• Title/Summary/Keyword: 폴리머 모르터

Search Result 40, Processing Time 0.022 seconds

A Study on Bond Properties of Plymer Cement Mortar (폴리머시멘트모르터의 부착특성에 관한 연구)

  • Park, Kyung-Sang;Lee, Woong-Jong;Chae, Jae-Hong;Lee, Jong-Ryul;Choi, Long
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1999.04a
    • /
    • pp.203-208
    • /
    • 1999
  • The purpose of this study is to examine the bond properties of polymer cement mortar. Generally, cement mortar using polymer has been used that recovering the deteriorative concrete structure performance. In this case, it is very important problem to become a monolithic construction by bonding property. In this study, it is evaluated with other properties that adhesion strength between polymer cement mortar and concrete substrate. And polymer cement mortar was compared with plain cement mortar by scanning electron microscope.

  • PDF

Drying Shrinkage Reduction of Redispersible Polymer Powder-Modified Mortars Using Powdered Shrinkage-Reducing Agent (분말수축저감제를 이용한 제유화형 분말수지 혼입 폴리머 시멘트 모르터의 건조수축 저감효과)

  • ;Ohama, Yoshihiko
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.04a
    • /
    • pp.231-236
    • /
    • 1998
  • In general, the drying shrinkage of polymer-modified mortars using redispersible polymer powders is much higher than that of unmodified mortar. The purpose of this study is to reduce the drying shringkage of polymer-modified mortars using a redispersible poly(ethylene-vinyl acetate) (EVA) powder, which is widely used for the manufacture of prepackaged-type polymer-modified mortar products at present. Polymer-modified mortars using the redispersible EVA powder with powdered shrinkage-reducing agent were prepared with various polymer-cement ratios and shrinkage-reducing agent contents, and tested for drying shrinkage and strength. From the test results, the drying shrinkage of the redispersible EVA powder-modified mortars with a powdered shrinkage agent is remarkably reduced with increasing shrinkage-reducing agent content, and becomes approximately a half of that of the redispersible EVA powder-modified mortars with the same polymer-cement ratios and without the shrinkage-reducing agent at a shrinkage-reducing agent content of 6%.

  • PDF

A Studyon the Properties of Polymer-Modified Mortar Using Asphalt Emulsion (아스팔트 에멀젼을 혼입한 폴리머 시멘트 모르터의 특성에 관한 연구)

  • Jean, Woo-Sung;Song, Hun;Jo, Young-Kug;Soh, Yang-Seob
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1997.10a
    • /
    • pp.375-380
    • /
    • 1997
  • The purpose of this study is to examine the properties of polymer-modified mortars using asphalt emulsion. The polymer-modified mortars using asphalt emulsion with various asphalt-cement ratios are prepared, and tested for flexural and compressive strengths, water absorption and permeability, carbonation, Cl ion penetration and chemical resistance. From the test results, the flexural and compressive strengths, water absorption and permeability, carbonation and Cl ion penetration depths of polymer-modified mortars using asphalt emulsion tend to be decreased with increasing asphalt-cement ratio, and chemical resistance is improved. It is evident that polymer-modified mortars using asphalt emulsion having an excellent properties as a waterproof and finish materials can be produced.

  • PDF

Flexural Behavior of Slab Repaired and Rehabilitated with Strand and Polymer Mortar (강연선과 폴리머 모르터에 의해 보수ㆍ보강된 슬래브의 휨거동 특성)

  • 황정호;양동석;박선규;엄준식
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.05a
    • /
    • pp.1007-1012
    • /
    • 2003
  • With deterioration of the nation's infrastructure comes the growing, need for effective means of rehabilitating structures. Possibly one for the most challenging tasks is to upgrade the overall capacity of concrete structure. This study focused on the flexural behavior of reinforced concrete slabs strengthened by PS strand and polymer mortar in the tension zone. The properties of slabs are 70×12㎝ rectangular and over a 220㎝ span. Test parameters in this experimental study were placing thickness, chipping, the number of strand, the kind of mortar. Attention is concentrated upon overall bending capacity, deflection, ductility index, failure mode and crack development of repaired and rehabilitated slabs.

  • PDF

Strength Properties of Prepacked Polymer Mortar Using MMA-Based Binders (MMA를 이용한 프리팩트 폴리머 모르터의 강도특성)

  • Yeon, Kyu-Seok;Lee, Hyun-Jong;Ryu, Neung-Hwan;Jin, Xing-Qi;Lee, Chi-Won
    • Proceedings of the Korean Society of Agricultural Engineers Conference
    • /
    • 2005.10a
    • /
    • pp.117-122
    • /
    • 2005
  • Prepacked polymer mortar that is mainly composed of MMA monomer and used for the patching and restoring materials of concrete structures was developed, and its hardening and strength properties were experimentally surveyed. Results of study show that the permeance of binder into the aggregate was excellent for the case of PMMA mixing ratio of below 10%, the surface hardening inferiority was not generated for the case of the ratio of over 5%. Working time of the prepacked polymer mortar and hardening shrinkage tended to decrease as the PMMA mixing ratio increased. On the other hand, the ratio turned out not to decisively affect on compressive and flexural strengths. Regardless of PMMA mixing content, the adhesive strength was about 2.5 MPa. Occurring the desquamation on the substrate of cement concrete showed the adhesive strength of MMA prepact polymer mortar was excellent.

