 코팅할 경우, 알루미늄 bulk의 밀도와 비교하여 약 94.7%의 밀도를 갖는 알루미늄 박막을 코팅할 수 있었다. 알루미늄 박막이 약 3 ${\mu}$m의 두께로 코팅된 냉연강판의 내부식성 평가(salt spray test, 5% NaCl) 결과, 평가를 시작한 후 72시간 후에도 적청이 발생하지 않았다.

  • PDF

Optimization of Process Variables for Insulation Coating of Conductive Particles by Response Surface Methodology (반응표면분석법을 이용한 전도성물질의 절연코팅 프로세스의 최적화)

  • Sim, Chol-Ho
    • Korean Chemical Engineering Research
    • /
    • v.54 no.1
    • /
    • pp.44-51
    • /
    • 2016
  • The powder core, conventionally fabricated from iron particles coated with insulator, showed large eddy current loss under high frequency, because of small specific resistance. To overcome the eddy current loss, the increase in the specific resistance of powder cores was needed. In this study, copper oxide coating onto electrically conductive iron particles was performed using a planetary ball mill to increase the specific resistance. Coating factors were optimized by the Response surface methodology. The independent variables were the CuO mass fraction, mill revolution number, coating time, ball size, ball mass and sample mass. The response variable was the specific resistance. The optimization of six factors by the fractional factorial design indicated that CuO mass fraction, mill revolution number, and coating time were the key factors. The levels of these three factors were selected by the three-factors full factorial design and steepest ascent method. The steepest ascent method was used to approach the optimum range for maximum specific resistance. The Box-Behnken design was finally used to analyze the response surfaces of the screened factors for further optimization. The results of the Box-Behnken design showed that the CuO mass fraction and mill revolution number were the main factors affecting the efficiency of coating process. As the CuO mass fraction increased, the specific resistance increased. In contrast, the specific resistance increased with decreasing mill revolution number. The process optimization results revealed a high agreement between the experimental and the predicted data ($Adj-R^2=0.944$). The optimized CuO mass fraction, mill revolution number, and coating time were 0.4, 200 rpm, and 15 min, respectively. The measured value of the specific resistance of the coated pellet under the optimized conditions of the maximum specific resistance was $530k{\Omega}{\cdot}cm$.

An Assessment Study on Stability of Various Coating Treatment of Metallic Artifacts Using V-Flon (불소 수지(V-Flon)를 이용한 금속유물의 코팅 형성에 대한 안전성 평가 연구)

  • Lee, Jung-Min;Wi, Koang-Chul
    • Journal of Conservation Science
    • /
    • v.26 no.2
    • /
    • pp.149-156
    • /
    • 2010
  • One of resins, V-Flon is useful as a coating material because YK-D80, which is a solvent for V-Flon, is not highly volatile. However, it can not completely harden and can flow out when metal artifacts are joined and restored in the process of the treatment. Therefore, after the impregnation process in order to accelerate the hardening speed of a coating material, usually a dry oven was adopted. This study focused on finding the problems on the dry oven which is employed to increase the speed and investigating the most effective solvent and its composition by checking any change occurred depending on the concentration of solvents. Six different types of solvents were selected and samples were prepared in a manner that they were impregnated with solvents in three concentrations respectively (10%, 20%, 30%). To determine the condition of the samples, the stability evaluation was performed by measuring the change of color and the gloss, the thickness of coated layers, the corrosion after coating, the water resistance by contact angles. Through the comparative experiments between the natural drying and the artificial drying using a dry oven, it was found that when the dry oven is used, some problems are identified on the point of forming a uniform and stable layer because of the unstable data collected from the forced artificial dry. The experiments performed using 3 different concentration rates (10%, 20%, 30%) presented that in the case of 10% V-Flon in Xylene (using as a solvent), its layer was thin as well as it showed the high water-barrier property, which allows it to form the stably coated layer with the lower gloss and color change.