  • PDF

A study on utilizatio of metal-mine tailings for polymer cement mortars (폴리머 시멘트 모르터용 골재로서 금속광산 폐광미의 활용연구)

  • 민경원
    • Economic and Environmental Geology
    • /
    • v.32 no.1
    • /
    • pp.13-18
    • /
    • 1999
  • The tailings stocked at two tailing piles in Sangdong aea have raised collapse hazards and various environmental problems. A trial for effective utilization of tailings as fine aggregates for polymer concrete has been performed along with mineralogical and physical characterization of tailings. The tailings from the Sangdong mine, mainly composed of quartz, orthoclase, amphiboles and muscovite, are alkaline and tailings at the new tailing pile are generally finer in grain size than those at the old tailing pile. In case of using New Tailings as fine aggregates, cement mortar with equivalent amounts of tailings and sands shows the highest compressive strength. Cement mortars containing tailings show lower values of compressive strength, splitting tensile strength and flexural strength than those not-containing tailings. Mixture of polymers such as SBR and EVA in cement mortars raises strengths of cement mortars effectively, which shows potential possiblity to utilize the tailings in Sangdong area as fine aggregates for polymer concretes.

  • PDF

Properties of Cement Mortar Using Polymer Coated Powdered Rubber (폴리머 코팅 폐타이어 분말을 혼입한 시멘트 모르터의 특성)

  • Song, Hun;Jo, Young-Kug;Park, Hong-Shin;Soh, Yang-Seob
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1996.10a
    • /
    • pp.51-57
    • /
    • 1996
  • The purpose of this study is to improve the properties by increasing of the adhesion strength of styrene-butadiene rubber(SBR) latex coated powdered rubber in cement mortar. SBR-modified mortar using powdered rubber is also tested as the same method. From the test results, the cement mortar using SBR latex coated powdered rubber have a good mechanical properties compared with that using uncoated powdered rubber. The mechanical properties of SBR-modified mortar using powdered rubber with polymer-cement ratios of 10% are also improved.

  • PDF

The Effect of Curing condition on Adhesion in Tension of Polymer-Modified Mortars (양생존건이 폴리머 시멘트 모르터의 접착강도에 미치는 영향)

  • 전우성;조영국;소양섭
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1997.04a
    • /
    • pp.349-356
    • /
    • 1997
  • The purpose of this study is to evaluate the effect of curing conditions on adhesion in tension of polymer-modified mortar to cement mortar substrate in comparision with ordinary cement mortar. The polymer-modifies mortars using two polymer dispersions and a redispersible polymer power are prepared with various polymer-cement ratios, and tested for the adhesion in tension of the specimens subjected to five curing conditions. From the test results, the adhesion in tension of polymer-modified mortars tends to increase with increasing polymer-cement ratio irrespective of the polymer types and curing conditions. It is apparent that adhesion in tension of polymer-modified mortars is considerably influenced by curing conditions.

  • PDF

The Early Strength Prediction of Epoxy Mortars by the Maturity Method (적산온도법에 의한 에폭시 모르터의 초기강도 예측)

  • 연규석
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.42 no.2
    • /
    • pp.99-107
    • /
    • 2000
  • The objective of this study are to compare the development of compressive strength of epoxy mortars used as repairing materials with respect to maturity , and to propose a model predicting strength development of epoxy mortars. A series of tests are carried out for the hardener contents of 30, 40 and 50 percentage of epoxy resin and compressive strengths are measured at the age of 6, 12, 24, 72, 120 and 168 hours respectively under the cure temperature of 0, 10, 20 and 3$0^{\circ}C$. The datum temperature is estimated by measured strengths, and the maturity is calculated with the estimated datum temperature. The compressive strength of epoxy mortars can be predicted by regression analysis from the maturity-compressive strength relationship.

  • PDF

Performance Evaluation of Repair Methods for RC structures by Accelerating Test in Combined Deterioration Chamber and Long-Term Field Exposure Test (복합열화촉진실험 및 장기현장폭로실험에 의한 RC구조물 보수공법의 보수성능평가)

  • Kwon Young-Jin;Kim Jae-Hwan;Han Byung-Chan;Jang Seung-Yup
    • Journal of the Korean Society for Railway
    • /
    • v.9 no.4 s.35
    • /
    • pp.349-356
    • /
    • 2006
  • At present, the selecting system and analytic estimation criterion on repair materials and methods of the deteriorated RC structures have not yet been set up in domestic. Under these circumstances, deterioration such as shrinkage crack, corrosion of rebar has been often occurred after repair, and this finally results in too frequent repairs. In this study, three types of repair methods were experimentally investigated by the accelerating test in a combined deterioration chamber and long-term field exposure test. Three types of repair methods applied in this study belong to a group of polymer cement mortar, which is commonly used in repair works. According to the results of this study, durability of repair mortar layers and corrosion properties of recovered rebar could be investigated in short period by the accelerating test in a combined deterioration chamber, which can simulate the condition of repeated high-and-low temperature and repeated dry-and-wet environment, spraying chloride solution and emitting $CO_2$ gas. After 36 month long-term filed exposure test in the coastal area, harmful macro-cracks are observed in the polymer cement mortar layer of some repair methods. These crack are considered to result from drying shrinkage of polymer cement mortar. Also, after 36 month exposure, amount of corrosion area and weight loss of rebar are found to be different according to the types of repair methods.